Wear and fracture mode of ceramic tool for hardened SKD11 steel was investigated by face milling in this study. The cutting force and Acoustic Emission(AE) signal were utilized to detect the wear and fracture of ceramic tool. The following conclusions were obtained : (1) The wear and fracture modes of ceramic tool are characterized by three types: \circled1wear which has normal wear and notch wear, \circled2 wear caused by scooping on the rake face, \circled3 large fracture caused by thermal crack in the rake face. (2) The wear behaviour of ceramic tool can be detected by the increase of mean cutting force and the variation of the AE RMS voltage. (3) The catastrophic fracture of ceramic tool can be detected by the cutting force(Fz-component). (4) As the hardness of work material increased, Acoustic Emission RMS value and mean cutting force(Fz) increased linearly, but the tool life decreased.
Chip control is a major problem in automatic machining process, especially in finish turning operation. In this case, chip breaker is one of the important factors to be determined. As unbroken chips are grown. these deteriorate the surface roughness. and proces automation can not be carried out. In this study to get rid of chip curling problem while turning internal hole. optimal chip breaker is selected from the experiment. The experiment is planned with Taguchi's method that is based on the orthogonal arrary of design factors. From the response table. cutting speed, feedrate, depth of cut and tool geometry turn to be major factors affecting chip formation. Then, optimal chip breaker is selected. and this is verified as good enough for chip control from the experiment.
In order to investigate the residual stress evolution during the leveling process of hot rolled high strength coils for cold forming, the in-plane residual stress of plate sampled at SPM, rough leveler and finish leveler were measured by cutting method. Residual stress was localized near the edge of plate. As the thickness of plate was increased, the size of residual stress region was expanded. The gradient of residual stress within the plate was reduced during the leveling process. But the residual stress itself was not removed completely within the ranges of tested conditions. The exact camber of cut plate was able to be predicted by the measurement of residual stress distribution after leveling of the plate.
In order to investigate the residual stress evolution during the leveling process of hot rolled high strength coils for cold forming, the in-plane residual stress of plate sampled at SPM, rough leveler and finish leveler were measured by cutting method. Residual stress was localized near the edge of plate. As the thickness of plate was increased, the region with residual stress was expanded. The gradient of residual stress within plate was reduced during the leveling process. But the residual stress itself was not removed at the ranges of tested conditions. From the measured residual stress distribution within the plate, camber of plate cut to small width was predicted exactly within error range of experiment.
The purpose of this study was to observe the effect of dentin surface conditioners on the dentin surfaces. Freshly extracted human molars were used in this study. They were stored at $4^{\circ}C$ saline solution before experiment. The crown portions of the teeth were cut in various directions by means of wet diamond point to expose dentin which include transverse, vertical oblique, horizontal and oblique cut to the long axis (Fig. 1). Each tooth was then mounted with self curing acrylic resin in brass ring to expose the flattened dentin surfaces. Final finish was accomplished by grinding the dentin specimens with wet No. 180 and No. 600 grit silicon carbide abrasive paper until a 6.0mm in diameter on a dentin surface was exposed without pulp exposure. The specimens were divided into 9 groups according to the modes of dentin treatment procedure. The following surface treatments were applied on these preparation surfaces; Group 1: unetched (control group) after finish with No. 600 silicon carbide abrasive paper. Group 2: etched with 30% phosphoric acid for 60s Group 3: etched with 10-3 solution for 60s Group 4: Cleaned with 5% NaOCl for 30s Group 5: applied Dentin Adhesit Group 6: cleaned with 5% NaOCl followed by applying the Dentin Adhesit$^{(R)}$ Group 7: applied Photo Bond on the unetched dentin followed by applying the Photo Clearfil Bright Group 8: Etched with 30% phosphoric acid followed by applying Photo Bond and Photo Clearfil Bright Group 9: etched with 10-3 solution followed by applying Photo Bond and Photo Clearfil Bright All the specimens were stored in $37^{\circ}C$ under 50% relative humidity for 24 hours before observations. The specimens in 7, 8, and 9 group, omitting the group 1 to 6, were demineralized in 10% HCl for 10s in order to observe the resin tags. All the specimens in each group were then dried at room temperature. The dried specimens were ion coated with Eiko ion coater (Eiko-engineering Co.), and observed in Hitachi S-430 Scanning electron microscope (Hitachi, Co. Tokyo) at 15KV. The following results were obtained as follows; 1. The smear layers were still remained in group 1,2,4,5, and 6. 2. There is no effect of 5% NaOCl and 30% phosphoric acid on the changes of dentin morphology 3. The dentin treated with 10-3 solution, indicating the tubules opened when the smear layer and the dental plug dissolved. 4. In case of applying the bonding agents the resin tag was not formed at the deep area of dentinal tubules, but in case of applying the Dentin Adhesit$^{(R)}$ that was not.
