• 제목/요약/키워드: Curie temperature ($T_c$)

검색결과 117건 처리시간 0.025초

Mossbauer Study of nano-sized (Li_{0.5x}Fe_{0.5x}Zn_{1-x})Fe_2O_4$ particles

  • J. C. Sur;Kim, T. S.;T. Y. Ha;Lee, J. K.;S. H. Gee;Y. K. Hong;Park, M. H.;D. W. Erickson;P. J. Lamb
    • 한국자기학회:학술대회 개요집
    • /
    • 한국자기학회 2002년도 동계연구발표회 논문개요집
    • /
    • pp.92-93
    • /
    • 2002
  • The substituted lithium ferrites combine useful ferromagnetic properties with high Curie temperature ranging from 55$0^{\circ}C$ to 85$0^{\circ}C$, [1] high saturation magnetization, [2] and low microwave dielectric loss.[3] Saturation magnetization of (Z $n_{1-x}$ F $e_{x}$)A[L $i_{0.5x}$F $e_{ 2-0.5x}$]$_{B}$ $O_4$ increased with zinc concentration, followed by a decrease at x = 0.7.[4] This is attributed to a dilution of the A-site with zinc which initially causes an increase in saturation magnetization due to the dominance of the B-site. (omitted)d))d)d))

  • PDF

Si1-xMnxTe1.5 단결정의 구조적, 광학적, 자기적 특성에 관한 연구 (Structural, Optical, and Magnetic Properties of Si1-xMnxTe1.5 Single Crystals)

  • 황영훈;엄영호;조성래
    • 한국자기학회지
    • /
    • 제16권3호
    • /
    • pp.178-181
    • /
    • 2006
  • 본 연구에선는 수직 Bridgman 법으로 묽은 자성 반도체 $Si_{1-x}Mn_xTe_{1.5} $ 단결정을 성장시켜 Mn의 조성비 변화에 따른 광학적, 전지적, 그리고 자기적 특성을 조사하였다. X-선 회절 실험으로부터 육방정계(hexagonal) 구조임을 확인하였다. 광흡수 측정으로부터 에너지 띠 간격은 조성비 x와 온도 증가에 대하여 감소함을 보였다. 성장시킨 시료의 경우 강자성 특성을 나타내었으며, Curie 온도는 80K 이상이었다. Mn의 조성비가 증가함에 따라 평균 자기 모멘트와 보자력 값은 증가하였다.

저온에서 소결된 Ba(Ti0.9Zr0.1)O3 세라믹스의 유전 특성 및 전기 열량 효과 (Dielectric Properties and Electro-Caloric Effects of Low Temperature Sintering Ba(Ti0.9Zr0.1)O3 Ceramics)

  • 류주현
    • 한국전기전자재료학회논문지
    • /
    • 제30권1호
    • /
    • pp.13-16
    • /
    • 2017
  • In this study, in order to develop composition ceramics for refrigeration device application, $Ba(Ti_{0.9}Zr_{0.1})O_3$ composition was fabricated using conventional solid-state method. Electrocaloric effect of this ceramic was investigated using the characteristics of P-E hysteresis loops at wide temperature range from room temperature to $150^{\circ}C$. Curie temperature of $Ba(Ti_{0.9}Zr_{0.1})O_3$ ceramics showed $80^{\circ}C$. The maximum value of ${\Delta}T=0.12^{\circ}C$ in ambient temperature of $115^{\circ}C$ under 30 kV/cm was appeared. It is concluded that $Ba(Ti_{0.9}Zr_{0.1})O_3$ ceramics can be applied as refrigeration device application.

Ba(Ti1-xZrx)O3 세라믹스의 유전 및 전기열량 특성 (Dielectric and Electrocaloric Properties of Ba(Ti1-xZrx)O3 Ceramics)

  • 라철민;류주현;이지영
    • 한국전기전자재료학회논문지
    • /
    • 제30권4호
    • /
    • pp.223-228
    • /
    • 2017
  • In this study, in order to develop composition ceramics for refrigeration device application at a temperature of less than $90^{\circ}C$, a $Ba(Ti_{1-x}Zr_x)O_3$ composition was fabricated using a conventional solid-state method. Electrocaloric properties of these ceramics were investigated using the characteristics of P-E hysteresis loops in a wide temperature range from room temperature to $150^{\circ}C$. The Curie temperature of $Ba(Ti_{1-x}Zr_x)O_3$ ceramics decreased with the increase of x. The maximum value of ${\Delta}T=0.07^{\circ}C$ in an ambient temperature of $85^{\circ}C$ under 30 kV/cm appeared when x = 0.125. It was concluded that the composition (x = 0.125) ceramics can be used for refrigeration device applications.

