Comparison of internal porosity of dental titanium castings with different casting machines (주조방식에 따른 티타늄 주조체의 내부결함 비교)

  • Lee, Kyung-Eun;Kim, Bu-Sob;Chung, In-Sung
    • Journal of Technologic Dentistry
    • /
    • v.29 no.2
    • /
    • pp.129-140
    • /
    • 2007
  • The purpose of this study was to evaluate the titanium castability (internal porosity) between pressure type casting machine & centrifugal casting machine with air-vent or not. Internal porosity is a well-known problem in dental titanium casting, resulting in inferior mechanical properties of dental restorations. To evaluate the castability, the square plate was chosen. 40 plate patterns($20{\times}20{\times}1.8mm$)were attached to funnel-shaped sprue. Then 20 plate patterns were attached air-vent. They were invested in titanium investment material and cast in a pressure type casting machine(20castings) and centrifugal casting machine(20castings). Each group were divided with air-vent(10castings) or not(10castings). The titanium castings were evaluated by radiographic photograph for the location of the internal porosities. The percentage porosity of each specimen was determined using standardized digital radiographs. The results were analyzed with analysis of variance and t-test for paired comparison between two groups.

  • PDF

Comparison of effect of desensitizing agents on the retention of crowns cemented with luting agents: an in vitro study

  • Jalandar, Sonune Shital;Pandharinath, Dange Shankar;Arun, Khalikar;Smita, Vaidya
    • The Journal of Advanced Prosthodontics
    • /
    • v.4 no.3
    • /
    • pp.127-133
    • /
    • 2012
  • PURPOSE. Many dentists use desensitizing agents to prevent hypersensitivity. This study compared and evaluated the effect of two desensitizing agents on the retention of cast crowns when cemented with various luting agents. MATERIALS AND METHODS. Ninety freshly extracted human molars were prepared with flat occlusal surface, 6 degree taper and approximately 4 mm axial length. The prepared specimens were divided into 3 groups and each group is further divided into 3 subgroups. Desensitizing agents used were GC Tooth Mousse and $GLUMA^{(R)}$ desensitizer. Cementing agents used were zinc phosphate, glass ionomer and resin modified glass ionomer cement. Individual crowns with loop were made from base metal alloy. Desensitizing agents were applied before cementation of crowns except for control group. Under tensional force the crowns were removed using an automated universal testing machine. Statistical analysis included one-way ANOVA followed by Turkey-Kramer post hoc test at a preset alpha of 0.05. RESULTS. Resin modified glass ionomer cement exhibited the highest retentive strength and all dentin treatments resulted in significantly different retentive values (In Kg.): GLUMA ($49.02{\pm}3.32$) > Control ($48.61{\pm}3.54$) > Tooth mousse ($48.34{\pm}2.94$). Retentive strength for glass ionomer cement were GLUMA ($41.14{\pm}2.42$) > Tooth mousse ($40.32{\pm}3.89$) > Control ($39.09{\pm}2.80$). For zinc phosphate cement the retentive strength were lowest GLUMA ($27.92{\pm}3.20$) > Control ($27.69{\pm}3.39$) > Tooth mousse ($25.27{\pm}4.60$). CONCLUSION. The use of $GLUMA^{(R)}$ desensitizer has no effect on crown retention. GC Tooth Mousse does not affect the retentive ability of glass ionomer and resin modified glass ionomer cement, but it decreases the retentive ability of zinc phosphate cement.

Mechanical and interfacial characterization of laser welded Co-Cr alloy with different joint configurations

