  • This study, involving thirty-two patients with carcinoma of uterine cervix treated by high dose rate intracavitary irradiation using a remotely controlled afterloading system, compares the doss at point A and 8 with the Curie-minutes prescription. A linear least-square regression analysis was used to compare the two sets of date. Correlation coefficients between doses at points A and B and the Ci-min prescription are 0.92 (p<0.001) and 0.90 (p<0.001), respectively, and linear relationship is observed between these two system. The limitation and significance of the comparison of the two approaches to intracavitary dosimetry is discussed.

  • PDF

압전세라믹 $(Pb_{1-x}C_{ax})((Co_{\frac{1}{2}}W_{\frac{1}{2}})_yTi_{1-y})O_3+(MnO_2, NiO)$ (Fabrication and Properties of $(Pb_{1-x}C_{ax})((Co_{\frac{1}{2}}W_{\frac{1}{2}})_yTi_{1-y})O_3+(MnO_2, NiO)$ piezoelectric ceramic)

  • 문동진;도시홍;장지원
    • 한국음향학회지
    • /
    • 제6권4호
    • /
    • pp.55-63
    • /
    • 1987
  • $PbTiO_3$는 perovskite구조를 가진 강유전체로써 Curie온도가 높고 유전율이 작아 고온. 고주파재료로 주목되어왔으나 curie온도 이하에서 결정이방성(C/a)이 크기 때문에 소결 후 결정립(grain)이 입계(grain boundary)에서 분리되어 치밀하고 기계적으로 강한 세라믹을 얻을 수 없었고, 항전력이 커 분극이 어려위 실용화 되지 않았다. 본 연구에서는 $PbTiO_3$에 Pb일부를 Ca로 치환하고 Mn, Ni, Co및 W의 산화물을 첨가하여 치수가 크고 기계적으로 강한 세라믹을 제조하였고, 그 분극 조건도 PZT의 분극 조건과 같은 정도로 개선하였다. 그리고 결합계수이방성(Kt/Kp)이 $5\sim6$으로 크고, 기계적 품질계수 Qm이 $310\sim480$ 정도로 낮으며, 유전상수가 200대의 값으로 PZT보다 1/5정도 작은 고온, 고주파. 광대역 초음파 발진자 재료로 적합한 압전세라믹을 제조 연구하였다.

  • PDF

Mn Oxide의 첨가에 따른 PSS-PT-PZ 세라믹의 초전특성 (Pyroelectric Properties of Modified PZT Ceramics with $MnO_2$ Addition)

  • 신상현;김영훈;박기운;강동헌;김영호;길상근
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2002년도 하계학술대회 논문집 Vol.3 No.2
    • /
    • pp.746-748
    • /
    • 2002
  • The effect of $MnO_2$ addition in $0.05Pb(Sn_{0.5}Sb_{0.5})O_3-0.8PbZrO_3-0.15PbTiO_3$(0.05PSS-0.8PZ-0.15PT) ceramics on crystal structure and electrical properties were studied. The sintering temperature and time were $1230^{\circ}C{\sim}1270^{\circ}C$ and 2hr, respectively. Then crystal structure, dielectric and pyroelectric properties were investigated. All the poled specimens showed the lower dielectric constant and $tan{\delta}$ than the unpoled specimens. Dielectric constant at 1kHz of the 0.05PSS-0.8PZ-0.15PT(MnO2 0.3wt%) system specimen sintered at $1250^{\circ}C$ for 2hr were 270 and showed the lowest $tan{\delta}$ of 0.2% after poling of $2kV_{DC}/mm$ at $150^{\circ}C$ for 30 minutes. Pyroelectric coefficient was maximum value of $50nC/cm^2K$ and Curie temperature was $224^{\circ}C$.

