• Title/Summary/Keyword: Cu Plate

Search Result 237, Processing Time 0.026 seconds

Reduction of Electron Contamination Using a Filter for 6MV Photon Beam (6MV 광자선에서 전자오염 감소에 관한 연구)

  • Lee, Choul-Soo;Yoo, Myung-Jin;Yum, Ha-Yong
    • Radiation Oncology Journal
    • /
    • v.15 no.2
    • /
    • pp.159-165
    • /
    • 1997
  • Purpose : Secondary electrons generated by interaction between Primary X-rar beam and block tray in megavoltage irradiation, result in excess soft radiation dose to the surface layer To reduce the surface dose from the electron contamination, electron filters were attached under the tray when a customized block was used. Materials and Methods : Cu, Al or Cu/Al combined Plate with different thickness was used as a filter and the surface dose reduction was measured for each case. The measurement to find optimal filter was performed with $10m\times10cm$ field size and 78.5cm source to surface distance. The measurement points are positioned with 2mm intervals from surface to maximum build-up point. To acquire the effect of field size dependence on optimal electron filter, the measurement was performed from $4cm\times4cm\;to\;25cm\times25cm$ field sizes. Results : The surface dose was slowly increased by increasing irradiation field but rapidly increased beyond $15cm\times15cm$ field size. Al plate was found to be inadequate filter because of the failure to have surface dose kept lowering than the dose of deep area. Cu 0.5mm plate and Cu/Al=0.28mm/1.5mm combined plate were found to be optimal filters. By using these 2 filters, the absorbed dose to the surface layer was effectively reduced by $5.5\%,\;11.3\%,\;and\;22.3\%$ for the field size $4cm\times4cm,\;10m\times10cm,\;and\;25cm\times25cm$, respectively. Conclusion : The surface dose attributable to electron contamination had a dependence on field size. The electron contamination was increased when tray was used. Specially the electron contamination in the surface layer was greater when the larger field was used. 0.5mm Cu Plate and Cu/Al=0.28mm/15mm combined plates were selected as optimal electron filters. When the optimal electron filter was attached under the tray, excessive surface dose was decreased effectively The effect of these electron filters was better when a larger field was used.

  • PDF

The Effcts of Temperature and Ni Addition on the Wetting Behaviour of Cu on W (텅스텐판상에서 구리액상의 습윤거동에 미치는 온도 및 니켈 첨가의 효과)

  • 이재성
    • Journal of the Korean institute of surface engineering
    • /
    • v.16 no.2
    • /
    • pp.41-47
    • /
    • 1983
  • An investigation has been performed on the effects of temperature and Ni addition on the wetting behaviour of Cu on W substrate in hydrogen atmosphere. An sessile drop method was used to measure a wetting angle. The concentration profiles of W, Cu and Ni elements in W/Cu - 5 Ni specimen were made by EPMA. With increasing temperature, the wetting angle of Cu droplet on W plate decreases and the time to reach an equilibrium wetting angle is shortened in hydrogen atmosphere. The addition of Ni improves appreciably the wettability of Cu on W. With increasing Ni content in Cu liquid droplet(0, 1, 3, 5%), the wetting angle is decreased from 21$^{\circ}$to 0$^{\circ}$.

  • PDF

Performance Analysis of Double-Glazed Flat Plate Solar Collector with Cu-based Solar Thermal Absorber Surfaces

