Nanofibers Comprising Mo2C/Mo2N Nanoparticles and Reduced Graphene Oxide as Functional Interlayers for Lithium-Sulfur Batteries (Mo2C/Mo2N 나노 입자와 환원된 그래핀 옥사이드가 복합된 나노 섬유 중간층이 적용된 리튬-황 전지)

  • Lee, Jae Seob;Yang, Ji Hoon;Cho, Jung Sang
    • Korean Chemical Engineering Research
    • /
    • v.60 no.4
    • /
    • pp.574-581
    • /
    • 2022
  • Nanofibers comprising reduced graphene oxide (rGO) and Mo2C/Mo2N nanoparticles (Mo2C/Mo2N rGO NFs) were prepared for a functional interlayer of Li-S batteries (LSBs). The well-dispersed Mo2C and Mo2N nanoparticles in the nanofiber structure served as active polar sites for efficient immobilization of dissolved lithium polysulfide. The rGO nanosheets in the structure also provide conductive channels for fast ion/electron transport during charging-discharging and ensured reuse of lithium polysulfide during redox reactions through a fast charge transfer process. As a result, the cell assembled with Mo2C/Mo2N rGO NFs-coated separator and pure sulfur electrode (70 wt% of sulfur content and 2.1 mg cm-2 of sulfur loading) showed a stable discharge capacity of 476 mA h g-1 after 400 charge-discharge cycles at 0.1 C. Furthermore, it exhibited a discharge capacity of 574 mA h g-1 even at a high current density of 1.0 C. Therefore, we believe that the proposed unique nanostructure synthesis strategy could provide new insights into the development of sustainable and highly conductive polar materials as functional interlayers for high performance LSBs.

Verification of Shielding Materials for Customized Block on Metal 3D Printing (금속 3D 프린팅을 통한 맞춤형 차폐블록 제작에 사용되는 차폐 재료 검증)

  • Kyung-Hwan, Jung;Dong-Hee, Han;Jang-Oh, Kim;Hyun-Joon, Choi;Cheol-Ha, Baek
    • Journal of the Korean Society of Radiology
    • /
    • v.17 no.1
    • /
    • pp.25-30
    • /
    • 2023
  • As 3D printing technology is used in the medical field, interest in metal materials is increasing. The Department of Radiation Oncology uses a shielding block to shield the patient's normal tissue from unnecessary exposure during electron beam therapy. However, problems such as handling of heavy metal materials such as lead and cadmium, reproducibility according to skill level and uncertainty of arrangement have been reported. In this study, candidate materials that can be used for metal 3D printing are selected, and the physical properties and radiation dose of each material are analyzed to develop a customized shielding block that can be used in electron beam therapy. As candidate materials, aluminum alloy (d = 2.68 g/cm3), titanium alloy (d = 4.42 g/cm3), and cobalt chromium alloy (d = 8.3 g/cm3) were selected. The thickness of the 95% shielding rate point was derived using the Monte Carlo Simulation with the irradiation surface and 6, 9, 12, and 16 energies. As a result of the simulation, among the metal 3D printing materials, cobalt chromium alloy (d = 8.3 g/cm3) was similar to the existing shielding block (d = 9.4 g/cm3) in shielding thickness for each energy. In a follow-on study, it is necessary to evaluate the usefulness in clinical practice using customized shielding blocks made by metal 3D printing and to verify experiments through various radiation treatment plan conditions.

Toxicity assessment of food additive(E171) in aquatic environments (식품첨가물 E171이 수생물에 미치는 독성 평가)

  • In-Gyu Song;Kanghee Kim;Hakwon Yoon;June-Woo Park
    • Korean Journal of Environmental Biology
    • /
    • v.41 no.1
    • /
    • pp.41-53
    • /
    • 2023
  • E171, a mixture of titanium dioxide, has been widely used as a food additive due to its whitening effect and low toxicity. However, it has been proven that E171 is no longer safe for public health. So far, there are insufficient studies on the toxic effects of E171 on organisms especially using standardized test methods. In this study, toxicity assessments of E171 to two aquatic species, water flea (Daphnia magna) and zebrafish (Danio rerio), were performed using modified standardized test methods based on the physicochemical properties of E171. The hydrodynamic diameter, polydispersity index, and turbiscan stability index (TSI) were measured to ensure the dispersion stability of E171 in exposure media during the test period. The EC50 for immobilization of water flea was 141.7 mg L-1 while zebrafish was not affected until 100 mg L-1 of E171. Measurements of reactive oxygen species (ROS) and antioxidant enzyme activities confirmed that E171 induced oxidative stress, leading to the activation of superoxide dismutase and catalase in both water flea and zebrafish, although the expression of antioxidant enzyme genes differed between species. These results suggested the potential risk of E171 to aquatic organisms and provided toxicological insights into the impacts of E171 on the environment.