  • PDF

Magnetic Properties of Transition Metal-implanted ZnO Nanotips Grown on Sapphire and Quartz

  • Raley, Jeremy A.;Yeo, Yung-Kee;Hengehold, Robert L.;Ryu, Mee-Yi;Lu, Yicheng;Wu, Pan
    • Journal of Magnetics
    • /
    • 제13권1호
    • /
    • pp.19-22
    • /
    • 2008
  • ZnO nanotips, grown on c-$Al_2O_3$ and quartz, were implanted variously with 200 keV Fe or Mn ions to a dose level of $5{\times}10^{16}cm^{-2}$. The magnetic properties of these samples were measured using a superconducting quantum interference device (SQUID) magnetometer. Fe-implanted ZnO nanotips grown on c-$Al_2O_3$ showed a coercive field width of 209 Oe and a remanent field of 12% of the saturation magnetization ($2.3{\times}10^{-5}emu$) at 300K for a sample annealed at $700^{\circ}C$ for 20 minutes. The field-cooled and the zero-field-cooled magnetization measurements also showed evidence of ferromagnetism in this sample with an estimated Curie temperature of around 350 K. The Mn-implanted ZnO nanotips grown on c-$Al_2O_3$ showed superparamagnetism resulting from the dominance of a spin-glass phase. The ZnO nanotips grown on quartz and implanted with Fe or Mn showed signs of ferromagnetism, but neither was consistent.

솔잎혹파리에 대한 방사선동위원소 표식방법에 관한 연구 (Radioisotope Labelling Method of Pine Gall Midge (Thecodiplosis japonensis UCHIDA et INOUYE))

  • 권신한;정규회;유준
    • 한국응용곤충학회지
    • /
    • 제17권3호
    • /
    • pp.155-160
    • /
    • 1978
  • 솔잎혹파리의 비산거리를 조사하기 위해서 방사성 동위원소인 $^{45}Ca$$^{32}P$의 표식방법에 관한 기초 실험을 하였다. 1. $^{45}Ca$를 유충기에 표식 시켰을때 성충에서는 방사능이 검출되지 않았다. 즉 생물학적 반감기가 짧아 체내축적이 않되었다. 2. 충영내 유충의 방사능 표식는 $^{45}Ca$ 처리시 10월이전에는 점차 증가하다가 10월 이후 부터는 점차 낮아져 평형상태를 유지하는 것으로 보아 유충은 10월 이후에 섭식을 작게 하는 것으로 본다. 3. $^{32}P$에 의한 충영내 노숙유충의 표식율은 3주째가 가장 높았으나 반감기가 짧은 까닭에 시일의 경과에 따라 급속한 표식방사능의 감소를 보인 결과로 미루어 $^{32}P$는 수간주입에 의해 성충을 표식하기에는 부적당하였다. 4. 월동 노숙유충체를$^{32}P$용액으로 처리하여 표식방사능을 검출할 수 있는 최적처리농도는 비방사능이 0.5uCi/ml에 침지을 30분간 한 후 흐르는 물에 10분간 세척하늘 방법이었다. 그러나 이 농도에서 침지시간은 20분 이상으로 하여야 $^{32}P$가 유충체내에 충분히 침투되었다

  • PDF

비정질 Ge1-xMnx 박막의 전기적, 자기적 특성에 미치는 열처리 효과 (Annealing Effect on Magnetic and Electrical Properties of Amorphous Ge1-xMnx Thin Films)

