Effects of $SiO_2$ and Seed on Ba-ferrite Synthesized by Molten Salt (용융염법으로 합성한 Ba-ferrite의 $SiO_2$ 및 Seed 첨가 효과)

  • 김영근;이승관;김현식;오영우
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 1996.11a
    • /
    • pp.326-329
    • /
    • 1996
  • In order to synthesize Ba-ferrite fine particles by molten salt method and inhibit the abnormal grain growth of sintered specimen, KCI anti NaCl were added to basic composition to 50% by weight, and added 1 male% of $SiO_2$ to control the shape of Ba-ferrite particles. $H_{c}$ and $M_{r}$ were decreased when F $e^{3+}$ was substituted with $Co_{2+}$ and $Ti_{4+}$ from x=0 to x=1.0 in $BaFe_{12-2x}$ $Ti_{x}$ $Co_{x}$ $O_{19}$ , and 1 mole% $SiO_2$ increased the size but shortened c-axis of hexagonal ferrite. Seeds added in Ba-ferrite particle effected inhibition of abnormal grain growth during sintering.ing.g.

  • PDF

The Production Technology of Surface Fine Grain Steels by Controlled Rolling and Cooling Technology (제어압연에 의한 표면미세립강의 제조 기술)

  • 신정호;박상덕;이정환;이용희;장병록
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 1999.08a
    • /
    • pp.188-197
    • /
    • 1999
  • Grain refinement of the structural steels was selected as the most effective method to meet improvement of strength and toughness without heat treatment. So, the future research and developing direction of ultra fine grain steels are more and more required to response to the production of eco - materials(environmental consciousness - materials) In this paper, the product of surface fine grain steels by CRCT and Inverse Transformation Method by warm deformation of martensite is carried out in order to improve the production process of Dowel Bar. It is possible to obtain surface ultra fine grain steel, when warm deformation of martensite formed after quenching is carried out from 730$^{\circ}C$ to 800$^{\circ}C$ in the finishing rolling step. The characters of surface with ultra fine grain steel is showing the cementite particles inside the ferrite grain and fine ferrite grain of about 1.2$\mu\textrm{m}$ in size.

  • PDF

Comparison of Tensile and Impact Properties of Hypo-Eutectoid Steels Containing Micro-Alloying Elements (미량합금 원소가 첨가된 아공석강의 인장 및 충격 특성 비교)

  • Lee, Seung-Yong;Cho, Yun;Hwang, Byoungchul
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.30 no.1
    • /
    • pp.6-12
    • /
    • 2017
  • In this study tensile and impact properties of three hypo-eutectoid steels containing different micro-alloying elements were investigated in terms of microstructural factors such as pro-eutectoid ferrite grain size, pearlite fraction, interlamellar spacing, and cementite thickness. Yield point phenomenon appeared in all the steel specimens during tensile testing, and ultimate tensile stress was mainly dependent on pearlite fraction. On the other hand, the refinement of austenite grain size caused by the addition of micro-alloying elements resulted in the increment of ferrite volume fraction and carbon contents in pearlite because of the refinement of pro-eutectoid ferrite grain size. As a result, cementite thickness in pearlite increased and had an effect on deteriorating the low temperature impact toughness.

The Effect of the Processing Conditions on the Magnetics Properties of Mn-Zn ferrite (제조공정에 따른 Mn-Zn 페라이트의 전자기적 특성변화)

  • 김종령;이해연;김현식;오영우;민복기
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2001.07a
    • /
    • pp.905-908
    • /
    • 2001
  • The microstructure and the magnetic properties of Mn-Zn ferrite, which were power loss and saturation magnetic flux density, were investigated as the function of the process before firing. The highest initial permeability and the lowest power loss were attained to the specimen with CaO 400 ppm as a resulted from the highest solubility to SiO$_2$and the creation of liquid phase which improved sintering. The biggest grain size, the highest saturation magnetic flux density and the lowest power loss, which was resulted from that the eddy current loss increased as grain size increased but the hysteresis loss much more decreased and the hysteresis loss strongly influenced on the total power loss rather than the eddy current loss, were obtained to the Mn-Zn ferrite added 2wt% PVA. The power loss was lowest and the saturation magnetic flux density was highest in case of 1 ton/$\textrm{cm}^2$ and the grain size was not influenced.