Current Trends in the Treatment of Ankle Ligament Injuries: Analysis of the Korean Foot and Ankle Society (KFAS) Member Survey (족관절 인대 손상 치료 동향: 대한족부족관절학회 회원 설문조사 분석)

  • Cho, Byung-Ki;Cho, Jaeho;Lee, Myoungjin;Lee, Jun Young;Bae, Su-Young;The Academic Committee of Korean Foot and Ankle Society,
    • Journal of Korean Foot and Ankle Society
    • /
    • v.26 no.1
    • /
    • pp.22-29
    • /
    • 2022
  • Purpose: Despite continuous updates of standard treatment guidelines for acute ankle sprain and chronic ankle instability (CAI), in practice preferred treatment protocols vary widely. Based on a Korean Foot and Ankle Society (KFAS) member survey, this study reports current trends in the management of ankle ligament injuries. Materials and Methods: A web-based questionnaire containing 34 questions was sent to all KFAS members in September 2021. Questions mainly addressed clinical experience and preferences for the diagnosis and treatment of ankle ligament injuries. Answers with a prevalence of ≥50% among respondents were considered to reflect tendencies. Results: Eighty-four of the 550 members (15.3%) responded. Answers that showed a tendency were as follows: commonest additional image study (ultrasound), conservative treatment modality (immobilization, oral medication), frequency of surgical treatment (<5 cases per annum), most important factor when deciding on surgical treatment (activity level, e.g., occupation or sport), and commonest surgical procedure (open ligament repair). Answers that showed a tendency for CAI were as follows: most important symptom (repeated sprain, giving way), radiological factors (talar tilt, osteochondral lesion, anterior talar translation), and patient factors (occupation, sports activities, recurrent instability after surgery, etc.). For decision making regarding surgical treatment and method, the most preferred surgical procedure was the modified Broström procedure, and the most common repair technique was suture anchor technique. The following were considered poor prognostic factors; generalized laxity, failed previous surgery, cavovarus, severe mechanical instability, heavy work, obesity, and dissatisfaction after surgery because of residual pain. Conclusion: This study updates information regarding current trends in the management of ankle ligament injuries in Korea, and reveals consensus opinions and variations in approaches to patients with an acute or chronic injury. The divergence of approaches identified indicates the need for further studies to determine standard guidelines and long-term results.

Effect of Impregnation and Modification on Activated Carbon for Acetaldehyde Adsorption (아세트알데하이드 흡착을 위한 활성탄의 첨착 및 개질 효과)

  • Jin Chan Park;Dong Min Kim;Jong Dae Lee
    • Korean Chemical Engineering Research
    • /
    • v.61 no.3
    • /
    • pp.472-478
    • /
    • 2023
  • In this study, the acetaldehyde removal characteristics of activated carbon (AC) for air purifier filters were investigated using metal catalysts-impregnation and functional group-modification method. The AC with a high specific surface area(1700 m2/g) and micropores was prepared by KOH activation of coconut charcoal and the efficiency of catalyst and functional group immobilization was examined by varying the drying conditions within the pores after immersion. The physical properties of the prepared activated carbon were analyzed by BET, ICP, EA, and FT-IR, and the acetaldehyde adsorption performances were investigated using gas chromatography (GC) at various impregnation and modified conditions. As the concentration of impregnation solution increased, the amount of impregnated metal catalysts increased, while the specific surface area showed a decreasing trend. The adsorption tests of the metal catalyst-impregnated and functional group-modified activated carbons revealed that excellent adsorption performance in compositions MgO10@AC, CaO10@AC, EU10@AC, and H-U3N1@AC, respectively. The MgO10@AC, which showed the highest adsorption performance, had a breakthrough time of 533.8 minutes and adsorption capacity of 57.4 mg/g for acetaldehyde adsorption. It was found that the nano-sized MgO catalyst on the activated carbon improved the adsorption performance by interacting with carbonyl groups of acetaldehyde.