  • Kokolis, John;Chakmakchi, Makdad;Theocharopoulos, Antonios;Prombonas, Anthony;Zinelis, Spiros
    • The Journal of Advanced Prosthodontics
    • /
    • v.7 no.1
    • /
    • pp.39-46
    • /
    • 2015
  • PURPOSE. The mechanical and interfacial characterization of laser welded Co-Cr alloy with two different joint designs. MATERIALS AND METHODS. Dumbbell cast specimens (n=30) were divided into 3 groups (R, I, K, n=10). Group R consisted of intact specimens, group I of specimens sectioned with a straight cut, and group K of specimens with a $45^{\circ}$ bevel made at the one welding edge. The microstructure and the elemental distributions of alloy and welding regions were examined by an SEM/EDX analysis and then specimens were loaded in tension up to fracture. The tensile strength (TS) and elongation (${\varepsilon}$) were determined and statistically compared among groups employing 1-way ANOVA, SNK multiple comparison test (${\alpha}$=.05) and Weibull analysis where Weibull modulus m and characteristic strength ${\sigma}_0$ were identified. Fractured surfaces were imaged by a SEM. RESULTS. SEM/EDX analysis showed that cast alloy consists of two phases with differences in mean atomic number contrast, while no mean atomic number was identified for welded regions. EDX analysis revealed an increased Cr and Mo content at the alloy-joint interface. All mechanical properties of group I (TS, ${\varepsilon}$, m and ${\sigma}_0$) were found inferior to R while group K showed intermediated values without significant differences to R and I, apart from elongation with group R. The fractured surfaces of all groups showed extensive dendritic pattern although with a finer structure in the case of welded groups. CONCLUSION. The K shape joint configuration should be preferred over the I, as it demonstrates improved mechanical strength and survival probability.

THE EFFECT OF SOLDER AND LASER WELD ON CORROSION OF DENTAL ALLOYS (납착법과 레이저융합법이 치과용 합금의 부식에 미치는 영향)

  • Baik Jin;Woo Yi-Hung;Choi Dae-Gyun;Choi Boo-Byung
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.43 no.2
    • /
    • pp.264-279
    • /
    • 2005
  • Statement of problem. Intraoral corrosion not only affects the esthetic and function of metallic dental restoration, but also has biologic consequences as well. Therefore, corrosion is considered a primary factor when choosing the dental alloy and laboratory technique. Purpose. The objective of this study was to compare the effects of solder and laser weld on corrosion Material and methods. Test specimens were made of 2 types of gold alloys, Co-Cr and Ni-Cr alloy and fabricated 3 methods, respectively: as cast, solder, and laser weld. For the analysis of corroding properties, potentiodynamic polarization test and immersion test conducted. The potentiodynamic polarization scan curve were recorded in 0.9% NaCl solution(pH 7) using Potentiostat/Galyanostat Model 273A. All specimens were exposed to 0.9% NaCl solution(pH 2.3) during 14 days. Elemental release into corrosive solution was measured by atomic emission spectrometry Differences in corrosion potential and mass release were determined using ANOVA. Results and conclusion. Through analyses of the data, following results were obtained. 1. In Pontor MPF and Wiron 99, corrosion potential of the solder group was statistically lower than as cast and laser weld group (p<0.05) , but there was no difference between corrosion potential of solder group and laser weld group in Pontor MPF and no differences between as cast and laser weld group (p>0.05). In Jel-Bios 10 and Wirobond, there was no difference of corrosion potential according to joining methods(p>0.05). 2. In all tested alloys, the amount of released metallic ion was greatest in the solder group(p<0.05). There was no difference between as cast group and laser weld group in Jel-Bios 10 and Wirobond(p>0.05). 3. In scanning electron microscopic examination. except soldered Wiron 99 specimens, it is impossible to discriminate the corrosive property of solder and laser weld. 4. Under the this experimental circumstances, laser weld appears superior to the solder when corrosion is considered.

A Study on How Cyclic Casting of Base Metal Alloy for Dental Ceramic Crown May Effects upon Its Mechanical Properties and Microstructure (치과 도재용착 주조관용 비귀금속 합금의 반복주조가 기계적 특성 및 미세조직에 미치는 영향)

  • Choi, Un-Jae;Shin, Moo-Hak;Chung, Hee-Sun;Koh, Myoung-Won
    • Journal of Technologic Dentistry
    • /
    • v.25 no.1
    • /
    • pp.9-20
    • /
    • 2003
  • Using a nickel-chrome casting alloy called 'Rexillium V' which is also available as base metal alloy for dental ceramic crown, 4 types of mixtures(A, B, C, D) with old and new metal were prepared for cyclic casting. The results of cyclic casting can be outlined as follows: 1. For Vickers hardness after casting, specimen A and D tended to have lower hardness in the course of cyclic casting, while specimen B and C tended to higher hardness. 2. The results of X-ray diffraction analysis showed that major crystal phase contained nickelchrome compounds and carbide. 3. The observation results of SEM photographs after cyclic casting show that there was a significant tendency to have similar structures among experimental groups. 4. The results of EDX analysis after cyclic casting showed that there were little differences in chemical composition between parent metal and base metal alloy. Although industrial nickel-chrome cast alloy did not show any significant change in material properties even through cyclic casting over several times, it is recommended that more there be more in-depth studies on how to detect any potential corrosion, discoloration and toxication of dental ceramic crown implanted in patient's oral cavity.

