티타늄합금의 연삭특성에 관한 연구 (A Study on the Grinding Characteristics of Titanium Alloy)

  • 김성헌;최환;이종찬
    • 한국기계가공학회지
    • /
    • 제1권1호
    • /
    • pp.55-62
    • /
    • 2002
  • This investigation reports the grinding characteristics of titanium alloy(Ti-6AI-4V). Grinding experiments were performed at various grinding conditions. The grinding forces were measured to investigate the grindability of titanium alloy with the five different wheels including Green carbide, Alumina, Resin Diamond, Resin CBN and Vitrified CBN. To investigate the grinding characteristics of titanium alloy grinding force, force ratio, specific grinding energy and grinding-ratio were measured. Surface roughness was also measured with tracer and the ground surfaces were observed with SEM Residual stress measurement was conducted on the X-Ray Diffractometer. Force ratio of grinding of titanium alloy was very lower than that of grinding of SKD-11 Surface roughness with Resin Diamond wheel was a little larger and rougher surface than that with other wheels Grinding ratio of titanium alloy was a little lower than that of other materials. Grinding ratio of titanium alloy with Diamond wheel was almost six times larger than that With CBN wheel. As a result of five different wheels, the most excellent wheel in grinding of Titanium alloy was Resin Diamond wheel.

  • PDF

티타늄 합금의 연삭에 관한 연구, Part2 : 초연마재를 사용한 연삭특성 (A Study on the Grinding of Titanium Alloy, Part2 : Grinding characteristics by using Superabrasives)

  • 김성헌;최환;이종찬;정선환
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 2001년도 춘계학술대회 논문집
    • /
    • pp.1076-1079
    • /
    • 2001
  • This investigation reports the grinding characteristics of titanium alloy(Ti-6Al-4V). Grinding experiments were performed at various grinding conditions. The grinding forces and grinding force ratio were measured to investigate the grindability of titanium alloy with the Diamond and CBN wheel. To investigate the grinding characteristics of titanium alloy grinding force ratio and grinding ratio were measured. Surface profile of wheel was also measured with tracer and the ground surfaces and chip were observed with SEM. Grinding-ratio of titanium alloy was much lower than that of other materials. Grinding-ratio of titanium alloy with Diamond wheel was almost six times larger than that with CBN wheel.

  • PDF

Evaluation of Wheel Life by Grinding Ratio and Static Force

  • Kwak, Jae-Seob;Ha, Man-Kyung
    • Journal of Mechanical Science and Technology
    • /
    • 제16권9호
    • /
    • pp.1072-1077
    • /
    • 2002
  • A degree of sharpness in wheel grains affects the surface roughness and dimensional accuracy in the grinding process. If a wheel with dull grains is used, the grinding force is increased and the surface roughness is deteriorated. In ovder to produce a precision component economically, the magnitude of the wear amount in the grinding wheel has to be limited. In this study, experimental evaluation of a wheel life varying with the grinding ratio and static grinding force was conducted. The grinding ratio and grinding force were measured to seek the grinding performance of the WA wheel. The relationship between the grinding ratio and static grinding force was presented.

티타늄 합금의 연삭에 관한 연구 Part 1: 연삭력, 비연삭에저니, 표면거칠기 , 연삭비 (A Study on the Grinding of Titanium Alloy Part 1 : Grinding force, Specific grinding energy, Surface roughness, G-ratio)

  • 김성헌;임종고;하상백;최환;이종찬
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 2000년도 추계학술대회 논문집
    • /
    • pp.870-874
    • /
    • 2000
  • This investigation reports the grinding characteristics of titanium alloy(Ti-6Al-4V). Grinding experiments were performed at various grinding conditions and the grinding forces and specific grinding energies were measured to investigate the grindability of titanium alloy with the three different wheels including Diamond, Green carbide and Alumina. To investigate the grinding characteristics of titanium alloy grinding force, force-ratio, specific grinding energy and grinding -ratio, were measured. Surface roughness was also measured with tracer and the ground surfaces were observed with SEM. Force-ratio of grinding of titanium alloy was very lower than that of grinding of SKD-11. Specific grinding energy are almost five times larger and rougher surface was obtained in titanium grinding.

  • PDF

단속연삭의 유제공급 특성 (Characteristics of Fluid Supply in Discontinuous Wheel Grinding)

  • 곽용길;홍순익;송지복;구양
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 1997년도 춘계학술대회 논문집
    • /
    • pp.857-861
    • /
    • 1997
  • In discontinuous wheel grinding, temperature is different form conventional grinding. The characteristics of discontinuous grinding with respect to various slotted wheel were compared with those of general grinding. Thermal conditions vary with intermittent ratio, direction of fluid supply for discontinous wheel. According to three direction of grinding fluid supply and intermittent ratio,temperature and surface roughness were analyzed.

