The microstructure and electrochemical analysis of welds of electric resistance welding(ERW) pipe were investigated. The direction of metal flow line in HAZ of ERW pipe shifted to the inner(or outer) surface of pipe by plastic deformation during welding. The lowest heat input welds of ERW pipe was showed crack by liquid penetrant testing. Accelerated corrosion test by constant current density of 20mA/$cm^{2}$ developed groove at the welds of ERW pipe and the measured grooving factors were about $1.2{\sim}1.5$. Corrosion potential of base metal obtained by cyclic polarization in artificial sea water(3.5wt.% NaCl solution) was 100mV higher than that of weld metal of ERW pipe.
Although leakage at a low carbon steel pipe made by electrical resistance welding (ERW) was reported due to grooving corrosion, the cause for the corrosion has not yet been cleared. In order to clarify the main cause, failure analysis on the leaked pipe was carried out, followed by metallographic investigation and corrosion test for the various ERW pipe made with different welding heat input. The microstructure, particularly inclusion content, of the weldment is dependant on the welding heat input applied. For an improper low heat input, the amount of inclusion at the weld was high. High inclusion content accelerated grooving corrosion at the weld. It is therefore that welding heat input should be controlled based on the carbon content of the pipe in order to improve the corrosion resistance of the ERW pipe.
Kim, Wan Keun;Koh, Seong Ung;Yang, Boo Young;Kim, Kyoo Young
Corrosion Science and Technology
/
제6권3호
/
pp.96-102
/
2007
The resistance of the linepipe steel to hydrogen-induced cracking (HIC) and sulfide stress cracking (SSC) is very important for steel to be used in sour oil/gas environments. Welding of steels is necessary to the construction of pipe-line transporting oil/gas. In this study, HIC and SSC resistance of an electric resistance welded (ERW) steel plate which belongs to API X70 grade was evaluated by using NACE TM0284-96A and NACE TM0177-96A methods. HIC and SSC fracturing behavior was investigated by observing fractured surfaces using optical microscopy (OM) and scanning electron microscopy (SEM). It was discussed in terms of metallurgical parameters such as the distribution of primary microstructure, second phases and inclusions. Results showed that the weld joint of ERW steel is more sensitive than base metal to HIC and SSC. This is due to difference in the contribution of metallurgical parameters to HIC and SSC nucleation and propagation.
청정에너지원의 수요가 증가함에 따라 에너지원의 공급로의 역할을 하는 강관의 수요가 증가하고 있다. 소재가공 기술의 발전과 함께 경량의 고장력 강재의 적용은 공급로의 역할을 하는 강관의 비용절감 및 자원의 효율적 이용 측면에서 지속적으로 연구 개발을 이어왔다. 이러한 추세에 따라 구조용 또는 라인파이프용 강관에서도 고장력 강재의 적용과 함께 고인성 그리고 용접성의 향상을 위한 다양한 라인파이프용 강재의 개발과 이의 적용이 그간 활발히 진행되어왔다. 용도상 반드시 필요한 특성인 고장력, 고인성, 용접성 등 외에도 다양한 강재의 사용에 따른 제조공정상 즉 용접공정에서 발생될 수 있는 용접부의 기계적 특성 변화에 대한 특성 연구 및 기술 연구가 계속 되어왔다. 주로 강관을 생산하는데 쓰이는 ERW (Electric Resistance Welding) 공정에서도 이러한 문제점을 해결하기 위해 많은 연구가 진행되고 있다. ERW는 높은 생산성과 낮은 제조비용의 장점을 가지고 있으나 용접 후 용접부의 기계적 특성 감소로 인한 단점이 있다. 때문에 기계적 특성향상을 위해 최적의 용접조건에 대해 연구해야 할 필요가 있다. 본 연구에서는 4가지 합금강관의 ERW 용접시 용접 입열량의 변화와 용접부의 후열처리를 통한 미세조직의 변화와 기계적 특성에 대해서 고찰하였다. 4강종 시편의 미세조직을 OM, SEM을 통한 분석 이후 인장시험 및 경도시험 등을 통해 기계적 특성을 평가하였다. 대부분의 시편에서 입열량의 증가에 따라 Ferrite 분율이 증가하였고 용접중앙부의 Ferrite 양이 용접경계부 보다 많았다. Ferrite 집중부의 분포가 극명하게 관찰되었던 DP780 (적정) 강종과 미세하게나마 Ferrite 집중부가 존재하였던 K55 (과소, 과대) 강종에서 나란히 경도 하락 현상이 관찰되었다. 이는 강종마다 고유의 Ceq, 합금 중 Mn 농도, 입열량 등에 의한 복합적인 이유 때문으로 판단된다. 탄소가 0.3~0.4 wt% 함유된 중탄소강인 S45C, K55의 경우 용접중앙부와 용접경계부의 페라이트 분율 차이가 큰 것을 알 수 있었다. 이는 용접시 열에 의한 탈탄현상으로 인해 나타나는 현상으로 판단된다.
