• Title/Summary/Keyword: External loading

Search Result 555, Processing Time 0.021 seconds

STRESS ANALYSIS OF SUPPORTING TISSUES AND IMPLANTS ACCORDING TO IMPLANT FIXTURE SHAPES AND IMPLANT-ABUTMENT CONNECTIONS (임플랜트 고정체의 형태와 연결방식에 따른 임플랜트 및 지지조직의 응력분포)

  • Han Sang-Un;Park Ha-Ok;Yang Hong-So
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.42 no.2
    • /
    • pp.226-237
    • /
    • 2004
  • Purpose: Four finite element models were constructed in the mandible having a single implant fixture connected to the first premolar-shaped superstructure, in order to evaluate how the shape of the fixture and the implant-abutment connection would influence the stress level of the supporting tissues fixtures, and prosthethic components. Material and methods : The superstructures were constructed using UCLA type abutment, ADA type III gold alloy was used to fabricate a crown and then connected to the fixture with an abutment screw. The models BRA, END , FRI, ITI were constructed from the mandible implanted with Branemark, Endopore, Frialit-2, I.T.I. systems respectively. In each model, 150 N of vertical load was placed on the central pit of an occlusal plane and 150 N of $40^{\circ}$ oblique load was placed on the buccal cusp. The displacement and stress distribution in the supporting tissues and the other components were analysed using a 2-dimensional finite element analysis . The maximum stress in each reference area was compared. Results : 1. Under $40^{\circ}$ oblique loading, the maximum stress was larger in the implant, superstructure and supporting tissue, compared to the stress pattern under vertical loading. 2. In the implant, prosthesis and supporting tissue, the maximum stress was smaller with the internal connection type (FRI) and the morse taper type (ITI) when compared to that of the external connection type (BRA & END). 3. In the superstructure and implant/abutment interface, the maximum stress was smaller with the internal connection type (FRI) and the morse taper type (ITI) when compared to that of the external connection type (BRA & END). 4. In the implant fixture, the maximum stress was smaller with the internal connection type (FRI) and the morse taper type (ITI) when compared to that of the external connection type (BRA & END). 5 The stress was more evenly distributed in the bone/implant interface through the FRI of trapezoidal step design. Especially Under $40^{\circ}$ oblique loading, The maximum stress was smallest in the bone/implant interface. 6. In the implant and superstructure and supporting tissue, the maximum stress occured at the crown loading point through the ITI. Conclusion: The stress distribution of the supporting tissue was affected by shape of a fixture and implant-abutment connection. The magnitude of maximum stress was reduced with the internal connection type (FRI) and the morse taper type (ITI) in the implant, prosthesis and supporting tissue. Trapezoidal step design of FRI showed evenly distributed the stress at the bone/implant interface.

An Experimental Study on the Strengthening Effect of RC Beam subjected to Repeated Loading during CFS Strengthening Process (탄소섬유 보강 중에 반복하중을 받은 RC보의 보강효과에 관한 실험적 연구)

  • Jang, Hee-Suk;Kim, Hee-Sung
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.10 no.1
    • /
    • pp.183-189
    • /
    • 2006
  • When RC structures are repaired or strengthened using FRP, it is required to cure for some Period under certain air temperature and then it is hopeful to avoid detrimental action caused by external vibration sources during that period. Therefore, an effect of repeated loading during Carbon Fiber Sheet(CFS) strengthening Process on the strengthening efficiency is studied through an experiment for a number of RC beams. Experimental results showed that the curing time of 24 hours without any repeated loading after CFS attachment were recommended for 1 ply strengthening, and 12 hours for 2 plies strengthening.

Cyclic behavior of extended end-plate connections with shape memory alloy bolts

  • Fanaie, Nader;Monfared, Morteza N.
    • Structural Engineering and Mechanics
    • /
    • v.60 no.3
    • /
    • pp.507-527
    • /
    • 2016
  • The use of shape memory alloys (SMAs) has been seriously considered in seismic engineering due to their capabilities, such as the ability to tolerate cyclic deformations and dissipate energy. Five 3-D extended end-plate connection models have been created, including one conventional connection and four connections with Nitinol bolts of four different prestress forces. Their cyclic behaviors have been investigated using the finite element method software ANSYS. Subsequently, the moment-rotation responses of the connections have been derived by subjecting them to cyclic loading based on SAC protocol. The results obtained in this research indicate that the conventional connections show residual deformations despite their high ductility and very good energy dissipation; therefore, they cannot be repaired after loading. However, while having good energy dissipation and high ductility, the connections equipped with Nitinol bolts have good recentering capability. Moreover, a connection with the mentioned specifications has been modeled, except that only the external bolts replaced with SMA bolts and assessed for seismic loading. The suggested connection shows high ductility, medium energy dissipation and very good recentering. The main objective of this research is to concentrate the deformations caused by cyclic loading on the connection in order to form super-elastic hinge in the connection by the deformations of the shape memory alloy bolts.

