15$0^{\circ}C$에서 시효처리한 80Sn-20Pb 합금 도금층의 파괴특성에 전착조건이 미치는 영향 (Effects of Electrodeposition condition on the fracture characteristics of 80Sn-20Pb electrodeposits aged at 15$0^{\circ}C$)

  • 김정한;서민석;권혁상
    • 한국표면공학회지
    • /
    • 제27권5호
    • /
    • pp.292-302
    • /
    • 1994
  • Alloy deposits of 80Sn-20Pb, electroplated on Cu-based leadframe alloy from an organic sulfonate bath were aged at $150^{\circ}C$ to form intermetallic phases between substrate and deposit, and effects of the deposit morphology, influenced by deposition conditions, on the fracture resistance of the 80Sn-20Pb deposit aged at $150^{\circ}C$ were examined. The growth rate of intermetallic compound layer on aging depended on the microstructure of deposit ; it was fastest in deposit formed using pulse current in bath without grain refining additive, but slowest in deposit formed using dc current in bath containing grain refining additive in spite of similar structure with equivalent grain size. The grain refining additive incorporated in electrodeposit appears to inhibit diffusion of atoms on aging, resulting in slow growth of intermetallic layer in the thickness direction but substantial growth in the lateral one. Density of surface cracks that were occurring when samples were subjected to the $90^{\circ}$-bending test increased with increasing the thickness of intermatallic layer on aging. For the same aged samples, the surface crack density of the sample electrodeposited from a bath containing the grain refining additive was the least due to the inhibiting effect of the additive incorporated into the deposit during electrolysis on atomic diffusion.

  • PDF

TEOS와 카올린으로부터 제조한 $\beta$-Sialon의 기계적 성질 (Mechanical Properties of Beta-Sialon Ceramics Prepared from TEOS and Kaolin)

  • 임헌진;이홍림
    • 한국세라믹학회지
    • /
    • 제26권5호
    • /
    • pp.637-644
    • /
    • 1989
  • Beta-sialon powder(Z=1) was synthesized by the simultaeous reduction and nitridation of the mixed powders of Hadong kaolin and silica. Silicon hydroxide was prepared from Si-alkoxide by a hydrolysis method and amorphous silica was obtained from the calcination of the prepared silicon hydroxide. Hadong kaolin was mixed with both the silicon hydroxide and amorphous silica, respectively. The average particle size was 4${\mu}{\textrm}{m}$ and the morphology of particle was rod-like and equiaxed in the case of beta-sialon powder prepared form Hadong kaolin and silicon hydroxide(COMPOSITION A), whereas the average particle size was 3${\mu}{\textrm}{m}$ and the morphology of particle was equiaxed in the case of beta-sialon powder prepared from Hadong kaolin and amorphous silica(COMPOSITION B). The synthesized beta-sialon powders were hot-pressed at 175$0^{\circ}C$ for 2 hours under 30 MPa in a nitrogen atmosphere after YAG composition(8wt%) was added to these powders as a sintering agent. The hot-pressed specimens were annealed a 140$0^{\circ}C$ for 4 hours in a nitrogen atmosphere. The mechanical properties of sintered bodies were investigated in terms of M.O.R., fracture toughness and hardness. The measured values are as follows. COMPOSITION A : M.O.R. 508MPa, KIC 3.5MN/m3/2, hardness 13.6GPa. COMPOSITION B : M.O.R. 653MPa, KIC 5.4MN/m3/2, hardness 13.5GPa.

  • PDF

CNT가 강화된 고분자 복합체의 모폴로지에 대한 인장변형의 영향 (Effect of strain on the morphology of CNT reinforced polymer composite)

  • 국정호;곽수경;김민정;양종석;박대희;나창운
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2006년도 추계학술대회 논문집 Vol.19
    • /
    • pp.164-165
    • /
    • 2006
  • Carbon nanotube(CNT)-reinforced poly(ethylene-co-ethyl acrylate)(EEA) nanocomposites were prepared by melt mixing with a Haake internal mixer. The CNT loading was vaned from 0 to 20 wt%. The changes m CNT dispersion and shape were investigated with FE-SEM observation with and without the Tensile strain of 40%. The CNT was protruded over the fracture surface upon Tensile strain, which is a very interesting behavior.

