• 제목/요약/키워드: Dislocation Formation

검색결과 87건 처리시간 0.031초

Microstructural Characterization of SS304 upon Various Shot Peening Treatments

  • He, Yinsheng;Li, Kejian;Cho, In Shik;Lee, Chang Soon;Park, In Gyu;Song, Jung-il;Yang, Cheol-Woong;Lee, Je-Hyun;Shin, Keesam
    • Applied Microscopy
    • /
    • 제45권3호
    • /
    • pp.155-169
    • /
    • 2015
  • Plastic deformation was introduced to the austenitic (${\gamma}$) stainless steel of SS304 by air blast shot peening, ultrasonic shot peening, and ultrasonic nanocrystalline surface modification. Various deformation structures were formed. The hardness, the deformation structure and the underlying grain refinement mechanism were investigated. In the deformed region, planar dislocation arrays and deformation twin (DT), the DT-DT intersection and ${\varepsilon}$-martensite structures, and ${\alpha}^{\prime}$-martensite were formed in the respective regions of low, medium, and high strain. The grain refinement mechanism is found to be closely related to the 1) sub-division of coarse grains by DT, shear bands and their intersection, and 2) formation of nano-sized ${\alpha}^{\prime}$-martensite due to the high plastic deformation.

보은(報恩) 탄전(炭田) 서부지역(西部地域)의 지질구조(地質構造) (Structural Geology in the Western Area of the Poun Coal Field)

  • 안중렬;장태우
    • 자원환경지질
    • /
    • 제24권3호
    • /
    • pp.287-299
    • /
    • 1991
  • The study area is mainly composed of metasedimentary rocks which are included in Ogchon, Choson and Pyongan Groups. Because of thrust faults which are developed in this area, a coal bearing formation is repeatedly distributed two times, and Choson Group is thrusted over Pyongan Group. Deformation in this area was taken place in a series of three phases ($D_1$, $D_2$ and $D_3$) ; $D_1$ was most intense whereas $D_3$ was weakest. Thrust faults developed in the upper curst duringD2 produced cataclastic rocks and fault breccia,truncating regional slaty cleavage and earlier folds which were formed during $D_1$ stage. The quartz microstructures of metapsammitic rocks in Choson and Pyongan Groups suggest that dislocation creep mechanism predominated early in fabric development, afterwards deformation mechanism was transfered to pressure solution which intensified the earlier fabrics. According to strain analysis using quartz grains and quartz aggregate grains, the strain magnitude(Es) of Pyongan Group represents larger values than that of Choson Group due to the contrast of constituent minerals, the size of original quartz grains and matrix content. Apparent flattening type in strain pattern appears in the whole area. It is suggested that the relationship between Ogchon Group and Choson Group may be thrust contact.

  • PDF

피코초 레이저 및 CDE를 이용한 TSV가공기술 (TSV Formation using Pico-second Laser and CDE)

  • 신동식;서정;조용권;이내응
    • 한국레이저가공학회지
    • /
    • 제14권4호
    • /
    • pp.14-20
    • /
    • 2011
  • The advantage of using lasers for through silicon via (TSV) drilling is that they allow higher flexibility during manufacturing because vacuums, lithography, and masks are not required; furthermore, the lasers can be applied to metal and dielectric layers other than silicon. However, conventional nanosecond lasers have disadvantages including that they can cause heat affection around the target area. In contrast, the use of a picosecond laser enables the precise generation of TSVs with a smaller heat affected zone. In this study, a comparison of the thermal and crystallographic defect around laser-drilled holes when using a picosecond laser beam with varing a fluence and repetition rate was conducted. Notably, the higher fluence and repetition rate picosecond laser process increased the experimentally recast layer, surface debris, and dislocation around the hole better than the high fluence and repetition rate. These findings suggest that even the picosecond laser has a heat accumulation effect under high fluence and short pulse interval conditions. To eliminate these defects under the high speed process, the CDE (chemical downstream etching) process was employed and it can prove the possibility to applicate to the TSV industry.

  • PDF

기계적 밀링법으로 제조된 마그네슘 분말의 밀링시간에 따른 미세구조 변화와 부식거동 (Corrosion Behavior and Microstructural Evolution of Magnesium Powder with Milling Time Prepared by Mechanical Milling)

  • 안진우;황대연;김긍호;김혜성
    • 대한금속재료학회지
    • /
    • 제49권6호
    • /
    • pp.454-461
    • /
    • 2011
  • In this study, the relationship between corrosion resistance and microstructural characteristics such as grain size reduction, preferred orientation, and homogenous distribution of elements and impurity by mechanical milling of magnesium powder was investigated. Mechanical milling of pure magnesium powder exhibited a complex path to grain refinement and growth together with preferred orientation reversal with milling time. It was also found that anisotropic formation of dislocation on the basal plane of magnesium was initially the dominant mechanism for grain size reduction. After 60 hrs of milling, grain coarsening was observed and interpreted as a result of the strain relaxation process through recrystallization. In spite of the finer grain size and strong (002) texture developed in the sample prepared by spark plasma sintering at $500^{\circ}C$ for 5 min after mechanical milling for 2hrs, the sample showed a higher corrosion rate. The results from this study will be helpful for better understanding of the controlling factor for corrosion resistance and behaviors of mechanical milled magnesium powders.

