• Title/Summary/Keyword: Interfacial electronic structure

Search Result 61, Processing Time 0.033 seconds

Nature of the Interfacial Regions in the Antiferromagnetically-coupled Fe/Si Multilayered Films

  • Moon, J.C.;Y.V. Kudryavtsev;J.Y.Rhee;Kim, K.W.;Lee, Y.P.
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2000.02a
    • /
    • pp.174-174
    • /
    • 2000
  • A strong antiferromagnetic coupling in Fe/Si multilayered films (MLF) had been recently discovered and much consideration has been given to whether the coupling in the Fe/Si MLF system has the same origin as the metal/metal MLF. Nevertheless, the nature of the interfacial ron silicide is still controversial. On one hand, a metal/ semiconductor structure was suggested with a narrow band-gap semiconducting $\varepsilon$-FeSi spacer that mediates the coupling. However, some features show that the nature of coupling can be well understood in terms of the conventional metal/metal multilayered system. It is well known that both magneto-optical (MO) and optical properties of a metal depend strongly on their electronic structure that is also correlated with the atomic and chemical ordering. In this study, the nature of the interfacial regions is the Fe/Si multilayers has been investigated by the experimental and computer-simulated MO and optical spectroscopies. The Fe/Si MLF were prepared by rf-sputtering onto glass substrates at room temperature with the number of repetition N=50. The thickness of Fe sublayer was fixed at 3.0nm while the Si sublayer thickness was varied from 1.0 to 2.0 nm. The topmost layer of all the Fe/Si MLF is Fe. In order to carry out the computer simulations, the information on the MO and optical parameters of the materials that may constitute a real multilayered structure should be known in advance. For this purpose, we also prepared Fe, Si, FeSi2 and FeSi samples. The structural characterization of Fe/Si MLF was performed by low- and high -angle x-ray diffraction with a Cu-K$\alpha$ radiation and by transmission electron microscopy. A bulk $\varepsilon$-FeSi was also investigated. The MO and optical properties were measured at room temperature in the 1.0-4.7 eV energy range. The theoretical simulations of MO and optical properties for the Fe/Si MLF were performed by solving exactly a multireflection problem using the scattering matrix approach assuming various stoichiometries of a nonmagnetic spacer separating the antiferromagnetically coupled Fe layers. The simulated spectra of a model structure of FeSi2 or $\varepsilon$-FeSi as the spacer turned out to fail in explaining the experimental spectra of the Fe/Si MLF in both intensity and shape. Thus, the decisive disagreement between experimental and simulated MO and optical properties ruled out the hypothesis of FeSi2 and $\varepsilon$-FeSi as the nonmagnetic spacer. By supposing the spontaneous formation of a metallic ζ-FeSi, a reasonable agreement between experimental and simulated MO and optical spectra was obtained.

  • PDF

Effects of transition layer in SiO2/SiC by the plasma-assisted oxidation

  • Kim, Dae-Gyeong;Gang, Yu-Seon;Gang, Hang-Gyu;Baek, Min;O, Seung-Hun;Jo, Sang-Wan;Jo, Man-Ho
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2016.02a
    • /
    • pp.193.2-193.2
    • /
    • 2016
  • We evaluate the change in defects in the oxidized SiO2 grown on 4H-SiC (0001) by plasma assisted oxidation, by comparing with that of conventional thermal oxide. In order to investigate the changes in the electronic structure and electrical characteristics of the interfacial reaction between the thin SiO2 and SiC, x-ray photoelectron spectroscopy (XPS), X-ray absorption spectroscopy (XAS), DFT calculation and electrical measurements were carried out. We observed that the direct plasma oxide grown at the room temperature and rapid processing time (300 s) has enhanced electrical characteristics (frequency dispersion, hysteresis and interface trap density) than conventional thermal oxide and suppressed interfacial defect state. The decrease in defect state in conduction band edge and stress-induced leakage current (SILC) clearly indicate that plasma oxidation process improves SiO2 quality due to the reduced transition layer and energetically most stable interfacial state between SiO2/SiC controlled by the interstitial C.

