• 제목/요약/키워드: Fireproof furnace

검색결과 10건 처리시간 0.019초

고강도 콘크리트의 내화성능향상을 위한 합성내화보드 개발에 관한 연구 - 1 면 간이가열로 방식 - (A Study on the Development Composite Fireproof Board Type for Fire Resistance Improvement of High Strength Concrete One Side Simplicity Heating Furnace Type - One Side Simplicity Heating Furnace Type -)

  • 신재경;최진만;이성찬;문형재;김정진;박순전
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2009년도 춘계 학술대회 제21권1호
    • /
    • pp.233-234
    • /
    • 2009
  • 본 연구는 고강도 콘크리트부재의 폭렬방지 대책에서 종래의 내화피복 방법의 문제점윤 개선하고 내화재료의 내화성능향상을 위한 합성내화보드 개발에 관한 가능성을 검토하였다.

  • PDF

자연대류 열전달을 고려한 Al 용탕 보온로의 수치해석 (Numerical Analysis of Molten Aluminum Furnace Considering Natural Convective Heat Transfer)

  • 박상수;김병민
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2004년도 추계학술대회논문집
    • /
    • pp.107-110
    • /
    • 2004
  • Application of aluminum alloy has been increasing for most of industry area because aluminum has a good mechanical properties and castability, especially automotive field for weight reduction. But, Furnace industry is sluggish. The purpose of this study is numerical analysis of aluminum holding furnace for reasonableness estimation when we design for new model of furnace. The numerical simulation involving fluid flow of inside air and heat transfer to fireproof material is presented in order to improve the understanding of aluminum furnace. First of all, we are carried out numerically for the two dimensional inside convection and surface radiation heat transfer in a square enclosure. Subsequently, we are established the analysis method of aluminum furnace considering natural convective heat transfer

  • PDF

터널 풍도슬라브에 사용된 내화패널의 적용성에 관한 실험연구 (An Experimental Study on the Application of Fireproof Panel in Tunnel Duct Slab)

  • 최우진
    • 한국재난정보학회 논문집
    • /
    • 제19권2호
    • /
    • pp.262-269
    • /
    • 2023
  • 연구목적: 터널에서 발생되는 화재로 인하여 구조물의 피해를 보호하기 위해 적용되는 PSC 슬래브에 부착된 내화패널의 성능을 평가할 목적으로 내화실험을 수행하였다. 연구방법: 내화실험은 RWS 화재 이력곡선 화재시간-온도곡선을 적용하였으며, 한국건설기술연구원(KICT)의 가열로를 이용하여 내화 성능을 평가하였다. 연구결과:국제터널학회(2004)에서 제시하는 기준으로 내화성능 실험을 실시한 결과, 내화패널과 콘크리트의 접촉면에서의 최대온도는 콘크리트에 손상을 주는 한계온도(380℃) 이하였으며, 접촉면과 25mm 이격된 지점에서의 최대온도는 철근에 손상을 주는 한계온도(250℃) 이하로 측정되었다. 실험결과로부터, 내화패널이 30mm두께로 부착된 PSC 슬래브 시험체는 내화성능을 가진 것으로 평가되었다. 결론: 터널이나 지하차도에서의 화재발생시 내화패널을 부착하는 보강방법은 화재로부터 구조물을 보호할 수 있으며 향후, 내화패널이 부착된 슬래브의 정적 성능시험을 수행하고, Pull-off test와 피로실험을 실시하여 내화패널의 부착성능을 확인하는 것이 필요하다.

펄라이트를 첨가한 실리콘 고무 복합체의 내화 및 난연 특성 향상에 관한 연구 (A Study on Improvement of Fire-resistant and Flame-retardant Properties of Silicone Rubber Composites Containing Perlite)

  • 이병갑;이종혁;방대석;원종필;장일영;박우영;지광환
    • Elastomers and Composites
    • /
    • 제46권2호
    • /
    • pp.164-170
    • /
    • 2011
  • 본 연구에서는 실리콘 고무의 내열 및 내화 특성과 같은 열적 특성을 향상시키기 위해 실리콘 고무와 친환경 재료인 펄라이트를 기계적인 방법으로 혼합하여 실리콘 고무/펄라이트 복합체를 제조하였다. 다양한 분석 방법을 통하여 실리콘 고무/펄라이트 복합체의 특성은 펄라이트의 함량에 의존한다는 것을 확인하였다. 열중량 분석에서 순수한 실리콘 고무보다 실리콘 고무/펄라이트 복합체가 더 높은 온도에서 분해가 시작됨을 확인하였다. 가스 토치 시험을 통하여 펄라이트가 첨가된 복합 재료의 후면 온도가 순수한 실리콘 고무에 비하여 현저히 낮음을 알 수 있었고, RABT(Richtlinien fur die Ausstatung und den Betrieb won Stra${\beta}$entunneln) 조건에 따른 내화로 시험 그리고 탄화로 시험에서 펄라이트의 함량이 5 wt% 와 10 wt%인 복합체가 뛰어난 열적 안정성을 나타내었다. 주사전자현미경 (SEM)으로 실리콘 고무 내에서 펄라이트의 분산정도를 관찰하였다. 또한 한계산소지수(LOI)는 펄라이트의 함량에 따라 증가함을 확인하였다.

