  • In previous studies, methods for enhancing cellular response on the Hydroxyapatite coated implant surface were described. In this study, the changes of surface characteristics such as surface roughness, contact angle, surface energy and surface morphology were observed when Hydroxyapatite coated Ti discs were immersed in NaCl solution for various time. Hydroxyapatite coated Ti discs were immersed in 0.9% NaCl solution for 7, 14 and 21 days at $37^{\circ}C$. The control group comprises dry identical discs not immersed in a solution. (n=3) All discs were dried in air completely and the surface roughness was measured using confocal laser scanning microscopy(CLSM). Static contact angle was recorded by video contact angle analyzer after dropping distilled water on the surface. The surface energy was calculated from contact angles of the three liquids. Surface was observed using a field emission-scanning electron microscope(FE-SEM). As a result, the surface roughness of immersed Hydroxyapatite coated Ti discs increased significantly and the contact angle decreased comparing with control group discs. The surface energy of immersed discs increased except for discs immersed for 14 days.

A study on the mechanical properties of TiN/DLC based functionally graded coatings

  • Song, Young-Sik;Kim, J.
    • Proceedings of the Korean Institute of Surface Engineering Conference
    • /
    • 2003.10a
    • /
    • pp.59-59
    • /
    • 2003
  • In recent, various functional coatings on artificial tooth implants have been conducted to enhance the bonding strength between implants and bones. Despite of these efforts, some previous reports argued that an adhesion strength between titanium implant and the final coatings like hydroxyapatite(HA) is weaker than the strength between coating and bone. In order to increase the adhesion force between the final coating and implant surface, TiN/DLC based functionally graded coating, which has higher mechanical strength than the titanium implant, was applied as a middle layer between titanium implant and final coating. Particularly we finally coated a biocompatible hydroxyapatite film on the DLC layer and examined the mechanical properties. As a result, TiN/DLC based functionally graded coating showed the higher adhesion strength compared with hydroxyapatite single layer coating on the titanium implant.

  • PDF

Randomized controlled clinical trial of 2 types of hydroxyapatite-coated implants on moderate periodontitis patients

  • Kim, Hyun-Suk;Yun, Pil-Young;Kim, Young-Kyun
    • Journal of Periodontal and Implant Science
    • /
    • v.46 no.5
    • /
    • pp.337-349
    • /
    • 2016
  • Purpose: The aim of this study was to compare and analyze the peri-implant tissue conditions and prospective clinical outcomes associated with 2 types of hydroxyapatite (HA)-coated implants: (1) fully HA-coated implants and (2) partially HA-coated implants with resorbable blast medium on the coronal portion of the threads. Methods: Forty-four partially edentulous patients were randomly assigned to undergo the placement of 62 HA-coated implants, and were classified as the control group (partially HA-coated, n=30) and the test group (fully HA-coated, n=32). All patients had chronic periodontitis with moderate crestal bone loss around the edentulous area. The stability and clinical outcomes of the implants were evaluated using the primary and secondary implant stability quotient (ISQ), as well as radiographic, mobility, and peri-implant soft tissue assessments around the implants. The Wilcoxon signed-rank test and the Mann-Whitney test were used to evaluate differences between and within the 2 groups, with P values <0.05 considered to indicate statistical significance. Results: The fully HA-coated implants displayed good retention of crestal bone, and insignificant differences were found in annual marginal bone loss between the 2 types of HA-coated implants (P>0.05). No significant differences were found in the survival rate (group I, 100%; group II, 100%) or the success rate (group I, 93.3%; group II, 93.8%). The fully HA-coated implants also did not significantly increase the risk of peri-implantitis (P>0.05). Conclusions: The fully HA-coated implants did not lead to an increased risk of peri-implantitis and showed good retention of the crestal bone, as well as good survival and success rates. Our study suggests that fully HA-coated implants could become a reliable treatment alternative for edentulous posterior sites and are capable of providing good retention of the crestal bone.

