• 제목/요약/키워드: Electrochemical hydrogenation

검색결과 20건 처리시간 0.025초

수소저장금속의 형상과 변형 (Shapes and Deformation of the Hydrogen Absorption Metal)

  • 정영관;박규섭;이근진;김경훈;김세웅
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 2003년도 춘계학술대회 논문집
    • /
    • pp.1382-1385
    • /
    • 2003
  • Deformation on shapes of the hydrogen absorption metal in this paper was investigated on hydrogen absorption-desorption cycling. In order to study this problem, the cold rolled palladium plate and the cold extrusion palladium bar as specimens had been used. By using the electrochemical method, the palladium specimens were cyclically hydrogenated in the 0.1 mol H$_2$SO$_4$ electrolyte. As results, it is noted that the thickness of the plate specimen gradually increased in increasing hydrogenation cycles whereas the width and the length decreased. But both the diameter and the length of the bar specimen increased with increasing hydrogenation cycles. Also, grains in the plate specimen were greatly deformed after hydrogenation cycling whereas internal grains in the bar specimen were pulverized. And deterioration of the hydrogen absorption rate of the bar specimen was lager than the plate specimen.

  • PDF

Laves phase계 수소저장합금의 전기화학적 수소화 반응 매카니즘에 관한 연구 (A Study on the Electrochemical Hydrogenation Reaction Mechanism of the Laves Phase Hydrogen Storage Alloys)

  • 이지열;김찬중;김대용
    • 한국수소및신에너지학회논문집
    • /
    • 제8권1호
    • /
    • pp.31-41
    • /
    • 1997
  • In order to investigate the mechanism of electrochemical hydrogenation reaction on Zr-based Laves phase hydrogen storage alloy electrodes, electrochemical charge/discharge characteristics, potentiostatic/dynamic polarizations and electrocehmical impedance spectroscopy(EIS) of Zr-Ti-Mn-Ni and Zr-Ti-Mn-Ni-M(M=Fe, Co, Al) alloys were examined. Electrochemical discharge capacities of the alloys were quite different with gas charge capacities. Therefore, it was considered that discharge capacities of the alloys depend on electrochemical kinetic factors rather then thermodynamic ones. Discharge efficiencies were increased linearly with exchange current densities. The results of potentiostatic/dynamic polarization measurements showed that electrochemical charge and discharge reaction of Zr-based Laves phase hydrogen storage alloys is controlled by charge transfer process at the electrode surface. The EIS measurements also confirmed this result.

  • PDF

수소저장-방출싸이클링에 의한 압연판재의 변형 (Deformation of the Rolled Plate with Hydrogen Absorption-Desorption Cycling)

  • 정영관;김경훈;정선환;김창덕;이근진;박규섭
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 2002년도 춘계학술대회 논문집
    • /
    • pp.861-864
    • /
    • 2002
  • Deformation of the specimen was investigated on hydrogen absorption-desorption cycling. In order to study this problem, the cold rolled palladium thin plate as the specimen had been used. By using the electrochemical method, the palladium plate specimen was cyclically hydrogenated in the 0.1 mol $H_2SO_4$ electrolyte. As results, it is noted that the thickness of the plate specimen gradually increased in increasing hydrogenation cycles whereas the width and the length decreased. Also, grains in the plate specimen were greatly deformed after hydrogenation cycling. But hydrogen absorption rate scarcely changed.

  • PDF

수소저장-방출싸이클링과 냉간가공과의 관계 (The Relation between Hydrogen Absorption-Desorption Cycling and Cold Work)

  • 정영관;이근진;박규섭;김경훈;김세웅
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 2002년도 추계학술대회 논문집
    • /
    • pp.829-832
    • /
    • 2002
  • Deformation of the specimens was investigated on hydrogen absorption-desorption cycling. In order to study this problem, the cold rolled and the annealed palladium thin plate as specimens had been used. By using the electrochemical method, the palladium plate specimens were cyclically hydrogenated in the 0.1mol $H_2SO_4$ electrolyte. As results, it is noted that the thickness of the plate specimens gradually increased in increasing hydrogenation cycles whereas the width and the length decreased. Also, Deformation of the cold rolled palladium specimen was lager than the annealed palladium specimen. And grains in the plate specimen were greatly deformed after hydrogenation cycling. But hydrogen absorption rate scarcely changed.

