Storage stability of silk solution for viscosity and electrospinnability

  • Kim, Su Jin;Um, In Chul
    • International Journal of Industrial Entomology and Biomaterials
    • /
    • 제33권2호
    • /
    • pp.138-143
    • /
    • 2016
  • In the present study, silk fibroin (SF) was dissolved in $CaCl_2/H_2O/EtOH$ solution at $85^{\circ}C$. After the dissolution, the SF solution was cooled down and stored at $4^{\circ}C$ for 28 d. The stability of the solution's viscosity and electrospinnability was observed to examine the stability of SF molecules during storage in $CaCl_2/H_2O/EtOH$ solution. The viscosities of $SF/CaCl_2/H_2O/EtOH$ solution and SF formic acid solution did not change during 28 days' storage of SF in $CaCl_2/H_2O/EtOH$ solution. The electrospinnability of the SF solution, mean diameter of the electrospun SF fiber, and crystallinity index of electrospun SF web did not change, regardless of the length of the storage period. These results imply that SF molecules do not degrade during 28 days' storage in $CaCl_2/H_2O/EtOH$ solution.

The Effect of Dissolution Condition on the Yield, Molecular Weight, and Wet- and Electro-spinnability of Regenerated Silk Fibroins Prepared by LiBr Aqueous Solution

  • Cho, Hee-Jung;Um, In-Chul
    • International Journal of Industrial Entomology and Biomaterials
    • /
    • 제20권2호
    • /
    • pp.99-105
    • /
    • 2010
  • In this paper, the regenerated silk fibroins were dissolved in LiBr aqueous solution with different dissolution temperature and time, and the effects of the dissolution condition on the regeneration yield, molecular weight, wet spinnability, and electrospinnability of regenerated silk fibroin were investigated. The regeneration yield, molecular weight distribution, and wet spinnability of regenerated silk fibroin were nearly affected by the dissolution temperature and time. However, the electrospinning performance of silk fibroin was influenced by the dissolution condition implying the electrospinning of silk fibroin is more sensitive process than the wet spinning in the range tested in this study. While $25^{\circ}C$ of dissolution temperature resulted in a good electrospinnability of regenerated silk fibroin, the electrospinnability was slightly deteriorated when silk fibroin was dissolved at $60^{\circ}C$ for 6 hours. Also, though the fiber diameters of electrospun silk fibroin produced by the dissolution at $25^{\circ}C$ for 6 hours and 24 hours were 443 and 451 nm, respectively, that at $60^{\circ}C$ for 5 min was reduced to 411 nm. The fiber diameter was more decreased to 393 nm when the dissolution time increased up to 6 hours at $60^{\circ}C$.

Electrochemical Properties of Activated Polyacrylonitrile/pitch Carbon Fibers Produced Using Electrospinning

  • Kim, Bo-Hye;Bui, Nhu-Ngoc;Yang, Kap-Seung;dela Cruz, Marilou E.;Ferraris, John P.
    • Bulletin of the Korean Chemical Society
    • /
    • 제30권9호
    • /
    • pp.1967-1972
    • /
    • 2009
  • The electrospinnability of pitch was improved by blending in a solution of polyacrylonitrile (PAN) resulting in the reduction of the average fiber diameter from 2000 to 750 nm. Activated carbon fibers (ACFs) derived by stabilization, carbonization and steam activation at 700, 800, and 900 ${^{\circ}C}$ of the PAN/pitch electrospun fibers for 60 min were investigated as electrodes for supercapacitors. The Brunauer, Emmett, Teller (BET) specific surface area ranged from 732 to 1877 $m^2g^{-1}$ and the specific capacitance from 75.5 to 143.5 $Fg^{-1}$, depending on the activation conditions. Electrodes from the electrospun web activated at 900 ${^{\circ}C}$ exhibited a particularly quick response showing a high frequency of 5.5 Hz at a phase angle of ‒$45^o$ of the impedance spectroscopy.

