• 제목/요약/키워드: Heat pressing technique

검색결과 18건 처리시간 0.022초

ECAP 강가공에 의한 마그네슘 AZ31합금의 결정립 미세화 및 미세조직 불안정성 (Grain Refinement and Microstructural Instability of an AZ31 Mg Alloy by Severe Plastic Deformation Using ECA Pressing)

  • 김호경;정강;현창용
    • 열처리공학회지
    • /
    • 제17권3호
    • /
    • pp.139-145
    • /
    • 2004
  • Equal channel angular pressing (ECAP) technique had been adapted to the Mg alloy (AZ31) for achieving effective grain refinement through severe deformation. The average grain size of $2.5{\mu}m$ could be obtained after 4 passes. The stability of the ECAPed structure at elevated temperatures was examined by annealing the ECAPed materials over a wide range of temperature between 473 and 748 K. The average activation energy, Q, for static grain growth of 1, 2 and 3 passes was 33.7 kJ/mole (=0.25QL, activation for lattice diffusion). The abnormally low Q value in the lower temperature range may indicate that grain growth occurs in the unrecrystallized microstructure where non-equilibrium grain boundaries containing a large number of extrinsic dislocations exist. The yield stresses of the ECAPed alloys decreased whereas the elongations increased after the ECAP process. These results should be related to the modification of texture for easier slip on basal plane.

나노표면 영역에서의 ECAP 변형된 알루미늄합금의 기계적 물성변화 측정 (Determination of Mechanical Properties of Equal Channel Angular Pressed Aluminum Alloys in Nano-surface Region)

  • 안성빈;김정석
    • 열처리공학회지
    • /
    • 제32권3호
    • /
    • pp.113-117
    • /
    • 2019
  • The effects of severe plastic deformation and heat treatment on the mechanical properties of Al 5052 and 6005 alloys were investigated using the metallurgical technique and nano-indentation technique in nano-surface region. Equal channel angular pressing (ECAP) was used to apply severe plastic deformation to the aluminum alloys in order to obtain fine grain sized materials. The elastic modulus was measured and interpreted in relation to the metallurgical observation. The elastic modulus increased after ECAP process due to evolution of the fine grains. However, the elastic modulus decreased after heat treatment due to generation of coarsened precipitates on the grain boundaries.

착색지르코니아 코어와 전장 도재 사이의 전단결합강도에 관한 연구 (A study on the shear bond strengths of veneering ceramics to the colored zirconia core)

  • 강선녀;조욱;전영찬;정창모;윤미정
    • 대한치과보철학회지
    • /
    • 제47권3호
    • /
    • pp.312-319
    • /
    • 2009
  • 연구목적: 지르코니아-도재 수복물에 있어 상부도재와 코어 사이의 결합 실패가 종종 보고되어 왔으며 특히 착색지르코니아 코어는 기존의 백색 지르코니아보다 상부 도재와의 결합력이 약하다고 보고된 바 있다. 이 연구의 목적은 착색 지르코니아 코어 위의 상부도재를 적층식과 열가압식으로 제작하여 그 전단결합강도를 알아보고, 이를 전통적인 금속-도재간 결합강도와 비교하여 그 임상적 안정성을 평가하는 것이다. 연구 재료 및 방법: 금속도재군 (MC)을 대조군으로 하였다. 전통적인 금속도재군 (MC)과 지르코니아 코어를 사용한 두가지 군 (ZB, ZP)에 대하여 각 시스템별로 10개씩, 총 30개의 시편을 제작했다. CAD/CAM을 이용해 직경 12 mm, 높이 2.8 mm의 원판형 지르코니아 코어 (Katana zirconia)를 제작하고, 그 상부에 직경 2.8 mm, 높이 3 mm의 도재를 축성했다. ZB군은 CZR을 이용하여 적층법으로 상부도재를 제작했으며 ZP군은 NobelRondo Press ingot를 열가압하여 제작했다. Shear bond test machine (R&B Inc. Daejeon, Korea)을 이용하여 분당 0.50 mm의 속도로 파절이 일어날 때까지 전단력을 가하여 최대적용력 (N)을 측정하여 전단결합강도를 계산하고, 일원배치 분산분석을 사용하여 유의수준 5%에서 검정하였다. 파절양상을 알아보기 위하여 전자주사현미경을 통해 파절단면을 관찰했다. 결과: 평균 전단강도 (SD)는 MC 대조군 29.14 (2.26); ZB 29.48 (2.30); ZP 29.51 (2.32) 이었다. 실험군과 대조군 사이에 유의한 차이는 없었다. 모든 실험군에서 접착성 실패와 응집성 실패가 혼재된 양상을 보였으며, 응집성 실패가 우세했다. 결론: 1. 착색지르코니아 코어와 상부도재들 간의 전단결합강도는 금속 도재간 전단결합강도와 유의한 차이가 없었다. 2. 착색지르코니아 코어의 상부도재를 제작하는 방식에 있어 적층법과 열가압법 간의 전단결합강도에 유의한 차이는 없었다 (P > .05). 3. 파절양상은 응집성 파절이 우세한 가운데 접착성 파절과 응집성 파절이 혼재되어 나타났다.

