• 제목/요약/키워드: Heat intensity

검색결과 778건 처리시간 0.024초

Teflon을 이용한 YAG:Ce 형광체 합성 (Combustion Synthesis of YAG:Ce Phosphor with Teflon)

  • 연정운;원창환;원형일
    • 대한금속재료학회지
    • /
    • 제50권6호
    • /
    • pp.439-443
    • /
    • 2012
  • YAG:Ce phosphor were prepared in a self-propagating high-temperature synthesis (SHS) using a $1.5Y_2O_3+2.5Al_2O_3+0.116CeO_2+3.0KClO_3+kCO(NH_2)_2+m(C_2F_4)_n$ precursor mixture. The heat for the combustion propagation was provided by the reaction of a $KClO_3+CO(NH_2)_2+(C_2F_4)n$ mixture. Pure-phase YAG phosphor was synthesized at the combustion temperature of $1210^{\circ}C$ from k=3.6 mole and m=0.3 mole. The as-prepared YAG:Ce phosphor had a particle size of $2-10{\mu}m$. The addition of Teflon to the precursor mixture increased the YAG particle size and its luminescent intensity. The emission peak of the YAG phosphor was blue-shifted with an increase of Teflon concentration.

세로축 화염안정기 형상이 램제트 연소실에서의 열전달 특성에 미치는 영향 (Influence of the Vertical Flame holder on Heat Transfer Characteristics of Ramjet Combustor)

  • 양강모;이건우;송지운;조형희;황기영
    • 한국추진공학회:학술대회논문집
    • /
    • 한국추진공학회 2008년도 제31회 추계학술대회논문집
    • /
    • pp.305-309
    • /
    • 2008
  • 본 연구에서는 화염 안정기 형상이 램제트 연소실에서의 단열 막냉각 효율에 미치는 영향에 대하여 실험을 수행하였다. 램제트 연소실 입구의 경사진 확장면의 끝에 화염안정기 형상을 설치하여 세로축 화염안정기에 의해 발생된 난류 유동이 다단 슬롯에 영향을 끼치도록 실험 장치를 구성하였다. 화염 안정기를 설치하였을 경우 화염안정기에 의해 발생된 유동의 높은 전단력과 난류강도로 인해 급격히 주유동과 혼합되어 화염안정기가 설치되지 않은 경우에 비해 전체적으로 냉각 성능이 감소함을 결과를 통해 확인하였다. 또한 각각의 경우 분사율을 높여주면 좀 더 양호한 막냉각 효율을 기대할 수 있었다.

  • PDF

열감지인광온도계를 이용한 물에 잠긴 물체 표면 온도장의 비접촉식 측정에 관한 연구 (A Study on Non-contact Surface Temperature Field Measurement of a Body Immerged in Water Using Thermographic Phosphor Thermometry)

  • 박윤성;차이타오;김경천
    • 한국가시화정보학회지
    • /
    • 제18권3호
    • /
    • pp.61-68
    • /
    • 2020
  • Thermographic phosphor (TP) thermometry is a noncontact optical measurement method and has been applied in many fields such as combustion and heat transfer. However, due to the limitation of bonding technology and measurement method, most TP thermometry studies were conducted only on the air environment with water-soluble binders. In this paper, a temperature measurement technology in water using TP is proposed by coatings of manganese activated magnesium fluorogermanate (Mg4FGeO6:Mn4+, MFG) with Polydimethylsiloxane (PDMS). Four MFG-PDMS coatings with different thicknesses were prepared. The lifetime of MFG was not affected by the thickness of the coating as a result of the experiment and analysis of phosphor intensity using a photomultiplier tube. To measure the surface temperature field of an immerged body in water, a cylinder-type cartridge heater was coated with MFG doped PDMS. Transient surface temperature field was successfully measured even the initial temperature is higher than the boiling point of water.

레이돔 표면에 금속 나노코팅을 적용한 적외선 저피탐 성능특성 연구 (Analysis on Infrared Stealth Performance of Metal Nano-coating on Radome Surface)

  • 이용우;장인중;남주영;배형모;조형희
    • 한국군사과학기술학회지
    • /
    • 제25권3호
    • /
    • pp.251-258
    • /
    • 2022
  • Infrared stealth technology used in aircraft is applied to reduce the infrared signal by controlling surface temperature and emissivity using internal heat sink, low emissivity material or metamaterial. However, there is one part of the aircraft where the use of this technology is limited, and that is the radome. Especially, radome should have transmittance for the specific radio frequency, therefore, common stealth technology such as emissivity control surfaces cannot be applied to radome surface. In this study, we developed metal nano-coating for infrared stealth which is applicable to radome surface. We designed slot-type pattern for frequency selective transmission in X-band, and also controlled thickness of metal nano-coating for long wavelength infrared emissivity control. As a result, our infrared stealth surface for radome has 93.2 % transmittance in X-band and various infrared emissivities from 0.17 to 0.57 according to nano-coatings thickness. Also, we analyzed infrared signature of radome through numerical simulation, and finally reduced contrast radiant intensity by 97.57 % compared to polyurethane surface.