Histomorphometric Analysis of Two Types of Coated Implants : a Preliminary Study Using the Rabbit Tibia Model

  • Yeo, In-Sung;Lee, Hyo-Jung
    • Journal of Korean Dental Science
    • /
    • v.2 no.1
    • /
    • pp.28-30
    • /
    • 2009
  • Purpose : The purpose of this pilot experiment was to evaluate early bone response in two types of coated implants using the rabbit tibia model. Materials and Methods : Screw type titanium implants manufactured with a calcium metaphosphate (CMP) coating and hydroxyapatite (HA) coating were placed in the tibiae of 3 New Zealand White rabbits. The bone responses at 2 weeks after insertion were evaluated and compared by histomorphometry. Results : There was no significant difference in bone-to-implant contact between the groups (P>.05). However, some qualitative differences on histologic views were found. Conclusions : CMP-coating is suggested to be the preferred candidate for fast osseointegration over HAcoating.

  • PDF

HISTOMORPHOMETRIC STUDY ON THE INFLUENCE OF STEROID TOPICAL IRRIGATION AND IMPLANT SURFACE ON BONE HEALING IN THE IRRADIATED RABBIT TIBIA (방사선 조사 후 매식한 임프란트의 표면 종류와 스테로이드 관주에 따른 골 치유 효과에 대한 조직 형태학적 연구)

  • Shin, Sung-Soo;Park, Yang-Ho;Park, Jun-Woo;Rhee, Gun-Joo;Kim, Hyun-Man;Ko, Jae-Seung
    • Journal of the Korean Association of Oral and Maxillofacial Surgeons
    • /
    • v.30 no.6
    • /
    • pp.455-464
    • /
    • 2004
  • The purpose of this study was to evaluate and compare the influence of Steroid topical irrigation and implant surface on bone healing in the irradiated rabbit tibia. Implant to bone contact surface ratio and the pattern of bone healing around hydroxyapatite(HA) coated implant and pure titanium (Ti) implant which were inserted into the irradiated rabbit tibia were compared. 16 Korean house mature male rabbits were used as experimental animal. Each rabbit received 15 Gy of irradiation. 4 weeks after the irradiation, two holes were prepared in the irradiated tibia of each rabbits, where two surface type of implants were inserted :1) HA coated type and 2) pure Ti type. Right before placing implants, one group of rabbit received steroid irrigation and the other group did saline. After the irrigation, two implants of HA coated type and pure Ti type were inserted into the tibia of each rabbits. Each rabbit were sacrificed at 2nd, 4th, and 8th week after the implantation and the specimens were observed by the light microscope. The pattern of bone healing and histomorphometric analysis of the implant-bone interface were done. The results were as follows. 1. All implants inserted into the irradiated tibia of rabbit did not show any sign of clinical mobility and the bone around implants inserted into the irradiated tibia of rabbit did not show any resorption. 2. The bone to implant contact surface ratio around HA coated implants that received steroid irrigation got more bone to implant contact surface ratio than that of the saline irrigation. This result showed statistically significant(p<0.05). There was no statistically significant difference in 8th week group. 3. Though there was no statistically significant difference HA coated implants had more bone to implant contact surface ratio than pure Ti implant in 2nd and 4th groups, and there was no difference in 8th week group. 4. All implants inserted into the irradiated tibia of rabbit had exhibited successful osseointegraion.

Hydroxyapatite-coated implant: Clinical prognosis assessment via a retrospective follow-up study for the average of 3 years

