Four diamond films were deposited by the microwave plasma assisted chemical vapor deposition method varying CH4 concentration from 2.5 to 10% in the feeding gases. Thermal conductivity was measured on these free standing films by the steady state method from 80 K to 400K. They showed higher thermal conductivity as the film deposited with lower methane concentration. One exception, 7.79% methane concentration deposited film, was observed to be the highest thermal conductivity. Phonon scattering processes were considered to analyze the thermal conductivity with the full Callaway model. The grain size and the concentration of the extended and the point defects were used as the fitting parameters. Microstructure of diamond films was investigated with the scanning electron microscopy and Raman spectroscopy.
[ $Li[Ni_{0.8}Co_{0.15}Al_{0.05}]O_2$ ]cathode material for lithium secondary battery is obtained using co-precipitation method. To determine the optimal metal solution concentration value, the CSTR coprecipitation was carried out at various concentration values(1-2 mol/L). The surface morphology of coated samples was characterization by SEM(scanning electron microscope) and XRD (X-Ray Diffraction)analyses. Impedance analysis and cyclic voltammogram presented that internal resistance of the cell was dependent upon the concentration of metal solution. such data is very helpful in determining the optimal content of metal solution concentration to enhancing electrochemical property by adjusting powder size distribution and crystal structure.
This research was conducted to determine the effects of chitosanoligosaccharide on liver poisoning induced by cadmium (Cd). Three groups of mice were used in this research. The group was only injected with cadmium (5.0 mg/kg; i.p.) (group Cd) and the other group was injected with cadmium and chitosanoligosaccharide (0.5% solution) at the same time (group Cd+Chi). In order to investigate the inhibitory action of chitosanoligosaccharide on liver damage, cadmium concentration in liver tissues and metallothionein (MT) concentration were relatively measured. In addition, histological observations were made to determine the morphologic injury of liver tissues. Cadmium concentration in liver tissues was drastically lower in groups Cd+Chi than in group Cd. MT concentration in liver tissues was lower in group Cd than in groups Cd+Chi. As the result of electron microscopic observation, mitochondria in group Cd showed a severe swelling phenomenon, RER fragment and ribosome dropout. However, in groups Cd+Chi, mitochondria with high electron density were distributed and RER forming a typical lamellae with ribosome was observed. From these results, cadmium toxicity on rat liver tissues could be lessened by chitosanoligosaccharide.
Seo, Hyun-Seung;Park, Mi-Ju;Choi, Eun-Chang;Lee, Sung-Uk;Kim, Hyung-Jin;Hong, Byung-You
Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
/
2008.11a
/
pp.435-436
/
2008
Dye-sensitized Solar Cells(DSSCs) which convert incident sun light into electricity were expected to overcome global warming and depletion of fossil fuels. And it is one of study that is lately getting into the spotlight because manufacturing method is more simple and inexpensive than existing silicon solar cells. In this respect, DSSCs are in the limelight as the next generation solar cells. DSSCs are generally composed of a dye-modified $TiO_2$ photoelectrode, a Pt counter electrode, and an electrolytes containing a redox couple$(I^-/I_3^-)$. Among these elements, pt electrode were prepared by applying electric potential to FTO substrate in the $H_2PtCl_6$ solution. In this study, we report the solar cell efficiency depending on $PtCl_4$ concentration change. $PtCl_4$ concentration was 1mM, 5mM, 10mM, and 20mM, and adhered on FTO glass substrate by sintering process. When applied each $PtCl_4$ counter electrode on DSSC, the best efficiency was found at 10mM of $PtCl_4$ concentration. The catalyst promotes the movement of electron from the counter electrode to the electrolyte the higher the molarity, the better the efficiency. However, in case of 20mM, it is estimated that over-deposited $PtCl_4$ tends to restrict the movement of electron due to its bundle formation.
Hydroxyapatite[COL] nanocomposite was prepared through coprecipitation process. The chemical bond formation between HAP and COL was confirmed by diffusive reflectance FT-IR and TEM observation. Higher concentration of COL in the preparation induced tiny nanocrystalline composite particles, but lower concentration of COL contributed to form the well developed HAP particles. From TEM observation and ED(Electron Diffraction) pattern the embedded HAP nanoparticles were oriented along the c-axis of COL fiber. In an aqueous system of constant [Ca$\^$2+/] and [PO$_4$$\^$3-/], quantity of soluble COL matrix was doing an important role of controlling the heterogeneous nucleation site for the formation of HAP nanocrystals. Higher concentration of COL will provide more nucleation sites for Ca$\^$2+/ and so the concentration of calcium ions for the total number of active nucleation sites will be getting relatively dilute.