주입선 및 열처리에 따른 IPS Empress 도재의 미세구조에 관한 연구 (A STUDY ON THE MICROSTRUCTURE OF IPS EMPRESS CERAMICS ACCORDING TO THE HEAT TREATMENT AND SPRUE TYPE)

  • 동진근;오상천
    • 대한치과보철학회지
    • /
    • 제36권5호
    • /
    • pp.772-785
    • /
    • 1998
  • This study was undertaken to clarify the microstructure of the different IPS Empress ingots by etching and to observe the change of leucite crystal structure according to subsequent heat treatment and the crystal distribution according to sprue types(${\phi}2.8mm$, single sprue; ${\phi}1.8mm$, double sprue) by scanning electron microscopy. IPS Empress T1, O1 ingots used for staining technique, and Dentin(A2) ingots used for layering technique were selected for this study. To observe the microstructures of these ingots before pressing, the specimens were prepared in splinters($3{\times}3{\times}3mm$) taken from the original ingots. And to estimate crystal distribution and microstructural change by sprue type and subsequent heat treatment. the specimens($3{\times}3{\times}3mm$) were heat-pressed through the two types of sprues with different diameters and numbers, and all specimens were fired according to the recommended firing schedule. The observed surface was ground with waterproof papers($#800{\sim}#1800$) on the grind polisher and was cleaned ultrasonically. All specimen were etched with 0.5% hydrofluoric acid. After etching, the surface was treated by ion sputter coating for SEM observation at an accelerating voltage of 20kV. In all specimens, the central area of ground surface was observed because there was less difference in microstructure between the peripheral area and the central area. The results were as follows ; 1. In the microstructure according to the ingot type, there was a wide difference between the staining (T1,O1) and layering(Dentin A2) ingots, but there was not a considerable difference between the T1 ingot and the O1 ingot for staining technique. 2. In all specimens, the crystal dispersion of IPS Empress ceramic using double sprue was significantly more scattered than that of IPS Empress ceramic using single sprue. The degree of scattering was strongest in the Dentin(A2) specimen and weakest in the O1 ingot. 3. In the microstructural change according to the subsequent heat treatment, all of ingots had some microcracks in the inside of the leucite crystal and the glass matrix after pressing. The inner splinters of the leucite crystal became smaller, and more microcracks occurred in the glass matrix due to increasing heat treatment times. 4. The size of leucite crystals varied from $1{\mu}m\;to\;5{\mu}m$. The mean size of mature crystals was about $5{\mu}m$. The form of the crystal was similar to a circle when it was smaller and similar to an ellipse when it was larger.

  • PDF

전기방사법으로 제조한 PEI/PVdF 블렌드 웹의 물리적 특성에 대한 후처리 영향 (Effect of Post-Process on Physical Properties of Electrospun PEI/PVdF Blend Nonwoven Web)

  • 석훈;박철민;김동영;조성무
    • 폴리머
    • /
    • 제36권5호
    • /
    • pp.606-611
    • /
    • 2012
  • Polyetherimide(PEI)와 poly(vinylidene flouride)(PVdF) 폴리머들을 블렌딩하여 전기방사를 통해 웹을 제조하였다. 낮은 기계적 물성을 증대시키기 위해서 압착과 연신이라는 후처리 공정을 이용하였으며 후처리 공정이 기계적 물성에 미치는 영향을 조사하였다. 물리적 특성을 확인하기 위해 SEM, 인장 시험 측정기를 이용하여 측정하였다. $180^{\circ}C$의 압착 온도에서 1/2, 1/3, 1/4, 1/5의 비율로 압착된 웹들은 초기 상태에 비해 대략 4~5배 가량 인장 강도가 증가하였으며, 이들을 $220^{\circ}C$의 온도에서 30~40% 연신함으로써 2~8MPa의 추가적인 인장 강도 증대를 보였다.