The Study on denitrification of low organic loading sewage by pre-denitrification process (유기물부하가 낮은 하수의 전달탈질공법에 의한 탈질방안)

  • Lee, Cheol Seung;Seo, Jong Hwan;Kim, Jin U
    • Journal of Environmental Science International
    • /
    • v.13 no.9
    • /
    • pp.779-878
    • /
    • 2004
  • This study was conducted to analyze the operating conditions of predenitrification process to improve the treatment efficiency in low organic loading sewage plant in use today, and to investigate the treatment efficiency of pilot plant added night soil as well as the nitrogen removal characteristics of pilot plant added carbon sources. In the operation under the condition of $BOD_{5}$ sludge load 0.03-0.28kg $BOD_{5}$/kg VSS/d and oxic ammoniac nitrogen sludge load 0.02-0.24 $kgNH_{4}^{+}$-N/kg MLVSS/d, nitrification efficiency is higher than 95%. In order to achieve 70% nitrogen removal at the T-N sludge loading 0.06kg T-N/kg VSSㆍd and the SRT 6~11 days, optimum operating factors were revealed to $CODc_{r}$/T-N ratio 9, recycle ratio 2.6, and denitrification volume ratio 0.33. At this time, denitrification capacity was approximately 0.09 kg $NO_{3}^{-}$-N/kg $CODc_{r}$; specific nitrification rate was 3.4mg $NH_{4}^{+}$-N/g MLVSS/hr; and specific denitrification rate was 4.8mg $NO_{3}^{-}$-N/g MLVSS/hr.

Vibration Fatigue for the Bogie frame of the Rubber Wheel AGT (고무차륜형 AGT 주행장치의 진동피로해석)

  • 유형선;윤성호;변상윤;편수범
    • Journal of the Korean Society for Railway
    • /
    • v.3 no.3
    • /
    • pp.117-124
    • /
    • 2000
  • The rubber wheel-type AGT has two major kinds of bogie; one is the bogie type and the other steering one. Both are important vehicular structure to support the whole running vehicle and passenger loads. This paper deals with the static analysis for the two types of bogie frame subjected to combined external forces, as well as independent ones specified in UIC 515-4. Furthermore, the dynamic analysis is performed under vibrational loading conditions so as to compare dynamic characteristics, Numerical results by using commercial packages, I-DEAS and NASTRAN show that maximum stresses do not exceed the yield strength level of material used for both bogies. From an overall viewpoint of strength, the bogie type turns out to be superior to the steering type except for the case of a lateral loading. It is also observed that the steering type shows a characteristics of low frequency behavior during a course of searching for structurally weak areas to be stiffened. The vibrational fatigue analysis for each bogie frame depends on the loading time history conditions which is applied. Time History Central Database List in the NASTRAN package. Subsequent1y, the fatigue life of bogie type is longer than the steering type.

  • PDF

Analysis of Post Weld Deformation at HAZ by External Forces Based on Inherent Strain (고유변형도 기반 열변형부의 후속 하중에 기인한 용접 후 변형 해석)

  • Kim, Jong-Tae;Ha, Yun-Sok;Jang, Chang-Doo
    • Journal of the Society of Naval Architects of Korea
    • /
    • v.43 no.2 s.146
    • /
    • pp.220-227
    • /
    • 2006
  • In case of welding, the inherent strains are generated, because a structure experiences the plastic yielding. The inherent strain is defined as the irrecoverable strain after removing structural restraints and loading. For the analysis method of welding distortion, equivalent loading method based on inherent strain is in general use due to its efficiency and effectiveness. However, it is generally difficult to know the final strain of the welded structure if additional loadings were applied after welding. for this reason, this study introduced the concept of the hardening and added the hardening term to the equivalent loading method based on inherent strain. Therefore, the purposes of this study are to develop the inherent strain formula considering the hardening effect and to calculate residual Stresses Using Proposed inherent Strain. Also, this Study Verified the availability Of proposed inherent strain method by loading-unloading experiment on welded plate.

Experimental behavior of eccentrically loaded R.C. short columns strengthened using GFRP wrapping

  • Elwan, S.K.;Rashed, A.S.
    • Structural Engineering and Mechanics
    • /
    • v.39 no.2
    • /
    • pp.207-221
    • /
    • 2011
  • This paper aims to study the behavior of short reinforced concrete columns confined with external glass Fiber Reinforced Polymers (GFRP) sheets under eccentric loads. The experimental part of the study was achieved by testing 9 specimens under eccentric compression. Three eccentricity ratios corresponding to e/t = 0, 0.10, 0.50 in one direction of the column were used. Specimens were divided into three groups. The first group was the control one without confinement. The second group was fully wrapped with GFRP laminates before loading. The third group was wrapped under loading after reaching 75% of failure loads of the control specimens. The third group was investigated in order to represent the practical case of strengthening a loaded column with FRP laminates. All specimens were loaded until failure. The results show that GFRP laminates enhances both failure load and ductility response of eccentrically loaded column. Moreover, the study also illustrates the effect of confinement on the first crack load, lateral deformation, strain in reinforcement and failure pattern. Based on the analysis of the experimental results, a simple model has been proposed to predict the improvement of load carrying capacity under different eccentricity ratios. The predicted equation takes into consideration the eccentricity to cross section depth ratio, the ultimate strength of GFRP, the thickness of wrapping laminate, and the time of wrapping (before loading and under loading). A good correlation was obtained between experimental and analytical results.