Journal of the Microelectronics and Packaging Society
/
v.28
no.4
/
pp.79-83
/
2021
In this study, hollow silica microspheres (HSM) of various sizes formed according to the concentration of surfactants using water glass as a precursor, which is advantageous for commercialization due to its lower unit cost compared to conventional silicon alkoxide (tetraethyl orthosilicate, TEOS) was synthesized. The physical properties of the silica hollow microspheres according to the concentration of surfactant were analyzed using Fourier transform infrared, contact angle measurement, Brunauer-Emmett-Teller and Barrett-Joyner-Halenda analyzers and field emission scanning electron microscopy. When porous water glass-based hollow silica spheres were prepared by adding a surfactant at an appropriate concentration, it was confirmed that excellent hollow silica spheres were formed with a specific surface area of 169 m2/g, an average particle size of 25.3 ㎛, and a standard deviation of 6.25.
Journal of the Korean Institute of Telematics and Electronics
/
v.20
no.2
/
pp.1-6
/
1983
The reduction of threshold voltage and punchthrough voltage of short channel MOS transistors has been measured experimentally with silicon gate NMOS transistors. The effects of the gate oxide thickness and substrate doping concentration on the threshold voltage and punch-through voltage have also been measured with sample devices with boron implantation and gate oxide thickness of 50 nm and 70 nm. Hot electron emission has been measured by floating gate method for the samples with 3 ${\mu}{\textrm}{m}$ channel length. It has been concluded from this measurement that hot electron emission is not significant for the channel length of 3${\mu}{\textrm}{m}$.
Kim, Gyeong-Nam;Jeong, Ha-Gyun;Park, Hui-Dong;Kim, Do-Jin
Korean Journal of Materials Research
/
v.11
no.9
/
pp.759-762
/
2001
Mg$_2$SnO$_4$having an inverse spinel structure was selected as a new host material of $Mn^{2+}$ activator. The luminescence of the $Mg_2$SnO$_4$:Mn phosphor prepared by the solid-state reaction were investigated under ultraviolet and low-voltage electron excitation. The Mn-doped magnesium tin oxide exhibited strong green emission with the spectrum centered at 500nm wavelength. It was explained that the green emission in $Mg_2$SnO$_4$:Mn phosphor is due to energy transfer from $^4T_1to ^6A_1\;of\; Mn^{2+}$ ion at tetrahedral site in the spinel structure. The optimum concentration of $Mn^{2+}$/ion exhibiting maximum emission intensity by the low-voltage electron excitation was 0.6mol%. ?
Radiation treatment with gamma-rays and electron-beams was used to remove polyvinyl alcohol(PVA), one of the main components of dyeing wastewater. PVA was effectively decomposed by radiation treatment, thus the removal was near 100 % at an initial PVA concentration of 44 mg/L. However, total organic carbon(TOC) removal was less than 5 % due to lower transformation of PVA to $CO_2$. This directly indicates the radiation treatment alone is not appropriate for the complete decomposition of PVA. In this sense, the improvement of biodegradability($BOD_5/COD$) of PVA by radiation treatment was studied. Both gamma-ray and electron-beam treatments significantly increased the biodegradability of PVA by transforming non-biodegradable PVA to biodegradable by-products. This suggests radiation treatment, especially electron-beam treatment that showed better improvement of biodegradability, can be used as a pre-treatment of biological degradation process of PVA.
The growth of Au films grown on a Si(100)-2x1 surface and Si films on a Ge(100)-2x1 substrate is studied using Positron-annihilation induced Auger Electron Spectroscopy(PAES), Electron induced Auger Electron Spectroscopy(EAES), and Low Energy Electron Diffraction(LEED). Previous work has shown that PAES is almost exclusively sensitive to the top-most atomic layer due to the trapping of positrons in an image potential well just outside the surface before annihilation. This surface specificity is exploited to profile the surface atomic concentrations during the growth of Au on Si(100) and Si on Ge(100) and EAES provides concentrations averaged over the top 3-10 atomic layers simultaneously. The difference in the probe-depth makes us possible to use PAES and EAES in a complementary fashion to estimate the surface and near surface concentration profiles. The results show that (i) the intermixing of Au and Si atoms occurs during the room temperature deposition, (ii) the segregated Ge layer is observed onto the Si layers deposited at 300k. In addition, the prior adsorption of hydrogen prevents the segregation of Ge on top of the deposited Si and that the hydrogen adsorption is useful in growing a thermally stable structure.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.