• 제목/요약/키워드: Continuous Wave Laser

검색결과 184건 처리시간 0.05초

40-W 200-ns 300-kHz Thulium-doped Fiber Laser at 2050 nm

  • Shin, Jae Sung;Cha, Yong-Ho;Chun, Byung Jae;Park, Hyunmin
    • Current Optics and Photonics
    • /
    • 제5권5호
    • /
    • pp.544-553
    • /
    • 2021
  • A 40-W 200-ns 300-kHz thulium-doped fiber laser at 2050 nm with a master oscillator power amplifier configuration was developed, for application to lithium-isotope separation. The master oscillator generated a 5.35 W continuous-wave beam, which the pulse generator then broke into 200-ns pulses at 300 kHz. Then, the laser beam was amplified by passing through a two-stage amplifier. The output power finally obtained was 42.0 W at 2050 nm, and was stable for a long time, over 2 hours. In spite of this achievement, mode instability was observed in the output beam. This can be solved in the future by using a method such as tight coiling.

High energy laser heating and ignition study

  • Lee, K.C.;Kim, K.H.;Yoh, J.J.
    • 한국추진공학회:학술대회논문집
    • /
    • 한국추진공학회 2008년 영문 학술대회
    • /
    • pp.525-530
    • /
    • 2008
  • We present a model for simulating high energy laser heating and ignition of confined energetic materials. The model considers effect of ablation of steel plate with long laser pulses and continuous lasers of several kilowatts and the thermal response of well-characterized high explosives for ignition. Since there is enough time for the thermal wave to propagate into the target and to create a region of hot spot in the high explosives, electron thermal diffusion of ultra-short(femto- and pico-second) lasing is ignored; instead, heat diffusion of absorbed laser energy in the solid target is modeled with thermal decomposition kinetic models of high explosives are used. Numerically simulated pulsed-laser heating of solid target and thermal explosion of cyclotrimethylenetrinitramine(RDX), triaminotrinitrobenzene(TATB), and octahydrotetranitrotetrazine(HMX) are compared to experimental results. The experimental and numerical results are in good agreement.

  • PDF

충격 시험시 발생하는 레이저 용접부의 파괴 이탈 현상 (Behavior of Fracture Deviation in the Impact Test of Narrow Laser Welds)

  • 나일;김재도
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 1993년도 특별강연 및 춘계학술발표 개요집
    • /
    • pp.120-124
    • /
    • 1993
  • The Charpy V impact test on subsize was performed on narrow laser welds of low carbon steel sheets, joined by using a continuous wave 3kW CO$_2$ laser. Under certain conditions, a bimodal fracture behaviour has been experienced in Charpy V impact test of narrow laser beam welds. Deviation of the fracture path from the fusion zone into the base metal was dominated at high test temperature. It can be seen that the deviation always occurred after ductile initiation. If the deviation occurs on a small testing specimen, the same trend would happen on the actual laser welded structure. Fracture will then propagate through the base material even if the weld metal has low toughness.

  • PDF

Pulsed laser surface modification for heat treatment and nano-texturing on biometal surface

  • Jeon, Hojeong
    • 한국표면공학회:학술대회논문집
    • /
    • 한국표면공학회 2016년도 추계학술대회 논문집
    • /
    • pp.118.1-118.1
    • /
    • 2016
  • The laser surface modification has been reported for its functional applications for improving tribological performance, wear resistance, hardness, and corrosion property. In most of these applications, continuous wave lasers and pulsed lasers were used for surface melting, cladding, alloying. Since flexibility in processing, refinement of microstructure and controlling the surface properties, technology utilizing lasers has been used in a number of fields. Especially, femtosecond laser has great benefits compared with other lasers because its pulsed width is much shorter than characteristic time of thermal diffusion, which leads to diminish heat affected zone. Moreover, laser surface engineering has been highlighted as an effective tool for micro/nano structuring of materials in the bio application field. In this study, we applied femtosecond and nanosecond pulsed laser to treat biometals, such as Mg, Mg alloy, and NiTi alloy, by heating to improve corrosion properties and functionalize their surface controlling cell response as implantable biomedical devices.

  • PDF

Allow 600 합금의 내부식성 향상을 위한 레이저 표면 합금화 (Laser Surface Alloying of Alloy 600 to Improve Its Corrosion Resistance)

  • 신진국;강석중;서정훈;국일현;김정수
    • 한국레이저가공학회지
    • /
    • 제2권1호
    • /
    • pp.16-21
    • /
    • 1999
  • The surface of Alloy 600 was alloyed using a continuous wave $CO_2$ laser beam in order to improve its corrosion resistance. Laser surface alloying (LSA) was done by melting the surface electroplated with Cr of the alloy. The Cr concentration of the alloyed surface was 28-30 at.%, which is similar to that of Alloy 690. Alloying elements in the alloyed layer was observed to be distributed very homogeneously all over the alloyed region. According to the electrochemical and modified Huey tests, the corrosion resistance, in particular the grain boundary corrosion resistance, of the LSA specimens was significantly improved, compared with that of the as-received(AR) specimen. This improved corrosion resistance of the alloyed specimen might be attributed to the high Cr content which could make possible formation of more stable and dense passive film onto its surface.

  • PDF

12%-Cr 강의 C0$_{2}$레이저 표면 경화

  • 김재도
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 1992년도 춘계학술대회 논문집
    • /
    • pp.84-88
    • /
    • 1992
  • Laser beam hardenling of 12%-Cr steel has been evaluated by using a continuous wave 3 kW CO$\_$2/ laser with a hardening mirror set. Experiment was performed on the optimum hardening condition with a laser power of 2.85kW and travel speed of 10 and 5 m/min. Multi passes have been alsotried to find the hardening characteristics of partly overlapped zone. The black paint to use at high temperature was adopted to increases the absorptivity of laser beam energy with the wavelength of 10.6 .mu. m at the surface of bese metal. The microstructure of the hardened layers was observed by using a light microscopy. SEM and TEM. A fine lamellar martensite formed in the hardened zones exhibits very high Vickers microhardness of 600 Hv, whereas the tempered martesite distributes in the base metal with Vickers microhardness of 240 Hv. It has been found that laser hardening with multi pass showed no significant drop of the hardness between adjacent passes.