• 제목/요약/키워드: Difficult to cut material

Search Result 113, Processing Time 0.024 seconds

A Study on the Standard Roughness for SUS440C Internal Diameter Machining Using a CNC Automatic Lathe (CNC 자동선반을 이용한 SUS440C 안지름 가공에 대한 표준 거칠기에 관한 연구)

  • Chul-Woong Choi;Sik-Won Choi
    • Journal of the Korean Society of Industry Convergence
    • /
    • v.26 no.4_2
    • /
    • pp.605-613
    • /
    • 2023
  • The multi-axis combined machining technology has enabled combined machining, which was difficult. However, the reality is that manufacturing costs are rising due to expensive equipment and there is a shortage of machine operation engineers. The purpose of this research is to present the optimum cutting conditions for the surface roughness when processing the inner diameter of SUS440C, which is an egg material, using a CNC automatic lathe. As a result of measuring the surface roughness, dry machining was the best at Ra0.481㎛ at a spindle speed of 4,000rpm, a feed rate of 0.05rev/min, and a cutting depth of 0.3mm. In wet machining, the highest value was Ra0.317 at a spindle speed of 2,000 rpm, a feed rate of 0.05 rev/min, and a cutting depth of 0.2 mm. The lower the feed rate, the better surface roughness appears. It was found that the feed rate had more influence than the number of revolutions and depth of cut.

ELECTRO-MICROSCOPE BASED 3D PLANT CELL IMAGE PROCESSING METHOD

  • Lee, Choong-Ho;Umeda Mikio;Takesi Sugimoto
    • Proceedings of the Korean Society for Agricultural Machinery Conference
    • /
    • 2000.11b
    • /
    • pp.227-235
    • /
    • 2000
  • Agricultural products are easily deformable its shape because of some external forces. However, these force behavior is difficult to measure quantitatively. Until now, many researches on the mechanical property was performed with various methods such as material testing, chemical analysis and non-destructive methods. In order to investigate force behavior on the cellular unit of agricultural products, electro-microscope based 3D image processing method will contribute to analysis of plant cells behavior. Before image measurement of plant cells, plant sample was cut off cross-sectioned area in a size of almost 300-400 ${\mu}$ m units using the micron thickness device, and some of preprocessing procedure was performed with fixing and dyeing. However, the wall structure of plant cell is closely neighbor each other, it is necessary to separate its boundary pixel. Therefore, image merging and shrinking algorithm was adopted to avoid disconnection. After then, boundary pixel was traced through thinning algorithm. Each image from the electro-microscope has a information of x,y position and its height along the z axis cross sectioned image plane. 3D image was constructed using the continuous image combination. Major feature was acquired from a fault image and measured area, thickness of cell wall, shape and unit cell volume. The shape of plant cell was consist of multiple facet shape. Through this measured information, it is possible to construct for structure shape of unit plant cell. This micro unit image processing techniques will contribute to the filed of agricultural mechanical property and will use to construct unit cell model of each agricultural products and information of boundary will use for finite element analysis on unit cell image.

  • PDF

Machining Characteristics of Cemented Carbides in Micro Cutting within SEM

  • Heo, Sung-Jung
    • International Journal of Precision Engineering and Manufacturing
    • /
    • v.5 no.3
    • /
    • pp.35-42
    • /
    • 2004
  • This research describes that the cutting characteristics and tool wear behavior in the micro cutting of three kinds of wear resistant cemented carbides (WC-Co; V40, V50 and V60) using PCD (Poly Crystalline Diamond) and PCBN (Poly crystalline Cubic Boron Nitride) cutting tools by use of the SEM (Scanning Electron Microscope) direct observation method. The purpose of this research is to present reasonable cutting conditions from the viewpoint of high efficient cutting refer to a precise finished surface and tool wear. Summary of the results is as follows: (1) The cutting forces tend to increase as the increase of the weight percentage of WC particles, and the thrust forces was larger than the principal forces in the cutting of WC-Co. These phenomena were different from the ordinary cutting such as cutting of steel or cast iron. (2) The cutting speed hardly influenced the thrust force, because of the frictional force between the cutting tool edge and small WC particles at low cutting speed region such as 2$\mu\textrm{m}$/s. It seemed that the thrust cutting force occurred by the contact between the flank face and work material near the cutting edge. (3) The wear mechanism for PCD tools is abrasion by hard WC particles of the work materials, which leads diamond grain to be detached from the bond. (4) From the SEM direct observation in cutting the WC-Co, it seems that WC particles are broken and come into contact with the tool edge directly. This causes tool wear, resulting in severe tool damage. (5) In the orthogonal micro cutting of WC-Co, the tool wear in the flank face was formed bigger than that in the rake face on orthogonal micro cutting. And the machining surface integrity on the side of the cutting tool with a negative rake angle was better than that with a positive one, as well as burr in the case of using the cutting tool with a negative rake angle was formed very little compared to the that with a positive one.