전기방사를 이용한 리그닌 나노섬유의 제조 (Fabrication of Lignin Nanofibers Using Electrospinning)

  • 이은실;이승신
    • 한국의류학회지
    • /
    • 제38권3호
    • /
    • pp.372-385
    • /
    • 2014
  • Lignin is an abundant natural polymer in the biosphere and second only to cellulose; however, it is under-utilized and considered a waste. In this study, lignin was fabricated into nanofibers via electrospinning. The critical parameters that affected the electrospinnability and morphology of the resulting fibers were examined with the aim to utilize lignin as a resource for a new textile material. Poly(vinyl alcohol) (PVA) was added as a carrier polymer to facilitate the fiber formation of lignin, and the electrospun fibers were deposited on polyester (PET) nonwoven substrate. Eleven lignin/PVA hybrid solutions with a different lignin to PVA mass ratio were prepared and then electrospun to find an optimum concentration. Lignin nano-fibers were electrospun under a variety of conditions such as various feed rates, needle gauges, electric voltage, and tip-to-collector distances in order to find an optimum spinning condition. We found that the optimum concentration for electrospinning was a 5wt% PVA precursor solution upon the addition of lignin with the mass ratio of PVA:lignin=1:5.6. The viscosity of the lignin/PVA hybrid solution was determined as an important parameter that affected the electrospinning process; in addition, the interrelation between the viscosity of hybrid solution and the electrospinnability was examined. The solution viscosity increased with lignin loading, but exhibited a shear thinning behavior beyond a certain concentration that resulted in needle clogging. A steep increase in viscosity was also noted when the electrospun system started to form fibers. Consequently, the viscosity range to produce bead-free lignin nanofibers was revealed. The energy dispersive X-ray analysis confirmed that lignin remained after being transformed into nanofibers. The results indicate the possibility of developing a new fiber material that utilizes biomass with resulting fibers that can be applied to various applications such as filtration to wound dressing.

멀티노즐/보조전극-Electrohydrodynamic 공정을 통한 PCL 나노파이버 제작 (Electrohydrodynamic Process Supplemented by Multiple-Nozzle and Auxiliary Electrodes for Fabricating PCL Nanofibers)

  • 윤현;김근형;김완두
    • 폴리머
    • /
    • 제32권4호
    • /
    • pp.334-339
    • /
    • 2008
  • 최근 전기방사공정은 다양한 고분자의 마이크로 및 나노 크기 섬유를 만드는 기술로서 널리 사용되어 왔다. 일반적으로 많은 연구자들에 의하면, 다중노즐 전기방사공정은 노즐들 사이의 전기장 간섭효과 때문에 짧은 시간에 높은 생산성을 갖기 어려웠다. 이러한 문제를 극복하기 위하여 본 연구에서는 다양한 보조전극을 이용한 다중노즐 전기방사공정을 개발하였다. 본 연구에서 사용된 물질은 바이오소재로서 많이 사용되고 있는 poly($\varepsilon$-carprolactone)(PCL)을 사용하였다. 다중노즐 시스템의 영향을 확인하기 위하여 전기방사의 안정성, 다중노즐을 사용하였을 때의 생산성 및 제조된 나노섬유의 크기와 안정성을 보조전극을 사용하였을 때와 사용하지 않았을 때를 비교하였다. 결과적으로 보조전극을 사용한 노즐의 안정성이 사용하지 않은 노즐에 비해 전기방사 안정성과 우수한 생산성을 보였다.

전기방사공정과 발포제를 이용한 Polycaprolactone 나노섬유 지지체 제작 (Polycaprolactone Nanofiber Mats Fabricated Using an Electrospinning Process Supplemented with a Chemical Blowing Agent)

  • 김근형;윤현;이행남;박길문
    • 폴리머
    • /
    • 제32권5호
    • /
    • pp.458-464
    • /
    • 2008
  • 생체재생용 지지체는 높은 다공구조와 적당한 기계적인 강도를 필요로 한다. 높은 다중성과 적당한 다공크기는 지지체와 주변 환경 사이에 영양분의 공급을 원활하게 하여 셀의 지지체에 대한 초기 집착력과 성장을 가능하게 하는 구조를 제공한다. 본 논문에서는 polycaprolactone(PCL) 나노섬유를 화학 발포제와 전기방사공정을 이용하여 다양한 조건하에서 제조하였다. PCL 용액의 농도가 8wt%, 발포제의 함량 0.5wt%, 발포온도 $100^{\circ}C$ 및 체류시간 2-3초에서 가공성 측면과 다공성 측면에서 우수한 발포된 나노섬유를 얻을 수 있었다. 또한 세포의 성장성을 측정하기 위하여 인체피부세포를 셀 켤츄어링하여, 발포되지 않은 나노섬유와 비교하였다.