• 제목/요약/키워드: Dielectric absorption

검색결과 215건 처리시간 0.026초

Environment-dependent Broadband Perfect Absorption of Metal-insulator-metal Metamaterial Systems

  • Feng Li;Yulong Tang;Qingsong Peng;Guosheng Hu
    • Current Optics and Photonics
    • /
    • 제7권2호
    • /
    • pp.136-146
    • /
    • 2023
  • Based on calculations using the macroscopic Maxwell's equations with mesoscopic boundary conditions, light absorption by a layered metal-insulator-metal (MIM) metamaterial system embedded in three different environments is investigated. Increasing the top metal thickness shifts the broad absorption band to lower dielectric-constant regions and longer wavelengths, for either TM or TE waves. Boosting the dielectric-layer thickness redshifts the broadband absorption to regions of larger dielectric constant. In air, for the dielectric-constant range of 0.86-3.40, the absorption of the system exceeds 98% across 680-1,033 nm. In seawater with optimized dielectric constant, ≥94% light absorption over 400-1,200 nm can be achieved; particularly in the wavelength range of 480-960 nm and dielectric-constant range of 0.82-3.50, the absorption is greater than 98%. In an environment with even higher refractive index (1.74), ≥98% light absorption over 400-1,200 nm can be achieved, giving better performance. The influence of angle of incidence on light absorption of the MIM system is also analyzed, and the angle tolerance for ≥90% broadband absorption of a TM wave is up to 40° in an environment with large refractive index. While the incident-angle dependence of the absorption of a TE wave is nearly the same for different circumstances, the situation is different for a TM wave.

ITO/$Alq_3$/Al 구조 박막의 유전분산과 흡수에 관한 연구 (A Study on the Dielectric Dispersion and Absorption of ITO/$Alq_3$/Al Thin Film)

  • 오용철;김상진;성낙진
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2007년도 하계학술대회 논문집 Vol.8
    • /
    • pp.490-491
    • /
    • 2007
  • We have investigated dielectric dispersion and absorption in organic light-emitting diodes using 8-hydroxyquinoline aluminum($Alq_3$) as an electron transport and emissive material. We analyzed the dielectric dispersion and absorption of organic light emitting diodes using impedance characteristics measurement by the auto-balancing bridge technique of ITO/$Alq_3$/Al. Impedance characteristics was measured complex impedance Z and phase e in the frequency range of 40Hz to $10^8Hz$. We obtained dielectric constant and loss tangent (tan $\delta$) of the device. From these analyses, we are able to interpret a dielectric dispersion and dielectric absorption contributed by an interfacial and orientational polarization.

  • PDF

충진재 함량 변화에 따른 에폭시 복합재료의 흡수율과 직류 절연파괴강도의 변화 (The variation of water absorption rate and DC dielectric breakdown strength of Epoxy composites due to filler content)

  • 이덕진;김탁용;신성권;김명호;김경환;김재환
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 1999년도 하계학술대회 논문집 E
    • /
    • pp.2349-2351
    • /
    • 1999
  • In this paper, the variable absorption rates and DC dielectric breakdown strength of epoxy composites were measured at boiling absorption condition in order to observe the influences of moisture in out door use. Also, in order to improve withstand voltage properties at moisture absorbtion condition. IPN (interpenetrating polymer network) method which had been already reported, was introduced and the influence was investigated. As a result, it was confirmed that the moisture absorption rate was increased and DC dielectric breakdown strength was degraded with boiling time and filler content increasing. On the other hand, it was confirmed that moisture absorption rate and DC dielectric breakdown strength degrading rate were lowered by the improvement of adhesion strength In IPN specimens.

