• 제목/요약/키워드: Electron probe micro-analyzer

검색결과 69건 처리시간 0.029초

열처리 조건에 따른 Tb이온의 확산 및 Nd-Fe-B 자석의 자기적 특성 (Inward Diffusion of Tb Ions and the Magnetic Properties of the Nd-Fe-B Magnets)

  • 오성욱;김동환;공군승;허영우;김정주;이준형
    • 한국전기전자재료학회논문지
    • /
    • 제30권1호
    • /
    • pp.27-31
    • /
    • 2017
  • In this study, the effect of Tb inward diffusion on the magnetic properties of the Nd-Fe-B sintered magnets was studied. After sintering of the magnets, $TbF_3$ slurries were dip-coated on the surface of the samples, then heat-treatment was followed for $TbF_3$ diffusion. The element distribution in the magnets and the diffusion profiles of Tb ions were analyzed by an EPMA (electron probe micro-analyzer). Prolonged heat treatment resulted in a deeper diffusion length of Tb ions. Coercivity of the $1^{st}$ heat-treated sample showed 21.86 kOe, while that of the $1^{st}$, $2^{nd}$ heat-treated and annealed sample revealed 34 kOe.

초기 한국 유화의 과학적 조사-동경예술대학 예술자료관 소장 유화 자화상을 중심으로 (An essay on the Korean early oil painting of self-portrait in the museum of Tokyo National Univerity of Fine Arts and Music)

  • 김지희
    • 보존과학연구
    • /
    • 통권15호
    • /
    • pp.59-103
    • /
    • 1994
  • Painting is well regarded as a stratified structure by the conservators and restorers. Hence, the scientific methods have been developed for the study of the interal layer of paintings. Examples of such methods are X-ray, infra-red, and ultra-violet photography. A more direct method is to look at the painting in cross section under the microscope and to analyze pigments using an electron probe X-ray micro analyzer(EPMA).In this research, I study and analyze twenty two Korean paintings of self-portraits including the first oil painting of Hui Dong Koh's self-portrait stored in the museum of Tokyo National University of Fine Arts and Music, employing these scientific techniques. The small fragments taken from the ground layers of the early oil paintings(1915∼1942)are analyzed using the EPMA. According to their main materials, the ground layers can be classified into five types ; 1. Lead white layer and double layer of calcium carbonate and lead white, 2. Zinc white with some mixiture of lead white, 3.Titanium white with some barium white, 4. Barium white, 5.Double layer of titanium white and zinc white.

  • PDF

방탄소재 활용을 위한 SLS 유리의 이온교환 효과 (Effect of SLS Glass for Bulletproof Materials by Ion Exchange Technique)

  • 김태윤;심규인;최세영
    • 한국군사과학기술학회지
    • /
    • 제13권1호
    • /
    • pp.114-119
    • /
    • 2010
  • There are a number of studies on chemically strengthened glass. Most of them are strengthened in molten salt bath below transformation range of glass. This research is distinguished from the aforementioned studies in that single $KNO_3$ powder was used by employing screen printing technique. In this study soda-lime-silicate(SLS) glasses for bulletproof glass application with various thicknesses were used. The maximum value of the bending strength is 791MPa heat treated at $480^{\circ}C$, which is about 4.3 times higher than the parent glass, which is the highest strength of all soda-lime glasses. In this study, it is also observed that Vickers hardness increased to $657H_v$, which is about 15% higher than the parent glass($568.7H_v$) and fracture toughness was not changed. Depth profiles measured by electron probe micro analyzer(EPMA) showed a correlation between the migrations of $K^+$ ions with bending strength of ion exchanged glasses.

A Study on the Crystalline Boron Analysis in CRUD in Spent Fuel Cladding Using EPMA X-ray Images

  • Jung, Yang Hong;Baik, Seung-Je;Jin, Young-Gwan
    • Corrosion Science and Technology
    • /
    • 제19권1호
    • /
    • pp.1-7
    • /
    • 2020
  • Chalk River Unidentified Deposits (CRUDs) were collected from the Korean pressurized water reactor (PWR) plant (A, B, and C) where the axial offset anomaly (AOA) occurred. AOA, also known as a CRUD-induced power shift, is one of the key issues in maintaining stable PWR plant operations. CRUDs were sampled from spent nuclear fuel rods and analyzed using an electron probe micro-analyzer (EPMA). This paper describes the characteristics of boron-deposits from the CRUDs sampled from twice-burnt assemblies from the Korean PWR. The primary coolant of a PWR contains boron and lithium. It is known that boron deposition occurs in a thick CRUD layer under substantial sub-cooled nucleate boiling (SNB). The results of this study are summarized as follows. Boron was not found at the locations where the existence was confirmed in simulated CRUDs, in other words, the cladding and CRUD boundaries. Nevertheless, we clearly observed the presence of boron and confirmed that boron existed as a lump in crystalline form. In addition, the study confirmed that CRUD existed in a crystal form with a unique size of about 10 ㎛.