광 도파관이 외부로 노출된 구조를 가지는 비분산적외선 이산화탄소 센서 (Non-dispersive infrared carbon dioxide sensor with an externally exposed optical cavity)

  • 정동건;이준엽;도남곤;정대웅
    • 센서학회지
    • /
    • 제30권6호
    • /
    • pp.456-460
    • /
    • 2021
  • In this study, a Non-Dispersive Infrared (NDIR) Carbon Dioxide (CO2) sensor with an externally exposed optical cavity is proposed for improving sensitivity. NDIR CO2 sensors with high performance must use a lamp-type infrared (IR) source with a strong IR intensity. However, a lamp-type IR source generates high thermal energy that induces thermal noise, interfering with the accuracy of the CO2 concentration measure. To solve this problem, the optical cavity of the NDIR CO2 sensor is exposed to quickly dissipate heat. As a result, the proposed NDIR CO2 sensor has a shorter warm-up time and a higher sensitivity compared to the conventional NDIR CO2 sensor.

SCALE-ORIGEN-ARP를 이용한 사용후핵연료 내 중성자 및 감마선원 분석 (An analysis of neutron sources and gamma-ray in spent fuels using SCALE-ORIGEN-ARP)

  • 차소희;박광헌
    • 한국표면공학회지
    • /
    • 제56권1호
    • /
    • pp.84-93
    • /
    • 2023
  • The spent nuclear fuel is burned during the planned cycle in the plant and then generates elements such as actinide series, fission products, and plutonium with a long half-life. An 'interim storage' step is needed to manage the high radioactivity and heat emitted by nuclides until permanent-disposal. In the case of Korea, there is no space to dispose of high-level radioactive waste after use, so there is a need for a period of time using interim storage. Therefore, the intensity of neutrons and gamma-ray must be determined to ensure the integrity of spent nuclear fuel during interim storage. In particular, the most important thing in spent nuclear fuel is burnup evaluation, estimation of the source term of neutrons and gamma-ray is regarded as a reference measurement of the burnup evaluation. In this study, an analysis of spent nuclear fuel was conducted by setting up a virtual fuel burnup case based on CE16×16 fuel to check the total amount and spectrum of neutron, gamma radiation produced. The correlation between BU (burnup), IE (enrichment), and CT (cooling time) will be identified through spent nuclear fuel burnup calculation. In addition, the composition of nuclide inventory, actinide and fission products can be identified.

Verification of mechanical failure mode through corrosion test of a pump for soil sterilizer injection

  • Han-Ju Yoo;Jooseon Oh;Sung-Bo Shim
    • 농업과학연구
    • /
    • 제50권4호
    • /
    • pp.817-828
    • /
    • 2023
  • Deteriorating soil physical properties and increasing soil pathogens due to the continuous cultivation of field crops are the leading causes of productivity deterioration. Crop rotation, soil heat treatment, and chemical control are used as pest control methods; however, each has limitations in wide application to domestic agriculture. In particular, chemical control requires improvement due to direct exposure to sterilizing solution, odor, and high-intensity work. To improve the overall domestic agricultural environment, the problems of time and cost, such as field maintenance and cultivation scale, must be addressed; therefore, mechanization technology for chemical control must be secured to derive improvement effects in a short period. Most related studies are focused on the control effect of the DMDS (dimethyl disulfide) sterilizer, and research on the performance of the sterilization spray device has been conducted after its introduction in Korea, but research on the corrosion suitability of the material is lacking. This study conducted a corrosion test to secure the corrosion resistance of a soil sterilizer injection pump, and a mechanical failure mode by corrosion by the material was established. The corrosion test comprised operation and neglect tests in which the sterilizing solution was circulated in the pump and remained in the pump, respectively. As a result of the corrosion test, damage occurred due to the weakening of the mechanical strength of the graphite material, and corrosion resistance to aluminum, stainless steel, fluororubber, and PPS (polyphenylene sulfide) materials was confirmed.