굴 패각을 골재로 사용한 내화 모르타르 바인더의 고로슬래그 치환율에 따른 강도성능에 관한 연구 (A Study on the Strength Performance According to Blast Slag Replacement of Fireproof Mortar using Oyster Shell Aggregate)

  • 허민회;정의인;김봉주
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2017년도 춘계 학술논문 발표대회
    • /
    • pp.75-76
    • /
    • 2017
  • In the case of B / a 1: 3, the intensity when the substitution rate increased to 15% showed a tendency to decrease, but it turned out that the strength increased at the substitution rate of 20%. In the case of B / a 1: 4 and 1: 5, it was found that when the substitution rate at the substitution rate of 10% was the highest and the substitution rate increased further, the strength was reduced. However, since the test body does not exist at the age of 3 days and the age of 7 days at the substitution rate of 0%, there is no specimen, so blast furnace slag binder substitution for increasing strength of refractory mortar is judged to be meaningless.

  • PDF

변전실용 몰드변압기의 난연성과 NAF S-III 소화에 관한 연구 (A Study on the Fireproof Characteristic and the Extinguishment by NAF S-III on a Molded Transformer in Substation)

  • 이수경;신효섭
    • 한국화재소방학회논문지
    • /
    • 제15권4호
    • /
    • pp.78-85
    • /
    • 2001
  • 본 논문에서는 몰드변압기의 난연성 및 NAF S-III에 의한 소화특성에 관해 연구하였다. 연구방법으로써 몰드변압기의 주재인 에폭시수지의 연소과정과 최근 청정소화약제로 사용되고 있는 NAF S-III의 소화과정을 이론적으로 고찰하였다. 또한 이의 증명을 위해 몰드변압기에 대한 연소.소화실험을 실시하였다. 실변압기를 전기실과 유사한 조건의 수평가열로에 장치하여 발화시킨 후, 이의 소화과정을 자연소화와 인위적 소화로 구분하여 관찰하였다. 발화된 변압기의 소화에는 NAF S-III계 소화약제가 분사되었다. 분사된 약제량은 연소중인 몰드변압기에 대한 소화능력을 갖춘 경제량이며, 이는 행정자치부 고시를 근거로 산출되었다. 이렇게 계산된 소화약제의 분사에 의해, 발화된 변압기는 1분만에 완전히 소화되었다. 연구 결과, 몰드변압기가 설치된 전기실의 경제적 소화약제량을 산출할 수 있었으며, 실험을 통해 몰드변압기의 난연성과 청정소화약제인 NAF S-III의 소화능력을 확인하였다. 이를 토대로 국내 전기실에 채용된 소화설비를 경제적이며, 환경보전의 목적으로 적용할 수 있는 규모를 예측할 수 있었다.

  • PDF

An experimental study on fire resistance of medical modular block

  • Kim, Hyung-Jun;Lee, Jae-Sung;Kim, Heung-Youl;Cho, Bong-Ho;Xi, Yunping;Kwon, Ki-Hyuck
    • Steel and Composite Structures
    • /
    • 제15권1호
    • /
    • pp.103-130
    • /
    • 2013
  • Fire performance and fire safety of high-rise buildings have become major concerns after the disasters of World Trade Center in the U.S. in 2001 and Windsor tower in Spain in 2005. Performance based design (PBD) approaches have been considered as a better method for fire resistance design of structures because it is capable of incorporating test results of most recent fire resistance technologies. However, there is a difficulty to evaluate fireproof performance of large structures, which have multiple structural members such as columns, slabs, and walls. The difficulty is mainly due to the limitation in the testing equipment, such as size of furnace that can be used to carry out fire tests with existing criteria like ISO 834, BS 476, and KS F 2257. In the present research, a large scale calorie meter (10 MW) was used to conduct three full scale fire tests on medical modular blocks. Average fire load of 13.99 $kg/m^2$ was used in the first test. In the second test, the weighting coefficient of 3.5 (the fire load of 50 $kg/m^2$) was used to simulate the worst fire scenario. The flashover of the medical modular block occurred at 62 minutes in the first test and 12 minutes in the second test. The heat resistance capacity of the external wall, the temperatures and deformations of the structural members satisfied the requirements of fire resistance performance of 90 minutes burning period. The total heat loads and the heat values for each test are calculated by theoretical equations. The duration of burning was predicted. The predicted results were compared with the test results, and they agree quite well.