잔류 자성원소 검출에 의한 금속간화합물의 기계적 합금화 공정에서의 합금화 정도 해석 (Determination of the Degree of Alloying by Detection of Residual Ferromagnetic Elements for Intermetallic Alloys Processed by Mechanical Alloying)

  • 어순철
    • 한국재료학회지
    • /
    • 제13권9호
    • /
    • pp.561-566
    • /
    • 2003
  • Mechanical alloying(MA) process using elemental powders followed by hot pressing has been applied to some intermetallic alloy system containing ferromagnetic elements, such as NiAl and $FeSi_2$. A modified thermogravimetric analysis (TGA) technique was used to investigate the degree of alloying in milled powders and hot consolidated specimens as well as heat-treated bulk specimens. It is shown that the measurement of Curie temperatures in MA intermetallic powders and consolidated specimens containing ferromagnetic components, when determined as a function of milling and heat treatment parameters, can give some insight into the progress and mechanism of alloying.

Evaluation of marginal discrepancy of pressable ceramic veneer fabricated using CAD/CAM system: Additive and subtractive manufacturing

  • Kang, Seen-Young;Lee, Ha-Na;Kim, Ji-Hwan;Kim, Woong-Chul
    • The Journal of Advanced Prosthodontics
    • /
    • 제10권5호
    • /
    • pp.347-353
    • /
    • 2018
  • PURPOSE. The purpose of this study was to evaluate the marginal discrepancy of heat-pressed ceramic veneers manufactured using a CAD/CAM system. MATERIALS AND METHODS. The ceramic veneers for the abutment of a maxillary left central incisor were designed using a CAD/CAM software program. Ten veneers using a microstereolithography apparatus (AM group), ten veneers using a five-axis milling machine (SM group), and ten veneers using a traditional free-hand wax technique (TW group) were prepared according to the respective manufacturing method. The ceramic veneers were also fabricated using a heat-press technique, and a silicone replica was used to measure their marginal discrepancy. The marginal discrepancies were measured using a digital microscope (${\times}160$ magnification). The data were analyzed using a nonparametric Kruskal-Wallis H test. Finally, post-hoc comparisons were conducted using Bonferroni-corrected Mann-Whitney U tests (${\alpha}=.05$). RESULTS. The $mean{\pm}SD$ of the total marginal discrepancy was $99.68{\pm}28.01{\mu}m$ for the AM group, $76.60{\pm}28.76{\mu}m$ for the SM group, and $83.08{\pm}39.74{\mu}m$ for the TW group. There were significant differences in the total marginal discrepancies of the ceramic veneers (P<.05). CONCLUSION. The SM group showed a better fit than the AM and TW groups. However, all values were within the clinical tolerance. Therefore, CAD/CAM manufacturing methods can replace the traditional free-hand wax technique.

치과 보철물에 사용되는 지르코니아 코어의 전단결합강도에 관한 연구 (Study about shear bond strength of zirconia core used in dental prosthesis)

  • 심지영;김재홍;김웅철;김혜영;김지환
    • 대한치과기공학회지
    • /
    • 제33권4호
    • /
    • pp.299-306
    • /
    • 2011
  • Purpose: This study aimed to investigate the shear bond strength by manufacturing the veneering porcelain on the IPS e.max $ZirCAD^{(R)}$ zirconia core, using the layering technique and heat-pressing technique, and to evaluate the clinical stability by comparing to the conventional metal ceramic system. Methods: The Schmitz-Schulmeyer test method was used to evaluate the core-veneer shear bond strength of zirconia core ceramic(IPS e.max $ZirCAD^{(R)}$) and their manufacture recommended two veneering ceramic systems(IPS e.max $ceram^{(R)}$, IPS e. max $ZirPress^{(R)}$). A metal ceramic system(Bellabond $plus^{(R)}$, VITA $VM13^{(R)}$) was used as a control group for the two all ceramic system test groups. The maximum loading and shear bond strength was measured. The average shear strength(MPa) was analyzed with the one-way ANOVA and the Tukey's test(${\alpha}$=.05). The fracture specimens were examined using Microscope to determine the failure pattern. Results: The mean shear bond strengths(SD) in MPa were MBSB control 43.62(2.13); ZBSB 18.65(1.76); ZPSB 18.89(1.54). The shear strengths of the zirconia cores were not significantly different(P>.05). Microscope examination showed that zirconia specimens presented mixed failure, and base metal alloy specimens showed adhesive failure. Conclusion: There was no siginificant different between the layering technique and the heat pressing technique in the veneering methods on the zirconia cores. None of the zirconia core and veneering ceramics could attain the high bond strength values of the metal ceramic combination.