Sintering Behavior and Mechanical Property of Transition Metal Carbide-Based Cermets by Spark Plasma Sintering (방전플라즈마 소결 공정 적용 전이금속 카바이드 서멧의 소결 및 기계적 특성)

  • Lee, Jeong-Han;Park, Hyun-Kuk;Hong, Sung-Kil
    • Korean Journal of Materials Research
    • /
    • v.32 no.1
    • /
    • pp.44-50
    • /
    • 2022
  • Transition metal carbides (TMCs) are used to process difficult-to-cut materials due to the trend of requiring superior wear and corrosion properties compared to those of cemented carbides used in the cutting industry. In this study, TMC (TiC, TaC, Mo2C, and NbC)-based cermets were consolidated by spark plasma sintering at 1,300 ℃ (60 ℃min) with a pressure of 60 MPa with Co addition. The sintering behavior of TMCs depended exponentially on the function of the sintering exponent. The Mo2C-6Co cermet was fully densified, with a relative density of 100.0 %. The Co-binder penetrated the hard phase (carbides) by dissolving and re-precipitating, which completely densified the material. The mechanical properties of the TMCs were determined according to their grain size and elastic modulus: TiC-6Co showed the highest hardness of 1,872.9 MPa, while NbC-6Co showed the highest fracture toughness of 10.6 MPa*m1/2. The strengthened grain boundaries due to high interfacial energy could cause a high elastic modules; therefore, TiC-6Co showed a value of 452 ± 12 GPa.

A Study on the Effect of Moisture Content of Wood upon the Absorption on Zinc Chloride Solution (침지처리법에(浸漬處理法)있어서 목재함수량(木材含水量)이 염화아연 흡수율(吸收率)에 미치는 영향(影響))

  • Shim, Chong-Supp;Shin, Dong-So
    • Journal of the Korean Wood Science and Technology
    • /
    • v.10 no.3
    • /
    • pp.133-134
    • /
    • 1982
  • This experiment has been made to investigate the absorption of watersoluble zinc chloride by Pinus densiflora S. et Z. at different moisture content, under soaking process, to decide the optimum content condition for the maximum absorption of zinc chloride by the wood tested and to investigate the concentration of zinc chloride affecting each moisture content of wood. Material was cut in the Dept. of Forest, College of Agr. S.N.U. Suwon, Korea. Sample was divided into sap and heartwood group and cut $2{\times}2{\times}2\;cm$ in size, having exact three dimensions, using the part of D.B.H. The numbers of sample were 20 pieces for each moisture content condition for both sap and heartwood. Especially, the samples were protected from exposure to keep moisture content in green condition. The ranges of moisture content tested were as the table 3 and 4. The conclusions were as follows: 1. With 3% zinc chloride solution, the rate of absorption decreased with the time increased, if the air seasoned Korean red pine (Pinus densiflora S. et Z.) was treated in steeping process. Initial absorption for 30 minutes was more than 50% of total absorpon for 24 hours. 2. Rate of absorption was same under the green condition, while rate of absorption under the moisture content 7 to 30% varied. 3. Although it was not quite proportional change in the absorption with the difference of moisture content, the great change in the absorption occured by seasoning. With exception sap green condition, sapwood twice more permeable than the heartwood in the oven dried condition and it has been observed the nearly same amount of absorption at the moisture content of 7%, 10% and 15% respectively in heartwood. 4. It was better from water in wood from view-point of absorption of zinc chloride solution, but it was difficult practically to obtain the smallest moisture content, and then it was decided that values of allowable moisture content, on the basis of mean absorption, were 15% to 20% in the sapwood, and in the heartwood, 10% to 15%. The mean absorption for each moisture content in the sap and the heartwood were as following. 5. In general, the concentration of zinc chloride after steeping was nearly same between moisture content and sap and heartwood respectively.

