• Title/Summary/Keyword: Die and Mold Parts

Search Result 179, Processing Time 0.021 seconds

The Effect of Thermo-Mechanical Treatment on Mechanical and Electrical Behavior of Cu Alloys (동합금의 가공열처리법에 의한 기계적·전기적 성질)

  • Kim, Hyung-Seok;Jeon, C.H.;Song, Gun;Kwun, S.I.
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.10 no.1
    • /
    • pp.20-29
    • /
    • 1997
  • Pure copper is widely used for base material for electrical and electronic parts because of its good electrical conductivity. However, it has such a low strength that various alloying elements are added to copper to increase its strength. Nevertheless, alloying elements which exist as solid solution elements in copper matrix severely reduce the electrical conductivity. The reduction of electrical conductivity can be minimized and the strengthening can be maximized by TMT(Thermo-Mechanical Treatment) in copper alloys. In this research, the effects of TMT on mechanical and electrical properties of Cu-Ni-Al-Si-P, Cu-Ni-Al-Si-P-Zr and Cu-Ni-Si-P-Ti alloys aged at various temperatures were investigated. The Cu alloy with Ti showed the hardness of Hv 225, electrical conductivity of 59.8%IACS, tensile strength of 572MPa and elongation of 6.4%.

  • PDF

Mechanical Properties and Formability of TWB Boron Steel (TWB 보론강의 기계적 특성 및 성형성)

  • Nam, K.W.;Hwang, S.H.;Kim, D.Y.;Lee, M.Y.;Lee, S.M.
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.36 no.10
    • /
    • pp.1221-1226
    • /
    • 2012
  • The hot-stamping technique is a forming method used for manufacturing high-strength parts, in which a part is cooled rapidly after press forming above the austenite transformation temperature. Boron steel, which contains a very small amount of boron, is one of the materials used for hot stamping. The purpose of this study is to investigate the mechanical properties of boron steel according to the heat-treatment conditions and the formability by using an Erichsen cupping test. Die quenching from various temperatures was conducted for different elapsed heat-treatment times. Laser-welded boron steel after quenching at 1173 K-0 s has a tensile strength of 1203 MPa. This is 79% of the tensile strength of the base metal (1522 MPa). The formability of boron steel was not significantly different from that at the mold temperature. However, it decreased with increasing forming speed. These properties provide practical information for the use of boron steels for hot stamping.

Study on the Development of Post-Processor for 5-Axis NC Machining (5축 가공용 Post-Processor 개발에 관한 연구)

  • Jo, E.J.;Hwang, J.D.;Jung, Y.G.
    • Transactions of the Korean Society of Machine Tool Engineers
    • /
    • v.15 no.3
    • /
    • pp.53-58
    • /
    • 2006
  • This study deals with the method of post-processing in the automatic tool path generation for 5-axis NC machining. The 5-axis NC machining cannot only cope with the manufacturing of complicated shapes, but also offers numerous advantages such as reasonable tool employment, great reduction of set-up process and so on. Thus 5-axis NC machining has been used for aircraft parts, mold and die as well as for complicated shapes such as impeller, propeller and rotor. However, most of the present CAM systems for 5-axis NC machining have limited functions in terms of tool collision, machine limits and post-processing. Especially 5-axis machine configurations are various according to the method which the rotational axes are adapted with the table and spindle. For that reason, In many cases the optimal numerical control (NC) data cannot be obtained or considerable time is consumed. To solve this problem, we applied a general post-processor for 5-axis NC machining. The validity of this post-processor should be experimentally confirmed by successfully milling to a helix shaped workpiece.

A study on the effects of polymer core gate sizes on thickness shrinkage rate (폴리머코어 게이트 크기 변화가 두께 방향 수축률에 미치는 영향에 대한 연구)