  • PDF

Dental hygienists work-related musculoskeletal symptoms and factor analysis (치과위생사의 직무관련 근골격계 자각증상과 요인분석)

  • Park, Sae-Rom;Shim, Youn-Soo;Jung, Sang-Hee
    • Journal of Korean society of Dental Hygiene
    • /
    • v.12 no.4
    • /
    • pp.685-693
    • /
    • 2012
  • Objectives : This research was conducted to find the subjective symptoms of musculoskeletal system for main jobs and job posture. Methods : A survey was conducted from September 15, 2011 to October 7, 2011 and 357 dental hygienists were responded. The survey was consisted of the working environment and medical equipments, psycho-social characteristics, health habits and education, job posture, subjective symptoms of musculoskeletal system pain, and so on. Results : In the survey on the frequency of job posture of dental hygienists by jobs, said they cast down or tilt their head by 15 degrees or more or twist or bend their back. The result of the analysis on the subjective symptoms of musculoskeletal system by main job showed that they experienced a pain in neck, shoulder, and back, although the order differed. The order of subjective symptoms of musculoskeletal system for casting down or turning head by 15 degrees or more, twisting or bending back, having shoulders not parallel to the ground, sitting at the end of a chair, and supporting the whole body with one leg or pressing on a pedal for treatment was from the shoulders to the neck to the back. The order of subjective symptoms of musculoskeletal system for having arms too far from the body or hunching for treatment and bending wrists inward or outward for treatment was from the shoulders to the back to the neck. Conclusions : Due to the characteristics of the job which requires one to have a proper view of a patient's oral cavity, most of the postures included casting down of head or bending of back. Therefore a development of new postures is needed to replace the existing job postures which pressure the musculoskeletal system. And shift rotation can be used as a preventive measure.

Effects of self-ligating brackets and other factors influencing orthodontic treatment outcomes: A prospective cohort study

  • Jung, Min-Ho
    • The korean journal of orthodontics
    • /
    • v.51 no.6
    • /
    • pp.397-406
    • /
    • 2021
  • Objective: The purpose of this study was to evaluate the effects of self-ligating brackets (SBs) and other factors that influence orthodontic treatment outcomes. Methods: This two-armed cohort study included consecutively treated patients in a private practice. The patients were asked to choose between SBs and conventional brackets (CBs); if any patient did not have a preference, he or she was randomly allocated to the CB or SB group. All patients were treated using an identical archwire sequence. Evaluated parameters were as follows: treatment duration, number of bracket failures, poor oral hygiene, poor elastic wear, extraction, use of orthodontic mini-implants (OMI), OMI failure, American Board of Orthodontics (ABO) Discrepancy Index (DI), arch length discrepancy, and ABO Cast-Radiograph Evaluation (CRE) score. Stepwise regression analysis was performed to generate the equation for prediction of the CRE. Results: The final sample comprised 134 patients with an average age of 22.73 years. The average DI, CRE, and treatment duration were 21.81, 14.25, and 28.63 months, respectively. Analysis of covariance showed a significant difference in CRE between the CB and SB groups after adjusting for the effects of confounding variables. Stepwise regression analysis using four variables, namely extraction, SB use, poor elastic wear, and additional appliance use, could explain only 25.2% of the variance in the CRE. Conclusions: Although the CRE was significantly better for CBs than for SBs, the clinical significance of this result seems to be limited. Extraction, SB use, poor elastic wear, and additional appliance use may have significant effects on treatment outcomes.

