Target-Composition Effect on Hydroxyapatite Thin Films Coated on Titanium by r.f. Sputtering

  • Hamagami, Jun-ichi;Kokubu, Daisuke;Umegaki, Takao;Yamashita, Kimihiro
    • The Korean Journal of Ceramics
    • /
    • 제4권4호
    • /
    • pp.372-376
    • /
    • 1998
  • Using calcium-phosphate-powder targets with the Ca/P ratios of 1.0-1.67, hydroxyapatite ($Ca_{10}(PO_4)_6(OH)_2$, HAp) thin films with 4-7㎛ thickness were prepared on titanium metal plates by r.f. magnetron sputtering, followed an annealing at $200^{\circ}C$ for 24 hr under a high water vapor pressure using an autoclave. All the specimens were systematically characterized by XRD, FT-IR, SEM and EDS analyses. The post-annealed films were confirmed to be a nonstoichiometric oxyhydroxyapatite by XRD and FT-IR measurements.

  • PDF

레진시멘트와 보철재료와의 접착 (Luting between Resin Cement and Dental Prosthetic Materials)

  • 김광만
    • 대한치과의사협회지
    • /
    • 제53권3호
    • /
    • pp.195-200
    • /
    • 2015
  • Cementation is the last procedure and an important factor to access successful fixed prosthodontic treatment. Even though there are many kinds of luting materials in dental field, the resin cements are popularly used in now. Metals, polymers and ceramics are used as a material of fixed dental prosthesis. The bonding mechanisms between teeth and fixed restorations are composed of mechanical and chemical mechanism. In dentistry, we are relying on mechanical bonding, but we tried to get chemical bonding and many ways are introduced. So, we have to approach luting procedure differently by the materials of prosthesis for clinical success. In this article, let us think the proper cementation ways according to each prosthesis material.

All-ceramic Crown 용 도재의 동적 피로특성 평가 (AN EVALUATION OF DYNAMIC FATIGUE CHARACTERISTICS OF DENTAL CERAMICS FOR ALL-CERAMIC CROWN)

  • 유형우;배태성;송광엽;박찬운
    • 대한치과보철학회지
    • /
    • 제35권4호
    • /
    • pp.781-792
    • /
    • 1997
  • This study was peformed to evaluate the dynamic fatigue characteristics of the dental ceramics for all-ceramic crown. A feldspathic porcelain of VMK68. glass ceramic of IPS-Empress, and glass infiltrated alumina ceramic of In-Ceram were used. Disc specimens were prepared to the final dimensions of 12 mm in diameter and 1 mm in thickness. The biaxial flexure test was conducted using a ball-on-three-ball method. 240 specimens were tested in $37^{\circ}C$ water by testing 20 samples at each of four loading rates:0.05, 0.2, 1, and 5mm/min. 60 specimens were tested in a moisture-free environment by testing 20 samples at 5mm/min. The inert strength of VMK68 was 80.25MPa, and the fatigue parameters were n=29.1, ${\sigma}_{fo}=52.90MPa$. The inert strength of IPS-Empress was 104.76MPa, and the fatigue parameters were n=32.46, ${\sigma}_{fo}=67.52MPa$. The inert strength of In-Ceram was 429.33MPa, and the fatigue parameters were n=31.46, ${\sigma}_{fo}=258.36MPa$. 10-year failure stresses of VMK68, IPS-Empress, and In-Ceram were 20.3MPa, 24.8MPa, and 93.6MPa, respectively. Failure strength and fatigue life showed the highest value in In-Ceram, and then, IPS-Empress and VMK68.

  • PDF

도재-금속의 결합 강도에 미치는 비금속 합금의 열처리 효과 (The effect of preheat treatment on ceramic to metal bond strength)

  • 김치영;김영곤;조현설
    • 대한치과기공학회지
    • /
    • 제24권1호
    • /
    • pp.33-41
    • /
    • 2002
  • In dental prosthetics, the application of metal-ceramic restorations has steadily increased since their introduction. This is due to excellent esthetics in combination with high mechanical stability. In order to optimum bond strength between metal and ceramics, controlled oxidation of metal substructure is essential factor. Beryllium containing and beryllium free Ni-Cr alloys for metal-ceramic restorations were evaluated for the metal-ceramic bond strength by changing heat treatment for oxide formation. A mechanical three-point bending test was employed to evaluate the interfacial bond strength of metal-ceramic. In each metal, plate type specimens were used for mechanical three-point bending test. With Ni-Cr alloys for metal ceramics, mechanical three-point bending test showed that double degassing was more available preheat treatment method than another. It was found that beryllium containing Ni-Cr alloys are more effective than beryllium-free for metal-ceramic bond strength.

