• 제목/요약/키워드: Fe-6.5Si

검색결과 412건 처리시간 0.025초

급속응고 Al-Si-Fe 합금의 압출거동 및 유한요소 해석 (Extrusion Behavior and Finite Element Analysis of Rapidly Solidified Al-Si-Fe Alloys)

  • 정기승
    • 한국분말재료학회지
    • /
    • 제6권1호
    • /
    • pp.56-61
    • /
    • 1999
  • The plastic deformation behaviors for powder extrusion of rapidly soildified Al-Si-Fe alloys at high temperature were investigated. During extrusion of Al-Si-Fe alloys, primary Si and intermetallic compound in matrix are broken finely. Additionally, during extrusion metastable $\delta$ phase($Al_4SiFe_2$) intermetallic compound disappears and the equilibrium $\beta$ phase($Al_5FeSi_2$) is formed. In gereral, it was diffcult to establish optimum process variables for extrusion condition through experimentation, because this was costly and time-consuming. In this paper, in order to overcome these problems, we compared the experimental results to the finite element analysis for extrusion behaviors of rapidly solidified Al-Si-Fe alloys. This ingormation is expected to assist in improving rapidly solidified Al-Si alloys extrusion operations.

  • PDF

급속응고된 Fe-6.5wt% Si 강판의 미세조직과 자기적 특성에 미치는 열처리의 영향 (Effect of Heat Treatment on Microstructures and Magnetic Properties of Rapidly Solidified Fe-6.5wt % Si sheet)

  • 황동하;이갑호;이태행;구자명
    • 열처리공학회지
    • /
    • 제8권2호
    • /
    • pp.149-154
    • /
    • 1995
  • The alloying of 6.5wt % Silicon in iron decreases the magnetization and the anisotropy and minimizes the iron loss noticeably. But it is very difficult to make thin sheets because of its poor ductility which is due to an ordering reaction (body centered cubic to CsCI type crystal structure). However the ordering reaction can be suppressed by rapid solidification method. The cooling rate of rapidly solidified Fe-6.5wt % Si alloy is about $10^3K/s$ and rapidly solidified structure are fine structure, cellular structure, dendrite and equiaxed grain from surface. The precipitates of $DO_3$ Phase emerges on $B_2$ matrix and the coercive force was 0.51 Oe (50cycle, 15KGauss) in Fe-6.5wt% Si alloy which was processed by heat treatment of $1150^{\circ}C$ for 1hr in high vacuum.

  • PDF

FeZrN/$SiO_2$ 연자성 다층 박막의 자기적 성질 (Magnetic Properties of FeZrN/$SiO_2$ Soft Magnetic Multilayer Thin Films)

  • 김택수;김종오
    • 한국재료학회지
    • /
    • 제6권11호
    • /
    • pp.1061-1066
    • /
    • 1996
  • RF magnetron reactive sputtering법으로 Fe75.5Zr8.3N16.2/SiO2(250$\AA$) 다층 박막을 FeZrN의 두께를 변화시키면서 제조하고, 제조된 박막을 진공 열처리하여 열처리 온도에 따른 포화자화, 보자력, 고주파에서의 투자율 그리고 열적 안정성을 조사하였다. Fe75.5Zr8.3N16.2/SiO2(250$\AA$) 다층박막은 FeZrN의 두께가 800$\AA$이상일 때 좋은 연자성을 나타내었다. Fe75.5Zr8.3N16.2/SiO2(250$\AA$)다층 박막을 45$0^{\circ}C$로 열처리 했을 때 포화자속밀도(1.08 T), 보자력 0.41 Oe, 1 MHz에서의 실효 투자율은 3000이상의 연자성을 나타내었다. 그 이유는 X-선 회절 분석 결과 열처리에 의해서 ZrN 미결정이 석출하여 $\alpha$-Fe 결정 성장이 억제되어 우수한 연자기적 성질이 나타난다고 판단된다. 이때 $\alpha$-Fe 입자 크기는 40-50$\AA$, ZrN의 입자 크기는 10-15$\AA$이다. 그리고 실효 투자율의 주파수 의존성에서 단층막에서는 5 MHz 이상에서 실효 투자율이 급격히 감소하는 경향을 보였으나, 다층막에서는 40MHz까지 실효 투자율이 1600이 되어 고주파에서의 연자성이 개선되었다.

  • PDF

면내 일축 이방성을 갖는 GMR 금속다층막의 형성 (Formation of GMR Metallic Multilayers with In-Plane Uniaxial Magnetic Anisotropy)

  • 송용진;김형준;이병일;주승기
    • 한국자기학회지
    • /
    • 제6권5호
    • /
    • pp.329-333
    • /
    • 1996
  • Cu/(NiFe/Ni/NiFe) 금속다층막을 Si(100), Si(111), $4^{\circ}\;tilt-cut\;Si(111)$, slide glass등의 기판 위에 형성하여 자기저항 특성 및 자기이방성을 고찰하였다. $50\;{\AA}$의 Cu를 바닥층으로 사용한 경우 $4^{\circ}\;tilt-cut\;Si(111)$ 기판 위에서 면내 일축 자기이방성을 보였으며 다른 기판 위에서는 자기이방성을 보이지 않았다. 바닥층이 없는 경우나 NiFe, Ni등을 바닥층으로 사용한 경우 $4^{\circ}\;tilt-cut\;Si(111)$ 기판 위에서 자기이방성은 나타나지 않았으며, Cu 바닥층을 증착하기 전 NiFe를 $10\;{\AA}$ 증착하고 형성한 금속다층막의 경우도 면내 자기이방성이 나타나지 않았다.

