ANALYSIS OF NECKING DEFORMATION AND FRACTURE CHARACTERISTICS OF IRRADIATED A533B RPV STEEL

  • Kim, Jin Weon;Byun, Thak Sang
    • Nuclear Engineering and Technology
    • /
    • v.44 no.8
    • /
    • pp.953-960
    • /
    • 2012
  • This paper reports the irradiation effect on the deformation behavior and tensile fracture properties of A533B RPV steel. An inverse identification technique using iterative finite element (FE) simulation was used to determine those properties from tensile data for the A533B RPV steel irradiated at 65 to $100^{\circ}C$ and deformed at room temperature. FE simulation revealed that the plastic instability at yield followed by softening for higher doses was related to the occurrence of localized necking immediately after yielding. The strain-hardening rate in the equivalent true stress-true strain relationship was still positive during the necking deformation. The tensile fracture stress was less dependent on the irradiation dose, whereas the tensile fracture strain and fracture energy decreased with increasing dose level up to 0.1 dpa and then became saturated. However, the tensile fracture strain and fracture energy still remained high after high-dose irradiation, which is associated with a large amount of ductility during the necking deformation for irradiated A533B RPV steel.

Measurement of Fracture Toughness of WC-Co Composites by Micro-Vickers Indentation Cracks (미소 비커스 압입균열에 의한 초경합금의 파괴 인성치 측정)

  • Lee, O.S.;Son, I.S.;Park, W.K.;Hwang, S.K.
    • Journal of the Korean Society for Precision Engineering
    • /
    • v.12 no.2
    • /
    • pp.5-13
    • /
    • 1995
  • Various techniques to measure fracture toughness which is an important parameter to predict fracture behavious of structural materials have been reported. Among these mathods, this paper describes the micro-Vickers indentation crack method to estimate the fracture toughness of some WC-Co composites. Two indentation crack patterns (such as radial-median cracks (orhalf-penny cracks) and Palmqvist cracks generated during indentation) are referred precisely. The fracture toughness of WC-4.7wt%Co, WC-6wr%Co and WE-9wr%Co composites were estimated by using some equations given by Shetty et al., Nihara et al. in this study. We show the reliability of indentation method by comparing the results with those from literatures. The appropriate equation to estimate the fracture toughness in the case of WC-Co composite is given. In addition, some technical informations in terms of the crack length by indentation in estimating the existence of the surface residual stress that prevents to obtain an accurate fracture toughness are presented.

  • PDF

A study of mixed-mode interlaminar fracture toughness of graphite/epoxy composite (炭素纖維强化 複合材料의 혼합모우드 層間破壞靭性値에 대한 硏究)

  • 윤성호;홍창선
    • Transactions of the Korean Society of Mechanical Engineers
    • /
    • v.10 no.2
    • /
    • pp.198-207
    • /
    • 1986
  • This study investigates interlaminar fracture characteristics of Graphite/Epoxy composite (HFG Graphite/Epoxy) under mode I (opening mode), mode II (sliding mode) and mixed mode loading conditions. The effects on interlaminar fracture toughness due to different fiber orientations on the crack surface are also investigated. The antisymmetric test fixture proposed by M. Arcan is used for this test. Both critical stress intensity foctors and critical energy release rates were determined and several mixed mode fracture criteria were compared to the experimental data. Also fracture surfaces were investigaed to obtain informations on the fracture behaviors of Graphite/Epoxy composite by means of a scanning electron microscope(SEM).

Fracture Characteristics of Carbonized Silicon Grinding Wheels (탄화규소 연삭숫돌의 파괴특성)

  • Oh, Dong-Seuk;Lee, Byong-Gon
    • Journal of the Korean Society of Safety
    • /
    • v.17 no.4
    • /
    • pp.45-51
    • /
    • 2002
  • In this study, the fracture characteristics of carbonized silicon grinding wheels were examined with tensile, compression, impact and bending test. The experiment was performed for the various grinding wheels with grain size #46, #80, and grade H, L, P, and one vitrified bond and one structure No.7. Also the centrifugal fracture rpm of carbonized silicon grinding wheels were measured and compared with the calculated values for the various wheel diameters and thicknesses. The results showed that the fracture tensile strength was $1.5~2.0Kg_f/mm^2$, and it was increased by decreasing grain size and increasing grade. The fracture compression loads were $1,600~3,000Kg_f$, and the inner stress was higher than outer's. And the absorption energy of impact test was 3.3~4.7 J, and it was increased by decreasing grain size but it was not effected by grade. The fracture bending stress was $0.1~0.2Kg_f/mm^2$, and it was increased by decreasing grain size and increasing grade. The centrifugal fracture rpm of carbonized silicon grinding wheel was about 8,500~12,000 and agreed well with the calculated value, and it was increased by decreasing diameter. However, it was almost constant for the reduction of wheel thickness.

Tension-Shear Experimental Analysis and Fracture Models Calibration on Q235 Steel

  • Huang, Xiaogang;Zhou, Zhen;Zhu, Yazhi;Zhu, Dongping;Lu, Lu
    • International journal of steel structures
    • /
    • v.18 no.5
    • /
    • pp.1784-1800
    • /
    • 2018
  • Tension-shear loading is a common loading condition in steel structures during the earthquake shaking. To study ductile fracture in structural steel under multiple stress states, experimental investigations on the different fracture mechanisms in Chinese Q235 steel were conducted. Different tension-shear loading conditions achieved by using six groups of inclined notch butterfly configurations covering pure shear, tension-shear and pure tension cases. Numerical simulations were carried out for all the specimens to determine the stress and strain fields within the critical sections. Two tension-shear fracture models were calibrated based on the hybrid experimental-numerical procedure. The equivalent fracture strain obtained from the round bar under tensile loading was used for evaluating these two models. The results indicated that the tension-shear criterion as a function of the shear fracture parameter had better performance in predicting the fracture initiation of structural steel under different loading conditions.