  • Lee, Jeong-Heon;Jeong, Da-Sol;Nam, Yeong-Seok
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2016.02a
    • /
    • pp.157.1-157.1
    • /
    • 2016
  • In this work, we experimentally investigated the solar absorption performance of Cu-based scalable nanostructured surfaces and compared their performance with the conventional TiNOX. We fabricated Cu-based nanostructured surfaces with a controlled chemical oxidation process applicable to a large area or complex geometry. We optimized the process parameters including the chemical compounds, dipping time and process temperature. We conducted both lab-scale and outdoor experiments to characterize the conversion efficiency of each absorber surfaces with single and double glazing setup. Lab-scale experiment was conducted with $50mm{\times}50mm$ absorber sample with 1-sun condition (1kW/m2) using a solar simulator (PEC-L01) with measuring the temperature at the absorber plate, cover glass, air gap and ambient. From the lab-scale experiment, we obtained ${\sim}91^{\circ}C$ and $94^{\circ}C$ for CuO and TiNOX surfaces after 1 hr of solar illumination at single glazing, respectively. To measure the absorber performance at actual operating condition, outdoor experiment was also conducted using $110mm{\times}110mm$ absorber sample. We measured the solar flux with thermopile detector (919P-040-50). From outdoor experiment, we observed ${\sim}123^{\circ}C$ and $131^{\circ}C$ for CuO and TiNOX with 0.6 kW/m2 insolation at double glazing, respectively. We showed that the suggested nanostructured CuO solar absorber has near-equivalent collection efficiency compared with the state-of-the-art TiNOX surfaces even with much simpler manufacturing process that does not require an expensive equipment.

  • PDF

Improvement of Wear Resistance of Aluminum by Metal-Ceramic Particle Composite Layer (알루미늄표면에 금속-세라믹입자 복합첨가에 의한 내마모성개선)

  • ;;;中田一博;松田福久
    • Journal of Welding and Joining
    • /
    • v.15 no.6
    • /
    • pp.96-104
    • /
    • 1997
  • The present study was aimed to correlate the microstructure and the hardness as well as the wear resistance of the metal-ceramic particulated composite layer on the pure Al plate. The composite layers were constructed by the addition of TiC particles on the surface of Al-Cu alloyed layers by PTA overlaying process. Initially, the Al-Cu alloyed layers were achieved by the deposition of Al-(25 ~ 48%) Cu alloys on the pure Al plate by TIG process. It was revealed that TiC particles were uniformly dispersed without any reaction with matrix in the composite layer. The volume fraction of TiC particles (TiC V F) increased from 12% to 55% with increasing the number of pass of composite layer. Hardnesses of (Al-48%Cu + TiC (3&4layers)) composite layer were Hv450 and Hv560, respectively, due to the increase of TiC V/F. Hardnesses of (Al-Cu + TiC) composite layers decreased gradually with insreasing temperature from 100$^{\circ}$C to 400$^{\circ}$C, and hardnesses at 400$^{\circ}$C were then reached to 1/5 - 1/10 of room temperature hardness depending on the construction of composite layers. The Specific wear of (Al + Tic) layer and Al-48%Cu alloyed layer decreased to 1/10 of the of pure Al, while the specific wear of (Al-48%Cu + TiC (4 layers)) composite layer exhibited 1/15 of that of steel such as SS400 and STS304.

  • PDF

Electrical Properties of Plate Typed Shunt Resistors with Low TCR Property (낮은 TCR 특성을 가지는 플레이트 션트저항의 전기적 특성)

  • Lim, Youngtaek;Kim, Eun-Min;Lee, Sang-Won;Ahn, Jeong-Rae;Lee, Sunwoo
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.32 no.3
    • /
    • pp.219-222
    • /
    • 2019
  • In this study, we fabricated plate-type shunt resistors with thermal stability by parallelly connecting metal alloy plates with positive temperature coefficient of resistance (TCR) and carbon nanotube (CNT) plates with negative TCR. The metal alloy plates, which were prepared by alloying Cu and Mn with a composition of 91 wt% of Cu and 9 wt% of Mn, showed around $800ppm/^{\circ}C$ of TCR, and the CNT plates prepared from the CNT solution by using the vacuum filtration method showed around $-800ppm/^{\circ}C$ of TCR. The shunt resistor that was fabricated by stacking metal alloy plates and CNT plates in this work showed about $46.93ppm/^{\circ}C$ of TCR. Therefore, we conclude that a shunt resistor with low TCR can be realized by simply adjusting the TCR of the metal alloy only, because the TCR of the CNT plate has an identical value.