자기 캐패시터용 (Ba Sr Mg)$TiO_3$ 세라믹스의 제조 및 유전특성 (The Preparation and Dielectric Properties of (Ba Sr Mg)$TiO_3$Ceramic Capacitors)

  • 김범진;박태곤
    • E2M - 전기 전자와 첨단 소재
    • /
    • 제10권7호
    • /
    • pp.674-681
    • /
    • 1997
  • Ternary compound ceramics, (1-y-x) BaTiO$_3$-y SrTiO$_3$-x MgTiO$_3$(0.00 x 0.20), were fabricated by the conventional ceramic process. The structural and dielectric properties of specimens were investigated while varying the composition and sintering temperature(1,200~1,45$0^{\circ}C$) in order to obtain the optimum condition of capacitor. As is well known, Curie temperature(T$_{c}$) of high dielectric-based ceramic(BaTiO$_3$) was shifted and temperature of capacitance was decreased in according to increase of solid solution with (Sr, Mg)TiO$_3$. As a result, a suitable condition of compound rate for capacitor was obtained such as the BSM-11(0.8BaTiO$_3$-0.1SrTiO$_3$-0.1MgTiO$_3$), and sintering temperature was sintered at 1,25$0^{\circ}C$ for two hours. In this case, dielectric constant<1,300, dielectric loss(tan$\delta$)<0.03, and the variation rate of capacitance had less than 3% in the range -10~7$0^{\circ}C$.>.

  • PDF

Pb(Sb1/2Sn1/2)O3-PbTiO3-PbZrO3 세라믹스의 유전 및 압전 특성에 관한 연구 (A Study on the Dielectric and Piezoelectric properties of the Pb(SbS11/2TSnS11/2T)OS13T-PbTiOS13T-PbZrOS13T Ceramics)

  • 정장호;류기원;이성갑;이영희
    • 대한전기학회논문지
    • /
    • 제41권5호
    • /
    • pp.517-524
    • /
    • 1992
  • In this study, 0.10Pb(SbS11/2TSnS11/2T)OS13T-(0.90-x)PbZrOS13T (0.25 x 0.40) ceramics were fabricated by the atmospheric method. The sintering temperature and time were 1250[$^{\circ}C$] and 2[2hr], respectively. The structureal, dielectric and piezoelectric properties with composition of PbTiOS13T were studied. As the results of XRD ans SEM, the crystal structure of a specimen was rhombohedral, lattice constant and average grain size were decreased with increasing the contents of PbTiOS13T. Relative dielectric constant and Curie temperature were increased with increasing the contents of PbTiOS13T, 0.10PSS-0.40PT-0.50PZ specimen had the highest values of 904 and 265[$^{\circ}C$], respectively. In increasing of PbTiOS13T contents form 25[mol%] to 40[mol%], piezoelectric charge constant and electromechanical coupling factors were increased form 114[pC/N] to 142[pC/N], 17[%] to 24[%] and mechanical quality factor were decreased with increasing the contents of PbTiOS13T. In the 0.10PSS-0.40PT-0.50PZ specimens, those values were 14.2[kV/cm] and 9.43[x10S0-6TC/cmS02T], resectively.

Magnetoresistance behavior of $La_{1-\chi}Sr_\chiCoO_{3-\delta}$ films around the metal-insulator transition

  • Park, J. S.;Park, H. G.;Kim, C. O.;Lee, Y. P.;V. G. Prokhorov
    • 한국진공학회지
    • /
    • 제12권S1호
    • /
    • pp.100-103
    • /
    • 2003
  • The magnetoresistance (MR) of $La_{1-\chi}S_{\chi}CoO_{3-\delta}$ films prepared by pulsed-laser deposition were investigated in order to clarify the magnetotransport properties around the metal-insulator transition. For the films in the metallic state ($\chi$ > 0.25), the MR(T) manifests a small peak at the Curie temperature due to the spin-disorder scattering. The transition of the film into the insulating state ($\chi\;\leq$ 0.25) is accompanied by an essential growth of the MR and results in a significant increase in the MR(T) with decreasing temperature, due to a phase separation into the ferromagnetic-metal clusters and the insulating matrix.

