High Temperature Deformation Behavior of Nano Grain W Produced by SPD-PM Process

  • Oda, Eiji;Ohtaki, Takao;Kuroda, Akio;Fujiwara, Hiroshi;Ameyama, Kei;Yoshida, Kayo
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part 1
    • /
    • pp.126-127
    • /
    • 2006
  • In this study, nano grain W is fabricated by Severe Plastic Deformation-Powder Metallurgy (SPD-PM) process. W powder and W-Re powder mixtures are processed by SPD-PM process, a Mechanical Milling (MM) process. As results, a nano grain structure, whose grain size is approximately 20nm, is obtained in W powder after MM for 360ks. A nano grain W compact, whose grain size 630nm, has excellent deformability above 1273K. A nano grain W-10Re compact is composed of equiaxed grain, a grain growth is restrained and has low dislocation density after the large deformation; therefore it is considered that W-Re compact shows superplasticity.

  • PDF

0.4 wt% Ni을 첨가한 W 활성소결체의 고온압축 특성 연구 (High Temperature Compressive Properties of Tungsten Activated Sintered Pare Prepared by 0.4 wt.% Ni-doped Tungsten Powder Compacts)

  • 이승익;김순욱;박영삼;문인형
    • 한국분말재료학회지
    • /
    • 제9권5호
    • /
    • pp.307-314
    • /
    • 2002
  • The high temperature deformation behavior of the activated sintered W powder compacts was investigated. The W compact showed the relative density of 94% with the average W grain size of $23\mutextrm{m}$ by activated sintering at $1400^{\circ}C$ for 1 hour. Compression tests were carried out in the temperature range of $900-1100^{\circ}C$ at the strain rate range of $10^{0}$/sec - $10^{-3}$/sec. True stress-strain curve and microstructure exhibited the grain boundary brittleness which was dependent on the compression test temperature. The activated sintered W compact showed that the maximum stress as well as the strain at the maximum stress was abruptly decreased as the test temperature increase from $900^{\circ}C$ to 1000 and $1100^{\circ}C$ regardless of the strain rate. The discrepancy of the microstructure in the specimen center was obviously observed with the increase of the test temperature. After compression test at $900^{\circ}C$ the W grain was severely deformed normally against the compression axis. However, after compression test at $1000^{\circ}C$ and $1100^{\circ}C$ the W grain was not deformed, but the microcrack was formed in the W grain boundary. The Ni-rich second phase segregated along the W grain boundary could be partly unstable over $900^{\circ}C$ and affect the poor mechanical property of the activated sintered W compact.

ECAP 공정에 따른 Zn-Al 합금의 집합조직 발달 및 소성 유동에 대한 실험적 연구 (Texture Development during ECAP and High Strain Rate Compression Behavior in Zn-Al Alloy)

  • 정재용;하태권;정효태
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2008년도 추계학술대회 논문집
    • /
    • pp.374-377
    • /
    • 2008
  • High temperature deformation behavior and texture evolution during ECAP(equal channel angular pressing) of Zn-0.3Al alloy were investigated in this study. ECAP was conducted at temperatures from $40^{\circ}C$ to $160^{\circ}C$ on the plate type specimen of 5mm thickness and 20mm width. The specimens obtained by ECAP showed typical texture with basal poles tilted away from the ND toward ED. A series of compression tests was carried out at temperatures from RT to $200^{\circ}C$ under the strain rate from 0.03 to 10/s. With the strain rate increased, serration behavior was observed to be prominent.

  • PDF

공작기계 주축계 열적거동에 관한 연구 (A Study on the Thermal Behaviro of Machine Tool Spindle System)

  • 김종관
    • 한국생산제조학회지
    • /
    • 제8권1호
    • /
    • pp.28-34
    • /
    • 1999
  • According to the development of tool material and the improvement of machinability of cutting material like aluminium alloy, the higher spindle speed is needed. However, the higher speed causes the heat generation of bearings, the deformation of spindle unit parts, and the rotational accuracy of spindle to be worse. Therefore, it is essential to analyze and control the heat generation and the thermal behavior of spindle unit in order to have higher speed and better rotational accuracy. This paper shows the analogy between the analyzation of heat generation and thermal behavior of high speed spindle system by finite element method and the test results of actual temperature rise through running test, and shows the necessity of cooling the spindle and inner ring side of bearings for the thermal balance of high speed spindle system.

