• 제목/요약/키워드: Fatigue crack propagation ratio

검색결과 194건 처리시간 0.024초

용접방법에 따른 하중전달 십자형 필렛 용접부의 피로특성 (Fatigue Characteristics of Load Carring Cruciform Fillet Welded Joints According to Welding Methods)

  • 이용복;오병덕
    • 한국공작기계학회:학술대회논문집
    • /
    • 한국공작기계학회 2002년도 춘계학술대회 논문집
    • /
    • pp.125-133
    • /
    • 2002
  • In this study, it was investigated about endurance limit and fatigue behavior of load carrying fillet welded cruciform joints according to welding methods of SMAW, SAW, MIG and FCAW commonly using for welding structures in present. Endurance limit carried omit highly in the order of SMAW, MIG, SAW, FCAW and fatigue crack propagation ratio carried out lowly in the order of SMAW, MIG, FCAW, SAW. By these results, it is needed to use SMAW or MIG welding methods for welding structures with small welding capacity and SAW or FCAW methods for large welding structures after due consideration about economic gains and operation efficiency of welding. Fatigue crack propagation ratio is more effected by strength of welding materials than endurance limit of welding materials according to welding methods.

  • PDF

역전파신경회로망을 이용한 피로손상모델링에 관한 연구 (A Study on Fatigue Damage Modeling Using Back-Propagation Neural Networks)

  • 조석수;장득열;주원식
    • 한국자동차공학회논문집
    • /
    • 제7권6호
    • /
    • pp.258-269
    • /
    • 1999
  • It is important to evaluate fatigue damage of in-service material in respect to assure safety and remaining fatigue life in structure and mechanical components under cyclic load . Fatigue damage is represented by mathematical modelling with crack growth rate da/dN and cycle ration N/Nf and is detected by X-ray diffraction and ultrasonic wave method etc. But this is estimated generally by single parameter but influenced by many test conditions The characteristics of it indicates fatigue damage has complex fracture mechanism. Therefore, in this study we propose that back-propagation neural networks on the basis of ration of X-ray half-value breath B/Bo, fractal dimension Df and fracture mechanical parameters can construct artificial intelligent networks estimating crack growth rate da/dN and cycle ratio N/Nf without regard to stress amplitude Δ $\sigma$.

  • PDF

미소원공주위의 피로크랙발생전파 거동에 관한 연구 (Behavior of Initiation and Propagation of Fatigue Cracks around Microholes)

  • 송삼홍;오환석
    • 한국해양공학회지
    • /
    • 제1권2호
    • /
    • pp.74-82
    • /
    • 1987
  • This study has been made to investigate into the behavior of fatigue limit, of fatigue crack initiation, and of fatigue crack propagation under the condition of rotating bending stress; specifically on the independency of stress field as well as the crack behavior of surface micro hole defect, which is made artificially through the specimen. The results obtained can be summarized as followa; 1) For the single micro hole defect, initiation of fatigue crack is occurred at both tips of microhole defect simultaneosly along the slip which are produced in the range of maximum principal stress arround micro hole defect independent of the size of micro hole defect. 2) For the neighbored deuble micro hole defects with equal size, in the range ($\frac{L}{r}$)ratio $\gtrsim$ 3 defined as the size of micro hole defect(2r) to the distance between the centers of micro hole defects (2L), the crack behavior of the micro hole defects is same as single one. However, for the range of $\frac{L}{r}$<3, the interference effect becomes significant as the ratio approaches to 1.

  • PDF

혼합모드 단일과대하중 하의 피로균열 전파거동에 관한 실험적 연구 (An Experimental Study on the Fatigue Crack Propagation Behavior Under Mixed-Mode Single Overload)

  • 송삼홍;이정무;홍석표
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2003년도 춘계학술대회
    • /
    • pp.119-124
    • /
    • 2003
  • In this study, retardation behavior of fatigue crack under single overloading of the mixed mode I+II state was experimentally investigated. To produce single overload in the mixed mode I+II state, the compact tension shear (CTS) specimen and loading device were used. The propagation tests for fatigue crack were performed under mode I loading overloading afterwards. We examined the observed deformation aspects, variation of fatigue life and crack propagation rate, and the aspects of retardation behavior from tests. The retardation effect of mixed-mode single overload on fatigue crack propagation behavior was smaller than that of mode I single overload. It has been confirmed that the retardation behavior did not immediately appear and the retardation length was short when the component of mixed-mode overload was changed.