Jangdo(Small Ornamental Knives) manufacturing process and restoration research using Odong Inlay application (오동상감(烏銅象嵌)기법을 활용한 장도(粧刀)의 제작기술 및 복원연구)

  • Yun, Yong Hyun;Cho, Nam Chul;Jeong, Yeong Sang;Jang, Chu Nam
    • Korean Journal of Heritage: History & Science
    • /
    • v.49 no.2
    • /
    • pp.172-189
    • /
    • 2016
  • In this research, literature research on the Odong material, mixture ratio, casting method and casting facility was conducted on contemporary documents, such as Cheongong Geamul. Also, a long sword was produced using the Odong inlay technique. The sword reproduction steps were as follows; Odong alloying, silver soldering alloying, Odong plate and Silver plate production, hilt and sheath production, metal frame and decorative elements, such as a Dugup (metal frame), production, Odong inlay assembly and final assembly. For the Odong alloy production, the mixture ratio of the true Odong, which has copper and gold ratio of 20:1, was used. This is traditional ratio for high quality product according to $17^{th}$ century metallurgy instruction manual. The silver soldering alloy was produced with silver and brass(Cu 7 : Zn 3) ratio of 5:1 for inlay purpose and 5:2 ratio for simple welding purpose. The true Odong alloy laminated with silver plate was used to produce hilt and sheath. The alloy went through annealing and forging steps to make it into 0.6 mm thick plate and its backing layer, which is a silver plate, had the matching thickness. After the two plates were adhered, the laminated plate went through annealing, forging, engraving, silver inlaying, shaping, silver welding, finishing and polishing steps. During the Odong colouring process, its red surface turns black by induced corrosion and different hues can be achieved depending on its quality. To accomplish the silver inlay Odong techniques, a Hanji saturated with thirty day old urine is wrapped around a hilt and sheath material, then it is left at warm room temperature for two to three hours. The Odong's surface will turn black when silver inlay remains unchanged. Various scientific analysis were conducted to study composition of recreated Odong panel, silver soldering, silver plate and the colouring agent on Odong's surface. The recreated Odong had average out at Cu 95.57 wt% Au 4.16wt% and Cu 98.04 wt% Au 1.95wt%, when documented ratio in the old record is Cu 95wt% and Au 5wt%. The recreated Odong was prone to surface breakage during manufacturing process unlike material made with composition ratio written in the old record. On the silver plate of the silver and Odong laminate, 100wt% Ag was detected and between the two layers Cu, Ag and Au were detected. This proves that the adhesion between the two layers was successfully achieved. The silver soldering had varied composition of Ag depending on the location. This shows uneven composition of the silver welding. A large quantities of S, that was not initially present, was detected on the surface of the black Odong. This indicates that presence of S has influence on Odong colour. Additional study on the chromaticity, additional chemical compounds and its restoration are needed for the further understanding of the origin of Odong colour. The result of Odong alloy testing and recreation, Odong silver inlay long sword production, scientific analysis of the Odong black colouring agent will form an important foundation of knowledge for conservation of Odong artifact.

Crystallization and Electrical Conductivity of $CuO-P_{2}O_{5}-V_{2}O_{5}$ Glass for Solid-state Electrolyte (고체전해질용 $CuO-P_{2}O_{5}-V_{2}O_{5}$유리의 결정화와 전기전도도)

  • 손명모;이헌수;구할본
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2001.07a
    • /
    • pp.1018-1021
    • /
    • 2001
  • 1018-1021 The CuO-P$_2$O$_{5}$ containing P$_2$O$_{5}$ as glass-former were prepared by press-quenching method on the copper plate. By post-heat treatment of these glasses, the CuO-P$_2$O$_{5}$ -V$_2$O$_{5}$ -g1ass ceramics was obtained and the crystallization behavior and dc conductivities were investigovted. The heat-treated glass-ceramics decreased in electrical conductivity by the order of 10$^1$ compared to amorphous glass. The linear relationship between In($\sigma$T) and T$^{-1}$ indicated that electrical conduction in CuO-P$_2$O$_{5}$ -V$_2$O$_{5}$ -gass occurred by a small polaron hopping.

