직관과 곡관의 경계 용접부에 존재하는 원주방향 표면균열에 대한 탄소성 파괴역학 해석 (Elastic-Plastic Fracture Mechanics Analyses For circumferential Part-through Surface Cracks At The Interface Between Elbows and Pipes)

  • 송태광;오창균;김윤재;김종성;진태은
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2007년도 춘계학술대회A
    • /
    • pp.1766-1771
    • /
    • 2007
  • This paper presents plastic limit loads and approximate J-integral estimates for circumferential part-through surface crack at the interface between elbows and pipes. Based on finite element limit analyses using elastic-perfectly plastic materials, plastic limit moments under in-plane bending are obtained and it is found that they are similar those for circumferential part-through surface cracks in the center of elbow. Based on present FE results, closed-form limit load solutions are proposed. Welds are not explicitly considered and all materials are assumed to be homogeneous. And the method to estimate the elastic-plastic J-integral for circumferential part-through surface cracks at the interface between elbows and straight pipes is proposed based on the reference stress approach, which was compared with corresponding solutions for straight pipes.

  • PDF

동적하중 하에서의 강도적 불균질부를 갖는 용접이음재의 강도 및 파괴 특성 (Characteristics of Strength and Fracture in Strength Mismatched Joint by Dynamic Loading)

  • 안규백;;;방한서
    • Journal of Welding and Joining
    • /
    • 제21권6호
    • /
    • pp.55-63
    • /
    • 2003
  • Welded joint generally has heterogeneity of strength, material, and fracture toughness and it is important to understand the characteristics of material strength and fracture of welded joint considering heterogeneous effect. Characteristics of strength and fracture of an undermatched joint under dynamic loading was studied by round-bar tension tests and thermal elastic-plastic analyses in this paper. The strength and fracture of the undermatched joints should be evaluated based on the effects of the strain rate and the temperature including temperature rise during the dynamic loading. The differences of fracture characteristics like such as ductile-to-brittle transition behavior are well precisely explained from the stress-strain distribution obtained by numerical analysis.

TiN 박막의 탄소성 유한요소해석 (Elastic-Plastic Finite Element Analysis of TiN Thin Film)

  • 김정실;김석삼
    • 한국윤활학회:학술대회논문집
    • /
    • 한국윤활학회 2001년도 제34회 추계학술대회 개최
    • /
    • pp.331-340
    • /
    • 2001
  • Elastic-Plasitc Finite element analysis is peformed about the TiN coated medium. The normal contact is simulated by a rigid asperity pressing the surface of an elastic-plastic half-surface. The case of a surface film stiffer than the substrate is considered, and general solutions for the subsurface stress and deformation fields are presented for several coating thickness. Additionally, the critical normal loads for deformation in the substrate and coating fracture are calculated when the yield of TiN film follows the Maximum Principal Stress Theory and Von Mises Theory. The results can be subsumed in failure maps for TiN thin film on steel.

  • PDF

용접부 3차원 표면균열선단에서의 구속상태 (The 3D Surface Crack-Front Constraints in Welded Joins)

  • 이형일;서현
    • 대한기계학회논문집A
    • /
    • 제24권1호
    • /
    • pp.144-155
    • /
    • 2000
  • 초록 The validity, of a single parameter such as stress intensity, factor K or J-integral in traditional fracture mechanics depends strongly on the geometry, and loading condition. Therefore the second parameter like T-stress measuring the stress constraint is additionally needed to characterize the general crack-tip fields. While many, research works have been done to verify, the J-T description of elastic-plastic crack-tip stress fields in plane strain specimens, limited works (especially. for bimaterials) have been performed to describe the structural surface crack-front stress fields with the two parameters. On this background, via detailed three dimensional finite element analyses for surface-cracked plates and straight pipes of homogeneous materials and bimaterials under various loadings, we investigate the extended validity or limitation of the two parameter approach. We here first develop a full 3D mesh generating program for semi-elliptical surface cracks, and calculate elastic T-stress from the obtained finite element stress field. Comparing the J-T predictions to the elastic-plastic stresses from 3D finite element analyses. we then confirm the extended validity of fracture mechanics methodology based on the J-T two parameters in characterizing the surface crack-front fields of welded plates and pipes under various loadings.

가압열충격 사고시 클래스 하부균열 안전성 평가 방법에 관한 연구 (A Study on the Integrity Evaluation Method of Subclad Crack under Pressurized Thermal Shock)

  • 구본걸;김진수;최재봉;김영진
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2000년도 추계학술대회논문집A
    • /
    • pp.286-291
    • /
    • 2000
  • The reactor pressure vessel is usually cladded with stainless steel to prevent corrosion and radiation embrittlement, and number of subclad cracks have been found during an in-service-inspection. Therefore assessment for subclad cracks should be made for normal operating conditions and faulted conditions such as PTS. Thus, in order to find the optimum fracture assessment procedures for subclad cracks under a pressurized thermal shock condition, in this paper, three different analyses were performed, ASME Sec. XI code analysis, an LEFM(Liner elastic fracture mechanics) analysis and an EPFM(Elastic plastic fracture mechanics) analysis. The stress intensity factor and the Maximum $RT_{NDT}$ were used for characterizing. Analysis based on ASME Sec. XI code does not completely consider the actual stress distribution of the crack surface, so the resulting Maximum allowable $RT_{NDTS}$ can be non-conservative, especially for deep cracks. LEFM analysis, which does not consider elastic-plastic behavior of the clad material, is much more non-conservative than EPFM analysis. Therefore, It is necessary to perform EPFM analysis for the assessment of subclad cracks under PTS.

