• Title/Summary/Keyword: High-early-Strength Concrete

Search Result 461, Processing Time 0.024 seconds

Fundamental Tests on Compressive Strength Development and Thermal Conductivity of Cement Pastes Including Fumed Silica (흄드 실리카 첨가에 따른 시멘트 페이스트의 강도발현 및 열전도 특성에 대한 기초 연구)

  • Park, Jong-Beom;Yoon, Hyun-Sub;Yang, Keun-Hyeok
    • Journal of the Korea Institute of Building Construction
    • /
    • v.18 no.5
    • /
    • pp.413-418
    • /
    • 2018
  • This fundamental study is to examine the significance and limitation of the fumed silica addition to enhance the early compressive strength gain and thermal conduction resistance of cement pastes. The fumed silica content varied from 0% to 1.6% of the cement content by wt% at an interval of 0.4%. Test results showed that the addition of fumed silica is favorable to enhancing the early strength gain of the cement pastes, indicating that 1-day compressive strength corresponded to 45% of the 28-day strength. This high-early strength gain rate is comparable to the trend commonly observed in steam-cured cement concrete. However, the addition of fumed silica little influenced the thermal conduction resistance of cement pastes.

Determination of Degree of Hydration, Temperature and Moisture Distributions in Early-age Concrete (초기재령 콘크리트의 수화도와 온도 및 습도분포 해석)

  • 차수원;오병환;이형준
    • Journal of the Korea Concrete Institute
    • /
    • v.14 no.6
    • /
    • pp.813-822
    • /
    • 2002
  • The purpose of the present study is first to refine the mathematical material models for moisture and temperature distributions in early-age concrete and then to incorporate those models into finite element procedure. The three dimensional finite element program developed in the present study can determine the degree of hydration, temperature and moisture distribution in hardening concrete. It is assumed that temperature and humidity fields are fully uncoupled and only the degree of hydration is coupled with two state variables. Mathematical formulation of degree of hydration Is based on the combination of three rate functions of reaction. The effect of moisture condition as well as temperature on the rate of reaction is considered in the degree of hydration model. In moisture transfer, diffusion coefficient is strongly dependent on the moisture content in pore system. Many existing models describe this phenomenon according to the composition of mixture, especially water to cement ratio, but do not consider the age dependency. Microstructure is changing with the hydration and thus transport coefficients at early ages are significantly higher because the pore structure in the cement matrix is more open. The moisture capacity and sink are derived from age-dependent desorption isotherm. Prediction of a moisture sink due to the hydration process, i.e. self-desiccation, is related to autogenous shrinkage, which may cause early-age cracking in high strength and high performance concrete. The realistic models and finite element program developed in this study provide fairly good results on the temperature and moisture distribution for early-age concrete and correlate very well with actual test data.

Effects of Fine LWA and SAP as Internal Water Curing Agents

  • de Sensale, Gemma Rodriguez;Goncalves, Arlindo Freitas
    • International Journal of Concrete Structures and Materials
    • /
    • v.8 no.3
    • /
    • pp.229-238
    • /
    • 2014
  • Typical high-performance concrete (HPC) mixtures are characterized by low water-cementitious material ratios, high cement contents, and the incorporation of admixtures. In spite of its superior properties in the hardened state, HPC suffers from many practical difficulties such as its sensitivity to early-age cracking (which is associated with self-desiccation and autogenous shrinkage). In this context, conventional curing procedures are not sufficiently effective to address these limitations. In order to overcome this issue, two strategies,which are based on the use of internal reservoirs of water, have been recently developed.One of these strategies is based on the use of lightweight aggregates (LWA), while the other is based on the use of superabsorbent polymers (SAP). This paper studies and compares the efficiency of the LWA and SAP approaches.Moreover, some of the theoretical aspects that should be taken into account to optimize their application for internal curing of HPC are also discussed. Two fine LWA's and one SAP are studied in terms of autogenous deformation and compressive strength. Increasing the amounts of LWAor SAP can lead to a reduction of the autogenous deformation and compressive strength (especially when adding large amounts). By selecting appropriate materials and controlling their amount, size, and porosity, highly efficient internal water curing can be ensured.