  • PDF

세라믹 연삭에서 다이아몬드 휠의 연삭 특성 및 마멸 거동 (Grinding Characteristics and Wear Behavior of Diamond Wheel in Ceramic Grinding)

  • 박병규;문홍현;김성청
    • 한국공작기계학회논문집
    • /
    • 제12권5호
    • /
    • pp.8-14
    • /
    • 2003
  • The characteristics of grinding and wear behavior of diamond wheel for grinding ceramic materials was investigated in this study. In case of $Si_3N_4$, the wear of wheel was large, the finding force was relatively stable and the fluctuation of surface roughness n small. On the other hand in case of $Al_2O_3$ and $ZrO_2$, the wear of wheel and surface roughness were decreasing, the grinding force was increasing. During grinding with vitrified bond wheel, $Si_3N_4$ shows renewal of cutting edge while $Al_2O_3$ and $ZrO_2$ show glazing phenomenon of cutting grains. We have found that it possible to observe the behavior of grinding wheel by grinding ratio, grinding resistance, surface roughness and cutting edge ratio. Through the grinding experiments, it was found that grinding life of diamond wheel is 20 times for $Si_3N_4$, and 40 times fir $Al_2O_3$ and $ZrO_2$.

다기공 연삭숫돌의 단속비에 의한 표면특성 분석에 관한 연구 (A Study on the Analysis of Surface Characteristics According to intermittent Ratio of Discontinuous Grinding Wheel with Multi-Porous Grooves)

  • 김정두;강윤희
    • 한국정밀공학회지
    • /
    • 제14권6호
    • /
    • pp.44-51
    • /
    • 1997
  • Crinding of stainless steel, aluminium alloy, copper alloy, and titanium alloy are difficult to obtain high quality finish, because they have the mechanical properties such as low hardness, high toughness. The low hardness and the high toughness result in the loading of wheel and the poor surface finish. In order to perform the grinding operations for these sorts of materials easily, the discontinuous grinding wheel wiht multi-porous grooves has been newly developed. The multi-porous grooves inthe discontinuous grinding wheel were formed during grinding wheel manufacturing process. In this paper, discontinuous grinding wheels having intermittent ratio 0.66, 0.81 and number of grooves 18,32 have been manufactured and grinding surface characteristics of these grinding wheels for SUS304 have been analyzed. Discontinuous grinding temperature according to intermittent ratiohas been also estimated by simulation. The discontinuous grinding wheels increase the grinding performance considerably. It is desirable to use the discontinuous grinding wheel in grinding the materials with high efficiency and accuracy.

  • PDF

머시닝센터를 이용한 평면 연삭가공에 관한 연구(I) (A Study on the Surface Grinding using the Machining Center (I))

  • 이승만;서영일;최환;이종찬;정선환
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 2000년도 춘계학술대회 논문집
    • /
    • pp.862-865
    • /
    • 2000
  • The surface grinding of STD-11 was attempted on the machining center. Grinding experiments were performed at the various grinding conditions and the grinding force, machining error, grinding ratio, and surface roughness were measured. The experimental results indicate that the grinding ratio decreases as the table speed and depth of cut increase. The surface roughness of ground surface was not affected by the change of depth of cut. The surface roughness values obtained on the experiments were 0.02 ~ 0.03${\mu}{\textrm}{m}$ which are fairy good and acceptable for ground surface.

  • PDF

원통 플런지 연삭에서의 연삭력에 관한 연구

  • 박종찬;박철우;이상조
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 1996년도 춘계학술대회 논문집
    • /
    • pp.34-38
    • /
    • 1996
  • Cylindrical plunge grinding is widely used for final machining process of precision parts such as automobile, aircraft, measurement units. In order to make parts which have high precison accuracy and high surface integrity, it is neccessary to consider grinding characteristics. these grinding characteristics are closely related grinding force. Soin this study, to examine closely characteristics of grinding force, effects of dressing condition, depth of cut and speed ratio on grinding force are considered. As the result, It is shown that grinding forces are affected bydressing condition, depth of cut and speed ratio and that there exist threshod grinding force and it also affected by dressing conditon.

  • PDF

전해 인프로세스 드레싱법(ELID)을 이용한 철강재료의 고능률 원통연삭 (High Efficient Cylindrical Grinding of Ferrous Materials Using Electrolytic In-process Dressing Method(ELID))

  • 이득우;고교일랑;대삼정;중천위웅
    • 한국정밀공학회지
    • /
    • 제12권8호
    • /
    • pp.99-105
    • /
    • 1995
  • This paper provides a highly efficient grinding for ferrous materials using ELID-grinding method. The grinding efficiency using ELID gring method with CIFB-cBN wheel and CB-cBN wheel is compared with general grinding method with V-cBN wheel. This paper measured grinding ratio for plunge grinding and grinding resistance for traverse grinding in order to investigate grinding ability. The results show that ELID grinding methods is useful for the high efficient grinding of ferrous materials.