  • PDF

Zirconia-Glass frit 조성에서 MgO 및 착색료가 소결체의 색상 변화에 미치는 영향 (Effect of MgO and coloring agents on the coloring in zirconia-glass frit system)

  • 권은자;최에스더;이규선;이채현
    • 한국산학기술학회논문지
    • /
    • 제10권8호
    • /
    • pp.2150-2156
    • /
    • 2009
  • 지르코니아($3Y-ZrO_2$)에 frit을 첨가하고 MgO를 조제로 첨가하거나 혹은 하소된 성형체에 액상의 착색료에 침지하는 방법을 통하여 착색하고 얻어진 소결체의 물성과 색상 변화를 고찰하였다. Frit가 20 wt% 첨가된 지르코니아-frit조성에 MgO가 첨가됨에 따른 색상의 변화는 소결온도가 높아짐에 따라 구별가능한 정도로 효과가 있음을 확인하였다. 이 때 색상의 변화 정도는 MgO의 첨가량 변화에 의한 효과 보다는 소결 온도의 변화에 의한 효과가 더 크게 나타났음을 확인할 수 있었다. 액상의 착색료에 침지한 후 소결한 경우에서는 frit의 첨가량이 증가함에 따라 반사도가 증가하는 것으로 나타났으며 착색료에 침지하지 않은 경우에 비하여 색상의 변화가 감소함을 알 수 있었고 frit은 색상의 변화를 억제하는 것으로 나타났다.

리튬디실리케이트 세라믹과 표면처리방법에 따른 라미네이트 베니어의 전단결합강도 비교 (Comparison of Shear Bonding Strength of Laminate Veneer by Lithium Disilicate Ceramics and Surface Treatment Methods)

  • 박상준;정인성
    • 대한치과기공학회지
    • /
    • 제41권3호
    • /
    • pp.177-185
    • /
    • 2019
  • Purpose: This study was to investigate the effect of three different surface treatments on the shear bond strength of lithium disilicate ceramics to enamel. Methods: Totally 60 lithium disilicate ceramic disc specimens were fabricated with IPS e.max press (Ivoclar Vivadent, Schaan, Liechtenstein) and Mazic Claro (Vericom, Korea). 30 specimens in each lithium disilicate ceramic were assigned to 3 groups of the each following surface treatment: 1) $50{\mu}m$ airborne particle abrasion+silane, 2) 9.5% hydroflouric acid etching (HF)+silane, 3) $50{\mu}m$ airborne particle abrasion+9.5% HF+silane. Lithium disilicate ceramic surfaces after surface treatments were AFM examined. The shear bond strength was measured in a universal testing machine at 0.5mm/min crosshead speed. All data were analyzed using a two-way ANOVA and Tukey's test(${\alpha}=0.05$). Results: The mean surface roughness of lithium disilicate ceramics ranged from $0.178{\mu}m$ to $0.441{\mu}m$. The mean shear bond strengths ranged from $23.81{\pm}2.78MPa$ to $33.99{\pm}4.85MPa$. Conclusion: 1. Mazic Claro showed higher shear bond strength than IPS e.max press at 3 different surface treatments, and no statistically significant was observed. 2. The shear bond strength of IPS e.max press was strongly enhanced as surface treated with $50{\mu}m$ airborne particle abrasion and 9.5% hydroflouric acid etching. And there was no statistical significance at the shear bond strength of Mazic Claro with surface treatments.