Long-term stability of dentoalveolar, skeletal, and soft tissue changes after non-extraction treatment with a self-ligating system

  • Basciftci, Faruk Ayhan;Akin, Mehmet;Ileri, Zehra;Bayram, Sinem
    • The korean journal of orthodontics
    • /
    • v.44 no.3
    • /
    • pp.119-127
    • /
    • 2014
  • Objective: To evaluate the long-term effects of self-ligating brackets (SLBs) on transverse dimensions of arches and skeletal and soft tissues and to quantitatively evaluate the treatment outcome after non-extraction treatment with SLBs. Methods: The sample consisted of 24 (18 female and six male) subjects, with a mean age of $14.23{\pm}2.19$ years, who received treatment with the Damon$^{(R)}$3 appliances. Complete records including cephalometric radiographs and plaster models were obtained before treatment (T1), immediately after treatment (T2), six months after treatment (T3), and two years (T4) after treatment. Digital study models were generated. Twenty lateral cephalometric, six frontal cephalometric, and eight dental cast measurements were examined. The Peer Assessment Rating index was used to measure the treatment outcome. The Wilcoxon test was applied for statistical analysis of the changes. Results: There were significant increases in all transverse dental cast measurements with active treatment. There was some significant relapse in the long term, particularly in maxillary width (p < 0.05). Statistically significant increases were found in nasal (p < 0.001), maxillary base, upper molar, lower intercanine, and antigonial (p < 0.05) widths in T1-T2. Lower incisors were proclined and protruded in T1-T2. Conclusions: SLBs correct crowding by mechanisms involving incisor proclination and protrusion and expansion of the dental arches, without induction of clinically significant changes in hard and soft tissues of the face.

The effect of the gold based bonding agents on the bond between Ni-Cr alloys and ceramic restorations (Ni-Cr합금과 도재간의 결합력에 gold-based bonding agent가 미치는 영향)

  • Lee, Jung-Hwan;Joo, Kyu-Ji
    • Journal of Technologic Dentistry
    • /
    • v.29 no.2
    • /
    • pp.213-223
    • /
    • 2007
  • The success of a porcelain fused to metal (PFM) restoration depends upon the quality of the porcelain-metal bond. The adhesion between metal substructure and dental porcelain is related to the diffusion of oxygen to the reaction layer formed on cast-metal surface during firing. The purposed of this investigation was to study the effects of gold based bonding agent on Ni-Cr alloy-ceramic adhesion between porcelain matrix, gold based bonding agent and metal substructure interface. gold based bonding agent have been applied as an intermediate layer between a metal substructure and a ceramic coating. gold based bonding agent(Aurofilm NP, Metalor, Swiss) was applied on Ni-Cr alloy surface by four method. Surfaces only air abraded with 110${\beta}\neq$ Al2O3 particles were used as control. metal ceramic adhesion was evaluated by a biaxial flexure test(N=5) and volume fraction of adherent porcelain was determined by SEM/EDS analysis. Result of this study suggest that the layering sequence of gold based bonding agent is very important and can improve porcelain adherence to PFM.

  • PDF

Study on the Corrosin Properties of Au-Ag-Cu Dental Alloys (치과용 Au-Ag-Cu계 합금의 부식특성에 관한 연구)

  • Kim, Bu-Sob
    • Journal of Technologic Dentistry
    • /
    • v.14 no.1
    • /
    • pp.23-43
    • /
    • 1992
  • Corrosion characteristics of four commerial gold-based dental alloys(C-1; Au75%, Ag13.9%, Pd3%, Cu & etc.,8.1%, C-2 ;Au 52.08, Ag 24%, Pd 5%, Cu & etc.,18.92, C-3 ; Au 53%, Ag 22%, Pd 5%, Pt 3% Cu & etc.,17%, C-4 ; Au 53%, Pd4, Pt1.5%, Ag & Cu & etc.,41.5%) and four experimental ternary Au-Ag-Cu alloys(E-1 ; Au 50%, Ag 30%, Cu 20%, E-2 ; Au 50%, Ag 20%, Cu 30%, E-3 ; Au 50%, Ag 10%, Cu 40%, E-4 ; Au 50%, Ag 40%, Cu 10%) were investigated by potentiodynamic polarization analysis and the structure was examined by optical microscope and SEM. All corrosion testing was conducted in 1% NaCl solution. The main results are as follows : 1. The corrosion resistence of commercial alloys was decreased in the order of C-1, C-3, C-4, C-2. C-2. 2. The E-1 and E-3 ternary alloys exhibits the higher corrosion resistence than E-2 and E-4 alloys. 3. The cast microstructure of alloys reveals dendrite morphology which shows the significant microsegregation caused by the difference in the diffusion rate between liquid and solid. 4. It is found that the surface corrosion products were mainly AgCl by X-ray diffraction results.

  • PDF