  • PDF

Design of an Electron Ohmic-Contact to Improve the Balanced Charge Injection in OLEDs

  • Park, Jin-U;Im, Jong-Tae;Yeom, Geun-Yeong
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2011.02a
    • /
    • pp.283-283
    • /
    • 2011
  • The n-doping effect by doping metal carbonate into an electron-injecting organic layer can improve the device performance by the balanced carrier injection because an electron ohmic contact between cathode and an electron-transporting layer, for example, a high current density, a high efficiency, a high luminance, and a low power consumption. In the study, first, we investigated an electron-ohmic property of electron-only device, which has a ITO/$Rb_2CO_3$-doped $C_{60}$/Al structure. Second, we examined the I-V-L characteristics of all-ohmic OLEDs, which are glass/ITO/$MoO_x$-doped NPB (25%, 5 nm)/NPB (63 nm)/$Alq_3$ (32 nm)/$Rb_2CO_3$-doped $C_{60}$(y%, 10 nm)/Al. The $MoO_x$doped NPB and $Rb_2CO_3$-doped fullerene layer were used as the hole-ohmic contact and electron-ohmic contact layer in all-ohmic OLEDs, respectively, Third, the electronic structure of the $Rb_2CO_3$-doped $C_{60}$-doped interfaces were investigated by analyzing photoemission properties, such as x-ray photoemission spectroscopy (XPS), Ultraviolet Photoemission spectroscopy (UPS), and Near-edge x-ray absorption fine structure (NEXAFS) spectroscopy, as a doping concentration at the interfaces of $Rb_2CO_3$-doped fullerene are changed. Finally, the correlation between the device performance in all ohmic devices and the interfacial property of the $Rb_2CO_3$-doped $C_{60}$ thin film was discussed with an energy band diagram.

  • PDF

The Structural and Electrical Properties of the BST Thin Film Prepared by Sol-Gel method. (Sol-Gel법으로 제조한 BST 박막의 구조 및 전기적 특성)

  • Kim, Kyoung-Duk;Chung, Jang-Ho;Bae, Seon-Gi;Lee, Young-Hie
    • Proceedings of the KIEE Conference
    • /
    • 1997.11a
    • /
    • pp.291-293
    • /
    • 1997
  • In this study, Sol-Gel derived $(Ba_{0.7}Sr_{0.3})TiO_3$ thin films were fabricated and investigated. The stock solution was synthesized and spin-coated on Pt/Ti/$SiO_2$/Si substrate at 4000(rpm] and then, annealed at $650{\sim}750[^{\circ}C]$. Crystallization condition, microstructural properties and interfacial structure were observed by XRD, AFM, SEM and TEM. It was found that the BST thin films were completely crystallized at 750[$^{\circ}C$] and showed nano-sized grains. The dielectric constant and loss of the BST thin films were 220, 0.01 at 1[kHz] respectively. Increasing the temperature, the dielectric constant and loss characteristics were not varied widely. At the applied voltage of 1.5[V], the leakage current density was under the $10^{-9}[A/cm^2]$.

  • PDF

Atomic layer chemical vapor deposition of Zr $O_2$-based dielectric films: Nanostructure and nanochemistry

  • Dey, S.K.
    • Electrical & Electronic Materials
    • /
    • v.16 no.9
    • /
    • pp.64.2-65
    • /
    • 2003
  • A 4 nm layer of ZrOx (targeted x-2) was deposited on an interfacial layer(IL) of native oxide (SiO, t∼1.2 nm) surface on 200 mm Si wafers by a manufacturable atomic layer chemical vapor deposition technique at 30$0^{\circ}C$. Some as-deposited layers were subjected to a post-deposition, rapid thermal annealing at $700^{\circ}C$ for 5 min in flowing oxygen at atmospheric pressure. The experimental x-ray diffraction, x-ray photoelectron spectroscopy, high-resolution transmission electron microscopy, and high-resolution parallel electron energy loss spectroscopy results showed that a multiphase and heterogeneous structure evolved, which we call the Zr-O/IL/Si stack. The as-deposited Zr-O layer was amorphous $ZrO_2$-rich Zr silicate containing about 15% by volume of embedded $ZrO_2$ nanocrystals, which transformed to a glass nanoceramic (with over 90% by volume of predominantly tetragonal-$ZrO_2$(t-$ZrO_2$) and monoclinic-$ZrO_2$(m-$ZrO_2$) nanocrystals) upon annealing. The formation of disordered amorphous regions within some of the nanocrystals, as well as crystalline regions with defects, probably gave rise to lattice strains and deformations. The interfacial layer (IL) was partitioned into an upper Si $o_2$-rich Zr silicate and the lower $SiO_{x}$. The latter was sub-toichiometric and the average oxidation state increased from Si0.86$^{+}$ in $SiO_{0.43}$ (as-deposited) to Si1.32$^{+}$ in $SiO_{0.66}$ (annealed). This high oxygen deficiency in $SiO_{x}$ indicative of the low mobility of oxidizing specie in the Zr-O layer. The stacks were characterized for their dielectric properties in the Pt/{Zr-O/IL}/Si metal oxide-semiconductor capacitor(MOSCAP) configuration. The measured equivalent oxide thickness (EOT) was not consistent with the calculated EOT using a bilayer model of $ZrO_2$ and $SiO_2$, and the capacitance in accumulation (and therefore, EOT and kZr-O) was frequency dispersive, trends well documented in literature. This behavior is qualitatively explained in terms of the multi-layer nanostructure and nanochemistry that evolves.ves.ves.