전기장에 의한 $Cs^+-Na^+$ 이온교환으로 제작된 유리 광도파로 (Glass optical waveguides made by electric-field-assisted $Cs^+-Na^+$ ion exchange)

  • 김영철;원영희;조두진
    • 한국광학회지
    • /
    • 제9권2호
    • /
    • pp.86-91
    • /
    • 1998
  • 소오다 석회유리를 기판으로 하고 전기장에 의한 $Cs^+-Na^+$ 이온교환으로 다중 모우드 평면 광도파로를 제작하였다. 광도파로의 각 모우드들에 대한 실효굴절률을 측정하였으며 변형 Fermi 함수 모양으로 맞춤한 굴절률 분포형태를 전자 현미분석기로 얻은 농도분포형태와 비교분석하여 설명하였다. 정량적인 분석결과 약 90%의 $Na^+$이온이 $Cs^+$이온으로 치환되었다. 주어진 인가전기장, 확산온도 및 확산시간으로부터 광도파로 깊이, 이동도 및 굴절률 변화를 구하는 식을 세웠다. 이 식에서 성립하는 광도파로의 깊이와 확산시간의 제곱근 사이의 선형관계 및 광도파로의 깊이와 인가전기장 사이의 선형관계를 실험으로 확인하였다.

  • PDF

WC-Co/Cu/SM45C강접합에 미세조직 및 접합강도에 미치는 냉각속도의 영향 (Effects of cooling rate on Microstructure and Bond Strength in WC-Co/Cu/SM45C steel joint)

  • 정승부;양훈모
    • Journal of Welding and Joining
    • /
    • 제17권2호
    • /
    • pp.104-111
    • /
    • 1999
  • The interfacial microstructure and bond strength were examined for WC-Co/Cu/SM45C steel join using a nickel-plated copper in vacuum at 1323K for 0.6ks∼3.6ks. After bonding, microstructure in bonding interface was observed by OM(Optical Microscopy), SEM(Scanning Electron Microscopy) and EPMA(Eelectron Probe Micro Analyzer). The oil cooling was carried out at 353K, the cooling rate in air and furnace was 22K/s and 4.4K/s. respectively. It was found that dendritic widths increased with the content of cobalt and bonding times at 1323K. As a whole, bond strength values at the same bonding condition decreased in this order: WC-13wt.%Co/SM45Csteel. WC-8wt.%Co/SM45Csteel and WC-4wt.%Co/SM45Csteel. The bond strength of WC-13wt.%Co/S45C steel joint in oil cooling was 273MPa. This value was greatly higher than those of 125MPa in furnace cooling and 93MPa in air cooling at 1323K for 0.6ks. The bond strength values were found to be closely associated with the content of cobalt in WC-Co and cooling rate.

  • PDF

Investigation of Pellet-Clad Mechanical Interaction in Failed Spent PWR Fuel

  • Jung, Yang Hong;Baik, Seung Je
    • Corrosion Science and Technology
    • /
    • 제18권5호
    • /
    • pp.175-181
    • /
    • 2019
  • A failed spent fuel rod with 53,000 MWd/tU from a nuclear power plant was characterized, and the fission products and oxygen layer in the pellet-clad mechanical interaction region were observed using an EPMA (Electron Probe Micro-Analyzer). A sound fuel rod burned under similar conditions was used to compare and analyze, the results of the failed fuel rod. In the failed fuel rod, the oxide layer represented $10{\mu}m$ of the boundary of the cladding, and $35{\mu}m$ of the region outside the cladding. By comparison, in the sound fuel rod, the oxide layer was $8{\mu}m$, observed in the cladding boundary region. The cladding inner surface corrosion and the resulting fuel-cladding bonding were investigated using an EPMA. Zirconium existed in the bonding layer of the (U, Zr)O compound beyond the pellet cladding interaction gap of $20{\mu}m$, and composition of UZr2O3 was observed in the failed fuel rod. This paper presents the results of the EPMA examination of a spent fuel specimen, and a technique to analyze fission products in the pellet-clad mechanical interaction region.