  • PDF

EPDM계 열가소성 가황체의 형태학적 연구 (Morphology of EPDM-based Thermoplastic Vulcanizates)

  • 이상진;김영규;박성수;조원제;하창식
    • Elastomers and Composites
    • /
    • 제32권3호
    • /
    • pp.157-165
    • /
    • 1997
  • The morphology of the thermoplastic vulcanizates prepared from ethylene-propylene-diene terpolymer, polypropylene and high density polyethylene(HDPE) or ethylene based ionomer were studied. Blends were prepared in a laboratory internal mixer where EPDM was cured in the presence of PP and HDPE or ionomer under shear with dicumyl peroxide(DCP). The effects of DCP concentration and rubber/plastics composition were studied. In the morphological analysis by scanning electron microscopy (SEM), a small amount of EPDM acted as a compatibilizer to HDPE and PP. It was also revealed that the dynamic vulcanization process could reduce the domain size of the crosslinked EPDM phase. When ionomer was added to EPDM/PP blend, the thermoplastic vulcanizate showed typical ductile fracture topology and the trend was more clearly observed when DCP contents and ionomer contents are higher.

  • PDF

Al-Li-(Be)합금 주괴의 미세조직과 기계적 성질 (Microstructure and Mechanical Properties in Al-Li-(Be) Alloys.)

  • 은일상;조현기
    • 한국주조공학회지
    • /
    • 제10권5호
    • /
    • pp.417-425
    • /
    • 1990
  • The purpose of this study is to investigate the effect of Be addition on the microstructure and mechanical properties of as-cast and homogenization treated Al-Li-(Be)alloys. The ductility of as-cast Al-Li alloy was increased by the addition of Be and the fracture morphology was changed from brittle to ductile mode. Also, hardness and strength have been decreased by homogenization treatment. The morphology of eutectic structure which consists of ${\alpha}(Al)$ and ${\alpha}(Be)$ was changed from lammellae to spherical type by homogenization treatment. The shape of ${\alpha}(Be)$ phase has been revealed as hollow type by TEM observation. It consists of outer surfaces with well defined crystal facets and the core filled with ${\alpha}(Al)$. The microstructure of as-cast Al-Li-Be alloys showed coarse ${\delta}'$, fine ${\delta}'$, and coarse ${\delta}$ phases. The coarse and fine ${\delta}'$ phases were formed at Be-rich phase /matrix interfaces and in matrix, respectively. By homogenization treatment, the ${\delta}$ phase in Al-Li and Al-Li-Be alloys dissolved and the size of ${\delta}$ phase in Al-Li-Be alloys was finer than that of Al-Li alloy.

  • PDF

Investigation of Ball Size Effect on Microstructure and Thermoelectric Properties of p-type BiSbTe by Mechanical Alloying

  • Lwin, May Likha;Yoon, Sang-min;Madavali, Babu;Lee, Chul-Hee;Hong, Soon-Jik
    • 한국분말재료학회지
    • /
    • 제23권2호
    • /
    • pp.120-125
    • /
    • 2016
  • P-type ternary $Bi_{0.5}Sb_{1.5}Te_3$ alloys are fabricated via mechanical alloying (MA) and spark plasma sintering (SPS). Different ball sizes are used in the MA process, and their effect on the microstructure; hardness, and thermoelectric properties of the p-type BiSbTe alloys are investigated. The phases of milled powders and bulks are identified using an X-ray diffraction technique. The morphology of milled powders and fracture surface of compacted samples are examined using scanning electron microscopy. The morphology, phase, and grain structures of the samples are not altered by the use of different ball sizes in the MA process. Measurements of the thermoelectric (TE) transport properties including the electrical conductivity, Seebeck coefficient, and power factor are measured at temperatures of 300-400 K for samples treated by SPS. The TE properties do not depend on the ball size used in the MA process.

Influence of Solid Loading on the Granulation of 3Y-TZP Powder by Two-Fluid Spray Drying

  • Jeong, Hyeongdo;Lee, Jong Kook
    • 한국세라믹학회지
    • /
    • 제55권4호
    • /
    • pp.337-343
    • /
    • 2018
  • The influence of solid loading in the slurry composition on the morphology of 3Y-TZP granules fabricated by two-fluid spray drying was investigated for solid contents varying between 30 wt% and 50 wt%. The resulting 3Y-TZP granules showed a sphere-like shape with diameters of $40-70{\mu}m$. However, a donut-like shape and a few cracks were observed on the granule surfaces fabricated using the slurry with 50 wt% solid content. The green density after cold isostatic pressing at 200 MPa was $2.1-2.2g/cm^3$, and a homogeneous fracture surface was obtained by complete destruction of granules. After sintering at $1500^{\circ}C$ for 2 h, all specimens had relative densities of 96.2 - 98.3%. With increasing solid content, the relative density decreased from 98.3% to 96.2%, but the grain size increased from $0.3{\mu}m$ to $0.6{\mu}m$. Highly sinterable zirconia granule powder could be obtained by controlling the slurry composition.