  • PDF

The effects of PWHT on the toughness of weld HAZ in Cu-containing HSLA-100 steel (Cu를 함유한 HSLA-100강 용접 열 영향부의 인성에 미치는 후열처리의 영향)

  • 박태원;심인옥;김영우;강정윤
    • Journal of Welding and Joining
    • /
    • v.13 no.4
    • /
    • pp.55-64
    • /
    • 1995
  • A study was made to examine the effects of postweld heat treatment(PWHT) on the toughness and microstructures in the weld heat affected zone(HAZ) of Cu-bearing HSLA-100 steel. The Gleeble thermal/mechanical simulator was used to simulate the weld HAZ. The details between toughness and PWHT of HAZ were studied by impact test, optical microscopy(O.M.), scanning electron microscopy (SEM), transmission electron microscopy(TEM) and differential scanning calorimetry(DSC). The decrease of HAZ toughness in single thermal cycle comparing to base plate is ascribed to the coarsed-grain formed by heating to 1350.deg.C. The increase of HAZ toughness in double thermal cycle comparine to single thermal cycle is due to the fine ferrite(.alpha.) grain transformed from austenite(.gamma.)formed by heating to .alpha./.gamma. two phase region. Cu precipitated during aging for increasing the strength of base metal is dissolved during single thermal cycle to 1350.deg.C and is precipitated little on cooling and heating during subsequent weld thermal cycle. It precipitates by introducing PWHT. Thus, the decrease of toughness in triple thermal cycle of $T_{p1}$ = 1350.deg.C, $T_{p2}$ = 800.deg.C and $T_{p3}$ = 500.deg.C does not occur owing to the precipitation of Cu. The behaviors of Cu=precipitates in HAZ is similar to that in base plate. PWHT at 550.deg.C shows highest hardness and lowest toughness, whereas PWHT at 650.deg.C shows reasonable toughness, which improves the toughness of as-welded state.state.

  • PDF

Freeze Drying Process and Pore Structure Characteristics of Porous Cu with Various Sublimable Vehicles (다양한 동결제를 이용하여 동결건조 공정으로 제조한 Cu 다공체의 기공구조 특성)

  • Lee, Gyuhwi;Oh, Sung-Tag;Suk, Myung-Jin;Jeong, Young-Keun
    • Journal of Powder Materials
    • /
    • v.27 no.3
    • /
    • pp.198-202
    • /
    • 2020
  • The effect of sublimable vehicles on the pore structure of Cu fabricated by freeze drying is investigated. The 5 vol% CuO-dispersed slurries with camphene and various camphor-naphthalene compositions are frozen in a Teflon mold at -25℃, followed by sublimation at room temperature. After hydrogen reduction at 300℃ and sintering at 600 ℃, the green bodies of CuO are completely converted to Cu with various pore structures. The sintered samples prepared using CuO/camphene slurries show large pores that are aligned parallel to the sublimable vehicle growth direction. In addition, a dense microstructure is observed in the bottom section of the specimen where the solidification heat was released, owing to the difference in the solidification behavior of the camphene crystals. The porous Cu shows different pore structures, such as dendritic, rod-like, and plate shaped, depending on the composition of the camphornaphthalene system. The change in pore structure is explained by the crystal growth behavior of primary camphor and eutectic and primary naphthalene.

Effects of PWHT on the toughness of weld HAZ in Cu-bearing HSLA-100 steel (Cu를 함유한 HSLA-100강 용접 열 영향부의 인성에 미치는 PWHT의 영향)

  • 박태원;심인옥;김영우;강정윤
    • Proceedings of the KWS Conference
    • /
    • 1995.04a
    • /
    • pp.91-93
    • /
    • 1995
  • A study was made to examine the effects of post-weld heat treatment (PWHT) on the toughness and microstructures in the weld heat-affacted zone(HAZ) of Cu-bearing HSLA-100 steel. The Gleeble thermal/mechanical simulator was used to simulate the weld HAZ. The behavior of Cu-precipitates in HAZ is similar to that in base plate. PWHT at 55$0^{\circ}C$ shows highest hardness and lowest toughness, whereas PWHT at $650^{\circ}C$ shows reasonable toughness. Cu precipitated during agcing for increasing the strength of base metal is dissolved during single thermal cycle to 135$0^{\circ}C$ and is precipitated little on cooling and heating during subsequent weld thermal cycle. It precipitates by introducing PWHT.

  • PDF