  • Jung, Jun-Hong;Kim, Sang-Yun;Yi, Yang-Jin;Lee, Bu-Kyu;Kim, Young-Kyun
    • The Journal of Advanced Prosthodontics
    • /
    • v.10 no.2
    • /
    • pp.85-92
    • /
    • 2018
  • PURPOSE. This research evaluated clinical outcomes of two types of hydroxyapatite (HA)-coated implants: OT (Osstem TS III-HA, Osstem implant Co., Busan, Korea) and ZM (Zimmer TSV-HA, Zimmer dental, Carlsbad, USA). MATERIALS AND METHODS. The research was conducted on 303 implants (89 of OT, 214 of ZM), which were placed from January 16, 2010 to December 20, 2012. The prognosis was evaluated in terms of success rates, survival rates, annual marginal bone loss, and implant stability quotients (ISQ). The samples were classified into immediate, early, conventional, and delayed groups according to the loading time. RESULTS. Overall, there were no significant differences between OT and ZM in success rates, survival rates, and annual marginal bone loss, except for the result of secondary stability. OT showed $77.83{\pm}8.23ISQ$, which was marginally higher than $76.09{\pm}6.90ISQ$ of ZM (P<.05). In terms of healing periods, only immediate loading showed statistically significant differences (P<.05). Differences between OT and ZM were observed in terms of two indices, the annual marginal bone loss ($0.17{\pm}0.58mm/year$ < $0.45{\pm}0.80mm/year$) and secondary stability ($84.36{\pm}3.80ISQ$ > $82.48{\pm}3.69ISQ$) (P<.05). OT and ZM did not have any statistically significant differences in early, conventional, and delayed loading (P>.05). CONCLUSION. OT (97.75%) and ZM (98.50%) showed relatively good outcomes in terms of survival rates. In general, OT and ZM did not show statistically significant differences in most indices (P>.05), although OT performed marginally better than ZM in the immediate loading and 1-stage surgery (P<.05).

The histometric analysis of osseointegration in hydroxyapatite surface dental implants by ion beam-assisted deposition

  • Kim, Min-Kyung;Choi, Jung-Yoo;Chae, Gyung-Joon;Jung, Ui-Won;Kim, Sung-Tae;Lee, In-Seop;Cho, Kyoo-Sung;Kim, Chong-Kwan;Choi, Seong-Ho
    • Journal of Periodontal and Implant Science
    • /
    • v.38 no.sup2
    • /
    • pp.363-372
    • /
    • 2008
  • Purpose: This study compared the effects of coating implants with hydroxyapatite (HA) using an ion beam-assisted deposition (IBAD) method prepared with machined, anodized, sandblasted and large-grit acid etched (SLA) surfaces in minipigs, and verified the excellency of coating method with HA using IBAD. Material and Methods: 4 male Minipigs(Prestige World Genetics, Korea), 18 to 24 months old and weighing approximately 35 to 40 kg, were chosen. All premolars and first molars of the maxilla were carefully extracted on each side. The implants were placed on the right side after an 8 week healing period. The implant stability was assessed by resonance frequency analysis (RFA) at the time of placement. 40 implants were divided into 5 groups; machined, anodized, anodized plus IBAD, SLA, and SLA plus IBAD surface implants. 4 weeks after implantation on the right side, the same surface implants were placed on the left side. After 4 weeks of healing, the minipigs were sacrificed and the implants were analyzed by RFA, histology and histometric. Results: RFA showed a mean implant stability quotient (ISQ) of $75.625{\pm}5.021$, $76.125{\pm}3.739$ ISQ and $77.941{\pm}2.947$ at placement, after 4 weeks healing and after 8 weeks, respectively. Histological analysis of the implants demonstrated newly formed, compact, mature cortical bone with a nearby marrow spaces. HA coating was not separated from the HA coated implant surfaces using IBAD. In particular, the SLA implants coated with HA using IBAD showed better contact osteogenesis. Statistical and histometric analysis showed no significant differences in the bone to implant contact and bone density among 5 tested surfaces. Conclusion: We can conclude that rough surface implants coated with HA by IBAD are more biocompatible, and clinical, histological, and histometric analysis showed no differences when compared with the other established implant surfaces in normal bone.