  • PDF

근위경골절골술(HTO)용 X-밴드 플레이트에 적용되는 고밀도 폴리에틸렌(HDPE)의 변형률속도에 따른 점탄성거동 (Viscoelastic Behavior of High Density Polyethylene Using High Tibial Osteotomy with Respect to the Strain Rate)

  • 황정훈;김철웅
    • 대한기계학회논문집B
    • /
    • 제36권4호
    • /
    • pp.431-438
    • /
    • 2012
  • 고밀도 폴리에틸렌(HDPE)과 같은 고분자재료의 기계적 거동은 시간과 온도에 의존적이다. 따라서 근위경골절골술(HTO)용 X-밴드 플레이트에 적용되는 HDPE의 각기 다른 변형률속도에 따른 인장거동에 대한 연구는 매우 중요하다. 일반적으로 엔지니어링 응력-변형률곡선에 기반을 둔 폴리메트릭 물질의 변형거동은 입자넥킹의 소성변형을 동반한 높은 비균질성을 나타내므로 매우 복잡한 거동을 나타낸다. 본 연구에서는 1~500%/min의 9가지 변형률속도를 적용하여 그에 따른 점탄성 거동을 평가하였다. 그 결과, 저속 변형률속도에서는 최대인장응력이 증가하고 변형률은 감소하였으나 고속 변형률속도에서는 점탄성거동이 급변하는 교차점(Ts)이 발생하였다. 또한 전이점($P_{st}$)에 의해 구해진 전이응력(${\sigma}_{ts}$)은 고속 변형률속도에서 최대인장응력(${\sigma}_{ult}$)보다 저하됨을 관찰할 수 있었고, 초기 모듈러스와 전이점에서의 시컨트 모듈러스의 비인 ${\beta}$를 이용하여 저속과 고속 변형률속도에서의 점탄성 거동을 평가한 결과 고속 변형률속도에서 급격한 ${\beta}$의 증가를 관찰할 수 있었다.

Zr계 비정질 복상 합금의 과냉 액상 영역에서의 유동 음력과 변형거동 (Flow Stress and Deformation Behavior of Zr-based Bulk Metallic Glass Composite in Supercooled Liquid Region)

  • 전현준;이광석;장영원
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2006년도 춘계학술대회 논문집
    • /
    • pp.417-420
    • /
    • 2006
  • The composition and structure of dendrite phase within $Zr_{76.11}Ti_{4.20}Cu_{4.51}Ni_{3.16}Be_{1.49}Nb_{10.53}$ bulk metallic glass (BMG) were confirmed by using an EPMA, XRD and TEM, respectively. The chief elements of dendrite phase were Zr-Ti-Nb and had a BCC structure. The thermal properties of this BMG have been then subsequently investigated by using a differential scanning calorimeter (DSC). The glass transition and crystallization onset temperatures were determined as $339.7^{\circ}C$ and $375.8^{\circ}C$ for this alloy, respectively. Mechanical properties have also been examined by conducting a series of uniaxial compression tests at various temperatures within supercooled liquid region under the strain rates between $10^{-4}/s$ and $3{\times}10^{-2}/s$. The deformation behavior of BMG composite within supercooled liquid region is similar to one of Vit-1 exhibiting amorphous single phase alloy. The flow stresses of BMG composite, however, are entirely higher than those of Vit-1 because dendrite phases are interfere with moving of atoms.