Cu - Ni Ferrite의 결정학적 및 Mossbauer 연구 (Crystallographic and Moss bauer Studies of Cu-Ni Ferrite)

  • 김우철;홍성렬;지상희;이승화;엄영랑;김철성
    • 한국자기학회지
    • /
    • 제7권2호
    • /
    • pp.76-81
    • /
    • 1997
  • $Cu_{0.9}Ni_{0.1}Fe_{2}O_{4}$의 결정학적 및 자기적 성질을 Mossbauer 분광법과 X-선 회절법으로 연구하였다. 결정구조는 입방 spinel구조 갖으며, 격자상수 $a_{0}$ = 0.386 .angs. 임을 알았다. 또한 thermal scan 방법에 의해 Curie 온도 $T<_{c}$ = 755 K로 결정하였다. 이성질체 이동결과 사면체(A) 자리와, 팔면체 (B) 자리 모두 철이온의 전하상태가 +3가 임을 알았다. A, B 자리의 Debye 온도는 각각 568 K 와 194 K 임을 알았다. 또한 $Fe^{+3}$ 이온이 A 자리에서 B 자리로의 원자이동은 350 K 근처에서 시작되었으며, 온도 증가에 따라 급격히 증가하여 550 K 에서 Fe 이온의 이동률은 71 % 이었다.

  • PDF

고온초전도 박막선재용 Ni-$W_{xat.%}$ 및 (Ni-$W_{3at.%}$)-$CU_{xat.%}$ 이축배향 금속 기판들의 자기적 특성 (Magnetic Properties of Both Ni-W and (Ni-3%W)-Cu Textured Substrates for ReBCO Coated Conductor)

  • 송규정;김태형;김호섭;고락길;하홍수;하동우;오상수;박찬;유상임;주진호;김민무;김찬중
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2006년도 추계학술대회 논문집 Vol.19
    • /
    • pp.28-29
    • /
    • 2006
  • The magnetic properties of a series of both annealed and as-rolled Ni-$W_y$ alloy tapes with compositions y = 0, 1, 3, and 5 at.%, were studied. To compare with Ni-W alloys, the magnetic properties of a series of both annealed and as-rolled $[Ni_{97at.%}W_{3at.%}]_{100-x}Cu_x$ alloy tapes with compositions x = 0, 1, 3, 5 and 7 at.%, were studied, as well. Both the isothermal mass magnetization M(H) of a series of samples, such as both Ni-W and [Ni-W]-Cu alloy tapes, at different fixed temperatures and M(T) in fixed field, were measured using a PPMS-9 (Quantum Design). The degree of ferromagnetism of Ni-$W_y$ alloys have reduced as W-content y increases. Both the saturation magnetization $M_{sat}$ and Curie temperature $T_c$ decrease linearly with W-content y, and both $M_{sat}$ and $T_c$ go to zero at critical concentration of $y_c$ ~ 9.50 at.% W. The effect of Cu addition on both the saturation magnetization $M_sat$ and Curie temperature $T_c$ decrease linearly with Cu-content x in $[Ni_{97at.%}W_{3at.%}]_{100-x}Cu_x$ alloy tapes with compositions x = 0, 1, 3, 5, and 7 at.%. The results confirm that [Ni-W]-Cu alloy tapes can have much reduced ferromagnetism as Cu-content x increases.

  • PDF

Nb2O5 첨가와 소결시간에 따른 Ba0.99(Bi0.5Na0.5)0.01TiO3 세라믹스의 PTCR 특성 (Positive Temperature Coefficient of Resistivity(PTCR) Behavior of Nb2O5 Added Ba0.99(Bi0.5Na0.5)0.01TiO3 Ceramics as a Function of Sintering Time)

  • 오영광;최승훈;류주현
    • 한국전기전자재료학회논문지
    • /
    • 제24권7호
    • /
    • pp.559-562
    • /
    • 2011
  • In this study, the effect of $Nb_2O_5$ and sintering time on the positive temperature of coefficient of resistivity (PTCR) behavior of lead free $Ba_{0.99}(Bi_{0.5}Na_{0.5})_{0.01}TiO_3$ (BBNT) ceramics were investigated in order to fabricate a PTC thermistor with high $T_c$ temperature more than $140^{\circ}C$. In particular, BBNT ceramic doped with 0.1mol% $Nb_2O_5$ and sintered at $1350^{\circ}C$ for 4 h has significantly increased Curie temperature ($T_c$) of about $200^{\circ}C$, showed good PTCR behavior of room-temperature resistivity ($\rho_{rt}$) of $40{\Omega}{\cdot}cm$, a high $\rho_{max}/\rho_{min}$ ratio of $43.78{\times}10^3$ and a large resistivity temperature factor (${\alpha}$) of 16.1%/$^{\circ}C$. With increasing addition of $Nb_2O_5$ content, the $\rho_{rt}$ decreased to a minimum value of $40\;{\Omega}cm$ at 0.1mol% $Nb_2O_5$ and the $\rho_{rt}$ increased for x value over 0.1 mol%.