  • 이병철;김동휘;찬티난안;임영언;김도진;김효진;유상수;백귀종;김창수
    • 한국자기학회지
    • /
    • 제19권3호
    • /
    • pp.89-93
    • /
    • 2009
  • 저온 증착법으로 성장시킨 비정질 $Ge_{1-x}Mn_x$ 박막을 열처리하여 전기적, 자기적 특성을 연구하였다. 비정질 박막의 두께는 $1,000{\sim}5,000\;{\AA}$이고 비정질 $Ge_{1-x}Mn_x$ 박막을 고 진공 분위기 하에서 각각 $300^{\circ}C$, $400^{\circ}C$, $500^{\circ}C$, $600^{\circ}C$, $700^{\circ}C$ 온도에서 3분 동안 열처리 하였다. 원 시료의 $Ge_{1-x}Mn_x$ 박막을 X-선 회절로 분석해보면 비정질 구조를 보였지만 열처리를 함으로써 결정화되었다. 비정질 $Ge_{1-x}Mn_x$ 박막에서 결정화가 이루어진 온도는 Mn 농도에 따라 변화하였다. 비정질 $Ge_{1-x}Mn_x$ 박막은 p형 캐리어를 가지고 있고 열처리 동안에도 캐리어 형태는 변하지 않았다. 하지만, 전기 비저항은 열처리 온도가 증가함에 따라 증가하였다. 자기적 특성에서 원 시료의 비정질 $Ge_{1-x}Mn_x$ 박막은 강자성특성을 보이면서 큐리온도는 약 130 K 정도이다. 열처리한 $Ge_{1-x}Mn_x$ 박막의 큐리온도와 포화 자화값은 열처리 온도에 따라 증가한다. 자화거동과 X-선 분석을 통해 열처리한 $Ge_{1-x}Mn_x$ 박막에 전기적, 자기적 특성의 변화는 강자성 $Ge_3Mn_5$ 상이 형성되었음을 나타낸다.

$La_2O_3$가 첨가된 modified PZT계의 제조 및 특성 (Fabrication and characteristics of modified PZT System doped With $La_2O_3$)

  • 황학인;박준식;오근호
    • 한국결정성장학회지
    • /
    • 제7권3호
    • /
    • pp.418-427
    • /
    • 1997
  • $La_2O_3$가 각각 0, 0.1, 0.3, 0.5, 0.7, 1, 3, 5 mole% 첨가된 $0.05pb(Sn_{0.5}Sb_{0.5})O_3+0.11PbTiO_30.84PbZroO_3+0.4Wt%MnO_2$ (이하 0.05PSS -0.11PT-0.84PZ+0.4wt%$MnO_2$)계를, $1250^{\circ}C$에서 $PbZrO_3$를 분위기 분말로 사용하여 성형체 무게의 1/2을 함께 넣고 소결체를 제조하여 그 특성을 분석하였다. 소결체의 밀도는 7.683 g/$\textrm {cm}^3$에서 7.515 g/$\textrm {cm}^3$ 범위였으며, 3 mole% $La_2O_3$를 첨가한 경우 가장 높은 값을 나타내었다. 0에서 5 mole% 범위에서 $La_2O_3$ 첨가량을 증가시킬 때 평균 입경이 9.0 $\mu \textrm{m}$에서 1.3 $\mu\textrm{m}$까지 감소되었다. 결정구조의 경우 $La_2O_3$첨가량을 0에서 1 mole%로 할 때 0.05PSS-0.11 PT-0,84PZ계에서 고용된 상을 형성하였으나 3, 5 mole%로 첨가량을 증가시킴에 따라 제2차 산이 형성되었고, 소결체를 $120^{\circ}C$ 또는 $140^{\circ}C$에서 $5 KV_{DC}$ /mm로 20분간 poling 전후에 $La_2O_3$ 첨가량이 0 에서 3 mlole%까지 증가될수록 1KHz에서의 유전 상수는 증가되었으며, 유전손실은 모든 경우에서 1 % 미만의 값을 나타내었다. $La_2$O$_3$첨가량이 0, 0.5, 1, 3 mole%로 증가됨에 따라 큐리온도가 208$^{\circ}C$, 183$^{\circ}C$, $152^{\circ}C$ 그리고 $127^{\circ}C$로 감소되었다. $La_2O_3$가 증가됨에 따라 대체로 $K_{p}$ 증가되었으며 0.7 mlole%의 $La_2O_3$를 첨가한 소결체를 $140^{\circ}C$에서 poling한 경우 가장 높은 $K_p$값으로 14.5 %를 나타내었다.