법랑질 표면의 탈회 및 재광화 후 EPMA (electron probe micro-analysis)를 이용한 칼슘, 인, 불소 변화의 정량적 분석 (A QUANTITATIVE STUDY OF THE CHANCE OF CALCIUM, PHOSPHATE, FLUORIDE USING EPMA AFTER IN VITRO DEMINERALIZATION AND REMINERALIZATION OF HUMAN TOOTH ENAMEL)

  • 홍경식;허복;이찬영;금기연
    • Restorative Dentistry and Endodontics
    • /
    • 제26권5호
    • /
    • pp.372-378
    • /
    • 2001
  • The aim of this in vitro study was to analyze the composition of human tooth enamel in terms of three components, Ca, P, and F after demineralization and remineralization in acid buffer solution. A total of 8 human premolars without any defects and cracks were selected and buccal and lingual sides of the teeth were cleaned with an ultrasonic device and pumice without fluoride 5$\times$5mm windows were opened, and other areas were completely covered with 3-coats of nail varnish to prevent from being in contact with demineralized and remineralized solutions. After demineralization process, each tooth was sectioned into two slices, highly polished one of them with$\gamma$-alumina, and then analyzed the composition of the demineralized tooth with EPMA(electron probe micro-analyzer). The other slices were put into the remineralized solution for 10 days, polished, and analyzed in the same manner. These data were statistically analyzed with one sample t-test(p<0.05). The results were as follows. 1. Normal tooth enamel consists of 49.76% Ca, 39.80% P, and 0.28% F. 2. After demineralization, percentage of Ca and P ratio were decreased by about 5.57 and 5.07% respectively. Percentage of F ratio was also decreased by about 0.01%, which was not statistically significant. 3. After remineralization, percentage of Ca, P increased about by 4.47 and 4.35% respectively Percentage of F decreased by about 0.01%, which was not statistically significant. In conclusion, remineralized solution used in our study has the potential to induce the uptake the Ca and P into the pore sites of the demineralized enamel. But, in the oral cavity. there were rapid temperature change, organic matrix that inhibits the movement of the ions, and limitation of continuous contact with this remineralized solution. Therefore, further in vivo study is necessary.

  • PDF

Al 합금과 STD61강의 소착에 미치는 첨가원소 Fe, Mn의 영향 (Effects of Fe, Mn Contents on the Al Alloys and STD61 Steel Die Soldering)

  • 김유미;홍성길;최세원;김영찬;강창석
    • 한국재료학회지
    • /
    • 제22권4호
    • /
    • pp.169-173
    • /
    • 2012
  • Recently, various attempts to produce a heat sink made of Al 6xxx alloys have been carried out using die-casting. In order to apply die-casting, the Al alloys should be verified for die-soldering ability with die steel. It is generally well known that both Fe and Mn contents have effects on decreasing die soldering, especially with aluminum alloys containing substantial amounts of Si. However, die soldering has not been widely studied for the low Si aluminum (1.0~2.0wt%) alloys. Therefore, in this study, an investigation was performed to consider how the soldering phenomena were affected by Fe and Mn contents in low Si aluminum alloys. Each aluminum alloy was melted and held at $680^{\circ}C$. Then, STD61 substrate was dipped for 2 hr in the melt. The specimens, which were air cooled, were observed using a scanning electron microscope and were line analyzed by an electron probe micro analyzer. The SEM results of the dipping soldering test showed an Al-Fe inter-metallic layer in the microstructure. With increasing Fe content up to 0.35%, the Al-Fe inter-metallic layer became thicker. In Al-1.0%Si alloy, the additional content of Mn also increased the thickness of the inter-metallic layer compared to that in the alloy without Mn. In addition, EPMA analysis showed that Al-Fe inter-metallic compounds such as $Al_2Fe$, $Al_3Fe$, and $Al_5Fe_2$ formed in the die soldering layers.

Sn-3Ag-0.5Cu Solder에 대한 무전해 Ni-P층의 P함량에 따른 특성 연구 (A Study of Properties of Sn-3Ag-0.5Cu Solder Based on Phosphorous Content of Electroless Ni-P Layer)

  • 신안섭;옥대율;정기호;김민주;박창식;공진호;허철호
    • 한국전기전자재료학회논문지
    • /
    • 제23권6호
    • /
    • pp.481-486
    • /
    • 2010
  • ENIG (electroless Ni immersion gold) is one of surface finishing which has been most widely used in fine pitch SMT (surface mount technology) and BGA (ball grid array) packaging process. The reliability for package bondability is mainly affected by interfacial reaction between solder and surface finishing. Since the behavior of IMC (intermetallic compound), or the interfacial reaction between Ni and solder, affects to some product reliabilities such as solderability and bondability, understanding behavior of IMC should be important issue. Thus, we studied the properties of ENIG with P contents (9 wt% and 13 wt%), where the P contents is one of main factors in formation of IMC layer. The effect of P content was discussed using the results obtained from FE-SEM(field-emission scanning electron microscope), EPMA(electron probe micro analyzer), EDS(energy dispersive spectroscopy) and Dual-FIB(focused ion beam). Especially, we observed needle type irregular IMC layer with decreasing Ni contents under high P contents (13 wt%). Also, we found how IMC layer affects to bondability with forming continuous Kirkendall voids and thick P-rich layer.