  • PDF

The Fundamentals of Reduction of UO22+ Ions on a Pt Electrode and Methods for Improving Reduction Current Efficiency

  • Yeon, Jei-Won;Pyun, Su-Il
    • 전기화학회지
    • /
    • 제10권2호
    • /
    • pp.73-81
    • /
    • 2007
  • This review article considered the electrochemical reduction of uranyl ions on a Pt surface. Specifically, we focussed on the improvement in its reduction current efficiency. First, this article briefly explained the fundamentals of the reduction of uranyl ($UO_2^{2+}$) ions on a Pt surface. Namely, they involved the electrochemical behaviour of uranium species, and electrochemical cell configurations for the reduction of $UO_2^{2+}$ ions. In addition, the effects of adsorbed hydrogen atoms were investigated on the reduction of $UO_2^{2+}$ ions. Finally, this article presented the methods for improving current efficiency of the reduction of $UO_2^{2+}$ ions on a Pt surface. Three different kinds of methods are introduced, which include electrochemical surface treatments of Pt electrode involving hydrogenation and anodisation, the use of catalyst poisons, and formation of thin mercury film on a Pt electrode. Moreover, this article provided some clues about how hydrogenation and catalyst poisons work on the reduction of $UO_2^{2+}$ ions.

고에너지 밀도 바나듐 레독스 흐름 전지를 위한 망간산화물 촉매와 다공성 탄소 기재의 시너지 효과 (Synergistic Effect of the MnO Catalyst and Porous Carbon Matrix for High Energy Density Vanadium Redox Flow Battery)

  • 김민성;고민성
    • 한국표면공학회지
    • /
    • 제52권3호
    • /
    • pp.150-155
    • /
    • 2019
  • The carbon electrode was modified through manganese-catalyzed hydrogenation method for high energy density vanadium redox flow battery (VRFB). During the catalytic hydrogenation, the manganese oxide deposited at the surface of the carbon electrode stimulated the conversion reaction from carbon to methane gas. This reaction causes the penetration of the manganese and excavates a number of cavities at electrode surface, which increases the electrochemical activity by inducing additional electrochemically active site. The formation of the porous surface was confirmed by the scanning electron microscopy (SEM) images. Finally, the electrochemical performance test of the electrode with the porous surface showed lower polarization and high reversibility in the cathodic reaction compared to the conventional electrode.

수소저장-방출싸이클링에 의한 수소저장금속의 변형거동에 관한 형상 및 가공의 영향 (Effect of Geometrical Shape and Cold Work on Deformation of the Hydrogen Absorption Metal with Hydrogen Absorption-Desorption Cycling)

  • 정영관
    • 한국수소및신에너지학회논문집
    • /
    • 제14권3호
    • /
    • pp.207-216
    • /
    • 2003
  • By using the electrochemical method, the relation between the deformation and the geometrical shape, and the effect of cold work on hydrogen absorption-desorption cycling in palladium were investigated, In order to study this problem, four kinds of the Pd specimens used were plates and bars as cold worked and annealed states. As results, it is found that the deformation of thickness direction in the palladium plates increased whereas other lateral directions decreased. But the palladium bars showed the same deformation ratio in all directions because of uniform distribution of the $\beta$ phase. Grains in the plate specimens were greatly deformed after hydrogenation cycling whereas grains in the bar specimens were pulverized. Also, deterioration of the hydrogen absorption rate of the bar specimen was larger than the plate specimen. And the effect of cold work on hydrogen absorption capacity was relatively small.