  • PDF

SS41강의 부식피로 균열 전파특성에 미치는 3.5% NaCl수용액의 영향 (The effects of 3.5% NaCl solution on the corrosion fatigue crack propagation characteristics of SS41 steel)

  • 오세욱;김재철;최영수
    • 한국해양공학회지
    • /
    • 제1권1호
    • /
    • pp.111-119
    • /
    • 1987
  • The corrosion fatigue crack propagation characteristics of SS41 steel in 3.5% NaCl solution have been evaluated for loading frequencies of 1Hz and 0.2Hz. A sine wave loading profile was used for fatigue testing. Each test was carried out at a constant stress ratio, R(0.1). The main results are summarized as follows; 1. Fatigue crack propagation rate was higher in 3.5% NaCl solution than in air, higher in the base metal than in the weld metal, and higher at f =0.2Hz than at f =1Hz. 2. The crack closure level of the base metal was not influenced by cyclic frequencies, but that of the weld metal was much influenced. 3. When the crack closure effect was eliminated in the evaluation of crack propagation characteristics by using $\Delta K_{eff}$, the envirommental influence was distinctly observed. At the base metal, crack propagation rate was enhanced by the hydrogen embrittlement, and the weld metal was reduced by the crac closure. 4. There was clearly observed hydrogen embrittlement and severely corroded aspect at fracture surface of lower frequency than that of higher frequency, and at that of base metal than that of the weld metal.

  • PDF

$2_{1/4}$ Cr-1 Mo강의 평활재상의 미소한 표면피로균열의 성장특성 (Propagation Characteristics of Fatigue Microcracks on Smooth Specimen of $2_{1/4}$ Cr-1 Mo Steel)

  • 서창민;우병철;장희락
    • 한국해양공학회지
    • /
    • 제4권2호
    • /
    • pp.100-111
    • /
    • 1990
  • In this paper, fatigue tests were carried out at stress test levels of 461 MPa, 441 MPa, and 431 MPa by using smooth specimen of$2_{1/4}$ Cr-1 Mo steel with the stress ratio(R) of 0.05. The initiation, growth and coalescense process of the major cracks and sub-cracks among the fatigue cracks on the smooth specimen are investigated and measured under each stress level at a constant cycle ratio by the replica technique with optical microscope. Some of the important results are as follows: In spite of the difference of stress levels, the major crack data gather into a small band in the curve of surface crack length and crack depth against cycle ratio N/Nf. The sub-crack data, however, deviate from the band of the major crack. The growth rates, da/dN, of major and sub-crack plotted against the stress intensity factor range, ${\Delta}K$, have the tendency to be compressed on a relatively small band. But it is more effective to predict fatigue life through major cracks. The propagation behavior of surface microcracks on the smooth specimens coincides with that of the specimen having an artificial small surface defect or through crack.

  • PDF

현가장치 STABILIZER BAR의 저온피로강도에 미치는 쇼트피닝의 영향 (Effect of Peening on Low Temperature Fatigue Strength Behavior of STABILIZER BAR in Suspension Material)

  • 정재욱;박경동
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2004년도 춘계학술대회
    • /
    • pp.353-358
    • /
    • 2004
  • We got the following characteristics from fatigue crack growth test carried out in the environment of room temperature and low temperature at $25^{circ}C$, $-60^{circ}C$, $-80^{circ}C$, and $-100^{circ}C$ in the range of stress ratio of 0.3 by means of opening mode displacement. And there is a difference between shot peened specimen and unpeened specimen. The purpose of this study is to predict the behavior of fatigue crack propagation as one of fracture mechanics on the compressive residual stress. Fatigue crack growth rate of shot peened metal was lower than that of unpeened metal. The compressive residual stress made an impact on tension and compression of the plasticity deformation in fatigue crack plasticity zone. That is. the constrained force about plasticity deformation was strengthened by resultant stress, which resulted from plasticity deformation and compressive residual stress in the process of fatigue crack propagation.

