• Title/Summary/Keyword: Interlaminar Delamination

Search Result 58, Processing Time 0.027 seconds

Evaluation of Mode I Interlaminar Fracture Toughness for Carbon Fabric/Expocy Composite for Tilting Train Carbody (틸팅열차 차체용 탄소섬유직물/에폭시 복합재의 모우드 I 층간파괴인성 평가)

  • Heo KWang-Su;Kim Jeong-Seok;Yoon Sung-Ho
    • Journal of the Korean Society for Railway
    • /
    • v.8 no.6 s.31
    • /
    • pp.573-580
    • /
    • 2005
  • Model I interlaminar fracture behaviors of the carbon/epoxy composite, one of the candidate composites for a tilting train carbody, were investigate by the use of DCB(Double cantilever beam) specimens. These specimens were made of CF3327 plain woven fabric with epoxy resin, and an artificial starter delamination was fabricated by inserting Teflon film with the thickness of $12.5{\mu}m$ of $25.0{\mu}m$ at the one end of the specimen. Mode I interlaminar fracture toughness was evaluated for the specimens with the different thickness of an inserter. Also delamination propagating behaviors and interlaminar fracture surface were examined through an ooptical travelling scope and a scanning electron microscope. We found that abruptly unstable crack propagation called as stick-slip phenomena was observed. In addition, interlaminar fracture behaviors were affected on the location and the morphology of a crack tip as well as an interface region.

Delamination growth analysis in composite laminates subjected to low velocity impact

  • Kharazan, Masoud;Sadr, M.H.;Kiani, Morteza
    • Steel and Composite Structures
    • /
    • v.17 no.4
    • /
    • pp.387-403
    • /
    • 2014
  • This paper presents a high accuracy Finite Element approach for delamination modelling in laminated composite structures. This approach uses multi-layered shell element and cohesive zone modelling to handle the mechanical properties and damages characteristics of a laminated composite plate under low velocity impact. Both intralaminar and interlaminar failure modes, which are usually observed in laminated composite materials under impact loading, were addressed. The detail of modelling, energy absorption mechanisms, and comparison of simulation results with experimental test data were discussed in detail. The presented approach was applied for various models and simulation time was found remarkably inexpensive. In addition, the results were found to be in good agreement with the corresponding results of experimental data. Considering simulation time and results accuracy, this approach addresses an efficient technique for delamination modelling, and it could be followed by other researchers for damage analysis of laminated composite material structures subjected to dynamic impact loading.

Evaluation of Mode I Interlaminar Fracture Toughness for Carbon Fabric/Epoxy Composite (탄소섬유직물/에폭시 복합제의 모우드 I 층간파괴인성 평가)

  • Lee Eun-Dong;Yoon Sung-Ho;Shin Kwang-Bok;Jeong Jong-Cheol
    • Proceedings of the KSR Conference
    • /
    • 2004.10a
    • /
    • pp.698-703
    • /
    • 2004
  • In this study, mode I interlaminar fracture phenomena of carbon fabric/epoxy composite for tilting train were investigated. Specimens were 25mm $\times$ 180mm $\times$ 4.7mm with an initial artificial delamination of 65mm at one end. This delamination with the thickness of 12.5$\mu$m and 25$\mu$m (teflon film) was used. Mode I interlaminar fracture toughness was measured using the double cantilever beam and the fractured surfaces were examined through a scanning electron microscope. The experimental results obtained in this study would be applicable in the design and structural analysis of the composite structures.

  • PDF

Delamination behavior of multidirectional laminates under the mode I loading (모드 I 하중조건하에 있는 다방향 적층 복합재료의 층간파괴거동)

  • Choi, Nak-Sam;Kinloch, A.J.
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.22 no.3
    • /
    • pp.611-623
    • /
    • 1998
  • The delamination fracture of multidirectional carbon-fiber/epoxy laminates under the Mode I condition has been studied using the modified beam analysis for a fracture mechanics approach. It was found that the variation of fracture energy $G_IC$ with increasing length of the propagating crack exhibited a minimum for the pure interlaminar fracture and a maximum for the intraply fracture,i.e. a rising "R-curve", which was strongly affected by the degree of fiber bridging and crack-tip splitting arising in the global delamination. The maximum $G_IC$ value was significantly dependent on such types of delamination as no crack jumping, crack jumping into the adjacent ply and edge-delamination. It was shown also that the value of "effective flexural modulus" estimated from the modified beam analysis increased much with the development of fiber bridging behind the crack tip.ehind the crack tip.

Optimal design of composite laminates for minimizing delamination stresses by particle swarm optimization combined with FEM

  • Chen, Jianqiao;Peng, Wenjie;Ge, Rui;Wei, Junhong
    • Structural Engineering and Mechanics
    • /
    • v.31 no.4
    • /
    • pp.407-421
    • /
    • 2009
  • The present paper addresses the optimal design of composite laminates with the aim of minimizing free-edge delamination stresses. A technique involving the application of particle swarm optimization (PSO) integrated with FEM was developed for the optimization. Optimization was also conducted with the zero-order method (ZOM) included in ANSYS. The semi-analytical method, which provides an approximation of the interlaminar normal stress of laminates under in-plane load, was used to partially validate the optimization results. It was found that optimal results based on ZOM are sensitive to the starting design points, and an unsuitable initial design set will lead to a result far from global solution. By contrast, the proposed method can find the global optimal solution regardless of initial designs, and the solutions were better than those obtained by ZOM in all the cases investigated.

