• Title/Summary/Keyword: Fe-Mn particle

Search Result 119, Processing Time 0.031 seconds

The Effect of Particle Size and Additives on the Thermoelectric Properties of P-type FeSi2 (P형 FeSi2의 열전물성에 미치는 입자크기 및 첨가물 영향)

  • Pai, Chul-Hoon
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.14 no.4
    • /
    • pp.1883-1889
    • /
    • 2013
  • Although Fe-Si based alloy has lower figure of merit than Si-Ge alloy applied for space probe, its low cost related to abundant raw material, rather simple processing, high temperature resistance and reliability up to $800^{\circ}C$ made it one of the most promising middle temperature thermoelectric generation materials. The effect of particle size and additive on the thermoelectric properties of p-$FeSi_2$ prepared by a RF inductive furnace was investigated. The electrical conductivity increased slightly with decreasing particle size and hence better grain-to-grain connectivity due to the increase of density. The Seebeck coefficient exhibited the maximum value at about 600~800K and decreased slightly with increasing particle size. This must be due to the amount of residual metallic phase ${\varepsilon}$-FeSi. $Fe_2O_3$ and/or $Fe_3O_4$-doped specimens showed the higher electrical conductivity and the lower Seebeck coefficient due to increase of the metallic phase and Si-vacancy. On the other hand, $SiO_2$-doped specimen showed the higher electrical conductivity and the higher Seebeck coefficients.

A Magnetization Study of Prussian-blue Analogue NaxMny[Fe(CN)6]

  • Minh, Nguyen Van;Phu, Phung Kim;Thuan, Nguyen Minh;Yang, In-Sang
    • Journal of Magnetics
    • /
    • v.13 no.4
    • /
    • pp.149-152
    • /
    • 2008
  • In this report, we present the results of a study on the effects of the particle size on the properties of the Prussian blue (PB) analog $Na_xMn_y[Fe(CN){_6}]$. A novel synthesis method of the $Na_xMn_y[Fe(CN){_6}]$ nano-particles using an organic solvent, formamide, is employed. The size of the PB particles is found to be 100-150 nm for the samples prepared in the formamide solvent, which is much smaller than that of the samples prepared using water only. The broadening of the X-ray diffraction peaks of the nano-sized PB samples is attributed to the lattice disorder and a dramatic reduction in the particle size. The compositions of the samples are confirmed by an energy-dispersive X-ray analysis (EDAX), and the result proves that the samples are actually $Na_xMn_y[Fe(CN){_6}]$ Prussian blue. The UV-vis spectra show a broad intervalence charge-transfer (CT) band in the visible region between 400 and 700 nm, and the absorption decreases abruptly in the green region for the nano-sized PB sample. A divergence between the field cooled (FC) and zero field cooled (ZFC) magnetization curves is observed for the nano-sized PB sample at 11 K, indicating that nanoparticles in the sample are single domain superparamagnets with a blocking temperature of 11 K. Our results reveal that the nano-sized PB samples show significantly different optical and magnetic properties than those of the bulk PB samples.

Aerosol Sampling with Two Stage Filter Sampler and Seasonal Variation of Metal Components in the Atmosphere (이단 필터 샘플러에 의한 대기 부유분진의 포집 및 금속 성분의 계절별 거동에 관한 연구)

  • Lee, Yong-Keun;Kim, Nam-Hoon;Myung, No-Seung;Whang, Kyu-Ja
    • Journal of Korean Society for Atmospheric Environment
    • /
    • v.4 no.2
    • /
    • pp.20-27
    • /
    • 1988
  • A simple two stage aerosol filter sampler which allows simultaneous and fractional collection of two different-size particles, coarse and fine, was constructed and applied to the collection of Seoul atmospheric particulate for inorganic analysis. The sampler consist of two 47-mm diameter filter holder, a pneumatic pump, and a flowmeter. Filtering rate normally runs around 20$\ell$/min for 8 hrs. Using the sampler, a series of seasonal aerosol samples were collected from June 1986 to March 1988 at Yonsei University campus, Seoul and subsequently analysed for ten environmentally important metals using an atomic absorption spectrometer and an inductively coupled plasma emission spectrometer. The analysed metals are Al, Cd, Cr, Cu, Fe, Mn, Ni, Pb, V, and Zn. The analytical results showed the following order of metal abundance; Al > Fe > Zn > Pb > Mn > Cu > V > Ni > Cr > Cd. Based upon their size distribution pattern, the analyzed matals could be clasified into two groups, those present primarily in coarse particle and those in fine particle. Fe, Al, Mn, V, and Cr belong to the former group while the rest to the latter. Most metal concentration were highest in spring or winter, and lowest in autumn. Statistical analysis showed strong correlations between Al and Fe, Pb and Zn, and Cu and Mn.