  • PDF

Electron Microscopic Studies of Human Keloid and Hypertrophic Scars (Keloid와 Hypertrophic Scar ( 비후성반흔 )의 형태학적 관찰)

  • Kim, Chung-Soak;Lew, Jae-Duk
    • Applied Microscopy
    • /
    • v.3 no.1
    • /
    • pp.29-38
    • /
    • 1973
  • Introduction. The human cutaneous scars manifest themselves many ways in different types according to the factors such as the age, sex, race of the patient as well as the location,. kind and heal ing process of the wound. Among the scars it is quiet difficult to verify the clinical course of the hypertrophic or keloidal scars from the true keloids. However, clinical observations indicate that stress, either mechanical or in the forms of chronic infections, can induce a functional change in the fibroblasts causing an excessive production of collagenous matrix. In this study, we preliminary attempt to justify any difference of the cellular structure between keloids and hypertrophic scars by using electron microscope. Material and Methods. A total of 23 cases: 2 scars, 2 hypertrophic scars and 19 keloids are examined. Immediately, the biopsy tissue was fixed in 10% neutral formalin and 4% glutaraldehyde solution in phosphate buffer for 4 hours, post fixed in 1 % osmium tetraoxide for two hours, dehydrated with graded alcohol, and embedded in Epon 812. Thick sections were stained with hematoxylin eosin, periodic acid-Schiff(PAS) and Van Gieson stain. Thin sections were cut and uranyle acetate, lead citratestain and examined with the electron microscope. Result. The morphologic features of keloid showed thick, homogenously eosinophilic bands of collagen and numberous large active fibroblasts. The hypertrophic scar and soft scar are more cellular than keloid and composed thinner collagenous fiber. For this paper in the etiology of keloids can not as be defined, but and interesting keloidal tissue fibroblast showed irregular nucleus with irregular shape dense bodies and fibril materials contained in to the cytoplasm.

  • PDF

A Study on the Machinability of Titanium (티타니움의 절삭성에 관한 연구)

  • Cheong, Seong-Gyu;Oh, Seok-Hyung;Seo, Nam-Seob
    • Journal of the Korean Society for Precision Engineering
    • /
    • v.6 no.2
    • /
    • pp.40-46
    • /
    • 1989
  • Recently, the researches on cutting the new material have been done for development of aerospace industrial engineering. Especially, titanium ally is well known as heat resisting, antiwear, anticorrosion and difficult-to-machine materials. Many studies on the analysis of shear angle have been done for improving productivity in cutting these materials. In case of titanium alloy, the saw-toothed type of chip which has wave surface of a triangular form, an eccentric from of a continuous type of chip that is produced in the cutting process, was checked. Nakayama supposed that a maximum shear strewss plane and the shear crack in the free surface made an angle of $45^{\circ}$ .deg. , but it's usually much larger than that. In this paper, the author analyzed the shear conditions of the cutting process in the quick-stopping device with the help SEM-photographs, and measured the hypotenuse angle directly in the photographs of the chips. In conclusion, the author tried to find the shear angle in the cutting process with the saw-toothed chip and compared it with the shear angles which can be calculated from the theories established by others. The results obtained are as follows. 1. In case of the saw-toothed chips, the equivalent cutting ratio can be calculated by using the chip thickness to two-thirds of ramp height. 2. The theory of Ernst-Merchant is not applicable to the titanium and its alloys which does not fractured in accordance with the theory of maximum shear stress. 3. When we cut the titanium alloys which produced the saw-toothed chips, the shear angle can be found with the theories of Rowe-Spick, P.K. Wright and the measurement of hypotenuse angle.

  • PDF

Mechanical Property Evaluation of WC-Co-Mo2C Hard Materials by a Spark Plasma Sintering Process (방전플라즈마 소결 공정을 이용한 WC-Co-Mo2C 소재의 기계적 특성평가)

  • Kim, Ju-Hun;Park, Hyun-Kuk
    • Korean Journal of Materials Research
    • /
    • v.31 no.7
    • /
    • pp.392-396
    • /
    • 2021
  • Expensive PCBN or ceramic cutting tools are used for processing of difficult-to-cut materials such as Ti and Ni alloy materials. These tools have the problem of breaking easily due to their high hardness but low fracture toughness. To solve these problems, cutting tools that form various coating layers are used in low-cost WC-Co hard material tools, and research on various tool materials is being conducted. In this study, binderless-WC, WC-6 wt%Co, WC-6 wt%Co-1 wt% Mo2C, and WC-6 wt%Co-2.5 wt% Mo2C hard materials are densified using horizontal ball milled WC-Co, WC-Co-Mo2C powders, and spark plasma sintering process (SPS process). Each SPSed Binderless-WC, WC-6 wt%Co-1 wt% Mo2C, and WC-6 wt%Co-2.5 wt% Mo2C hard materials are almost completely dense, with relative density of up to 99.5 % after the simultaneous application of pressure of 60 MPa and almost no significant change in grain size. The average grain sizes of WC for Binderless-WC, WC-6 wt%Co-1 wt% Mo2C, and WC-6 wt%Co-2.5 wt% Mo2C hard materials are about 0.37, 0.6, 0.54, and 0.43 ㎛, respectively. Mechanical properties, microstructure, and phase analysis of SPSed Binderless-WC, WC-6 wt%Co-1 wt% Mo2C, and WC-6 wt%Co-2.5 wt% Mo2C hard materials are investigated.