  • Choi, Han-Sol;Jeong, Eui-Chul;Park, Jun-Soo;Kim, Mi-Ae;Chae, Bo-Hye;Kim, Sang-Yun;Kim, Yong-Dae;Yoon, Kyung-Hwan;Lee, Sung-Hee
    • Design & Manufacturing
    • /
    • v.14 no.1
    • /
    • pp.1-7
    • /
    • 2020
  • In this study, the variation of the shrinkage in the thickness direction of the molded parts according to the gate size of the polymer core fabricated through the 3D printer using the SLS method was studied. The polymer cores are laser sintered and the powder material is nylon base PA2200. The polymer cores have lower heat transfer rate and rigidity than the metal core due to the characteristics of the material. Therefore, the injection molding test conditions are set to minimize the deformation of the core during the injection process. The resin used in the injection molding test is a PP material. The packing condition was set to 80, 90 and 100% of the maximum injection pressure for each gate size. The runner diameter used was ∅3mm, and the gates were fabricated in semicircle shapes with cross sections 1, 2, and 3 ㎟, respectively. Thickness measurement was performed for 10 points at 2.5 mm intervals from the point 2.5 mm away from the gate, and the shrinkage to thickness was measured for each point. The shrinkage rate according to the gate size tends to decrease as the cross-sectional area decreases as the maximum injection pressure increases. The average thickness shrinkage rate was close to 0% when the packing pressure was 90% for the gate area of 1mm2. When the holding pressure was set to 100%, the shrinkage was found to decrease by 3% from the standard dimension due to the over-packing phenomenon. Therefore, the smaller the gate, the more closely the molded dimensions can be molded due to the high pressure generation. It was confirmed that precise packing process control is necessary because over-packing phenomenon may occur.

The emissivity and opto-electrical properties of ZnO/Cu/ZnO thin films for the vehicle applications (ZnO/Cu/ZnO 박막의 차량용 저방사 및 전기광학적 특성 연구)

  • Yeon-Hak Lee;Sun-Kyung Kim;Tae-Yong Eom;Yong-Ha Jeong;Sang-Woo So;Young-Gil Son;Dong-Il Son;Daeil Kim
    • Journal of the Korean institute of surface engineering
    • /
    • v.56 no.6
    • /
    • pp.451-456
    • /
    • 2023
  • Transparent conducting films having a three layered structure of ZnO/Cu/ZnO (ZCZ) were deposited onto the glass substrates by using RF and DC magnetron sputtering at room temperature. The emissivity and opto-electrical properties of the films were investigated with a varying thickness(5, 10, 15 nm) of the Cu interlayer. With increasing the Cu thickness to 15 nm, the films showed a enhanced electrical properties. Although ZnO 30/Cu 15/ZnO 30 nm film shows a lower resistivity of 5.2×10-5 Ωcm, it's visible transmittance is deteriorated by increased optical absorbtion of the films. In addition, X-ray diffraction patterns indicated that the insertion of Cu interlayer improve the grain size of ZnO films, which is favor for the electrical and optical properties of transparent conducting films. From the observed low emissivity of the films, it is concluded that the ZCZ thin films with optimal thickness of Cu interlayer can be applied effectively for the car's window coating materials.

Springback Minimization using Bottoming in Al Can Deep Drawing Process (알루미늄 캔 딥드로잉에서 Bottoming을 이용한 스프링백 최소화)

  • Park, Sang-Min;Lee, Sa-Rang;Hong, Seokmoo
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.17 no.9
    • /
    • pp.302-307
    • /
    • 2016
  • The technology of multistage deep drawing has been widely applied in the metal forming industry, in order to reduce both the manufacturing cost and time. A battery can used for mobile phone production is a well-known example of multistage deep drawing. It is very difficult to manufacture a battery can, however, because of its large thickness to height aspect ratio. Furthermore, the production of the final parts may result in assembly failure due to springback after multistage deep drawing. In industry, empirical methods such as over bending, corner setting and ironing have been used to reduce springback. In this study, a bottoming approach using the finite element method is proposed as a practical and scientific method of reducing springback. Bottoming induces compression stress in the deformed blank at the final stroke of the punch and, thus, has the effect of reducing springback. Different cases of the bottoming process are studied using the finite element program, DYNAFORM, to determine the optimal die design. The results of the springback simulation after bottoming were found to be in good agreement with the experimental results. In conclusion, the proposed bottoming method is expected to be widely used as a practical method of reducing springback in industry.

