  • The effect of consolidation temperature on the microstructure, density and mechanical properties (especially, wear property) of $Al_{92.5}-Fe_{2.5}-Cr_{2.5}-Ti_{2.5}$ alloy fabricated by gas atomization and magnetic pulsed compaction was investigated. All consolidated alloys consisted of homogeneously distributed fine-grained fcc-Al matrix and intermetallic compounds. Relative higher mechanical properties in the MPCed specimen were attributed to the retention of the nanostructure in consolidated bulk without cracks. The as consolidated bulk by magnetic pulsed compaction showed the enhanced wear properties than that of a general consolidation process. In addition, the wear mechanism and fracture mode of MPCed bulk was discussed.

  • PDF

Sintered $Fe_3Al$ Intermetallic - A New Filter Element for Hot Gas Filtration

  • Xing, Y.;Kuang, X.;Wang, F.;Kuang, C.;Fang, Y.
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part 1
    • /
    • pp.597-598
    • /
    • 2006
  • Gas filtration at high temperature from industrial processes offers various advantages such as increasing process efficiency, improving heat recovery and materials resource recovery, etc. At the same time, it is an advanced environment protection technology. This paper describes a newly developed metallic filter element. The manufacturing process of sintered $Fe_3Al$ metallic powder and the mechanical and filtration characteristics of this filter element were investigated. In this work, the phase constituent changes of the $Fe_3Al$ powder during sintering were studied. The newly developed filter elements were found to have excellent corrosion resistance, good thermal resistance, high strength and high filtration efficiency.

  • PDF

Al-9Si-0.3Mg 주조용 합금에서 Sludge 형성이 금형소착 반응층 두께에 미치는 영향 (Effect of Sludge Formation on the Thickness of Die Soldering Reaction Layer in Al-9Si-0.3Mg Casting Alloy)

  • 김헌주
    • 한국주조공학회지
    • /
    • 제30권2호
    • /
    • pp.76-82
    • /
    • 2010
  • Effect of reaction time and sludge formation on the thickness of die soldering reaction layer has been studied in Al-9Si-0.3Mg casting alloy. Ternary ${\alpha}_{bcc}-Al_8Fe_2Si$ and ${\alpha}_{hcp}-Al_8Fe_2Si$ intermetallic compounds formed at the interface of SKD61 tool steel by interaction diffusion of Al, Fe and Si atoms after 0.5hr and 6hr immersion time, respectively. Binary ${\eta}-Fe_2Al_5$ additionally formed at the interface of SKD61 tool steel after 10hr immersion time. Thickness of soldering reaction layer in die surface increased as immersion time increased from 0.5hr to 24hr. Sludge formation was ascertained in the samples which were immersed in the melts more than 10hr. Reaction of die soldering after sludge formation was more accelerated than that of before sludge formation due to a decrease in Fe content, followed by higher diffusion rate of Al in the melt by sludge formation.

열처리된 A3003 알루미늄합금 용접부의 미세조직 및 기계적 특성 (Microstructrue and Mechanical Properties of A3003 Aluminium Alloy Welds by Heat-treatment)

  • 이일천;송영종;국진선;윤동주;김병일
    • Journal of Welding and Joining
    • /
    • 제25권5호
    • /
    • pp.51-57
    • /
    • 2007
  • The present work was aimed to examine the variation of microstructure and mechanical properties by annealing($100{\sim}620^{\circ}C$, $2{\sim}8hr$) in A3003 Al alloy welded pipes. The A3003 Al alloy pipes with 34 mm in external diameter and 1.3 mm in thickness were manufactured by high frequency induction welding with the V shaped convergence angle $6.7^{\circ}$ and power input 50 kW. The tensile and yield strength decreased with increasing the annealing temperature remarkably, but elongation increased remarkably. Vickers hardness in welds decreased with increasing the annealing temperature remarkably. The primary intermetallic compound of $Al_{12}(Fe,\;Mn)_2Si$ was precipitated in welds as the same base metal. In a certain experimental condition, the welds line in A3003 alloys disappeared at $450^{\circ}C$ for 2 hr because of the same mechanical property and structure between welds and base metal.

시효처리에 따른 Ti-6Al-4Fe-0.25Si 합금의 미세조직 변화 (Microstructure Evolution of Ti-6Al-4Fe-0.25Si through Aging Heat Treatment)

  • 송용환;강주희;박찬희;김성웅;현용택;강남현;염종택
    • 대한금속재료학회지
    • /
    • 제50권7호
    • /
    • pp.477-485
    • /
    • 2012
  • The effect of aging heat treatment on microstructure evolution of the Ti-6Al-4Fe-0.25Si alloy with an initial microstructure of an elongated alpha was investigated. Aging treatments of the samples were carried out at $550^{\circ}C$ for up to 100 hours. The microstructure of the 5 hours heat-treated sample consisted of alpha grains, beta matrix and some TiFe intermetallic compounds that were precipitated from the beta matrix. Increasing the aging time to 10 hours, most of the beta matrix was decomposed to very fine alpha grains (${\sim}0.5{\mu}m$) and TiFe, and thus the volume fraction of the beta matrix was significantly decreased. EBSD analysis revealed that newly formed tertiary-alpha-grains in the vicinity of TiFe had high angle boundaries with respect to the primary and secondary alpha grains. As a result of these phase transformations during aging, the fraction of the alpha/alpha grain boundary was increased while that of the alpha/beta phase boundary was decreased.