Is the Arch Index Meaningful

  • Lung, Chi-Wen;Yang, Sai-Wei;Hsieh, Lin-Fen
    • 한국운동역학회지
    • /
    • 제19권2호
    • /
    • pp.187-196
    • /
    • 2009
  • The foot type is classified into normal, high or low arch according to either foot print or medial longitudinal arch (MLA) height. Plantar fasciitis, heel pain, Achilles tendinitis, stress fracture, metatarsalgia, knee pain, shin splint pain, and etc are common foot disorders and associate to the foot type. The purpose of this study was to evaluate several suggested bony inclination used to classified the abnormal foot and if the arch index (AI) was correlated with foot morphology. Lateral view and dorso-plantar view of radiographic images and flatbed scanner measurements obtained from 57 college students were analyzed. Results showed that AI measured in this study was higher than Caucasian Americans and European, but similar with African. The ethnic origin could influent the AI distribution. The AI provided a simple quantitative means of assessing the structure of lateral and medial longitudinal arches. The correlation coefficients of true bone height with AI could be further improved by normalized foot width rather than foot length. AI also demonstrated as a good indicator of inclination between calcaneus-fifth metatarsal (CalM5) and calcaneus-first metatarsal (CalX), it is a good means to classify the foot type.

대기플라즈마 용사법으로 제조된 열차폐코팅의 열피로특성 평가 (Thermal Fatigue Behavior of Thermal Barrier Coatings by Air Plasma Spray)

  • 이한상;김의현;이정혁
    • 대한금속재료학회지
    • /
    • 제46권6호
    • /
    • pp.363-369
    • /
    • 2008
  • Effects of top coat morphology and thickness on thermal fatigue behavior of thermal barrier coatings (TBC) were investigated in this study. Thermal fatigue tests were conducted on three coating specimens with different top coat morphology and thickness, and then the test data were compared via microstructures, cycles to failure, and fracture surfaces. In the air plasma spray specimens (APS1, APS2), top coat were 200 and $300{\mu}m$ respectively. The thickness of top coat was about $700{\mu}m$ in the perpendicular cracked specimen (PCS). Under thermal fatigue condition at $1,100^{\circ}C$, the cycles to top coat failure of APS1, APS2, and PCS were 350, 560 and 480 cycles, respectively. The cracks were initiated at the interface of top coat and thermally grown oxide (TGO) and propagated into TGO or top coat as the number of thermal fatigue cycles increased. For the PCS specimen, additive cracks were initiated and propagated at the starting points of perpendicular cracks in the top coat. Also, the thickness of TGO and the decrease of aluminium concentration in bond coat do not affect the cycles to failure.

A Study on the Effect of Petroleum Resin on Vibration Damping Characteristics of Natural Rubber Composites

  • Yun, Yu Mi;Lee, Jin Hyok;Choi, Myoung Chan;Kim, Jung Wan;Kang, Hyun Min;Bae, Jong Woo
    • Elastomers and Composites
    • /
    • 제56권4호
    • /
    • pp.201-208
    • /
    • 2021
  • In this study, the effect of petroleum resin on the mechanical strength, morphology, and vibration damping characteristics of natural rubber (NR) composites was observed. The NR composites plasticized by adding petroleum resin showed decreased hardness and mechanical properties. A morphology analysis indicated that as the amount of petroleum resin increased, carbon black aggregates (or agglomerates) observed at the fracture surface decreased, resulting in an improvement in the dispersibility. In addition, as 20 phr of petroleum resin was added, the effective damping temperature range increased by approximately 11.4%, the hysteresis loss rate increased by 15.2%, and the resilience decreased by 36.6%. Therefore, it was confirmed that the vibration damping characteristics improved with the addition of petroleum resin. This was because the rubber-filler interaction between the NR molecular chain of the NR composite and the carbon black particles improved by the addition of petroleum resin.