  • PDF

레이저간섭변위 게이지로 관찰한 용접재에서의 피로균열 열림거동과 피로균열 전파속도 (Fatigue crack Propagation Rate and Crack Opening behavior in Weldment Observed by Laser ISDG Method)

  • 송삼홍;김현;최진호
    • 대한기계학회논문집
    • /
    • 제19권4호
    • /
    • pp.908-917
    • /
    • 1995
  • The constant .DELTA.K fatigue tests are performed in SS41 and its weldments to investigate crack opening behavior and fatigue crack propagation behavior at each parts of weldment and its boundary layer. The weldments were annealed after welding for the purpose of relieving residual stress. Every weldments has notch at weld metal zone, and fatigue crack propagates from weld metal zone to vase metal zone perpendicular to weld line. The Laser ISDG method is used in order to determine the crack opening ratio, this method is more precise than indirect measurement method, and faster and easier than other direct measurement method.

주철의 피로전파거동에 미치는 미세조직의 영향 (The Effects of the Microstructures on the Fatigue Crack Propagation Behaviors of Cast Irons)

  • 김석원;박진성;이형철;김동건;우기도
    • 한국주조공학회지
    • /
    • 제25권1호
    • /
    • pp.16-22
    • /
    • 2005
  • This study aims to investigate the effects of the microstructures and nodule type on the fatigue characteristics of cast iron. Fatigue tests were carried out in tension-tension mode using a servo-hydraulic testing machine with load control mode operating at a frequency of 15 Hz. The tests were conducted at stress ratio R=Kmin/Kmax, of 0.1. Initial crack ${\Dalta}K$ values were highly performed with increase in tensile strength of DCI fatigue specimens. ${\Dalta}K_{th}$ region, fatigue crack propagation was primarily advanced through cell boundary and in periphery of near nodule. Fatigue crack propagation rate of D2 consisted with 2Phase(Ferrite+Pearlite) was slow due to crack closure enhanced by crack deflection and occurred crack branching. The generation of crack branch was occurred due to interaction of crack-nodule. At Threshold and Paris zone, the fractographs of the fatigue fracture surface for DCI show typical striations of a ductile fracture and isolated cleavage planes near graphite. The effect of microstructure on fatigue crack propagation of GC strongly depends on the type of flake. The generation of crack branch occurred due to interaction of crack-nodule. The fractographs of the fatigue fracture surface for GC show cleavage plane along the flake graphite.

원자로압력용기강에서 하중변수와 온도가 피로균열진전에 미치는 영향 (Effect of Loading Variables and Temperature on Fatigue Crack Propagation in SA508 Cl.3 Nuclear Pressure Vessel Steel)

  • Kim, B. S.;Lee, B. H.;Kim, I. S.
    • Nuclear Engineering and Technology
    • /
    • 제27권6호
    • /
    • pp.825-832
    • /
    • 1995
  • SA508 Cl.3 원자로 압력용기강에서 하중변수와 온도가 공기 중에서 피로 균열성장률에 미치는 영향에 대하여 조사하였다. 피로 균열성장률 시험은 12.7mm 두께의 CT(compact tension) 시편을 이용하였으며, 균열길이 추정은 컴플라이언스 방법을 사용하였다. 시험은 0.1, 0.5 하중비와 1, 10Hz의 하중주파수로 상온에서 40$0^{\circ}C$ 까지 온도를 변화시키면서 수행하였다. 12$0^{\circ}C$ 이하의 비교적 낮은 온도에서는 피로균열전파속도는 하중주파수와 온도에 영향을 받지 않았지만, 12$0^{\circ}C$이상의 경우 피로 균열성장률은 온도가 높을수록, 하중주파수가 낮을수록 증가하였다. 이러한 피로균열진전속도의 빨라짐은 균열선단에서의 산화속도의 증가로 인한것으로 생각된다. 또한 하중비의 영향으로 균열닫힘과 산화의 상호작용으로 피로 균열성장률은 상온에서 두드러졌다.

  • PDF