Urea Conversion via Enzymes Immobilized on Magnetic Microparticles (자성 미세입자에 고정된 효소를 통한 요소 전환)

  • Yeseul Park;Jieun Kwon;Seungjun Jung;Hyukjin Cho;Gounhanul Shin;Gangik Cho;Jin-Won Park;Kyung-Hyuk Lee
    • Korean Chemical Engineering Research
    • /
    • v.61 no.3
    • /
    • pp.407-411
    • /
    • 2023
  • The urease is covalently immobilized on the surface of the magnetic particles to catalyze the conversion of urea to bicarbonate anion. The conversion was confirmed qualitatively using high-pressure liquid chromatography and UV/Vis spectrometry, and analyzed quantitatively with cyclic voltammetry. The amount of conversion with respect to time was measured and analyzed by the reaction rate equation to calculate a reaction rate constant of 0.0474 min-1. In the 1 to 3 cycles, a conversion percentage of over 90% was found, and it was possible to reuse the urease 8 times up to the percentage of 50%. It was also observed that the stability evaluated for storage for 30 days was maintained. As a result of this study, it can be seen that the urease covalently immobilized on the scaffold can be used for urea removal for the purpose of producing ultrapure water.

Fabrication and Characterization of Carbon Nanotube-modified Carbon Paper-based Lactate Oxidase-catalase Electrode (탄소나노튜브로 개질된 탄소종이 기반 젖산산화효소 - 카탈레이즈 전극 제작 및 특성 분석)

  • Ke Shi;Varshini Selvarajan;Yeong-Yil Yang;Hyug-Han Kim;Chang-Joon Kim
    • Korean Chemical Engineering Research
    • /
    • v.61 no.4
    • /
    • pp.576-583
    • /
    • 2023
  • This study aimed to investigate the impact of enhancing the electrode conductivity and mitigating the production of hydrogen peroxide - a by-product arising from lactate oxidation - on the performance of lactate electrodes. The electrical conductivity of the electrode was improved by modifying the surface of carbon paper with single-walled carbon nanotubes. Catalase was introduced to effectively eliminate the hydrogen peroxide produced during the lactate oxidation reaction. The carbon paper electrode, with simultaneous immobilization of both lactate oxidase and catalase, yielded a current 1.7 times greater than the electrode where only lactate oxidase was immobilized. The electrode in which lactate oxidase and catalase were co-immobilized on the surface of carbon paper modified with single-walled carbon nanotubes, produced a current of 171 µA, which was more than twice as much current as the carbon paper with only lactate oxidase immobilized. The optimized electrode showed a linear response up to lactate concentration of 20 mM, confirming that it can be used as a sensor electrode.

Evaluating the Usability of Medical Body Wrap in Whole Body Bone Scan (전신 뼈 검사에서 의료용 신체 고정구의 유용성 평가)

  • Dong-Oh Shim;Woo-Young Jung;Jae-Kwang Ryu;Cheol-Hong Park;Yoon-Jae Kim
    • The Korean Journal of Nuclear Medicine Technology
    • /
    • v.28 no.1
    • /
    • pp.49-56
    • /
    • 2024
  • Purpose: When performing nuclear medicine examinations, body wraps or plastic supports are used to support and immobilize the patient's upper extremities to prevent patient safety accidents. However, the existing plastic supports compromised patient and staff safety, including finger entrapment and falls. Moreover, the body wrap provided by manufacturers compromised image quality such as upper extremities cutoff during whole body bone scan. Therefore, a new design of body wrap was developed to improve the issue, and this study aims to evaluate the usability of this medical body wrap. Materials and Methods: To evaluate the usability of the newly designed medical body wrap, a quality assessment of whole body bone scan images and a user satisfaction survey were conducted. Adult patients (male:female=129:152, age: 60.3±12.4 years, BMI: 24.0±4.2) aged 16 years or older who underwent a whole body bone scan during two periods: June to July 2022 (before improvement, n=139) and June to July 2023 (after improvement, n=142) were randomly selected for image quality evaluation. Five radiotechnologists visually evaluated the posterior view of the whole body bone image, including the left and right elbow (2 points), arm (2 points), whether the hand is extended (2 points), whether the hand is included (2 points), and the number of visible fingers (10 points), with a total of 18 points, which were converted to 100 points and analyzed for difference before and after improvement using an independent sample t-test. The user satisfaction questionnaire was evaluated using a 5-point Likert scale among 16 radiotechnologists from three general hospitals who experienced the new body wrap. Results: The image quality assessment was 82.0±13.8 before the improvement and 89.3±10.1 after the improvement, an average of 7.3 points higher, with a statistically significant difference (t=5.02, p<0.01). The user satisfaction survey showed an overall satisfaction rating of 4.1±0.8 for ease of use, 3.8±0.7 for scan preparation time, 3.9±0.7 for patient safety, 3.8±1.2 for scan accuracy, and 4.2±0.7 for recommendation (87.5% questionnaire response rate). Conclusion: The developed body wrap showed higher image quality and user satisfaction compared to the old method. Considering these results, it is deemed that the new body wrap may be more useful than existing methods.