  • PDF

냉간압연한 고 Mn 오스테나이트계 스테인리스강의 기계적 성질에 미치는 서브제로처리의 영향 (Effect of Subzero Treatment on the Mechanical Properties of Cold-Rolled High Manganese Austenitic Stainless Steel)

  • 황태현;정목환;이종영;이향백;강창룡
    • 열처리공학회지
    • /
    • 제25권5호
    • /
    • pp.233-238
    • /
    • 2012
  • The effect of subzero treatment on the mechanical properties of cold rolled high manganese austenitic stainless steel was investagated. ${\alpha}$'-martensite was formed by cold rolling, and it was formed with surface relief and specific direction or crossing each other. The volume fraction of martensite increased by subzero treatment, and it was increased with longer time of subzero treatment and higher temperature of subzero treatment. The hardness and strength increased by subzero treatment, while the elongation decreased. With the increase of volume fraction of martensite, the hardness and strength was increased steeply with proportional relationship, elongation was decreased slowly. The results show that the hardness and strength was strongly controlled by the volume fraction of martensite, and the elongation was affected by transformation behavior of deformation induced martensite in the initial stage of deformation.

자동차 휠용 6061 Al합금의 단조 및 T6 열처리 전후의 미세조직과 기계적 특성 평가 (Evaluation of Mechanical Property and Microstructure of Forged and T6-treated 6061 Aluminum Alloy Wheel)

  • 이지혜;정헌수;염종택;김정한;박노광;이용태;이동근
    • 소성∙가공
    • /
    • 제16권5호통권95호
    • /
    • pp.354-359
    • /
    • 2007
  • Effects of forging and mechanical properties of 6061 aluminum alloy wheel for automobiles were investigated in the present study. Microstructural and tensile characteristics of automobile wheel after hot forging process using dynamic screw press were analyzed to evaluate effect of metal flow on mechanical properties. The results showed advanced mechanical properties of 6061 alloy wheel because of $Mg_2Si$ precipitation by T6, elongated grain by forging, and work hardening by dense metal flow, etc. Hot compression tests were conducted in order to characterize high temperature compression deformation behaviors and microstructural variation in the range of $300{\sim}450^{\circ}C$, in the strain rate range of $10^{-3}{\sim}10^1\;sec^{-1}$. As strain rate increased, maximum compression stress increased but it was shown the reverse linear relation between temperature and maximum stress irrelevant to strain rate variation. On the other hand, temperature and yield stress didn't have any linear relation and its relation showed big deviation by a function of strain rate and test temperature.

비조질강의 경도 자기제어에 미치는 합금원소의 영향 (Effect of Alloying Elements on Hardness Self-Control of Non-Heat-Treatable Steels)

  • 조기섭;권훈
    • 열처리공학회지
    • /
    • 제30권2호
    • /
    • pp.67-73
    • /
    • 2017
  • Transformation behavior and hardness change were studied in five kinds of self-control steels; standard, high V, modified Ni, W, and high C-Ni steels. In the cooling rates of $10-100^{\circ}C/min$, the primary ferrite and bainite were formed, and the amount of the former increased with decreasing cooling rate. The bainite transformation temperature, Bs, was measured as 570, 560, 590, 575, and $565^{\circ}C$ in experimental steels, respectively, which was similar to the calculated temperature. The self-control, that is, the consistency in hardness, was observed, in which the hardness increased with the decrease in Bs. In the case of hot compression testing, the lower temperature deformation led to the enhancement in hardness.

Cr-Mo 강의 열화도 평가를 위한 Advanced Indentation System의 응용 (Application of Advanced Indentation System for Evaluati Tensile Property Degradation of Cr-Mo Steel)

  • 장재일;최열;이윤희;권동일;김정태
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2001년도 춘계학술대회논문집A
    • /
    • pp.231-236
    • /
    • 2001
  • A newly developed Advanced Indentation System (AIS), which is a portable and nondestructive system for evaluating tensile properties, was used to measure mechanical behavior of materials used under high temperature and pressure conditions. This test measures indentation load-depth curve during indentation and analyzes the mechanical properties related to deformation and fracture. Aging effects of Cr-Mo and Cr-Mo-V steel at high temperature were simulated. Tensile properties including yield strength and tensile strength at various temperature are obtained from the test. For all test materials and conditions, the AIS-derived results were in good agreement with those from conventional standard test method. Examples of the test results ate given and potential applications of the AIS to assess the integrity of aging structures are briefly discussed.