Ball-end milling process is widely used in the die and mold manufacturing because of suitable one for the machining of free-form surface. During the process, the pencil cutting operation can be adopted before finish cut to eliminate overload in uncut area caused by large diameter of ball-end mill. The ball-end mill cutter for the pencil cutting is easily deflected by cutting force due to the long and thin shape, and the tool deflection in pencil cutting is one of the main reason of the machining errors in a free-form surface. The purpose of this study is to find the characteristics of deflected cutter trajectory by constructing measurement system with eddy-current sensor. It was found that the severe reduction of corner radius produced the overcut during the plane cutting. Up cutting method induced the overcut both plane and slope cutting, but down cutting one induced the undercut. From the experiments, down cutting with upward cutting path can generate the small undercut surface.
This study was designed to compare the effect of polishing on surface roughness of composite resin. We used Z100(3M) composite resin and placed the composite resin in the hole (4mm thick and 4mm in diameter) of vinyl plate and polymerized it under manufacturer's instructions. Samples were divided into 5 groups by polishing methods. Group 1 was control: resin was polymerized under glass plate, Group 2: resin was polymerized without any polishing procedure, Group 3: resin was polymerized with a polishing procedure of abrasive disc, Group 4: bonding agent was applyed in thin layer and polymerized on the polished polymerized resin surface. Group 5: resin was polymerized under transparent celluloid strip. The surface roughness of each specimen was measured with Sufacoder SEF-30D (Kosaka lab. Ltd) under 0.08mm cut off, 0.05mm/s stylus speed, ${\times}40$ horizontal magnification, ${\times}5000$ vertical magnification. The results were as follows : 1. Group 1 showed the most smooth surface in this study. 2. Group 3 showed more rough surface than Group 2. Considering the surface roughness, it would be better to make the shape completely before polymerize the resin. To finish and polish after the polymerization of resin makes less smooth surface. 3. When we use the transparent celluloid strip, minimum finishing procedures are recommended. Any polishing procedure could not recover the smooth resin surface of celluloid strip. 4. Application and polymerization of the thin layer of bonding agent on the polished surface showed the minimum surface smoothing effect.
This paper investigates the micro-cutting of cemented carbides using PCD (polycrystalline diamond) and PCBN (polycrystalline cubic boron nitride) cutting tools are performed with SEM direct observation method. The purpose of this study is to make clear the cutting mechanism of cemented carbides and the fracture of WC particles at the plastic deformation zone in orthogonal micro-cutting. And also to achieve systematic understanding, the effect of machining parameter on chip formation and machined surface was studied, including cutting speed, depth of cut and various tool rake angle. Summary of the results are shown below. (1) Three type of chip formation process have been proposed by the results of the direct observation in orthogonal micro-cutting of cemented carbide materials. (2) From the whole observation of chip formation, primary WC particles are crushed and/or fine grained in the shearing deformation zone. A part of them are observed to collide directly with a cutting edge of tool by following the micro-cutting. (3) Surface finish, surface morphology and surface integrity is good to obtain by cutting with PCD cutting tool compared with PCBN. (4) The machined surface has the best quality near the low cutting speed of 10${\mu}m$/sec with a cutting depth of 10 ${\mu}m$ using 0$^\circ$ rake angle and 3$^\circ$ flank angle in this condition, but it was found that excessively low speed, for example the extent of 1 ${\mu}m$/sec, is not good enough to select for various reason.
The characteristics of wire deflection, surface roughness and roundness were observed on changing discharge time for electrical discharge machining(EDM) of tungsten carbide in various conditions of thickness. The wire deflection was decreased as increasing discharge time and wire tension, the gap of deflection was decreased after thickness 60mm and discharge time of 6$\mu\textrm{s}$ due to the changing from fundamental mode to vibration mode. The deflection is the smallest at the water specific resistivity of 7.5 kΩ ㆍcm. The deflection is found to be decreased as increasing dwell time, and the result is due to the vibration of the pressure and the amount of the dielectric. The component of copper(Cu) and zinc(Zn), which is the main material of wire electrode, was observed for rough wire-cutting EDM of STD-11. This phenomena is found to be decreased as the number of EDM is increased. But it will be improved by changing the material and the shape of wire. The roundness of middle is found to be worse than that of upper and it is increased as the thickness of material is increased.
This paper presents an experimental investigation of high speed machining of dies and molds. Several critical issues involved with the high speed machining of QRO90 tool steel of hardness up to HRc62, have been studied and explained from a detail analysis of experimental observations. The experiments were performed using ball end mills. The effect of different process parameters on tool life and surface finish produced was also investigated. The cutting parameters involved were; cutting speeds in the range of 100 to 40 / m/min, axial depth of cut from 0.1 to 0.5mm, pick feed of 0.1 to 0.5mm. Run out and acceleration signals were observed during the experiment to investigate cutting slates. Compressed air and flood coolant were used and the effect of coolant on tool life was also determined.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.