  • PDF

$C_{22}$-quinolinium(TCNQ) langmuir-blodgett 박막의 열처리 온도에 따른 광학적 및 유전특성 (Optical and electrical properties of $C_{22}$-quinolinium(TCNQ) langmuir-glodgett films depending on the annealing temperatures)

  • 홍언식;유덕선;김태완
    • E2M - 전기 전자와 첨단 소재
    • /
    • 제8권4호
    • /
    • pp.458-463
    • /
    • 1995
  • The optical and electrical properties of $C_{22}$-Quinolinium(TCNQ) Langmuir-Blodgett films have been studied depending on the annealing temperatures. The optimal properties were investigated using UV/visible(300-800[nm]) absorption spectra and FTIR(Fourier-transformed- infrared) absorption measurements. The electrical properties were investigated in a frequency range of 10[Hz]-13[MHz]. The UV/visible absorption spectra at room temperature show that there are four characteristic peaks at 320, 380, 494 and 678[nm]. These absorption peaks decrease very rapidly above the annealing temperature of 180[.deg. C], which is due to a structural change of TCNQ. The FTIR absorption measurements strongly support the result of the UV/visible absorption spectra, because the absorption peak of TCNQ- at 2181[$cm^{-1}$ /] also decreases above 140[.deg. C]. The frequency-dependent dielectric constant shows that there is a dielectric dispersion near 1[MHz] which is due to an orientational polarization of the molecules inside the film. The overall frequency-dependent dielectric constant is higher near 80[.deg. C]. It may be due to a softness of the alkyl chains.s.

  • PDF

메틸렌기의 길이에 따른 LB막의 유전 특성 비교 (Comparison to Dielectric Properties of LB Films for Length of Methylene Group)

  • 강기호;김도균;최용성;장정수;권영수
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 1999년도 하계학술대회 논문집 D
    • /
    • pp.1843-1845
    • /
    • 1999
  • We have investigated the dielectric characteristics of palmitic acid(PA), stearic acid (SA) and arachidic acid(AA) Langmuir-Blodgett(LB) films because these fatty acid systems have a same hydrophilic group and a different hydrophobic one (alkyl chain length). In this work. fatty acid systems were used as LB films and the status of the deposited films was confirmed by evaluating the transfer ratio. the UV absorption and the capacitance. Also, the dielectric characteristics such as the frequency-capacitance characteristics and the dielectric dispersion and absorption characteristics of PA, SA and AA through-plane were measured. The relative dielectric constants of PA, SA and AA LB films were about $2.6\sim4.6$, $2.4\sim4.1$ and $2.2\sim3.8$, respectively. That is, the relative dielectric constants were decreased in proportion to the chain length of methylene group. And, the dielectric dispersion and absorption of each fatty acid LB films have arisen from spontaneous polarization of dipole polarization in the range of $10^4\sim10^5[Hz]$.

  • PDF

흡수열화에 따른 Epoxy/$SiO_2$ 복합체의 전기적 특성 및 수명예측 (Electrical Properties and Lifetime Prediction of Epoxy/$SiO_2$Composites with Water Absorption Ageing)

  • 김탁용;이덕진;홍진웅
    • 한국전기전자재료학회논문지
    • /
    • 제13권9호
    • /
    • pp.758-763
    • /
    • 2000
  • Dielectric strength of insulators made of epoxy composites rapidly decreases due to ageing to interfaces between the matric resin and filler particles. The adhesion variation of interfaces caused by moisture absorption also alters electrical properties that are the basic characteristics of insulators, particularly, in outdoor use. In this paper, electrical properties of epox/SiO$_2$composites were investigated at boiling absorption condition to observe the influences of moisture. In order to analyze the basic physical properties of samples, scanning electron microscopy and DC, AC and impulse voltage dielectric strength were measured. Also, the breakdown time of samples was measured under AC 6[kV] applied voltage, and the variation of lifetime was verified by using Weibull distribution function.

  • PDF

IMI-O 초박막의 착체농도에 대한 유전 특성 (Dielectric Properties of Complex Cconcentration in IMI-0 Thin Films)

  • 정상범;유승엽;박재철;권영수
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 1999년도 춘계학술대회 논문집
    • /
    • pp.345-348
    • /
    • 1999
  • The monolayer behaviors at the air-water interface and the dielectric properties of MI-0 LB films for complex concentration were investigated by the surface pressure-area ($\pi$-A) isotherms and dielectric constant. The molecular area was expanded with increase of metal ions concentration. It is considered that the expansion of molecular area is due to electrostatic repulsion between the polymer chains andhydrophobic increase of ionic strength. In the frequency-dependent complex dielectric constant at room temperature, the real part of dielectric constant($\varepsilon'$) is about 6.0~10.0 in the low-frequency range and is decreasing slowly upto $1O^4$Hz. It decreased abruptly near $1O^5Hz$. It seems to be dielectric dispersion in this frequency range. Also, the imaginary part of dielectric constant ($\varepsilon"$) shows a peak in $1O^5$~$1O^6Hz$. It seems to be dielectric absorption in this frequency range.ange.