Probing into the optimum preparation and the chemical durability of Sr0.5Zr2(PO4)3-SmPO4 dual-phase ceramics for nuclear waste forms via in-situ synthesis

  • Kunqi Liu;Junxia Wang;Anhang Wu;Jin Wang;Die Liu;Xiaoling Ma
    • Nuclear Engineering and Technology
    • /
    • v.56 no.6
    • /
    • pp.2174-2181
    • /
    • 2024
  • In this work, Sr0.5Zr2(PO4)3-SmPO4 dual-phase ceramics were prepared via in-situ synthesis process, which is a potential novel nuclear waste form for immobilizing the fission product 90Sr and the trivalent actinide radionuclides in high-level waste (HLW). And the preparation technology, microstructure and chemical durability of Sr0.5Zr2(PO4)3-SmPO4 dual-phase ceramics were systematically investigated. It was confirmed that the optimum microwave-sintering temperature (1050 ℃) and heat preservation time (1.5 h) is estimated by Archimedes method. Besides, the as-prepared samples that were consisted of strontium zirconium phosphate (SrZP) and monazite showed the remarkable densification, in which the two crystalline phases were intermixed well with each other. Meanwhile, the formation and evolution of microstructure was also consistent with the variational rule of Sr0.5Zr2(PO4)3/SmPO4, indicating that there was not mutual reaction during the in-situ synthesis process. The PCT and MCC-1 experimental results demonstrated that the elemental normalized leaching rates of tested samples are all at a low level (LRSr ~10-4 g·m-2·d-1, LRZr ~10-8-10-6 g·m-2·d-1, LRSm ~10-7-10-5 g·m-2·d-1 and LRP ~10-4 g·m-2·d-1). It is indicated that Sr0.5Zr2(PO4)3-SmPO4 dual-phase ceramics possesses excellent chemical durability for HLW disposal.

Investigation of the Rice Plant Transfer and the Leaching Characteristics of Copper and Lead for the Stabilization Process with a Pilot Scale Test (논토양 안정화 현장 실증 시험을 통한 납, 구리의 용출 저감 및 벼로의 식물전이 특성 규명)

  • Lee, Ha-Jung;Lee, Min-Hee
    • Economic and Environmental Geology
    • /
    • v.45 no.3
    • /
    • pp.255-264
    • /
    • 2012
  • The stabilization using limestone ($CaCO_3$) and steel making slag as the immobilization amendments for Cu and Pb contaminated farmland soils was investigated by batch tests, continuous column experiments and the pilot scale feasibility study with 4 testing grounds at the contaminated site. From the results of batch experiment, the amendment with the mixture of 3% of limestone and 2% of steel making slag reduced more than 85% of Cu and Pb compared with the soil without amendment. The acryl column (1 m in length and 15 cm in diameter) equipped with valves, tubes and a sprinkler was used for the continuous column experiments. Without the amendment, the Pb concentration of the leachate from the column maintained higher than 0.1 mg/L (groundwater tolerance limit). However, the amendment with 3% limestone and 2% steel making slag reduced more than 60% of Pb leaching concentration within 1 year and the Pb concentration of leachate maintained below 0.04 mg/L. For the testing ground without the amendment, the Pb and Cu concentrations of soil water after 60 days incubation were 0.38 mg/L and 0.69 mg/l, respectively, suggesting that the continuous leaching of Cu and Pb may occur from the site. For the testing ground amended with mixture of 3% of limestone + 2% of steel making slag, no water soluble Pb and Cu were detected after 20 days incubation. For all testing grounds, the ratio of Pb and Cu transfer to plant showed as following: root > leaves(including stem) > rice grain. The amendment with limestone and steel making slag reduced more than 75% Pb and Cu transfer to plant comparing with no amendment. The results of this study showed that the amendment with mixture of limestone and steel making slag decreases not only the leaching of heavy metals but also the plant transfer from the soil.