Energy resistance welding (ERW) is a pipe-producing process that has high productivity and low manufacturing cost. However, the high heat input of ERW degrades the mechanical property of the pipe. This study investigates the effect of heat input and alloying elements on microstructure and mechanical properties of ERW pipes. As the heat input increased, the ferrite amount increased. The ferrite amount in the weld centerline was larger than t at in the weld boundary. Medium carbon steels (S45C and K55) having 0.3~0.4wt.% carbon yielded a significant difference of ferrite amount in the weld centerline and weld boundary. High alloyed steels (DP780 and K55) having 1.5~1.6wt.% Mn showed a ferrite rich zone in the weld centerline. These phenomena are probably due to decarburization and demanganisation in the weld centerline. As the ferrite fraction increased, the hardness decreased a little for the S45C steels. In addition, DP780 steels and K55 steels showed that the hardness drops when those steels have a ferrite rich zone. But we demonstrated the good tensile property of the DP780 steels and K55 steels in which Mn is included.
To ensure driver safety, high-strength steel pipes are utilized in the chassis and internal structures design of automobiles. ERW(electric resistance welding) pipes, fabricated through welding at joints using electrical resistance, form a Heat-Affected Zone (HAZ) during the welding process. Due to characteristics such as increased hardness and reduced ductility compared to the base material, HAZ poses challenges in finite element analysis (FEA) for pipe shapes. In this study, for FEA considering HAZ properties, mechanical properties were measured through uniaxial tensile testing and digital image correlation (DIC) techniques after specimen fabrication. These measurements were validated using reverse engineering methods. Furthermore, hardness measurements and gaussian functions were employed to ascertain the hardness distribution within the HAZ, serving as a basis for subdividing the HAZ and modeling the pipe shape. To validate the effectiveness of the HAZ modeling approach, models were interpreted incorporating only base material properties and models incorporating average-calculated HAZ properties. Comparative analysis was performed, revealing that the model subdividing the HAZ based on hardness measurements closely approximated experimental values. This validation offered a methodology for HAZ modeling in FEA.
In this study, the optimal welding condition of the input power was selected experimentally through the ERW simulator, which is equal to welding status of ERW part in pipe. This condition is the input power 250kW in the heat treatment of the $900^{\circ}C$ normalizing derived from the nondestructive technique and impact energy. In order to evaluate the variation of the fatigue life in the pipe, fatigue surface crack growth test of base and optimal welded metal were performed statistically. As stress intensity factor range (${\Delta}K_s$) increases, the fatigue crack propagation rate (da/aN) of the base metal is faster than that of the welded joint. The variation of the fatigue life in the ERW pipe was estimated statistically using Monte-Carlo simulation with the standard deviation of material constants (C and m) of the paris law in the specimen.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.