Low Temperature Harding Property of UP with MMA Proportions (MMA 모노머 혼입률에 따른 UP의 저온경화 특성)

  • Song, Hun;Lee, Jung-Hui;Chu, Yong-Sik;Lee, Jong-Kyu
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2009.05a
    • /
    • pp.497-498
    • /
    • 2009
  • Unsaturated polyester(UP) and epoxy resin require 8${\sim}$11 hours long harding times and heating systems used by reinforcement liner. This study is to evaluate the effects of low temperature harding property of UP with methyl methacrylate(MMA) monomer mixing proportions.

  • PDF

Compressive Behavior of SHCCCStrain-hardening cement composite) mixmg Fly ash (플라이애시를 혼입한 변형경화형 시멘트 복합체(SHCC)의 압축거동)

  • Cha, Jun-Ho;Song, Seon-Hwa;Jang, Yong-Heon;Kim, Sun-Woo;Kim, Yun-Yong;Yun, Hyun-Do
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2009.05a
    • /
    • pp.483-484
    • /
    • 2009
  • The purpose of this study is to evaluate the compressive behavior of SHCC mixing Fly ash. The parameter of this study are replacement level of fiber and Fly ash.

  • PDF

Mechanical & Physical Properties of Flowable Fill Using Bottom Ash (폐석탄회를 사용한 저강도충전재의 물리.역학적 특성)

  • 원종필;이용수
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2000.10b
    • /
    • pp.915-920
    • /
    • 2000
  • The effectiveness of bottom ash on the slump flow, compressive strength of flowable fill is investigated in this study. This study was undertaken on the use of bottom ash as a fine aggregate in flowable fill. Bottom ash is combined with portland cement, fly ash, and water to flowable fill with slump flow(20~30cm). Four different level of bottom ash with fly ash contents, 25%, 50%, 75%, 100% are investigated. Laboratory test results conclude that the inclusion of bottom ash increases the demand for mixing water n obtaining the require slump flow.

Experimental Study on the Mechanical Properties of Carbon Fiber Reinforced Fly Ash-Cement Composites (II) (탄소섬유 보강 플라이애쉬.시멘트 복합체의 역학적 특성에 관한 실험적 연구(II))

  • 박승범;윤의식
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 1991.10a
    • /
    • pp.99-106
    • /
    • 1991
  • Result of an experimental study on the manufacture, the mechanical properties and waterightness of pitch-based carbon fiber reinforced fly ash.cement composites are presented in this paper. The carbon fiber reinforced fly ash.cement composites using early strength cement, silica powder and a small amount of stylene butadiene rubber latex are prepared with carbon fiber, foaming agents and mixing conditions. As a result, the mechanical and plysical properties such as compresive, tensile and flectural strengths, watertightness and cement composites are improved by using a small amount of stylene butadiene rubber latex.

  • PDF

Characterization of Cement Waste Form for Final Disposal of Decommissioned Concrete Waste (해체 콘크리트 폐기물 최종처분을 위한 시멘트 고화체 특성 평가)

  • Lee, Yoon Ji;Hwang, Doo Seong;Lee, Ki Won;Jeong, Gyeong Hwan;Moon, Jei Kwon
    • Journal of Nuclear Fuel Cycle and Waste Technology(JNFCWT)
    • /
    • v.11 no.4
    • /
    • pp.271-280
    • /
    • 2013
  • Since the decommissioning of nuclear plants and facilities, large quantities of slightly contaminated concrete waste have been generated. In Korea, the decontamination and decommissioning of the KRR-1, 2 at the KAERI have been under way. And concrete waste was generated about 800 drums of 200 L. The conditioning of concrete waste is needed for final disposal. The concrete waste is conditioned as follows: mortar using coarse and fine aggregates is filled void space after concrete rubble pre-placement into 200 L drum. Thus, this research has developed an optimizing mixing ratio of concrete waste, water, and cement and has evaluated characteristics of a cement waste form to meet the requirements specified in disposal site specific waste acceptance criteria. The results obtained from compressive strength test, leaching test, thermal cycling test of cement waste forms conclude that the concrete waste, water, and cement have been suggested to have 75:15:10wt% as the optimized mixing ratio. Also, the compressive strength of cement waste form was satisfied that including fine powder up to maximum 40wt% in concrete debris wastes about 75%. As a result of scale-up test, the mixture of concrete waste, water, and cement is 75:10:15wt% meet the satisfied compressive strength because the free water increased with and increased in particle size.

Evaluation of fracture reduction performance of fiber reinforced mortar according to fiber type (섬유종류에 따른 섬유보강 모르타르의 파괴저감성능 평가)

  • Roh, Jong-Chan;Kim, Gyu-Yong;Kim, Hong-Seop;Koo, Kyung-Mo;Yoon, Min-Ho;Yoo, Jae-Chul
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2013.11a
    • /
    • pp.38-39
    • /
    • 2013
  • In this study, in regard to fiber reinforced mortar mixing steel fiber and 4types of organic fiber, impact test was carried out. Because to predict fracture reduction performance with flexural, tensile strength when types of fiber were different as impact reduction performance of concrete is closely related with toughness such as flexural strength, tensile strength and fracture energy etc. As a result, enhancement of toughness by fiber reinforcement controls the spall of rear. On the other hand in case of steel fiber relatively turned up high toughness in appropriate load compared with organic fiber but in same mixing rate, impact reduction performance by projectile showed low performance due to few number of an individual of mixing.