Changes in Mechanical Properties of WC-Co by Ultrasonic Nanocrystal Surface Modification Technique (UNSM 기술을 이용한 초경의 기계적 특성변화)

  • Lee, Seung-Chul;Kim, Jun-Hyong;Kim, Hak-Doo;Choi, Gab-Su;Amanov, Auezhan;Pyun, Young-Sik
    • Tribology and Lubricants
    • /
    • v.31 no.4
    • /
    • pp.157-162
    • /
    • 2015
  • In this study, an ultrasonic nanocrystalline surface modification (UNSM) technique is applied to tungsten carbide-cobalt (WC-Co) to extend the service life of carbide parts used in press mold. The UNSM technique modifies the structure, reduces the surface roughness, increases the surface hardness, induces the compressive residual stress, and increases the wear resistance of materials by introducing severe plastic deformation. The surface roughness, hardness, and compressive residual stress of WC after UNSM treatment improve by about 42, 10, and 71%, respectively. A wear test under dry conditions is used to assess the effectiveness of the UNSM technique on the friction and wear behavior of WC. The UNSM technique is found to reduce the WC friction coefficient by approximately 21% and enhance the wear resistance by approximately 85%. The improved friction and wear behavior of WC may be mainly attributed to the increased hardness and compressive residual stress. Moreover, the WC specimen is treated by UNSM technique using three different WC, silicon nitride (Si3N4) and stainless steel (STS304) balls. The surface treated by WC balls shows the highest hardness when compared with treatment by stainless steel and silicon nitride balls. According to the obtained results, the UNSM technique is believed to increase the durability of the carbide component by improving the friction and wear behavior.

Industrial analysis according to lithography characteristics of digital micromirror device and polygon scanner (Digital Micromirror Device와 Polygon scanner의 Lithography 특성에 따른 산업적 분석)

  • Kim, Ji-Hun;Park, Kyu-Bag;Park, Jung-Rae;Ko, Kang-Ho;Lee, Jeong-woo;Lim, Dong-Wook
    • Design & Manufacturing
    • /
    • v.15 no.4
    • /
    • pp.65-71
    • /
    • 2021
  • In the early days of laser invention, it was simply used as a measuring tool, but as lasers became more common, they became an indispensable processing tool in the industry. Short-wavelength lasers are used to make patterns on wafers used in semiconductors depending on the wavelength, such as CO2 laser, YAG laser, green laser, and UV laser. At first, the hole of the PCB board mainly used for electronic parts was not thin and the hole size was large, so a mechanical drill was used. However, in order to realize product miniaturization and high integration, small hole processing lasers have become essential, and pattern exposure for small hole sizes has become essential. This paper intends to analyze the characteristics through patterns by exposing the PCB substrate through DMD and polygon scanner, which are different optical systems. Since the optical systems are different, the size of the patterns was made the same, and exposure was performed under the optimal conditions for each system. Pattern characteristics were analyzed through a 3D profiler. As a result of the analysis, there was no significant difference in line width between the two systems. However, it was confirmed that dmd had better pattern precision and polygon scanner had better productivity.

Blank Design of SPFH 590 Steel Sheet for Stamping of Center Hinge of Automotive via Analysis of Transfer Forming Process with Multi-Stages (다단 이송 성형 공정 해석을 통한 자동차 센터 힌지 성형용 SPFH 590 고강도 강판 블랭크 설계)

  • Ahn, Dong-Gyu;Song, Dong-Han;Sohn, Sang-Sik;Han, Gil-Young
    • Journal of the Korean Society for Precision Engineering
    • /
    • v.27 no.5
    • /
    • pp.75-84
    • /
    • 2010
  • The aim of this paper is to design the blank shape of SPFH 590 high strength steel for stamping of the center hinge of automotive via numerical analyses and experiments for multi-stages transfer forming process. Three-dimensional elasto-plastic finite element analyses for the transfer forming process with six stages were performed using a commercial code AUTOFORM V4.2. The influence of the blank shape on the formability and the shape conformity were quantitatively examined through the FE analyses. From the results of the FE analysis, a feasible shape of the blank and the forming load were estimated. Stamping experiments were carried out using the proposed blank shape. The results of experiments were shown that the center hinge parts with the desired shapes can be manufactured successfully as the proposed blank shape is used. Through the comparison of the results of the experiments with those of the analyses, it was shown that the estimation of blank shape using the FE analysis is a proper methodology to create a feasible shape of the blank for the center hinge of automotive.