Analysis of Cutting Force and Plastic Deformation Occurring During Machining of Ti-6Al-4V Alloy Aircraft Parts (Ti-6Al-4V 합금 항공기 부품 가공 시 발생하는 절삭추력 및 소성변형에 대한 해석)

  • Son, Hwi Jun;Kim, Seok;Park, Ki-Beom;Jung, Hyoun Chul;Cho, Young Tae
    • Journal of the Korean Society of Manufacturing Process Engineers
    • /
    • v.21 no.8
    • /
    • pp.25-31
    • /
    • 2022
  • Recently, investment in the aerospace industry has increased, and titanium alloys have been widely adopted for manufacturing parts in the aerospace industry. The Ti-6Al-4V alloy has high strength in high-temperature and high-pressure environments and is evaluated as a material with excellent heat, corrosion, and abrasion. However, titanium alloys are expensive, difficult to cut, and possess a large cutting load during the drilling process. In this study, the cutting force generated in the drilling process of Ti-6Al-4V alloy was verified via finite element analysis (FEM) and cutting force measurement experiments. A structural analysis was performed based on the cutting analysis data to verify the plastic deformation occurring during the drilling process of cylindrical Ti-6Al-4V alloy aircraft parts. Methods were proposed to predict the amount of deformation that occur during the manufacturing process of titanium-alloy aircraft parts and control the external environment, to minimize the amount of deformation.

An Investigation on 'Kwa-Jung';Traditional Korean Confectionery Items, Found in Korean Literatures Prior to the 17th Century (17세기 이전 조선시대 과정류의 문헌적 고찰)

  • Cho, Shin-Ho;Chung, Rak-Won;Choi, Young-Jin;Kim, Eun-Mi;Won, Sun-Im;Cha, Gyung-Hee;Kim, Hyun-Sook;Lee, Hyo-Gee
    • Korean journal of food and cookery science
    • /
    • v.24 no.3
    • /
    • pp.312-324
    • /
    • 2008
  • In this study, we investigated the names and various types of "kwa-jung" along with their recipes and ingredients occurring in Korean cookbooks published before the 17th century. The kwa-jungs were classified into 7 groups including Yoomilkwa, Yookwa, Dasik, Junkwa, Kwapyun, Yutganjung and Dang. A total of 72 kinds of kwa-jung were found. 26 kinds of Yoomilkwa, 18 kinds of Yookwa, 7 kinds of Dasik, 10 kinds of Junkwa, 1 kind of Kwapyun, 3 kinds of Yutganjung and 8 kinds of Dang. Among the types of Yoomilkwa, Yackwa was recognized as the best food according to the references. Also the cooking methods for items had a tendency to become simpler as society became modernized. Original and rare Ingredients were often substituted with other items that could be found more easily where people lived As recorded, the Yookwa group included kangyung, sanja, and bingsakwa. And as society became modernized, people tended to buy Yookwa in the store rather than making it at home due to its complicated and often difficult cooking process. The Dasik items were a kneaded mixture of flour, or the flour of chestnuts, with honey. These were formed into various patterns like birds, animals, butterflies, tree leaves and flowers, or as ki-wha by using printing cooking utensils Honey was used as a sweetener and as a combining material. The Junkwa consisted of roots or fruits that could be easily obtained these cooked or raw foodstuffs were then mixed with sugar and simmered. The Kwapyun used sour fruit juices as a main ingredient. These were then combined with sugar and simmered and allowed to harden. Then they were cut into square shapes after cooling. Yutkangjung was a mixture of yut, chochung, honey or syrup and pine nuts. which was combined over low heat. After mixing and stirring it was cut into square shapes. Finally, the Yut was typically cooked with grains and powdered malt and stirred until thickened.