기체분무형 공정으로 제조된 Zr계 금속수소화물의 수소화반응 및 Ni-MH 2차전지 전극 특성에 관한 연구 (Hydrogneation and Electrochemical Characteristics of Gas-atomized Zr-based $AB_2$ Hydride for Ni-MH Secondary Battery)

  • 김진호;황광택;김병관;한정섭
    • 한국수소및신에너지학회논문집
    • /
    • 제20권6호
    • /
    • pp.505-511
    • /
    • 2009
  • The hydriding and electrochemical characteristics of Zr-based $AB_2$ alloy produced by gas atomization have been extensively examined. For the particle morphology of the as-cast and gas-atomized powders, it can be seen that the mechanically crushed powders are irregular, while the atomized powder particles are spherical. The increase of jet pressure of gas atomization process results in the decrease of hydrogen storage capacity and the slope of plateau pressure significantly increases. TEM and EDS studies showed the increase of jet pressure in the atomization process accelerated the phase separation within grain of the gas-atomized alloy, which brought about a poor hydrogenation property. However, the gas-atomized $AB_2$ alloy powders produced by jet pressure of 50 bar kept up the reversible $H_2$ storage capacity and discharge capacity similar to the mechanically crushed particles. In addition, the electrode of gas-atomized Zr-based $AB_2$ alloy of 50 bar showed improved cyclic stability over that of the cast and crushed particulate, which is attributed to the restriction of crack propagation by grain boundary and dislocation with ch/discharging cycling.

이온전도성 세라믹 기반 고온 전기화학 멤브레인 반응기 응용기술 (Electrochemical Ceramic Membrane Reactors)

  • 엄성현;박재량;서민혜
    • 공업화학
    • /
    • 제24권4호
    • /
    • pp.337-343
    • /
    • 2013
  • 멤브레인 반응기는 멤브레인과 반응기를 결합하여 반응과 분리의 단위공정을 하나로 결합함으로써 전체공정을 단순화하고 반응효율을 높이고자 하는 혁신 기술로써, 멤브레인을 이용한 생성물의 선택적 제거를 통해 열역학적 평형을 뛰어넘는 전환율, 부반응물 생성 억제에 의한 반응 효율 및 선택성을 향상시킬 수 있다. 특히 이온전도성 세라믹을 이용한 멤브레인 반응기는 연료전지의 개발, 고순도 산소/수소의 분리/정제, 이산화탄소의 전환 및 다양한 화학제품제조에 까지 응용될 수 있기 때문에 시장의 확대와 더불어 크게 발전할 수 있을 것으로 기대된다. 본 총설에서는 수소이온 전도성 세라믹 멤브레인 반응기에 대한 연구동향과 다양한 응용분야 및 향후 전망 등에 고찰해 보고자 한다.

연료전지의 수소저장용 합금에 대한 수소확산반응의 속도론적 해석 (Kinetic Parameter Analysis of Hydrogen Diffusion Reaction for Hydrogen Storage Alloy of Fuel Cell System)

  • 김호성
    • 조명전기설비학회논문지
    • /
    • 제20권2호
    • /
    • pp.45-49
    • /
    • 2006
  • 본 논문은 마이크로 전극 시스템에 의하여 연료전지 및 Ni-MH 전지로의 응용을 가정한 $AB_5$계 수소저장합금인 $MmNi_{3.55}Co_{0.75}Mn_{0.4}Al_{0.3}$의 단일 입자에 대하여 전기화학적인 평가를 수행하였다. 즉 Carbon fiber 마이크로 전극을 합금 입자 한개 위에 전기적인 접촉을 이루도록 조정하고, 합금 입자 내에서 수소원자의 겉보기 화학적 확산계수를 계산하기 위하여 Potential-Step 실험을 실시하였다. 여기에서 사용되는 합금입자는 치밀하고 전도성이 있는 구형이므로 데이터 해석을 위해 구형확산 모델을 적용하였다. 실험결과로서 겉보기 확산계수($D_{app}$)는 수소 흡장 및 방출되는 전 과정에서 $10^{-9}$$10^{-10}[cm^2/s]$ 수준인 것으로 확인되었다. 마이크로 전극 측정 시스템에 의한 단일 입자의 전기화학적 평가는 기존의 Composite Film 전극에 비해 수소저장합금에 대해 보다 상세하고 정확한 정보를 쉽게 얻을 수 있었다.