ADC12 다이캐스팅 합금의 미세조직 및 기계적 특성에 미치는 개량 원소 첨가의 영향 (Effect of Alloying Element Addition on the Microstructure and Wear Properties of Die-casting ADC12 Alloy)

  • 강연지;윤상일;김동현;이기안
    • 소성∙가공
    • /
    • 제28권1호
    • /
    • pp.34-42
    • /
    • 2019
  • In this study, various alloying elements (Cr, Sr, Ca, Cd) were added to improve the mechanical properties of ADC12 fabricated by a die casting process. The effect of alloying elements on the microstructure and mechanical properties were investigated. The phase analysis results of the modified ADC12 alloy with conventional ADC12 alloy, showed the similar characteristics of Al matrix, Si phase, $CuAl_2$ phase and the Fe intermetallic phase. As a result of the microstructure observation, the secondary dendrite arm spacing (SDAS) was shown to have decreased after the addition of the alloying elements. The eutectic Si phase, which existed as flake form in the conventional ADC12 alloy, was modified finely as a fiber form in the modified ADC12 alloy. It was observed that the $CuAl_2$ phase as the strengthening phase was relatively finely distributed in the modified ADC12 alloy. The Fe intermetallic appeared as a Chinese script shaped $Al_6$ (Mn,Fe) which is detrimental to mechanical properties in conventional ADC12 alloy. On the other hand, in the modified ADC12 alloy, polyhedral ${\alpha}-Al_{15}Si_2$ $(Fe,Mn,Cr)_3$ was observed. The tensile properties were improved in the modified ADC12 alloy. The yield strength and tensile strength increased by 12.4% and 10.0%, respectively, in the modified ADC12 alloy, and the elongation was also seen to have been increased. As a result of the pin on disk wear test, the wear resistance properties were also improved by up to about 7% in the modified ADC12 alloy. It is noted that the wear deformation microstructures were also observed, and it was found that the fine eutectic Si and strengthening phases greatly improved abrasion resistance.

Al-Si 합금 증착 전기강판의 열확산 거동 (Thermal Diffusion behavior of Al-Si Deposited Electrical Steels)

  • 김찬욱;조기현;석한길
    • 한국표면공학회지
    • /
    • 제40권5호
    • /
    • pp.214-218
    • /
    • 2007
  • The objective of this study is to evaluate the diffusion behavior of Al and Si from a coatings in the microstucture of Fe-Si steel. Steel samples deposited with Al-Si alloy are prepared by ion plating process, followed by annealing treatments for diffusion at $1050^{\circ}C$. Several intermetallic phases are found in the coatings and they are identified as Fe-Al and an orderd Fe-Si compounds. Series of different concentration profiles through the sample have been obtained and Si content reaches about 5 wt% in case of 90 minutes of diffusion time.

공정 변수에 따른 Al 모재와 Fe계 합금 분말의 레이저 오버레이층 거동 (Effect of Process Parameters on Laser Overlay Behavior of Fe-based Alloy Powder on Aluminum Substrate)

  • 유연곤;강남현;김철희;김정한;김목순
    • Journal of Welding and Joining
    • /
    • 제25권1호
    • /
    • pp.30-36
    • /
    • 2007
  • A joining of dissimilar metal combination faces significant problems such as poor strength and cracking associated with brittle intermetallic compounds(IMC) formed. An application of laser allows low heat input; leading to less dilution and smaller heat affected zone. The $CO_2$ laser overlay was conducted on an AC2B alloy with feeding Fe-based powders. The overlay area was significantly influenced from the travel velocity rather than the powder feeding rate. The interface between the overlay and substrate consisted of the hard and brittle IMC($FeAl_3,\;Fe_3Al,\;Fe_2Al_5$), which initiating and propagating the crack. The reciprocating test for the slide wear was conducted on a multi-pass overlay experiment. Comparing with the multi-pass overlay with no overlap, the overlay with 50% overlap showed better wear resistance.

복합주조용 Al-Si-Mg합금의 미세조직 및 인장성질에 미치는 Fe 및 Cu 첨가의 영향 (Effects of Fe and Cu Addition on the Microstructure and Tensile Properties of Al-Si-Mg Alloy for Compound Casting)

  • 김정민;정기채;김채영;신제식
    • 한국주조공학회지
    • /
    • 제41권1호
    • /
    • pp.3-10
    • /
    • 2021
  • 알루미늄 합금과 주철의 복합주조 공정 중에는 주철로부터 철 성분이 용해되어 알루미늄 용탕에 혼입될 수 있으므로 다양한 Fe함유 금속간 화합물이 형성되며, 이로 인해 알루미늄 합금의 인장 특성이 크게 저하 될 수 있다. 반면 불순물로 첨가되는 Fe와 는 달리 Cu의 경우 알루미늄 합금의 기계적 물성을 향상시키기 위해 첨가되는 합금원소이다. 본 연구에서는 Fe와 Cu의 첨가로 인한 알루미늄 합금의 미세조직 및 인장특성의 변화를 조사하였다. 첨가된 Fe 함량이 1% 이상일 경우 조대한 Al5FeSi 상과 같은 Fe 함유 화합물들이 다량 형성되어 인장 특성이 현저히 감소하는 것으로 나타났다. Cu가 첨가 된 알루미늄 합금의 경우 Al2Cu 상이 추가로 형성되었으며, 인장 강도가 뚜렷하게 향상되는 결과를 보였다.