Investigations on the behaviour of corrosion damaged gravity load designed beam-column sub-assemblages under reverse cyclic loading

  • Kanchanadevi, A.;Ramanjaneyulu, K.
    • Earthquakes and Structures
    • /
    • v.16 no.2
    • /
    • pp.235-251
    • /
    • 2019
  • Corrosion of reinforcement is the greatest threat to the safety of existing reinforced concrete (RC) structures. Most of the olden structures are gravity load designed (GLD) and are seismically deficient. In present study, investigations are carried out on corrosion damaged GLD beam-column sub-assemblages under reverse cyclic loading, in order to evaluate their seismic performance. Five GLD beam-column sub-assemblage specimens comprising of i) One uncorroded ii) Two corroded iii) One uncorroded strengthened with steel bracket and haunch iv) One corroded strengthened with steel bracket and haunch, are tested under reverse cyclic loading. The performances of these specimens are assessed in terms of hysteretic behaviour, energy dissipation and strength degradation. It is noted that the nature of corrosion i.e. uniform or pitting corrosion and its location have significant influence on the behaviour of corrosion damaged GLD beam-column sub-assemblages. The corroded specimens with localised corrosion pits showed in-cyclic strength degradation. The study also reveals that external strengthening which provides an alternate force path but depends on the strength of the existing reinforcement bars, is able to mitigate the seismic risk of corroded GLD beam-column sub-assemblages to the level of control uncorroded GLD specimen.

Impact performance study of filled thin-walled tubes with PM-35 steel core

  • Kunlong Tian;Chao Zhao;Yi Zhou;Xingu Zhong;Xiong Peng;Qunyu Yang
    • Structural Engineering and Mechanics
    • /
    • v.91 no.1
    • /
    • pp.75-86
    • /
    • 2024
  • In this paper, the porous metal PM-35 is proposed as the filler material of filled thin-walled tubes (FTTs), and a series of experimental study is conducted to investigate the dynamic behavior and energy absorption performance of PM-35 filled thin-walled tubes under impact loading. Firstly, cylinder solid specimens of PM-35 steel are tested to investigate the impact mechanical behavior by using the Split Hopkinson pressure bar set (SHP); Secondly, the filled thin-walled tube specimens with different geometric parameters are designed and tested to investigate the feasibility of PM-35 steel applied in FTTs by the orthogonal test. According to the results of this research, it is concluded that PM-35 steel is with the excellent characteristics of high energy absorption capacity and low yield strength, which make it a potential filler material for FTTs. The micron-sizes pore structure of PM-35 is the main reason for the macroscopic mechanical behavior of PM-35 steel under impact loading, which makes the material to exhibit greater deformation when subjected to external forces and obviously improve the toughness of the material. In addition, PM-35 steel core-filled thin-wall tube has excellent energy absorption ability under high-speed impact, which shows great application potential in the anti-collision structure facilities of high-speed railway and maglev train. The parameter V0 is most sensitive to the energy absorption of FTT specimens under impact loading, and the sensitivity order of different variations to the energy absorption is loading speed V0>D/t>D/L. The loading efficiency of the FTT is affected by its different geometry, which is mainly determined by the sleeve material and the filling material, which are not sensitive to changes in loading speed V0, D/t and D/L parameters.

Structural Behavior of Sandwich Type GFRP Arch and Field Applicability (샌드위치형 GFRP 아치의 구조적 거동 및 현장 적용성)

  • Hwang, Dae-Won;Kim, Kwang-Woo;Kim, Yong-Seong;Yeon, Kyu-Seok
    • Journal of The Korean Society of Agricultural Engineers
    • /
    • v.60 no.2
    • /
    • pp.85-93
    • /
    • 2018
  • This study investigated the structural behavior and field applicability of sandwich type GFRP arches with polymer mortar in core. As a result, in case of crack loading and failure loading, total strains at crown were the highest; the fracture strain at crown was 0.01690, which is 4.2 times greater than the fracture strain (0.004) of cement concrete. The 3 % deflection load was 17.42 kN, the flexural strength was $163.98{\times}10^{-3}GPa$, and the flexural elastic modulus was 11.884 GPa. From load-deflection relationship up to 3.5 % deflection, 3D analysis results and experimental values were observed to be almost identical. It was considered reasonable to set a deflection rate limit to be 3 % for structural safety purpose. The standard external flexural strength of semicircular arch used in this study was approximately 2.64 times higher than that of hume pipe (2 type standard) and tripled composite pipe. The external pressure strength at fracture was approximately 1.57 times higher than that of hume pipe. It was confirmed that the implementing semicircular arch had mechanically more advantage than the circular pipe. Optimum member thickness was 8~53 mm according to arch radius of 450~1,800 mm and cover depth of 2~10 m. It was found that the larger strength could be obtained even if the thickness of member was smaller than that of concrete structure. In field application study, figures and equations were derived for obtaining applicable cover depth and optimum member thickness according to loading conditions. These would be useful data for design and manufacture of sandwich type semicircular arch.