가압성형용 치과도재의 제조와 특성 (Fabrication and Properties of the Pressable Dental Porcelain)

  • 이은희;최희락;정해용
    • 한국재료학회지
    • /
    • 제16권3호
    • /
    • pp.157-162
    • /
    • 2006
  • Pressable ceramics have many applications in the field of dental industry because of their excellent esthetic, compressive strength, chemical durability. Despite these attractive characteristics, they have not been widely used since they are very brittle and extremly sensitive to porcelain. In this study, the fabrication of pressable dental porcelain ($SiO_2-Al_2O_3-K_2O-Na_2O$) as a function of contents of $Al_2O_3,\;BaO\;and\;ZrO_2$ were investigated. And then compressive strength, Vickers hardness, density and thermal expansion coefficient (TEC) tests have been carried out to evaluate properties of pressable dental porcelain fabricated. The property of pressable dental porcelain fabricated by adding of 15%$Al_2O_3$ and 2%BaO contents was closely approximated to that of natural tooth.

도재주조용 합금에 있어서 알루미륨 첨가에 따른 metal-ceramic과의 결합력 증진에 관한 연구 (A Study on Improvement of Metal-Ceramic Bonding Strength by Addition of Aluminum to Casting Metal Alloy)

  • 이재원;민병국;한민수
    • 대한치과기공학회지
    • /
    • 제23권2호
    • /
    • pp.161-170
    • /
    • 2002
  • The Purpose of this study was to investigate the chemically improvement of metal-ceramics bond strength in the course of recasting Ni-Cr metal composite system with 10wt.%, 20wt.% and 30wt.% aluminum respectively. We have tested the bond strength, micro-structure, chemical composition of each metal composites and metal- ceramic bond interfaces by 3-point bending strength tester, SEM and EDS. We have made the conclusions through this study as follow: 1. The most suitable amount of aluminum to the Ni-Cr metal composite recasting is 20wt. % for improving metal-ceramics bond strength with debonding strength value of 49.54 kgf/mm2. 2. The aluminum must be changed to small spread alumina like phases and second aluminum-metal composites phases in the morphology of Ni-Cr metal composite system by adding during it's casting. These second phases have inclined functional oxide phases mixed with metal elements and they must take roll to improvement of metal-ceramics bond strength. 3. In the case of 30wt.% aluminum appended to Ni-Cr metal composite system, an excess of second inclined functional oxide phases produce cracks and spalling of them apart from it's base material. It must be a important factor of reduction of metal-ceramics bond strength.

  • PDF

The effects of different polishing techniques on the staining resistance of CAD/CAM resin-ceramics

  • Sagsoz, Omer;Demirci, Tevfik;Demirci, Gamze;Sagsoz, Nurdan Polat;Yildiz, Mehmet
    • The Journal of Advanced Prosthodontics
    • /
    • 제8권6호
    • /
    • pp.417-422
    • /
    • 2016
  • PURPOSE. The purposes of this study were to evaluate the staining resistance of CAD/CAM resin-ceramics polished with different techniques and to determine the effectiveness of the polishing techniques on resin-ceramics, comparing it with that of a glazed glass-ceramic. MATERIALS AND METHODS. Four different CAD/CAM ceramics (feldspathic ceramic: C-CEREC Blocs, (SIRONA) and three resin-ceramics: L-Lava Ultimate, (3M ESPE), E-Enamic, (VITA) and CS-CeraSmart, (GC)) and one light cure composite resin: ME-Clearfil Majesty Esthetic (Kuraray) were used. Only C samples were glazed (gl). Other restorations were divided into four groups according to the polishing technique: nonpolished control group (c), a group polished with light cure liquid polish (Biscover LV BISCO) (bb), a group polished with ceramic polishing kit (Diapol, EVE) (cd), and a group polished with composite polishing kit (Clearfil Twist Dia, Kuraray) (kc). Glazed C samples and the polished samples were further divided into four subgroups and immersed into different solutions: distilled water, tea, coffee, and fermented black carrot juice. Eight samples ($8{\times}8{\times}1mm$) were prepared for each subgroup. According to CIELab system, four color measurements were made: before immersion, immersion after 1 day, after 1 week, and after 1 month. Data were analyzed with repeated measures of ANOVA (${\alpha}=.05$). RESULTS. The highest staining resistance was found in gl samples. There was no difference among gl, kc and cd (P>.05). Staining resistance of gl was significantly higher than that of bb (P<.05). Staining resistances of E and CS were significantly higher than those of L and ME (P<.05). CONCLUSION. Ceramic and composite polishing kits can be used for resin ceramics as a counterpart of glazing procedure used for full ceramic materials. Liquid polish has limited indications for resin ceramics.