  • PDF

Quasi-Static and Dynamic Torsional Deformation Behavior of API X70 and X80 Linepipe Steels (API X70 및 X80급 라인파이프강의 준정적 및 동적 비틀림 변형 거동)

  • Kim, Yongjin;Kim, Yang Gon;Shin, Sang Yong;Lee, Sunghak
    • Korean Journal of Metals and Materials
    • /
    • v.48 no.1
    • /
    • pp.8-18
    • /
    • 2010
  • This study aimed at investigating quasi-static and dynamic torsional deformation behavior of three API X70 and X80 linepipe steels. Quasi-static and dynamic torsional tests were conducted on these steels. having different grain sizes and volume fractions of acicular ferrite and polygonal ferrite, using a torsional Kolsky bar. The test data were then compared via microstructures and adiabatic shear band formation,. The dynamic torsional test results indicated that the steels rolled in the single phase region had higher maximum shear stress than the steel rolled in the two phase region, because the microstructures of the steel rolled in the single phase region were composed mainly of acicular ferrites. In the X80 steel rolled in the single phase region, the increased dynamic torsional properties could be explained by a decrease in the overall effective grain size due to the presence of acicular ferrite having smaller effective grain size. The possibility of adiabatic shear band formation was analyzed from the energy required for void initiation and variation in effective grain size.

Effect of Microstructure on the Strain Aging Properties of API X70 Pipeline Steels (API X70 라인파이프 강재의 변형 시효 특성에 미치는 미세조직의 영향)

  • Lee, Seung-Wan;Im, In-Hyuk;Hwang, Byoungchul
    • Korean Journal of Materials Research
    • /
    • v.28 no.12
    • /
    • pp.702-708
    • /
    • 2018
  • This study deals with the effect of microstructure factors on the strain aging properties of API X70 pipeline steels with different microstructure fractions and grain sizes. The grain size and microstructure fraction of the API pipeline steels are analyzed by optical and scanning electron microscopy and electron backscatter diffraction analysis. Tensile tests before and after 1 % pre-strain and thermal aging treatment are conducted to simulate pipe forming and coating processes. All the steels are composed mostly of polygonal ferrite, acicular ferrite, granular bainite, and bainitic ferrite. After 1 % pre-strain and thermal aging treatment, the tensile test results reveal that yield strength, tensile strength and yield ratio increase, while uniform elongation decreases with an increasing thermal aging temperature. The increment of yield and tensile strengths are affected by the fraction of bainitic ferrite with high dislocation density because the mobility of dislocations is inhibited by interaction between interstitial atoms and dislocations in bainitic ferrite. On the other hand, the variation of yield ratio and uniform elongation is the smallest in the steel with the largest grain size because of the decrease in the grain boundary area for dislocation pile-ups and the presence of many dislocations inside large grains after 1 % pre-strain.

Effects by Variation of Raw Materials on Physical Properties of Ni-Zn Ferrite (원료 변화에 따른 Ni-Zn Ferrite의 물리적 특성에 미치는 영향)