  • PDF

Synthesis and photoluminescence characteristics of SrAl2O4:Mn4+ phosphor for LED applications (LED용 SrAl2O4:Mn4+ 형광체 합성 및 발광특성 연구)

  • Byoung Su Choi;Jun Ho Lee;Sungu Hwang;Jin Kon Kim;Byeong Woo Lee;Hyun Cho
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.33 no.1
    • /
    • pp.1-16
    • /
    • 2023
  • A non-rare earth-based strontium-aluminate red light emitting phosphor was synthesized by a solid-state reaction method and the effect of synthesis temperature and Mn4+ activator concentration on the photoluminescence characteristics of the phosphor was studied. The synthesized SrAl2O4:Mn4+ phosphor showed broad band absorption characteristics in the near-ultraviolet and blue regions with peaks at wavelengths of near 330 and 460 nm, and a triple band deep red emission consisted of three peaks at near 644, 658, and 673 nm. The SrAl2O4:Mn4+ phosphor synthesized at a temperature 1600℃ and a Mn4+ activator concentration of 0.5 mol% showed the strongest PL emission intensity, and concentration quenching was observed at concentrations higher than 0.7 mol%. FE-SEM and DLS particle size distribution analysis showed that the synthesized SrAl2O4:Mn4+ phosphor had a particle size distribution of 2~6.4 ㎛ and an irregular spherical shape with an average particle size of ~4 ㎛.

A Study on the Metal Ion Components of Airborn Particulates during Yellow Sand Phenomena in Seoul (황사현상시 서울지역 대기분진의 성분에 관한 연구)

  • 신찬기;박태술;김윤신
    • Journal of environmental and Sanitary engineering
    • /
    • v.6 no.1
    • /
    • pp.47-62
    • /
    • 1991
  • Yellow Sand Phenomena was observed from April 8 th to 10 th in 1990. During this period particle was collected to investigate the chacteristics of chemical composition of particulate by High Volume Air Sampler and Andersen Air Sa~npler in Seoul. During this period the particle concentration was 350 yg/$m^3$ and the anions, cations, and metal concentrations were increased and the orders of these were $S0_4\;^{-2}>N0_3\;^->Cl^->F^-, Na^+>Ca^{+2}>NH_4\;^+>Mg^{2+}>K^+$, and Fe>Al>Si>Zn>Pb respectively. The principal source of Yellow Sand were identified soil and sea salt. Mn used by the trace element of soil, the persentage of contribution from soil was calculated to be about 81.3% for the particle increased by Yellow Sand Phenomena. Also the principal chemical compounds of particle were estimate metals(Fe, Al, Si, Zn) oxides, $CaSO_4, NaSO_4, MgSO_4, NaC1, MgCl_2$ and $(NH_4)_2SO_4$.

  • PDF

Structural Elucidation and Magnetical Properties of La0.5Ca0.5MnO3 Powders and Pellets (La0.5Ca0.5MnO3 분말과 Pellet의 구조분석 및 자기적 성질)

  • Jung, Miewon;Lee, Jiyun;Kim, Hyunjung
    • Korean Chemical Engineering Research
    • /
    • v.43 no.1
    • /
    • pp.71-75
    • /
    • 2005
  • $La_{0.5}Ca_{0.5}MnO_3$ colossal magnetoresistance (CMR) powders and pellets were synthesized by sol-gel process. The structural changes were investigated by FT-IR, CP/MAS $^{13}C$ solid state NMR spectroscopy and XRD. The particle characterization, microstructure of sintered samples, and cation composition of gel powders were studied by FE-SEM/EDS, TEM and ICP-AES. The structure refinement reveals that $La_{0.5}Ca_{0.5}MnO_3$ has orthorhombic, perovskite type unit cell. The magnetic characterizations were identified through measurement of magnetic moment by VSM.

Synthesis of Ultra Eine MnxZn1-xFe2O4(x = 0.69~0.74) Powder and Its Magnetic Properties (초미립 MnxZn1-xFe2O4(x = 0.69~0.74)분말의 제조 및 자기적 성질)

  • Kwak, Jae-Eun;Lee, Wan-Jae
    • Journal of Powder Materials
    • /
    • v.9 no.6
    • /
    • pp.449-454
    • /
    • 2002
  • $MnxZn_{1-x}Fe_2O_4$ (x=0.69~0.74) powders synthesized by the thermal decomposition of organic acid salts. The obtained powders were uniform in composition and ultra-fine particle with about 400 nm. The amount of spinel phase of these powders was about 50% in X-ray diffraction patterns. The calcination of powder was carried out at $900^{\circ}C$ for 2 hours in air. After the powders were calcined. the mean size of powder was about 500 nm and the amount of spinel phase was increased over about 65%. The maximum amount of spinel phase was about 75% in the specimen of X=0.72. The magnetic properties of calcined $Mn_{0.72}Zn_{0.28}Fe_2O_4$ powders were the best among the different among the different compositions.