  • PDF

FeSiCr에 Fe50Ni가 첨가된 폴리머 복합 시트의 전자파 흡수 특성 (Electromagnetic Wave Absorbing Properties of FeSiCr and Fe50Ni Flaky Powder-Polymer Composite Sheet)

  • 이석문;김상문
    • 한국전기전자재료학회논문지
    • /
    • 제27권7호
    • /
    • pp.462-467
    • /
    • 2014
  • In this paper, we studied the magnetic composite sheets for electromagnetic wave noise absorber of quasi-microwave band by using soft magnetic FeSiCr and Fe50Ni flakes with the thickness of about $1{\mu}m$ and polymer. The magnetic hysteresis curve including saturation magnetization and residual magnetization and the complex permeability characteristics of the composite sheets were investigated to clarify the mixing effect on electromagnetic wave absorption properties. The saturation magnetization was decreased about 10% while the residual magnetization was increased about 15% and the real parts of complex permeability at below 500 MHz were increased 0.6~4 while those values at above 500 MHz were decreased 0.4~2.5 according to the change of contents of FeSiCr and Fe50Ni powders. As a result, the reflection loss can be moved to the lower frequency from 2~3 GHz to 1~1.5 GHz as the contents of Fe50Ni flaky powder into FeSiCr flaky powder was increased up to 50%.

Al-7Si-0.4Mg-1Fe 주조합금의 미세조직과 인장성질에 미치는 Mn, Cr 및 Sr 첨가의 영향 (Effects of Mn, Cr, and Sr Additions on the Microstructure and Tensile Properties of Al-7Si-0.4Mg-1Fe Casting Alloy)

  • 김정민;박준식;김하영;조재익;정창열
    • 한국주조공학회지
    • /
    • 제29권1호
    • /
    • pp.27-32
    • /
    • 2009
  • The microstructure of Al-7Si-0.4Mg-1Fe alloy mainly consists of aluminum dendrites, Al-Si eutectics, and $Al_5FeSi$ needles. When Mn was added to the alloy, the substantial amount of $Al_5FeSi$ phase was changed into Al(Mn,Fe)Si, however the needle-like morphology was almost unchanged. Combined additions of Cr or Sr with Mn to the base alloy resulted in rod-like Al(Mn, Fe,Si)Si phase. The tensile properties of as-cast alloys were enhanced by the Mn addition, especially when it was added with Sr. The tensile properties after T6 heat treatment was a little improved with 0.7%Mn addition, but Cr or Sr additions with Mn didn't show any positive effect on the properties of heat-treated alloys.

기공을 포함한 피로손상 알루미늄 6061-T6의 초음파 특성평가 (Ultrasonic linear and nonlinear properties of fatigued aluminium 6061-T6 with voids)

  • 강토;송성진;;박진호
    • 한국가스학회지
    • /
    • 제19권5호
    • /
    • pp.41-46
    • /
    • 2015
  • 알루미늄 6061-T6는 $Mg_2Si$${\beta}-Al_5FeSi$로 구성되며, 피로 손상도가 증가하면 ${\beta}-Al_5FeSi$주변에서 기공이 발생하고 성장하는 것으로 알려져 있다. 본 연구에서는 우선 알루미늄 6061-T6 시편에 대한 SEM 촬영을 통해 이러한 현상을 확인하였다. 이후, 피로 손상도에 따라 이 시편의 전위댐핑 (dislocation damping), 정합변형률 (coherency strain), 및 기공 (void)이 감쇠계수와 비선형인자에 미치는 영향을 실험적으로 관찰하였다. 그 결과 비선형인자는 피로 손상도가 증가에 따라 증가하다가 피로수명 75% 이후에서는 감소하는 것을 확인하였다. 이는 전위댐핑과 정합변형률이 증가할수록 비선형인자는 증가하지만, 기공이 증가하면 초음파의 산란이 커져 비선형인자가 감소하는 것으로 해석할 수 있다. 따라서, 피로에 따라 조직변화가 복잡하게 나타나는 재료의 열화 평가에 있어서는 비선형인자를 주의하여 활용하여야 한다는 결론을 얻었다.

Al2O3 + (Fe2O3, Al, Cr and Si) 소결 복합재료의 고온 부식 특성 (High-temperature corrosion properties of Al2O3 + (Fe2O3, Al, Cr and Si) mixed sintering materials)

  • 김민정;원성빈;봉성준;이동복;손인진
    • 한국표면공학회:학술대회논문집
    • /
    • 한국표면공학회 2012년도 춘계학술발표회 논문집
    • /
    • pp.170-171
    • /
    • 2012
  • $Fe_2O_3$, Al, Cr과 Si 분말을 고 에너지 볼 밀링해서 나노분말을 제조한 후 고주파유도 가열 활성 연소합성 장치로 1분 이내의 짧은 시간에 합성 및 소결한 $Al_2O_3+4.65(Fe_{0.43}Cr_{0.17}Al_{0.323}Si_{0.077})$, $Al_2O_3$ + 5.33 ($Fe_{0.375}Cr_{0.11}Al_{0.3}Si_{0.075}$), $Al_2O_3$ + 6.15 ($Fe_{0.325}Cr_{0.155}Al_{0.448}Si_{0.072}$), $Al_2O_3$ + 3.3 ($Fe_{0.6}Cr_{0.3}Al_{0.6}$) 소결체 시편을 $700^{\circ}C$의 온도에서 100시간 동안 공기 중에서 산화 및 $N_2-H_20-H_2S$ 혼합 가스 내에서 황화 부식을 실시하였다. 그 결과 산화 및 황화 부식 후에 ${\alpha}-Al_2O_3$가 표면에 생성되어 보호 피막으로 작용하여 우수한 내식성을 보였다.

  • PDF