  • PDF

Interlayer and Interfacial Exchange Coupling of IrMn Based MTJ

  • Wrona, J.;Stobiecki, T.;Czapkiewicz, M.;Kanak, J.;Rak, R.;Tsunoda, M.;Takahashi, M.
    • Journal of Magnetics
    • /
    • v.9 no.2
    • /
    • pp.52-59
    • /
    • 2004
  • As deposited and annealed MTJs with the structure of $Ta(5 nm)/Cu(10 nm)/Ta(5 nm)/Ni_{80}Fe_{20}(2 nm)/Cu(5 nm)/ Ir_{25}Mn_{75}(10 nm)/Co_{70}Fe_{30}(2.5 nm)/Al-O/Co_{70}Fe_{30}(2.5nm)/Ni_{80}Fe_{20}(t)/Ta(5nm)/Ni_{80}Fe_{20}(t)/Ta(5 nm)$, where t=10, 30, 60 and 100 nm were characterized by XRD and magnetic hysteresis loops measurements. The XRD measurements were done in grazing incidence $(GID scan-2{\theta})$ and ${\theta}-2{\theta}$ geometry, by rocking curve $(scan-{\omega})$ and pole figures in order to establish correlation between texture and crystallites size and magnetic parameters of exchange biased and interlayer coupling. The variations of shifting and coercivity field of free and pinned layers after annealing in $300^{\circ}C$ correlate with the improvement of [111] texture and grains size of $Ni_{80}Fe_{20}$ and $Ir_{25}Mn_{75}$ respectively. The exchange biased and the coercivity fields of the pinned layer linearly increased with increasing grain size of $Ir_{25}Mn_{75}$, The reciprocal proportionality between interlayer coupling and coercivity fields of the free layer and grain size of $Ni_{80}Fe_{20}$ was found. The enhancement of interlayer coupling between pinned and free layers, after annealing treatment, indicates on the correlated in-phase roughness of dipolar interacting interfaces due to increase of crystallites size of $Ni_{80}Fe_{20}$.

Probing the Molecular Orientation of ZnPc on AZO Using Soft X-ray Spectroscopies for Organic Photovoltaic Applications

  • Jung, Yunwoo;Lee, Nalae;Kim, Jonghoon;Im, Yeong Ji;Cho, Sang Wan
    • Applied Science and Convergence Technology
    • /
    • v.24 no.5
    • /
    • pp.151-155
    • /
    • 2015
  • The interfacial electronic structure between zinc phthalocyanine (ZnPc) and aluminumdoped zinc oxide (AZO) substrates has been evaluated by ultraviolet photoemission spectroscopy and angle-dependent x-ray absorption spectroscopy to understanding the molecular orientation of a ZnPc layer on the performance of small molecule organic photovoltaics (OPVs). We find that the ZnPc tilt angle improves the ${\pi}-{\pi}$ interaction on the AZO substrate, thus leading to an improved short-circuit current in OPVs based on phthalocyanine. Furthermore, the molecular orientation-dependent energy level alignment has been analyzed in detail using ultraviolet photoemission spectroscopy. We also obtained complete energy level diagrams of ZnPc/AZO and ZnPc/indium thin oxide.