Effects of the combination of bone morphogenetic protein-2 and nano-hydroxyapatite on the osseointegration of dental implants

  • Pang, KangMi;Seo, Young-Kwon;Lee, Jong-Ho
    • Journal of the Korean Association of Oral and Maxillofacial Surgeons
    • /
    • v.47 no.6
    • /
    • pp.454-464
    • /
    • 2021
  • Objectives: This study aimed to investigate the in vitro osteoinductivity of the combination of bone morphogenetic protein-2 (BMP-2) and nanohydroxyapatite (nHAp) and the in vivo effects of implants coated with nHAp/BMP-2. Materials and Methods: To evaluate the in vitro efficacy of nHAp/BMP-2 on bone formation, bone marrow-derived mesenchymal stem cells (BM-MSCs) were seeded onto titanium disks coated with collagen (Col), Col/nHAp, or Col/nHAp/BMP-2. Protein levels were determined by a biochemical assay and reverse transcriptase-polymerase chain reaction. Stem cell differentiation was analyzed by flow cytometry. For in vivo studies with mice, Col, Col/nHAp, and Col/nHAp/BMP-2 were injected in subcutaneous pockets. Titanium implants or implants coated with Col/nHAp/BMP-2 were placed bilaterally on rabbit tibias and evaluated for 4 weeks. Results: In the in vitro study, BM-MSCs on Col/nHAp/BMP-2 showed reduced levels of CD73, CD90, and CD105 and increased levels of glycosaminoglycan, osteopontin, and alkaline phosphatase activity. After 4 weeks, the Col/nHAp/BMP-2 implant showed greater bone formation than the control (P=0.07), while no differences were observed in bone implant contact and removal torque. Conclusion: These results suggest that a combination of BMP-2 and an nHAp carrier would activate osseointegration on dental implant surfaces.

Comparative study of removal torque of 3 different hydroxyapatite coated implants in the femur of rabbits (가토의 대퇴골에 식립한 3종류의 수산화인회석 코팅 임플란트에 대한 제거회전력 비교 연구)

  • Kim, Sang-Soo;Lee, Ju-Hyung;Yu, Seok-Hyun;Lee, Hyung-Ju;Moon, Jee-Won;Park, In-Sook;Sohn, Dong-Seok
    • Journal of the Korean Association of Oral and Maxillofacial Surgeons
    • /
    • v.37 no.1
    • /
    • pp.49-53
    • /
    • 2011
  • Introduction: This study compared the strength of osseointegration as determined by the resistance to reverse torque rotation of three different hydroxyapatite coated implants in the rabbit femur model. Materials and Methods: Three hydroxyapatite coated implants (HAPTITE), Tapered Screw-Vent (TSV) and BioTite-H - were used. A total of 40 implants were placed in the femur of 20 adult male rabbits. The animals were divided into two groups. In group A (n=10); one HAPTITE was placed into each right femur and one TSV was placed into each left femur. In group B (n=10); one HAPTITE was placed into each right femur and one BioTite-H was placed into each left femur. Five rabbits of each group were sacrificed at 4 and 8 weeks. The implants were removed by reverse torque rotation using a digital torque-measuring device. A total of 40 implants in 20 rabbits were used for the removal torque measurements. Results: In the Group A, 4 weeks after implant placement, the mean removal torque for the HAPTITE and TSV was $70.7{\pm}31.6$ N cm and $28.9{\pm}15.1$ N cm, respectively. Eight weeks after implant placement, the mean removal torque for the HAPTITE and TSV was $87.9{\pm}26.2$ N cm and $54.9{\pm}22.4$ N cm, respectively. In the Group B, 4 weeks after implant placement, the mean removal torque for the HAPTITE and BioTite-H was $58.0{\pm}29.6$ N cm and $37.7{\pm}14.1$ N cm, respectively. Eight weeks after implant placement, the mean removal torque for the HAPTITE and BioTite-H was $91.4{\pm}47.1$ N cm and $30.8{\pm}9.8$ N cm. HAPTITE showed a higher removal torque than the other implants. Conclusion: These results suggest that HAPTITE increases the strength of osseointegration significantly as determined by the resistance to reverse torque rotation.