In vitro evaluation of fracture strength of zirconia restoration veneered with various ceramic materials

  • Choi, Yu-Sung;Kim, Sung-Hun;Lee, Jai-Bong;Han, Jung-Suk;Yeo, In-Sung
    • The Journal of Advanced Prosthodontics
    • /
    • 제4권3호
    • /
    • pp.162-169
    • /
    • 2012
  • PURPOSE. Fracture of the veneering material of zirconia restorations frequently occurs in clinical situations. The purpose of this in vitro study was to compare the fracture strengths of zirconia crowns veneered with various ceramic materials by various techniques. MATERIALS AND METHODS. A 1.2 mm, $360^{\circ}$ chamfer preparation and occlusal reduction of 2 mm were performed on a first mandibular molar, and 45 model dies were fabricated in a titanium alloy by CAD/CAM system. Forty-five zirconia copings were fabricated and divided into three groups. In the first group (LT) zirconia copings were veneered with feldspathic porcelain by the layering technique. In the second group (HT) the glass ceramic was heat-pressed on the zirconia coping, and for the third group (ST) a CAD/CAM-fabricated high-strength anatomically shaped veneering cap was sintered onto the zirconia coping. All crowns were cemented onto their titanium dies with Rely $X^{TM}$ Unicem (3M ESPE) and loaded with a universal testing machine (Instron 5583) until failure. The mean fracture values were compared by an one-way ANOVA and a multiple comparison post-hoc test (${\alpha}$= 0.05). Scanning electron microscope was used to investigate the fractured interface. RESULTS. Mean fracture load and standard deviation was $4263.8{\pm}1110.8$ N for Group LT, $5070.8{\pm}1016.4$ for Group HT and $6242.0{\pm}1759.5$ N for Group ST. The values of Group ST were significantly higher than those of the other groups. CONCLUSION. Zirconia crowns veneered with CAD/CAM generated glass ceramics by the sintering technique are superior to those veneered with feldspathic porcelain by the layering technique or veneered with glass ceramics by the heat-pressing technique in terms of fracture strength.

전부도재수복물을 위한 수종의 코어 세라믹의 반투명도 및 색 안정성 (Translucency and Color Stability of Various Core Ceramics for All-Ceramic Restoration)

  • 오상천;이해형;신미란;박광수
    • 구강회복응용과학지
    • /
    • 제23권2호
    • /
    • pp.157-170
    • /
    • 2007
  • Purpose: This investigation was designed to determine the translucency and color stability of various core ceramics for all-ceramic restoration using the CIE $L^*a^*b^*$ system. Material and Methods: IPS e.max Press ceramic(Ivoclar-Vivadent, Liechtenstein), $LAVA^{TM}$ All Ceramic(3M-Espe, Germany), Cercon Smart Ceramic(Dentsply, Germany), and Z-match Ceramic(DentAim, Korea) were used for this study. For the specimens of zirconia oxide ceramics, the as-sintered cylindrical blanks($11.0{\times}25.0mm$) were machined into the shape of a disk(0.4, 0.8, 1.5 mm in thickness, 10 mm in diameters) with a diamond grind machine. The IPS e.max Press specimens ($0.8{\times}10mm$) were fabricated using the "lost wax" technique. CIE $L^*a^*b^*$ coordinates and light transmission were recorded for each specimen with a spectrophotometer(CM-2600d, Minolta, Japan). Color differences were calculated using the equation, ${\Delta}E^*ab=[({\Delta}L^*)2+({\Delta}a^*)2+({\Delta}b^*)2]1/2$. Results: The results were obtained as follows: 1. The most translucent group was IPS e.max Press ceramic that is a glass-ceramic, and $Lava^{TM}$ and Z-match ceramic were more translucent than Cercon Smart ceramic in zirconia ceramic group. 2. In the all groups, there was no significant translucent change after 6 times heat-treatments required to make a final restoration. 3. Colored zirconia was showed more yellowish and dark than uncolored zirconia. 4. After heat-pressing, IPS e.max Press ceramic was showed high ${\Delta}E^*ab$ value(4.1 of eM1, 6.8 of eM2) that means to be more whiter than before heat-pressing. However, there was no color change after additive heat treatments for final restoration. 5. In the colored zirconia groups, there was no significant color change after some heat-treatments required to make a final restoration.