Employing TLBO and SCE for optimal prediction of the compressive strength of concrete

  • Zhao, Yinghao;Moayedi, Hossein;Bahiraei, Mehdi;Foong, Loke Kok
    • Smart Structures and Systems
    • /
    • v.26 no.6
    • /
    • pp.753-763
    • /
    • 2020
  • The early prediction of Compressive Strength of Concrete (CSC) is a significant task in the civil engineering construction projects. This study, therefore, is dedicated to introducing two novel hybrids of neural computing, namely Shuffled Complex Evolution (SCE) and Teaching-Learning-Based Optimization (TLBO) for predicting the CSC. The algorithms are applied to a Multi-Layer Perceptron (MLP) network to create the SCE-MLP and TLBO-MLP ensembles. The results revealed that, first, intelligent models can properly handle analyzing and generalizing the non-linear relationship between the CSC and its influential parameters. For example, the smallest and largest values of the CSC were 17.19 and 58.53 MPa, and the outputs of the MLP, SCE-MLP, and TLBO-MLP range in [17.61, 54.36], [17.69, 55.55] and [18.07, 53.83], respectively. Second, applying the SCE and TLBO optimizers resulted in increasing the correlation of the MLP products from 93.58 to 97.32 and 97.22%, respectively. The prediction error was also reduced by around 34 and 31% which indicates the high efficiency of these algorithms. Moreover, regarding the computation time needed to implement the SCE-MLP and TLBO-MLP models, the SCE is a considerably more time-efficient optimizer. Nevertheless, both suggested models can be promising substitutes for laboratory and destructive CSC evaluative models.

Analysis of the Characteristics of Manufactured Concrete, according to the Type of Admixture used when Remixing and Placing it (혼화제 종류별로 제조된 콘크리트의 재 혼합 타설시 특성 분석)

  • Ryu, Hyun-Gi;Shin, Sang-Yong
    • Journal of the Korea Institute of Building Construction
    • /
    • v.10 no.5
    • /
    • pp.95-102
    • /
    • 2010
  • In recent years, the demand for the development of high quality and cost effective materials, as well as the competition to ensure a diverse and sufficient amount of ready-mixed concrete, has been increasing rapidly. In this experiment, concretes made with different admixtures are blended with each other in different combinations and ratios, in order to identify potential problems. The first test was a slump level test, in which all of the concretes met the required numbers, as they also did in the test for air content. Plain organic acid concrete scored the highest in bleeding amount, but organic acid mix in general showed a similar outcome. In the early measurement of compressive strength, plain naphthalene concrete was the strongest. Of the blends, the 5:5 mix of organic acid and naphthalene was the strongest. In the standard measurement, the 5:5 mix of naphthalene and lignin was the strongest. Tensile strength tests revealed similar results. Length change rate proved to be greater in blended concrete than in plain concrete, and dry shrinkage rate was highest in the 7:3 ratio blends. Through SEM photo analysis, it was confirmed that the 7:3 ratio blends contained more micro-voids. In conclusion, with the exception of a specific few combinations, it was found that the blending of different types of concrete is undesirable due to the delayed coagulation time as well as the early decrease in strength.

Influence of high axial compression ratios in RC columns on the seismic response of MRF buildings

  • Sergio Villar-Salinas;Sebastian Pacheco;Julian Carrillo;Francisco Lopez-Almansa
    • Structural Engineering and Mechanics
    • /
    • v.90 no.1
    • /
    • pp.51-70
    • /
    • 2024
  • Poorly designed reinforced concrete (RC) columns of actual moment-resisting frame (MRF) buildings can undergo Axial Compression Ratios (ACR) so high as their demand exceeds their capacity, even for serviceability gravity load combinations, this lack commonly leads to insufficient seismic strength. Nonetheless, many seismic design codes do not specify limits for ACR. The main contribution of this research is to investigate the need to limit the ACR in seismic design. For this purpose, three prototype 6 and 11-story RC MRF buildings are analyzed in this paper, these buildings have columns undergoing excessive ACR, according to the limits prescribed by standards. To better that situation, three types of alterations are performed: retrofitting the abovementioned overloaded columns by steel jacketing, increasing the concrete strength, and reducing the number of stories. Several finite element analyses are conducted using the well-known software SAP2000 and the results are used for further calculations. Code-type and pushover analyses are performed on the original and retrofitted buildings, the suitability of the other modified buildings is checked by code-type analyses only. The obtained results suggest that ACR is a rather reliable indicator of the final building strength, hence, apparently, limiting the ACR in the standards (for early stages of design) might avoid unnecessary verifications.

