• 제목/요약/키워드: Elevated temperature uniaxial tensile test

검색결과 5건 처리시간 0.021초

열처리된 알루미늄 6061, 7075 합금의 온간 액압 성형 적용을 위한 온도 및 변형 속도 변화에 따른 변형 특성 연구 (A study on the deformation characteristic of heat-treated 6061,7075 aluminum alloy with changes of elevated temperature and strain rate for warm hydroforming)

  • 이혜경;문영훈;손성만;이문용;서동우;이상용
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2004년도 추계학술대회논문집
    • /
    • pp.23-26
    • /
    • 2004
  • The deformation behaviors of fully annealed or T6-treated 6061 and 7075 aluminum tubes are investigated at elevated temperature using uniaxial tensile test. Fully annealed 6061 and 7075 tube, and T6-treated 7075 tube do not show sharp local necking with an elongation of $50\%$ at tensile temperature of $300^{\circ}C$, accordingly, it is expected that warm hydroforming process can be applied. The increase of tensile temperature does not significantly affect the total elongation of T6-treated 6061 tube.

  • PDF

온간액압성형공정 적용을 위한 알루미늄 6061, 7075 튜브의 열처리조건에 따른 변형특성연구 (A Study on Deformation Behaviors of Al 6061, 7075 Tube at Different Heat Treatments for Warm Hydroforming)

  • 이혜경;문영훈
    • 열처리공학회지
    • /
    • 제20권1호
    • /
    • pp.1-10
    • /
    • 2007
  • The deformation behaviors of full annealed and T6 treated 6061, 7075 aluminum tubes are investigated at various temperature performing uniaxial tensile test. Full annealed Al 6061 and Al7075 tubes, and T6 treated Al7075 tube don't show sharp local necking with an elongation of 50% at $300^{\circ}C$. So it is expected that influenced by elevated tempterature. At $300^{\circ}C$ and strain rate of 0.001/s, many micro-cracks are observed in T6 treated Al 6061 tube, which is believed to be responsible for the decrease of total elongation.

티타늄 합금판재(Ti-6Al-4V)의 고온 소성면형특성(1) (Plastic deformation characteristic of titanium alloy sheet (Ti-6Al-4V) at elevated temperature)

  • 박진기;김정한;박노광;김영석
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2009년도 춘계학술대회 논문집
    • /
    • pp.158-163
    • /
    • 2009
  • Titanium alloy sheets have excellent specific strength and corrosion resistance as well as good performance at high temperature. Recently, titanium alloys are widely employed not only aerospace parts but also bio prothesis and motorcycle. However, due to the low formability and large spring back at room temperature, titanium alloy sheets were usually formed by slow forming or hot forming with heating die and specimen. In the sheet metal forming area, FE simulation technique to optimize forming process is widely used. To achieve high accuracy FE simulation results, Identification of material properties and deformation characteristic such as yield function are very important. In this study, uniaxial tensile and biaxial tensile test of Ti-6Al-4V alloy sheet with thickness of 1.0mm were performed at elevated temperature of 873k. Biaxial tensile tests with cruciform specimen were performed until the specimen was breakdown to characterize the yield locus of Ti-6Al-4V alloy sheet. The experimental results for yield locus are compared with the theoretical predictions based on Von Mises, Hill, Logan-Hosford, and Balat's model. Among these Logan-Hosford's yield criterion well predicts the experimental results.

  • PDF

AZ31 합금의 온간 부풀림 성형시 결정립 변화에 관한 연구 (Grain Evolution during Bulge Blow forming of AZ31 Alloy)

  • 백성규;이영선;이정환;권용남
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2008년도 추계학술대회 논문집
    • /
    • pp.452-455
    • /
    • 2008
  • In the present study, blow forming characteristics of commercially roiled AZ31 alloy sheets were investigated. Two different kinds of AZ31 sheets were originally fabricated by using direct casting and strip casting methods respectively. Both sheets have similar grain sizes of about $7{\mu}m$ with a relatively equiaxed structure after rolling. A series of tensile tests were carried out to get flow behavior in terms of temperature and strain rate. Also, grain size effect was investigated by annealing as-received sheet at elevated temperatures. Elongation increased with temperature increment as well expected. However, the differences in tensile test condition did not give much difference in elongation even at the temperature range where a large elongation would be expected with such as fine grain of $7{\mu}m$. Blow forming experiments showed that forming condition did not result in higher difference in dome height. However, the interesting feature from this study was that formability of this AZ31 alloy got different with stress condition. Firstly, biaxial stress condition might result in lower temperature and strain rate dependencies compared to uniaxial tension results for both DC and SC sheets. Secondly, DC showed slower grain growth in uniaxial tension than in biaxial stress state while SC has much higher grain growth rage in uniaxial tension than in bulging.

  • PDF

온간 딮 드로잉에서 이종금속판재(STS430-Al3004-AZ31)의 파단 및 두께 예측을 위한 연구 (Prediction for Thickness and Fracture of Stainless Steel-Aluminum-Magnesium Multilayered Sheet during Warm Deep Drawing)

  • 이영선;이광석;김대용
    • 소성∙가공
    • /
    • 제21권1호
    • /
    • pp.49-57
    • /
    • 2012
  • It is difficult to estimate the properties of multilayered sheet because they are composed of one or more different materials. Plastic deformation behavior of the multilayered sheet is quite different as compared to each material individually. The deformation behavior of multilayered sheet should be investigated in order to prevent forming defects and to predict the properties of the formed part. In this study, the mechanical properties and formability of stainless steel-aluminum-magnesium multilayered sheet were investigated. The multilayered sheet needs to be deformed at an elevated temperature because of its poor formability at room temperature. Uniaxial tensile tests were performed at various temperatures and strain rates. Fracture patterns changed mainly at a temperature of $200^{\circ}C$. Uniform and total elongation of multilayered sheet increased to values greater than those of each material when deformed at $250^{\circ}C$. The limiting drawing ratio (LDR) was obtained using a circular cup deep drawing test to measure the formability of the multilayered sheet. A maximum value for the LDR of about 2 was achieved at $250^{\circ}C$, which is the appropriate forming temperature for the Mg alloy. Fracture patterns on a circular cup and thickness of formed part were predicted by a rigid-viscoplastic FEM analysis. Two kinds of modeling techniques were used to simulate deep drawing process of multilayered sheet. A single-layer FE-model, which combines the three different layers into a macroscopic single layer, predicted well the thickness distribution of the drawn cup. In contrast, the location and the time of fracture were estimated better with a multi-layer FE model, which used different material properties for each of the three layers.