Behavior for 2 Ply Rubber/Cord Laminates (2층 고무/코드 적층판의 층간거동)

  • 이윤기;임동진;윤희석;김민호;김춘휴
    • Composites Research
    • /
    • v.16 no.4
    • /
    • pp.1-9
    • /
    • 2003
  • 2 ply laminated composite is regarded to simulate the interply behavior of the belt layer of the tire. It was cone with 3 dimensional FE(Finite Element) analysis to determine interply shear stress and strain. Widthwise, the shear strain was measured by the pin method. These results are compared with those of CLT(classical lamination theory) in center region and those of Kassapoglou's and Kelsey's theory in edge region. In the FE analysis. rubber is assumed as linear elastic material. and rubber/cord laminate as the orthotropic material composed of cord and rubber In the FE result, interlaminar shear stress causing the interlaminar delamination has the largest value in the edge region of the inner rubber layer. Numerical results obtained coincides with CLT well in the center region, and agrees with other theoretical result little in the edge region.

A Study on Sliding Shear(Mode II) Delamination of Woven Fabric composites for Carbody Structure (차체 구조용 섬유직물 복합재의 평면 전단(mode II) 층간분리 거동에 대한 시험적 연구)

  • Kim, Seung-Chul;Kim, Jung-Seok;Yoon, Hyuk-Jin;Seo, Sung-Il
    • Proceedings of the KSR Conference
    • /
    • 2010.06a
    • /
    • pp.557-563
    • /
    • 2010
  • Mode II interlaminar fracture toughness was measured and fractured surfaces were observed of carbon/epoxy and glass/epoxy woven fabric composites for carbody structure. Woven fabric carbon/epoxy and glass/epoxy composites that made with prepreg and epoxy resin(RS1222) are used in carbody structure of Korean tilting train(TTX) and low floor bus. ENF(End Notched Flexure) specimens having $120mm{\times}20m{\times}5mm$ shape and 35mm initial crack were made with each composites and three point bending tests according to ASTM D790 were conducted for these specimens. Crack lengths in tests were recorded using optical microscope and digital camcorder. NL(Non Linear), 5% offset and Max. load points in load -displacement curves were checked and mode II interlaminar fracture toughness of these points were calculated and compared. Fractured surfaces of specimens were observed using optical microscope and mode II delamination behavior of each composites was discussed.

  • PDF

Mechanical Behavior of Fiber Metal Laminates with Local Delamination Defects (국부적 적층분리결함을 갖는 섬유금속적층판의 기계적 거동 특성)

  • Choi, Heungsoap;Choi, Hyungjip;Choi, Wonjong;Ha, Minsu
    • Journal of Aerospace System Engineering
    • /
    • v.1 no.1
    • /
    • pp.25-35
    • /
    • 2007
  • In this paper, the interlaminar crack problems of a fiber metal laminate (FML) under generalized plane deformation are studied using the theory of anisotropic elasticity. The crack is considered to be embedded in the matrix interlaminar region (including adhesive zone and resin rich zone) of the FML. Based on Fourier integral transformation and the stress matrix formulation, the current mixed boundary value problem is reduced to solving a system of Cauchy-type singular integral equations of the 1st kind. Within the theory of linear fracture mechanics, the stress intensity factors are defined on terms of the solutions of integral equations and numerical results are obtained for in-plane normal (mode I) crack surface loading. The effects of location and length of crack in the 3/2 and 2/1 ARALL, GLARE or CARE type FML's on the stress intensity factors are illustrated.

  • PDF

The Effect of Variable Electric Fields on the PZT Characteristic and Laminate Configuration in LIPCA (LIPCA에 공급되는 전기장의 변화가 PZT 특성과 적층배향에 미치는 영향)

  • Kim Cheol-Woong;Nam In-Chang;Yoon Kwang-Joon
    • Proceedings of the Korean Society of Precision Engineering Conference
    • /
    • 2006.05a
    • /
    • pp.397-398
    • /
    • 2006
  • The advanced piezoelectric ceramic composite actuator, which is called LIPCA with the FRP and the optimization of the laminate configuration, was performed to maximize the stress transfer and the fiber bridging effect. This study evaluated the effect of variable electric fields on the PZT characteristic, laminate configuration and fatigue characteristics under the resonance frequency, which meant the largest performance range and the changes of its interlaminar phase were also evaluated by stages. In conclusions, Comparing with the fatigue lift of intact LIPCA, the fatigue life of LIPCA embedded by the artificial delamination was decreased up to 50%. The micro void growth and the coalescence of epoxy were actively made at the interlaminar phase subject to the large tensile stress.

  • PDF

Analysis of Mixed Mode Delamination in Graphite/Epoxy Composite (흑연/에폭시 복합재료의 혼합모우드 층간분리 해석)

  • Yum, Y. J.;You, H.
    • Transactions of the Korean Society of Automotive Engineers
    • /
    • v.4 no.4
    • /
    • pp.171-178
    • /
    • 1996
  • DCB(pure mode I) and CLS(mixed mode) tests were performed to investigate the effect of fracture mode on the interlaminar fracture of composite laminate. Mode I critical strain energy release rate was found to be $133J/m^2$ from the DCB test and total strain energy release rate decreased from $1, 270J/m^2$ as thickness ratio(tl/t) varied from 0.333 to 0.667 from the crease from the CLS test. Crack length had no effect on the total strain energy release rate and load was almost constant during the crack growth of the specimen which had the specific thickness ratio. Crack initiated when the stress of the strap ply reached constant stress $42kgf/mm^2$ which was found to be independent of the thickness ratio.

  • PDF