  • PDF

The Mechanical Properties of Alkali Resistance Glass Fiber Reinforced Cement under Different Curing Conditions

  • Jeong, Moon-Young;Song, Jong-Taek
    • The Korean Journal of Ceramics
    • /
    • 제4권3호
    • /
    • pp.189-192
    • /
    • 1998
  • The mechanical properties of alkali resistance (AR) glass fiber reinforced cement(GFRC) under different curing conditions were investigated in this study. The specimens were formed by extrusion process, and then steam cured and autoclaved. An autoclaved specimen showed the elastic-brittle behavior up to 4% of fiber volume fraction. However, it was found that the fracture behavior for cured specimen was changed to the elastic-plastic with crack branches fracture at greater than 3 vol.% of fiber.

  • PDF

CORRELATION BETWEEN J-INTEGRAL AND CMOD IN IMPACT BEHAVIOR OF 3-POINT BEND SPECIMEN

  • Han, M.S.;Cho, J.U.
    • International Journal of Automotive Technology
    • /
    • 제7권3호
    • /
    • pp.337-343
    • /
    • 2006
  • Numerical calculations are made in order to find a possible correlation between the J-integral and the crack mouth opening displacement(CMOD) in dynamic nonlinear fracture experiments of 3-point bend(3PB) specimens. Both elastic-plastic and elastic-viscoplastic materials are considered at different impact velocities. The J-integral may be estimated from the crack mouth opening displacement which can be measured directly from photographs taken during dynamic experiments.

비대칭 원주방향 관통균열 배관의 탄소성 J-적분 계산식 (Elastic-Plastic J Estimations for Pipes with Off-Centred Circumferential Through-Wall Cracks)

  • 심도준;허남수;김윤재;김영진
    • 대한기계학회논문집A
    • /
    • 제27권7호
    • /
    • pp.1170-1178
    • /
    • 2003
  • This paper provides approximate J estimates for off-centred, circumferential through-wall cracks in cylinders under bending and under combined tension and bending. The proposed method is based on the reference stress approach, where the dependence of elastic and plastic influence functions of J on the cylinder/crack geometry, the off-centred angle and strain hardening is minimised through the use of a proper normalising load. Based on published limited FE results for off-centred, circumferential through-wall cracks under bending, such normalising load is found, based on which the reference stress based J estimates are proposed for more general cases, such as for a different cylinder geometry and for combined loading. Comparison of the estimated J with extensive FE J results shows overall good agreements for different crack/cylinder geometries and for combined tension and bending, which provides sufficient confidence in the use of the proposed method to fracture mechanics analyses of off-centred circumferential cracks. Furthermore, the proposed method is simple to use, giving significant merits in practice.

탄소강의 피로균열에 대한 탄소성파괴 해석에 관한 연구 (A Study on the Elastic Plastic Fracture Analysis for Carbon Steel with a Fatigue Crack)

  • 이종형;정형식;유덕상;김영문
    • 한국산업융합학회 논문집
    • /
    • 제9권2호
    • /
    • pp.117-122
    • /
    • 2006
  • This paper is to provide some of the analysis procedures of the FAD(Failure Assessment Diagram), which is applied th the safety test of the atomic pressure vessels and other structures. Harrison proposed R-6 Diagram, and Bloom developed the method of DPFAD(Deformation Plasticty Failure Assessment Diagram). Analysis of J-integration of the plastic materials give the failure test curve for the materials with serious work hardening effect. J value was obtained form both FEM(Finite Element Mothod) and the experiment using compact type specimen for J=JIC, and the results were compared. In this study, the results of analysis using DPFAD and the factors affecting DPFAD in Static fatigue and fracture were reviewed. It was shown that the concept of DPFAD can be applied to test the safety of the structures.

  • PDF

코스틱스방법을 이용한 고온 크리프 파괴현상에 관한 연구 (An Investigation of High Temperature Creep Phenomena by the Method of Caustics)

  • 이억섭;홍성경
    • 대한기계학회논문집
    • /
    • 제18권10호
    • /
    • pp.2543-2553
    • /
    • 1994
  • Caustics method has been applied successfully to determine the fracture parameters such as stress intensity factor and the J-integral for elastic and/or elastic-plastic stress field around the crack tip. For stress fields at the vicinity of crack tip in the creep domain, no experimental report concerning fracture mechanics parameters by using the caustics method has been published up to date. This study investigated creep behavior at the vicinity of crack tips at high temperature($175^{\circ}C$) and attempted to determine of proper fracture parameters for A1 5086 H24 specimens by using the caustics method. The results obtained from the limited experimental investigation are as follows; $J_{th}/J_{caus}$ is found to approach to 1 more rapidly than $K_{th}/K_{caus}$ does during incipient period(within 80 minutes). It is confirmed that experimental $K_{caus}$ approached to theoretical $K_{th}$ after 80 minutes by analyzing the ratio of $K_{th}$ to $K_{caus}$. Unlike the case of room temperature, it is confirmed experimentally that caustics diameter enlarged gradually even the distance between specimen and screen keeps constant. It showed that initial curve of the caustics was initially located in the plastic zone, but it grew out rapidly into the elastic zone for Al 5086 H24 at $175^{\circ}C$. It is confirmed that caustics is a function of time, temperature and distance between specimen and screen at high temperature.