전로용 MgO-C질 내화벽돌의 손상요인 (Wear Mechanisum of Carbon Bearing BOF Refreactories)

  • 김의훈;오영우;이철수;김종성;김종희
    • 한국세라믹학회지
    • /
    • 제23권1호
    • /
    • pp.51-59
    • /
    • 1986
  • It was the first time the MgO-C brick was developed for the lining materials in the hot spots in electric are furnace in 1972. MgO-C brick is high registant to thermal and structural spalling. Futhermore for the reason that carbon is hard to react with slag and MgO is high fireproof MgO-C brick shows a high corrosion registance to slag attack compared with conventional basic refractories. Owing to their excellent properties the use of MgO-C refractories are being developed widely in the field of shaped refractories and even in that of monolithic refractories. In this paper the oxidation of carbon the infiltration of slag into the brick texture and effects of additions were investigated. The results obtained were as follows : 1) The use of fused MgO-clinker and high purity carbon as raw materials increased the corosion registance and hot modulus of rupture of MgO-C brick. 2) As the oxidation reaction of the carbon proceeded the slag infiltrated into the brick texture. And then the slag components reacted with the MgO grains and formed low melting point compounds particulary CaO.MgO.$SiO_2$ and 3CaO.MgO.$2SiO_2$ that resulted in the wear of the brick. 3) It is recongnized the Al, Si, $B_3C$ effects on the oxidation registant properties of MgO-C brick by contribu-ting to the decrease of permeability according to the formation of $Al_4C_3$, SiC, $B_2O_3$ and the decrease of open pores relating to the formation of MgO.Al2O3, $SiO_2$, 3MgO.$B_2O_3$ at the decarbonized layer.

  • PDF

폴리프로필렌 섬유를 혼입한 폴리머 시멘트 모르타르의 폭렬특성에 관한 연구 (A Study on the Spalling Properties of Polymer Modified Cement Mortar Using Polypropylene Fiber)

  • 김민성;심상락;류동우
    • 한국건축시공학회지
    • /
    • 제20권4호
    • /
    • pp.305-311
    • /
    • 2020
  • 기존 폴리머 시멘트 모르타르(PCM)는 일반적인 시멘트 모르타르에 비해 부착강도, 휨강도, 내약품성 등의 성능을 향상시킬 수 있어 철근콘크리트(RC)구조물의 보수·보강 시 폭넓게 사용하고 있다. 하지만 PCM은 화재와 같은 고온 환경에서 폭렬발생 가능성이 높아 구조안전성에 문제를 발생시킨다. 본 연구에서는 폭렬저감 PCM 개발을 목적으로 폴리머 혼입률(2%, 4%, 6%), PP 섬유길이(6mm, 12mm, 6+12mm), PP 섬유혼입률(0.05 Vol%, 0.1 Vol%)을 실험인자로 선정하여 전기로 가열실험(600℃, 800℃)을 진행하였다. 폭렬특성을 비교분석한 결과 폴리머 혼입률이 6% 이상인 경우에는 섬유혼입에 따른 폭렬저감 효과를 기대할 수 없었다.

지하철 변전실용 진공주형형 몰드변압기의 난연성 확인에 관한 연구 (A Study on the Confirmation of non-flammabikity of the Cast Resin Mold Transformer in Subway Substation)

  • 정용기;장성규;곽희로
    • 조명전기설비학회논문지
    • /
    • 제12권2호
    • /
    • pp.99-107
    • /
    • 1998
  • 본 논문에서는 최근 사용이 증가하고 있는 몰드변압기의 난연성을 확인하기 위해 연소시험을 하였다. 먼저 지하철 변전소의 몰드변압기 설치현황과 호선 및 제작사별로 정류기용변압기와 고압배전용 변압기의 장애현황에 대하여 조사하였다. 다음으로 수평가열로내에 실제 몰드변압기의 고압 권선부를 설치하고, KSF 2257(건축구조 부분의 내화시험방법 : 1993)의 표준 가열 온도 곡선에 의해 가열하였다. 몰드변압기의 연소특성을 파악한 결과, KSF 2257 연소시험곡선에 의한 완전연소까지는 78분이 소요되었으며, 착화후 수평로 가열을 중지한 후 화염의 진행상황을 확인한 바 화염의 진행이 되지 않았으며, 자기소화특성을 나타냄으로써 몰드변압기의 난연성 및 자체 소화성을 확인할 수 있었다. 본 연구 결과 몰드변압기의 사고는 단락 및 과부하 등에 화재사고 보다는 몰드내 다른원인에 의해 사고 진전이 확대됨을 확인할 수 있었다.

  • PDF