Reason of Die Fracture in Hot Forging of an Aluminum Fixed Scroll and Its Practical Measures (알루미늄 고정 스크롤 열간 단조공정의 금형 파괴 원인 및 실용적 대책)

  • Kim, Y.S.;Joun, M.S.
    • Transactions of Materials Processing
    • /
    • v.26 no.3
    • /
    • pp.156-161
    • /
    • 2017
  • In this study, the reason of die fracture occurring in hot forging of an aluminum fixed scroll was studied, based on experiments and finite element predictions. The material is assumed to be rigid-viscoplastic, and the die is rigid for the finite element predictions. The stress in the tension at the wrap root is known to cause brittle fracture, and the increase in the tensile stress is owing to the unbalanced filling of material into the die cavities between both sides of the warp. Based on the empirical and numerical achievements, the effects of geometrical parameters of the material on the die fracture were examined to find practical measures for elongated die life. It has been shown from the parametric study that the material with the optimized trapezoidal cross-section, which can be easily made during cutting or the optimized cylindrical billet with its eccentric placement in the die cavity, can considerably reduce the magnitude of the tensile stress around the die corner fractured, indicating that economical manufacturing with reduced number of stages and elongated die life can be realized at once using the optimized practical initial material.

Structural Integrity Assessments of Pressurized Pipes with Gouge using Stress-Modified Fracture Strain Criterion (삼축응력 기반의 파괴변형률 기준을 적용한 가우지 손상배관의 건전성 평가)

  • Oh C.K.;Kim Y.J.;Park J.M.;Baek J.H.;Kim Y.P.;Kim W.S.
    • Proceedings of the Korean Society of Precision Engineering Conference
    • /
    • 2005.10a
    • /
    • pp.808-813
    • /
    • 2005
  • Structural integrity assessment of defected pipe is important in fitness for service evaluation and proper engineering assessment is needed to determine whether pipelines are still fit for service. This paper present a failure prediction of gas pipes made of APIl X65 steel with gouge using stress-modified true fracture strain, which is regarded as a criterion of ductile fracture. For this purpose, API X65 pipes with gouge are simulated using elastic-plastic FE analyses with the proposed ductile failure criterion and the resulting burst pressures are compared with experimental data. Agreements are quite good, which gives confidence in the use of the proposed criteria to defect assessment fer gas pipelines. Then, further extensive finite element analyses are performed to obtain the burst pressure solution of pipes with gouge as a function of defect depth, length and pipeline geometry.

  • PDF

Reinforcing Characteristics on Volume and Shape of Ductile Short-Fiber in Brittle Matrix Composites (취성기지 복합재료에서 연성 단섬유의 함유량 및 형상에 관한 보강특성)

  • Sin, Ik-Jae;Lee, Dong-Ju
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.24 no.1 s.173
    • /
    • pp.250-258
    • /
    • 2000
  • The reinforcing effects of ductile short-fiber reinforced brittle matrix composites are studied by, measuring flexural strength, fracture toughness and impact energy as functions of fiber volume fraction and length. The parameters of fracture mechanics, K and J are applied to assess fracture toughness and bridging stress. It is found that fracture toughness is greatly, influenced by the bridging stress ill which fiber pull-out is occur. For the reinforcing effects as functions of fiber volume fraction($V_f$ = 1, 2, 3 %) and length(L = 3, 6. 10cm), the flexural strength is maximum at $V_f$ = 1% and both fracture toughness.

Numerical Analysis of Concrete Fracture Properties (콘크리트 파괴특성의 수치해석)

  • 연정흠
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 1995.04a
    • /
    • pp.237-244
    • /
    • 1995
  • Fracture properties for LEFM, S-FPZ and NS-FPZ models were determined using by finite element method and energy balance from the experimental results of three-point bend tests. For the LEFM model the stress intensity factor needed to increase continuously with crack extension, and for the S-FPZ model the fracture process zone characteristics need to change continuously if the critical stress intensity factor was to remain constant. The LEFM model showed the largest resistance and the slowest crack extension, while the NS-FPZ model showed the smallest resistance and the fastest crack extension. The responses for the S-FPZ model were intermediate between those for the LEFM and NS-FPZ models and the total fracture energy densities for the S-FPZ and NS-FPZ models and the total fracture energy densities for the S-FPZ and NS-FPZ models were equal.

  • PDF

Effects of Moisture Content on Non-Fracture Dynamic Properties and Fracture Quality of Pacific Whiting Surimi

  • Esturk, Okan;Park, Jae-Won;Raik, Moo-Yeol;Kim, Byung-Yong
    • Food Science and Biotechnology
    • /
    • v.15 no.6
    • /
    • pp.856-859
    • /
    • 2006
  • The effects of moisture content on non-fracture dynamic properties and fracture gel quality of Pacific whiting surimi were investigated to determine their relationships. Surimi samples were tested at various moisture contents (75, 78, and 81 %). Torsion test showed that shear stress decreased rapidly and strain values decreased gradually as moisture concentration increased. Dynamic storage modulus (G') also decreased as moisture content increased. A strong positive correlation ($R^2=0.90$ to 0.99) was found between the G' measured at temperatures between 10 and $45^{\circ}C$ and fracture stress values. The results indicate that dynamic rheological measurements could be used as a tool for early gel quality assessment.