스페이서 가터 스프링 코일 X-750 소재 정밀 조직 분석 방법 (Microstructure characterization technique of spacer garter spring coil X-750 material)

  • 진형하;류이슬;이경근
    • 한국압력기기공학회 논문집
    • /
    • 제17권2호
    • /
    • pp.109-118
    • /
    • 2021
  • In the periodic surveillance material test for the spacer component of fuel channel assembly in CANDU, a microstructural characterization analysis is required in addition to the mechanical property evaluation test. In this study, detailed microstructure analysis and simple mechanical property evaluation of archive spacer parts were conducted to indirectly support the surveillance test and assist in the study of spacer material degradation. We investigated the microstructural characteristics of the spacer garter spring coil through comparative analysis with the plate material. The main microstructure characteristics of the garter spring coil X-750 are represented by the fine grain size distribution, the ordering phase distribution developed inside the matrix, the high dislocation density inside the grains, and the arrangement of coarse carbides. In addition, the yield strength of the garter spring coil X-750 was indirectly evaluated to be approximately 1 GPa. We also established an analytical method to elucidate the microstructural evolution of the radioactive spacer garter spring coil X-750 based on Canadian research experiences. Finally, we confirmed the measurement technique for helium bubble formation through TEM examination on the helium implanted X-750 material.

Atomistic simulations of defect accumulation and evolution in heavily irradiated titanium for nuclear-powered spacecraft

  • Hai Huang;Xiaoting Yuan;Longjingrui Ma;Jiwei Lin;Guopeng Zhang;Bin Cai
    • Nuclear Engineering and Technology
    • /
    • 제55권6호
    • /
    • pp.2298-2304
    • /
    • 2023
  • Titanium alloys are expected to become one of the candidate materials for nuclear-powered spacecraft due to their excellent overall performance. Nevertheless, atomistic mechanisms of the defect accumulation and evolution of the materials due to long-term exposure to irradiation remain scarcely understood by far. Here we investigate the heavy irradiation damage in a-titanium with a dose as high as 4.0 canonical displacements per atom (cDPA) using atomistic simulations of Frenkel pair accumulation. Results show that the content of surviving defects increases sharply before 0.04 cDPA and then decreases slowly to stabilize, exhibiting a strong correlation with the system energy. Under the current simulation conditions, the defect clustering fraction may be not directly dependent on the irradiation dose. Compared to vacancies, interstitials are more likely to form clusters, which may further cause the formation of 1/3<1210> interstitial-type dislocation loops extended along the (1010) plane. This study provides an important insight into the understanding of the irradiation damage behaviors for titanium.

TEM investigation of helium bubble evolution in tungsten and ZrC-strengthened tungsten at 800 and 1000℃ under 40keV He+ irradiation

  • I. Ipatova;G. Greaves;D. Terentyev;M.R. Gilbert;Y.-L. Chiu
    • Nuclear Engineering and Technology
    • /
    • 제56권4호
    • /
    • pp.1490-1500
    • /
    • 2024
  • Helium-induced defect nucleation and accumulation in polycrystalline W and W0.5 wt%ZrC (W0.5ZrC) were studied in-situ using the transmission electron microscopy (TEM) combined with 40 keV He+ irradiation at 800 and 1000℃ at the maximum damage level of 1 dpa. Radiation-induced dislocation loops were not observed in the current study. W0.5ZrC was found to be less susceptible to irradiation damage in terms of helium bubble formation and growth, especially at lower temperature (800 ℃) when vacancies were less mobile. The ZrC particles present in the W matrix pin the forming helium bubbles via interaction between C atom and neighbouring W atom at vacancies. This reduces the capability of helium to trap a vacancy which is required to form the bubble core and, as a consequence, delays, the bubble nucleation. At 1000 ℃, significant bubble growth occurred in both materials and all the present bubbles transitioned from spherical to faceted shape, whereas at 800 ℃, the faceted helium bubble population was dominated in W.