The Interfacial Electronic Structure of Organic-organic Heterojunction: Effect of Molecular Orientation

  • Jo, Sang-Wan
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2014.02a
    • /
    • pp.114.2-114.2
    • /
    • 2014
  • The orientation of the constituent molecules in organic thin film devices can affect significantly their performance due to the highly anisotropic nature of ${\pi}$-conjugated molecules. We report here an angle dependent x-ray absorption study of the control of such molecular orientation using well-ordered interlayers for the case of a bilayer heterojunction of chloroaluminum phthalocyanine (ClAlPc) and C60. Furthermore, the orientation-dependent energy level alignment of the same bilayer heterojunction has been measured in detail using synchrotron radiation-excited photoelectron spectroscopy. Regardless of the orientation of the organic interlayer, we find that the subsequent ClAlPc tilt angle improves the ${\pi}-{\pi}$ interaction at the interface, thus leading to an improved short-circuit current in photovoltaic devices based on ClAlPc/C60. The use of the interlayers does not change the effective band gap at the ClAlPc/C60 heterointerface, resulting in no change in open-circuit voltage.

  • PDF

Soft X-ray Spectroscopy of ClAlPc/Pentacene/ITO Interfaces: Role of ClAlPc on Energetic Band Alignment

  • Kim, Min-Su;Heo, Na-Ri;Lee, Sang-Ho;Jo, Sang-Wan;Smith, Kevin E.
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2014.02a
    • /
    • pp.190.1-190.1
    • /
    • 2014
  • The interfacial electronic structure of a bilayer of chloroaluminum phthalocyanine (ClAlPc) and pentacene grown on indium tin oxide (ITO) has been studied using synchrotron radiation-excited photoelectron spectroscopy. The energy difference between the highest occupied molecular orbital (HOMO) level of the pentacene layer and the lowest unoccupied molecular orbital (LUMO) level of the ClAlPc layer (EDHOMO - EALUMO) was determined and compared with that of C60/pentacene bilayers. The EDHOMO - EALUMO of a heterojunction with ClAlPc was found to be 1.4 eV, while that with C60 was 1.0 eV. This difference is discussed in terms of the difference of the ionization energy of each acceptor materials. We also obtained the complete energy level diagrams of ClAlPc/pentacene/ITO and C60/pentacene/ITO, respectively.

  • PDF

Top-Emitting Organic Light-Emitting Diodes Based on the Interfacial Electronic Structures of Bis(8-Quinolinolato)Aluminum (III)/Barium

  • Im, Jong-Tae;Yeom, Geun-Yeong
    • Proceedings of the Korean Institute of Surface Engineering Conference
    • /
    • 2007.04a
    • /
    • pp.5-6
    • /
    • 2007
  • 반투명 전도성 음극 (semi-transparent conducting cathode)인 Ba (x nm)/Au (20 nm)/ITO (100 nm)을 이용하여 전면발광 유기전계 발광 소자 (top-emitting organic light-emitting didodes, TEOLEDs)를 제작했다. Ba과 bis(8-quinolinolato)aluminum (III) ($Alq_3$) 계면의 전자구조는 엑스선 광전자 분광법 (X-ray photoelectron spectroscopy, XPS), 자외선 광전자 분광법 (ultraviolet photoelectron spectroscopy, UPS) 및 가까운 끝머리 엑스선 흡수 미세구조 (near-edge x-ray absorption fine structure, NEXAFS) 스펙트럼의 광 방출 특성을 통하여 조사되었다. $Alq_3$/Ba 계면 특성에 있어서 XPS와 NEXAFS 특성에 의하면, $Alq_3$ (10.0 nm) 위에 Ba이 연속적으로 증착됨에 따라 Ba으로부터 $Alq_3$로의 전자전달 (electron charge transfer) 특성은 꾸준희 증가된다. 그러나 Ba의 두께가 1.0 nm 이상 초과되면 Ba의 전자전달에 기인한 반응성때문에 $Alq_3$의 분자구조가 해리된다. 한편, 제작된 TEOLEDE의 전류-전압-휘도 곡선의 경우에서도 바륨의 증착 두께가 1.0 nm일 때 가장 우수한 구동특성을 나타냈다.

  • PDF