Catalytic Combustion of Benzene over Perovskite-type Oxides Prepared Using Malic Acid Method (능금산법으로 제조된 페롭스카이트형 산화물에서 벤젠의 촉매연소반응)

  • Jung, Won-Young;Hong, Seong-Soo
    • Clean Technology
    • /
    • v.18 no.3
    • /
    • pp.259-264
    • /
    • 2012
  • Perovskite-type oxides were successfully prepared using malic acid method, characterized by TG/DTA, XRD, XPS, TEM and $H_2$-TPR and their catalytic activities for the combustion of benzene were determined. Almost of catalyst showed perovskite crystalline phase and 15-70 nm particle size. The $LaMnO_3$ catalysts showed the highest activity and the conversion reaches almost 100% at $350^{\circ}C$. The catalysts were modified to enhance the activity through substitution of metal into the A or B site of the perovskite oxides. In the $LaMnO_3$-type catalyst, the partial substitution of Sr into site the A-site enhanced the catalytic activity in the benzene combustion. In addition, the partial substitution of Co or Cu into site the B-site also enhanced the catalytic activity and the catalytic activity was in the order of Co > Cu > Fe in the $LaMn_{1-x}B_xO_3$ (B = Co, Fe, Cu) type catalyst.

Comparison of Metal Contents in Respirable Particulate Mass by Particle Size and Season in Seoul and Asan City (서울.아산지역 호흡성먼지의 금속함량에 관한 연구)

  • Choi, Yun-Na;Jeon, Yong-Taek;Jang, Bong-Ki;Yang, Won-Ho;Yom, Yoon-Ki;Son, Bu-Soon
    • Journal of environmental and Sanitary engineering
    • /
    • v.23 no.1
    • /
    • pp.33-48
    • /
    • 2008
  • The purpose of this study was to characterize background mass concentration of $PM_{10},\;PM_{2.5}$ and metallic composition from June 2004 to June 2005 in comparison with Seoul and Asan city. The results were as follows: 1. Annual mean of $PM_{10}$ concentrations in Seoul and Asan were $56.95({\pm}25.63){\mu}g/m^3,\;57.02({\pm}27.22){\mu}g/m^3$ respectly. 2. Annual mean of $PM_{2.5}$ concentrations in Seoul and Asan were $46.97({\pm}40.36){\mu}g/m^3,\;42.16({\pm}21.79){\mu}g/m^3$ respectly. 3. The average $PM_{2.5}/PM_{10}$ ratio was 0.82 in Seoul and 0.74 in Asan city. 4. The concentration of $PM_{10},\;PM_{2.5}$ were the highest in spring and the lowest in summer. Asan was higher than Seoul in spring and summer. 5. The results showed that average $PM_{10}$ composition order as Si>Fe>Pb>Zn>Mn in Seoul and Si>Fe>Zn>Pb>Mn in Asan. The concentration of metals in $PM_{10}$ of Seoul that Cr, Cu, Fe, Mn were high in spring and Zn was low in Fall. Fe, Mn were high in spring of Asan. 6. The results showed that average $PM_{2.5}$ composition order as Si>Pb>Fe>Zn>Mn in Seoul and Si>Fe>Pb>Zn>Cr in Asan. The concentration of metals in $PM_{2.5}$ of Seoul that Cr was high in spring. 7. The result showed that relation between Cr and Cu, Cu and Fe, Fe and Mn, Mn and Zn, Zn and Si in Seoul, Cr and Zn, Cu and Pb, Zn and Pb, Pb and Mn in Asan. The result showed that $PM_{10}$ concentration exceeding $50{\mu}g/m^3$(US-EPA Standard) and $PM_{2.5}$ concentration exceeding $15{\mu}g/m^3$(US-EPA Standard). In urban area, the monitoring of $PM_{2.5}$ permits the anthropogenic sources and the interference of natural sources with respect to $PM_{10}$ measurements.

Synthesis and Characterization of NixMn1-xFe2O4 Nanoparticles by a Reverse Micelle Process

  • Kim, Sun-Woog;Kim, Hyeon-Cheol;Kim, Jun-Seop;Kim, Hyun-Ju;Bae, Dong-Sik
    • Korean Journal of Materials Research
    • /
    • v.18 no.6
    • /
    • pp.298-301
    • /
    • 2008
  • A preparation of $Ni_xMn_{1-x}Fe_2O_4$ nanoparticles produced via the reduction of Nickel nitrate hexahydrate, Manganese (II) nitrate hexahydrate and Iron nitrate nonahydrate with hydrazine in Igepal CO-520/cyclohexane reverse micelle solutions was investigated. Transmission Electron Microscope (TEM), X-ray Diffraction (XRD) and Vibration Sample Magnetometer (VSM) analyses showed that the resultant nanoparticles increased the molar ration of water to Igepal CO-520 as the concentrations of Nickel nitrate hexahyrate, Manganese (II) nitrate hexahydrate and Iron nitrate nonahydrate increased. The average size of the synthesized particles calcined at $600^{\circ}C$ for 2hrs was in the range of 20 nm to 30 nm, and the particle distribution was broadened. The phase of the synthesized particles was crystalline, and the magnetic behavior of the synthesized particles was superparamagnetism. The effect of the synthesis parameters of the molar ratio of water to surfactant and the calcination temperature was discussed.