지형면 분류 및 트렌치 조사에 의한 일광단층의 단층활동시기 추정 (The Ages of Fault Activities of the Ilgwang Fault in Southeastern Korea, Inferred by Classification of Geomorphic Surfaces and Trench Survery)

  • 장호;이진한;안윤성;주병찬
    • 한국제4기학회지
    • /
    • 제18권1호통권22호
    • /
    • pp.21-30
    • /
    • 2004
  • 일광단층은 NNE-SSW 방향으로 한반도 남동부의 울산에서 부산 해운대까지 연장되며 그 길이는 40 Km이다. 본 연구는 신고리 원자력발전소 1,2호기 건설과 관련된 일관단층석의 제4기 활동 여부를 판단하기 위해서, 지형면 분류와 트렌치 조사로 일광단층의 활동시기를 추정한 것이다. 일광역 부근의 해안에서 산록까지는 모래해안 및 충적면, 10m 해성단구면(MIS 5a), 20 m 해상단면(MIS 5e), 45m 해성단구면(MIS 7 or 9)의 변형면, 소기복침식면의 5개 지형면으로 분류된다. 일광단층선을 경계로 기반침식면은 해안 쪽에 분포하는데도 불구하고 내률 쪽의 45m 해성구면의 변형면 보다 비고가 10m 이상 높다. 그러나 동일한 단층선이 지나고 있는 20m 해성단구면은 변위를 나타내지 않는다. 10m 해성단구면과 20 m 해성단구면이 직선적으로 접하는 지대를 트렌치 조사하였으나 단층선이나 퇴적층의 변위를 관찰할 수 없어, 이 지대는 10m 해성단구면의 옛 해안선[구정선(구汀線)]으로 추정한다. 이에 45m 해성단구면 형성기의 고지리(古地理)로는 소기복침식면은 당시의 해수면 보다 높은 '섬' 이였을 것이며, 일광단층은 이천리층 형성 이후-45m 해성단구면 형성기(22만년 내지 32만년 전) 이전에 이루어졌을 것으로 판단한다.

  • PDF

The Transmanubrial Approach for Cervicothoracic Junction Lesions : Feasibility, Limitations, and Advantages

  • Park, Jong-Hyun;Im, Soo Bin;Jeong, Je Hoon;Hwang, Sun Chul;Shin, Dong-Seung;Kim, Bum-Tae
    • Journal of Korean Neurosurgical Society
    • /
    • 제58권3호
    • /
    • pp.236-241
    • /
    • 2015
  • Objective : We report on the technical feasibility and limitations of the transmanubrial approach for cervicothoracic junction (CTJ) lesions and emphasize the advantage of bisecting the upper part of the manubrium in an inverted Y-shape. Methods : Thirteen patients who underwent the fourteen transmanubrial approach for various CTJ lesions were enrolled during 2005-2014. For the evaluation of the accessibility for the CTJ lesion, we analyzed the two parallel line defined as a straight line parallel to the inferior and superior plateau of the upper and lower healthy vertebrae, the angle of the two parallel lines and the distance from the sternal notch to lines at the sternum on preoperative magnetic resonance images. Surgical limitations and perspectives, as well as postoperative clinical outcomes were evaluated retrospectively. Results : The CTJ lesions were six metastases, three primary bone tumors, two herniated discs, and one each of a traumatic dislocation with syrinx formation and tuberculous spondylitis and ossification of the posterior longitudinal ligament. If two parallel lines pass below the sternal notch, the manubriotomy should be inevitably performed. The mean preoperative Visual analogue scale score was 8 (range, 5-10), which improved to 4 (range, 0-6) postoperatively. Seven cases showed an increase in Frankel score postoperatively. Conclusion : The spatial relationship between the sternal notch and the two parallel lines to the lesion was rational to determine the feasibility of manubriotomy. The transmanubrial approach for CTJ lesions can achieve favorable clinical outcomes by providing direct decompression of lesion and effective reconstruction.

MA법으로 제조된 Ni기 합금에서 Y2O3 첨가에 따른 인장강도변화와 시효처리 효과 (Variation of Tensile Strength by Addition of Y2O3 and Effect of Aging Treatment in Ni Base Alloy Fabricated by MA Method)

  • 김일호;이원식;고세현;장진만;권숙인
    • 한국분말재료학회지
    • /
    • 제15권1호
    • /
    • pp.23-30
    • /
    • 2008
  • Ni-20Cr-20Fe-5Nb alloy with or without $Y_2O_3$ was manufactured by mechanical alloying process and consolidated by spark plasma sintering (SPS). The grain size of the alloy with $Y_2O_3$ was smaller than that of alloy without $Y_2O_3$ which results from the effect of $Y_2O_3$ suppressing grain growth. The tensile strength at room temperature was increased by the addition of $Y_2O_3$ but decreased abruptly at temperature above $600^{\circ}C$. It seems to result from the change of deformation mechanism due to fine grain size, that is, grain boundary sliding is predominant at above $600^{\circ}C$ while internal dislocation movement is predominant at below $600^{\circ}C$. After conventional heat treatment process of solution treatment and aging, a small amount of ${\delta}(Ni_3Nb)$ phase was formed in Ni-20Cr-20Fe-5Nb alloy while a large amount of ${\gamma}"(Ni_3Nb)$ was formed in Inconel 718 in the previous report. This is due to exhaustion of Nb content by the formation of NbC during consolidation.