  • PDF

메틸렌기의 길이에 따른 지방산계 LB막의 유전 및 전기적 특성 (Dielectric and Electrical Characteristics of Fatty Acid System LB Filmes According to Length of Methylene Group)

  • 김도균;강기호;최용성;권영수
    • 한국전기전자재료학회논문지
    • /
    • 제13권4호
    • /
    • pp.300-305
    • /
    • 2000
  • We have investigated the dielectric and electrical characteristics of palmitic acid(PA) stearic acid(SA) and arachidic acid(AA) Langmuir-Blodgett(LB) films because these fatty acid systems have a same hydrophilic group and a different hydrophobic one(methylene group or alkyl chain length). The fatty acid systems were used as LB films and the status of the deposited films was confirmed by evaluating the transfer ratio the UV absorption and the capacitance. The dielectric characteristics such as the frequency-capacitance characteristics and the dielectric dispersion and absorption characteristics of PA SA and AA through-plane were measured. The relative dielectric constants of PA, SA and AA LB films were about 3.0~4.6, 2.7~3.0 and 2.4~3.0 respectively. That is the relative dielectric constants were decreased in proportion to the chain length of methylene group. Also the dielectric dispersion and absorption of each fatty acid LB films have arisen from spontaneous polarization of dipole polarization in the range of 10$^4$~10$^{5}$ [Hz]. The conductivity of PA, SA and AA LB films obtained from I-V characteristics were about 9$\times$10$^{-14}$ , 3$\times$10$^{-14}$ and 5$\times$10$^{-15}$ [S/cm]. respectively. These results have shown the insulating materials and could control the conductivity y changing the length of methylene group. Also we have confirmed that the barrier height of fatty acid systems were almost the same ones obtained from dielectric characteristics.

  • PDF

DGEBA/MDA/SN/천연 제올라이트계의 절연파괴현상에 미쳐는 흡습의 영향 (Effect of Moisture Absorption on Dielectric Breakdown Phenomena of DGEBA/MDA/SN/Natural Zeolite System)

  • 김유정;이홍기;김상욱
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 1999년도 추계학술대회 논문집 학회본부 C
    • /
    • pp.994-996
    • /
    • 1999
  • Hygrothermal aging at the elevated temperature induces the long-term degradation of the epoxy resin. We investigated the effects of hydrothermal stress on the dielectric breakdown phenomena of epoxy composite filled with natural zeolite. The cured specimens absorbed the moisture in the autoclave at $120^{\circ}C$. $T_g$ of the deteriorated composite by moisture absorption decreased. The dielectric breakdown strength decreased with the moisture absorption cycle. It was concluded that the thermal stress and the high water-vapour-pressure deteriorated the natural zeolite filled epoxy resin system, consequently and the tree growth rate increased.

  • PDF

Spectroscopic ellipsometer를 이용한 삼원 SiO박막의 증착조건에 따른 유전율 특성 (The dielectric properties of triple SiO thin film using spectroscopic ellipsometer)

  • 김창석;황석영
    • E2M - 전기 전자와 첨단 소재
    • /
    • 제8권2호
    • /
    • pp.129-135
    • /
    • 1995
  • SiO thin films are deposited by evaporator the refractive index of wave length, photon energy and the absorptive rate of these films are measured by spectroscopic ellipsometer. It is derived the absorptive rate and permitivity of SiO thin films from the equations that calculating the refractive index. And the result show good agreement with the calculated values and experimental values. As a result, the wave length of light is increased in the condition that the angle of incidence is fixed on SiO thin film, the basic absorption and the absorption impurities are found in the low wave length (below 450 nm in this study) and the reflective absorption and conductive absorption is increased by the form of exponential function over the low wavelength. The absorptive rate is increased by increased the angle of incidence and thickness of SiO film for the insulating layer. As the thickness of SiO film is increased, the value of complex permitivity is decreasing and as wave length of incidence is increased., the value of dielectric is linearly increasing.

  • PDF