Properties of High Performance Concrete Corresponding to the Replacement Ratio of the Blast Furnace Slag (고로슬래그 미분말의 치환율 변화에 따른 고성능 콘크리트의 특성분석)

  • Kim, Seoung-Hwan;Son, Ho-Jung;Pei, Chang-Chun;Han, Min-Cheol;Baek, Joo-Hyun;Han, Cheon-Goo
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2008.04a
    • /
    • pp.669-672
    • /
    • 2008
  • To analyze possibility for high performance concrete that massively displaces blast furnace slag, this study analyzed the characteristics of concrete by blast furnace slag displacement rate changes, and the results are summarized as follows. Firstly, as for fresh concrete characteristics, flow tended to increase and air amount decreased with increase in blast furnace slag displacement rate, and settling time was shown delayed. As for hardened concrete characteristics, in conditions where blast furnace slag displacement rate increased up to 50%, the compressive strength decreased below OPC at early age, however at age 28 days, its level was no less than that of OPC, and as for temperature rise by simple insulation, it decreased as displacement rate increased at early stage of hydration, but in the latter stage, hydration progress slowed down and hydration heat increased.

  • PDF

Setting Characteristics of Cement Mortar with Super Retarding Agent Mixing Rate in High Temperature (고온조건에서의 초지연제 혼입율 변화에 따른 모르타르의 응결 특성)

  • Lim, Gun Su;Han, Soo Hwan;Jeong, Yeong Jin;Hyun, Seung Yong;Han, Min Cheol;Han, Cheon Goo
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2021.05a
    • /
    • pp.131-132
    • /
    • 2021
  • In this study, as part of the study to reduce and integrate heat of hydration of concrete, the performance change of super retarding agent is examined in the mortar area under high temperature conditions. It was confirmed that the setting time delay can be adjusted from several hours to several days depending on the high temperature and the change of super retarding agent mixing rate. With the increase of super retarding agents, the early age strength was delayed while at 28 days the use of super retarding agent results in an increase of strength remakably.

  • PDF

The Performance of Concrete Used High Strength Development Polycarboxylate Superplasticizer (고강도용 폴리카르본산계 고성능 감수제가 사용된 콘크리트의 성능)

  • Lee, Wan-Jo;Kang, Sung-Gu;Hwang, In-Dong;Lee, Jae-Yong;Park, Sung;Chug, Yun-Joong
    • Journal of the Korean Ceramic Society
    • /
    • v.42 no.3 s.274
    • /
    • pp.182-187
    • /
    • 2005
  • There are many kinds of polycarboxylate superplasticizer as a functional classification which are introduced to domestic; Water Reducer, Retention, Ultra High Strength Superplasicizer. These are showed different physical behaviors because of the difference in the chemical system and the manners after cement mixing. In the case of water reducer, when $1.2\% of cement weight used, water reducing which is over $30\% is observed, but it take with segregation and the reduction of slump flow shows over 30 cm after 45 min of concrete produce. In the case of retention, when the same quantity used, water reducing which is about $25\% is observed and slump flow which is up to 45 min shows under 15 cm. And in the case of ultra high strength, when $1.2\% of cement weight used, water reducing which is over $30\% is observed, and slump flow which is up to 45 min recorded fewer than 15 cm. Compressive strength of ultra high strength superplasticizer has take effect of early age strength, and in the condition of specific mixing, 18 h-compressive strength is insured for more than $60\;Kgf/cm^2$ and 24 h-compressive strength is insured for more than $80\;Kgf/cm^2$.