  • Koh, Jae-Gui
    • Korean Journal of Materials Research
    • /
    • v.16 no.9
    • /
    • pp.578-583
    • /
    • 2006
  • We studied the physical properties of Ni-Zn ferrites by adding different chemicals such as $SO_4$, Cl, and $NO_3$. Specimens were prepared by the coprecipitation method and sintered at temperatures $950^{\circ}C,\;1,150^{\circ}C,\;and\;1,350^{\circ}C$, respectively. X-ray diffractions showed a spinel structure and the optical microscopy revealed grain size of 0.3 to 0.6 ${\mu}m$. The optimum sintering temperature to obtain fine, sintered microstructure depended on the additive : Cl and $NO_3\;at\;950^{\circ}C\;and\;SO_4\;at\;1,150^{\circ}C$. According to particle size analysis, higher magnetic permeability and magnetization value were observed with Cl and $NO_3\;than\;SO_4$. As sintering temperature was raised from $950^{\circ}C$ to $1,350^{\circ}C$, the average grain diameter, initial permeability and the magnetic moment also increased.

Microstructure and Magnetic Properties of Hexagonal Barium-Ferrite (BaM) Thin Films with Various Underlayers (여러 하지층을 첨가한 Hexagonal Barium-Ferrite(BaM) 박막의 미세구조와 자기적 특성)

  • 김동현;남인탁;흥양기
    • Journal of the Korean Magnetics Society
    • /
    • v.11 no.3
    • /
    • pp.122-128
    • /
    • 2001
  • In this paper, we studied structural and magnetic properties of Ba-ferrite thin film deposited on Si(100) substrate with various underlayers. Ba-ferrite thin films with various underlayers were deposited by reactive RF/DC magnetron sputtering system at room temperature. various underlayers was reactive sputtered with O$_2$. After deposition, the thin films were annealed at 850 $^{\circ}C$ to get the crystallized sample. Underlayers were used to prevent interdiffusion from Ba-ferrite thin film to substrate. The growth of Ba-ferrite thin films was influenced by underlayers. Easy magnetization direction is in-plane. From these results the Ba-ferrite film with various underlayers can be used as longitudinal recording media.

  • PDF

Effect of Molar Ratio of $Fe_2O_3$ and BaO Addition on the Characteristics of Sr-Ferrite ($Fe_2O_3$몰비 및 B\ulcorner첨가가 Sr-Ferrite 특성에 미치는 영향)

  • 문기훈;심영재;조성걸
    • Journal of the Korean Ceramic Society
    • /
    • v.34 no.5
    • /
    • pp.453-460
    • /
    • 1997
  • Sr-ferrite having magnetoplumbite structure is similar to Ba-ferrite in magnetic characteristics, but better magnetic characteristics for using motor application. To improve remanence magnetic flux density(Br) and coercive force(iHc), it is necessary that sintered ferrites must have high density and grain size less than 1 $\mu$m. By varying n values in SrO.nFe2O3 basic composition, calcination temperature, and BaO addition, Sr-ferrite powder and sintered specimen was prepared. The n values, calcination temperature, and BaO addition affected secondary phase formation, particle size, and particle shape. BaO addition enhanced Fe2O3 secondary phase and hexagonal shape particle. Fe2O3 phase reduced sintered density which greatly decreased Br.

  • PDF

The Power Loss Characteristics of Mn-Zn Ferrites at MHz Region with Sintering Condition (소성조건에 따른 MHz 대역의 Mn-Zn ferrite 전력손실 특성)

  • Suh J.J.;Song B.M
    • Resources Recycling
    • /
    • v.12 no.6
    • /
    • pp.26-31
    • /
    • 2003
  • The power loss characteristics of Mn-Zn ferrite were observed with the sintering temperature. In case of $1150 ^{\circ}C$ sintering, the core loss increased with measuring temperature, and does not have minimum value at the point where the magnetocrystalline anisotropy be 'zero'. This reason mainly due to the change of core loss mechanism with grain size which affects residual loss. The grain size and sintered density slightly increased with equilibrium oxygen partial pressure at$ 1150 ^{\circ}C$ sintering. The resistivity and initial permeability showed no significance with atmosphere, these results due to complex effect of $Fe^{2+}$ concentration and microstructure change. The core loss at $100^{\circ}C$ decreased as the equilibrium oxygen partial pressure increased.e increased.