Mechanical properties of CaO-MgO-Al2O3-SiO2-based glass-ceramic glaze for ceramic tiles fabricated by controlled heat-treatment

  • Jeong-U Eom;Seunggu Kang;Kangduk Kim;Jin-Ho Kim
    • Journal of Ceramic Processing Research
    • /
    • 제22권5호
    • /
    • pp.568-575
    • /
    • 2021
  • Glass-ceramic glazes were prepared using a CaO-MgO-Al2O3-SiO2 system and were used to fabricate low-temperature firing,high-hardness glazes in ceramic tiles. Additives (B2O3) and a nucleating agent (TiO2) were added to the glaze, and crystallineglazes were obtained by sintering at 1000 ~ 1100 oC for 30 or 60 min. X-ray diffraction analysis of the glazes suggested thatcordierite (Mg2Al4Si5O18) and anorthite (CaAl2Si2O8) crystal phases were present, and the peak intensity of the cordieritecrystal phase increased with increasing sintering temperature. All samples showed high crystallinities of 70% or more,irrespective of sintering temperature or time. The glaze density increased with increasing sintering temperature and decreasedat 1100 oC. The Vickers hardness test results of the glazes indicated high hardness values of 6.79 and 6.77 GPa after 30 minheat treatment at 1000 oC and 60 min at 1050 oC, respectively. Glass-ceramic glaze with high hardness at low temperature wasfabricated through crystallization of glaze for tiles.

(CexLu1-x)3MgAl3SiO12 황색 형광체의 광학적 특성 (Optical properties of (CexLu1-x)3MgAl3SiO12 yellow phosphor)

  • 이정일;김태완;오호라;홍창우;류정호
    • 한국결정성장학회지
    • /
    • 제26권1호
    • /
    • pp.14-18
    • /
    • 2016
  • $Ce^{3+}$ 이온을 도핑한 $(Ce_xLu_{1-x})_3MgAl_3SiO_{12}$ 형광체 샘플을 고상합성법으로 합성하였다. 열처리 온도를 1250부터 $1550^{\circ}C$ 온도영역에서 조절하면서 5 h 동안 소성하였으며, 소성된 샘플들의 XRD와 PL 특성을 조사하여 가장 최적의 열처리 온도를 구하고자 하였다. 또한 $Ce^{3+}$ 이온의 도핑농도를 2.0에서 10.0 mol%로 변화시키면서 $Ce^{3+}$ 이온의 도핑농도와 광학적 특성과의 관계를 고찰하였다. $Ce^{3+}$ 이온의 도핑농도에 따른 형광체들의 PL 강도, 피크위치, 반치폭을 계산하여 실제적인 LED 패키징에 가장 적절한 Ce 도핑 농도를 구하고자 하였다. 또한 최적의 소성온도와 Ce 도핑농도 조건에서 합성한 형광체 샘플의 입도와 입형을 분석하였다.

열간단조된 $\gamma$-TiAl 합금의 이방성에 관한 연구 (Anisotropy Studies on Hot-forged $\gamma$-TiAl Alloys)

  • 이재승;박노진;김성진;김승언;오명훈
    • 한국재료학회지
    • /
    • 제10권9호
    • /
    • pp.629-635
    • /
    • 2000
  • 본 논문에서는 Ti-48.5at%Al-0.96at%Mo 조성을 갖는 $\gamma$-TiAl 합금은 항온 단조 및 후속 조직제어 열처리 시 발달하는 집합조직의 변화에 관해 연구하였다. 특히, 동적 재결정 후 조직제어 열처리 온도와 시간의 증가에 따라 발생하는 lamellar volume fraction 과 집합조직 변화에 주목하여 관찰하였다. 동적 재결정 후 집합조직은 ND$\perp${302) 선분과, TD$\perp${100) 및 이에 비해 상대적으로 다소 약한{111) 성분들이 발달하였으며, 열처리 온도와 시간이 증가함에 따라 lameller volume fraction 은 증가했고 동일한 성분의 집합조직도 점차 강하게 발달함을 알 수 있었다. 하지만 상온인장시험 결과는 lameller volume fraction이 증가할수록 낮은 상온 연신을 보였는데, 이는 준 층상조직을 갖는 $\gamma$-TiAl합금의 상온인장특성이 집합조직의 영향보다는 lameller volume fractio과 같은 미세조직 특성에 더욱 강하게 영향을 받기 때문인 것으로 판단된다.

  • PDF