  • PDF

Analysis of Setting Delay Performance Change of Super Retarding Agent According to the Change of Mixing Rate at 20℃ (20℃ 조건에서 초지연제 혼입율 변화에 따른 응결지연 성능 변화 분석)

  • Lim, Gun-Su;Han, Soo-Hwan;Hyun, Seung-Yong;Kim, Jong;Han, Min-Choel;Han, Cheon-Goo
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2020.11a
    • /
    • pp.127-128
    • /
    • 2020
  • This research is part of the research for unifying the mass concrete and utilizing the rate of super retarding agent. We analyzed the performance of super retarding agent 20℃ conditions. It was found that there was no deterioration in fluidity and air quality due to the change in the super retarding agent mixing rate. It was found that when super retarding agent was mixed up to 0.5 %, it was delayed for 22.3 hours at 20℃. Therefore in order to ensure the performance required at the site, the super retarding agent mixing rate must be determined by fully considering the situation at the site. In addition it will be analyzed that super retarding agent performance analysis at high temperature will be required in subsequent studies.

  • PDF

Insulation Properties of CLC according to Mixing Ratio of EPS Bead (EPS Bead 혼입비율에 따른 CLC의 단열특성)

  • Lee, Jeong-Taek;Lee, Sang-Soo
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2023.05a
    • /
    • pp.45-46
    • /
    • 2023
  • CLC is used as a filling material for many buildings, and according to energy saving design standards, CLC also requires insulation performance. However, it shows lower insulation performance compared to organic insulation, so additional research is needed. Therefore, in this study, the insulation properties of CLC were analyzed by incorporating EPS beads with high insulation performance into CLC. In this experiment, EPS beads and blast furnace slag were replaced, and W/B was fixed at 33%. The EPS Bead mixing ratio was divided into 5 levels: 0, 0.5, 1.0, 1.5, 2.0 (%), and the experimental items were measured for apparent density and thermal conductivity. As a result of the experiment, the apparent density and thermal conductivity tended to decrease as the mixing ratio of EPS beads increased. It is judged that the density decreased due to the low density and the micropores inside, and the thermal conductivity also decreased.

  • PDF

A Study of the Characteristics of the High-flowable Concrete according to the change of charge-time of superplasticize (유동화제 첨가시기에 따른 콘크리트의 특성에 관한 실험적 연구)

  • Kwon, Chun-Ahn;Jeon, Hyun-Kyu
    • Journal of the Korea Institute of Building Construction
    • /
    • v.3 no.1
    • /
    • pp.115-122
    • /
    • 2003
  • In order to analyze liquidity change according to increasing the charge of superplasticizer, we inputted charges by dividing into six steps, 0% through 1.25%; at the same time, to observe liquidity change according to the change of charge-time, we carried out the experiment applying 30-minute intervals, i.e. at beginning of mixing, 30, 60 and 90 minutes. The results are below. 1) According to increasing the charge of superplasticizer, the liquidity of concrete was enhanced, however, when inputted 1.25%, a little segregation was occurred, which allowed us to make a conclusion that concrete performance would be deteriorated due to this segregation. 2) When we inputted 1.25% of superplsticizer, steady liquidity features were shown regardless of the charge-time of concrete, which allowed us to make a conclusion that this input would be the best for liquidity performance considering only liquidity features. 3) After analyzing the dynamical features of liquid concrete, the result showed that there was not significant effect on revelation of compressive strength. We concluded form this result that there was no influence on the stripping-time of a mold form. 4) When we charge superplasticizer in concrete more than 1%, we, in advance, should clearly judge the concrete performance required during constructing in site, as it were, the compressive strength or liquidity etc.; furthermore, we had better decide a charge and input-time of superplasticizer to meet the required performance.

Properties of pervious concrete containing high-calcium fly ash

  • Sata, V.;Ngohpok, C.;Chindaprasirt, P.
    • Computers and Concrete
    • /
    • v.17 no.3
    • /
    • pp.337-351
    • /
    • 2016
  • This paper presents the properties of pervious concrete containing high-calcium fly ash. The water to binder ratios of 0.19, 0.22, and 0.25, designed void ratios of 15, 20, and 25%, and fly ash replacements of 10, 20, and 30% were used. The results showed that the use of fly ash as partial replacement of Portland cement enhanced the mixing of paste resulting in a uniform mix and reduced amount of superplasticizer used in the mixture. The compressive strength and flexural strength of pervious concrete were slightly reduced with an increase in fly ash replacement level, while the abrasion resistance increased due mainly to the pozzolanic and filler effects. The compressive strength and flexural strengths at 28 days were still higher than 85% of the control concrete. The aggregate size also had a significant effect on the strength of pervious concrete. The compressive strength and flexural strength of pervious concrete with large aggregate were higher than that with small aggregate.