An investigation of water magnetization and its influence on some concrete specificities like fluidity and compressive strength

  • Khorshidi, N.;Ansari, M.;Bayat, M.
    • Computers and Concrete
    • /
    • v.13 no.5
    • /
    • pp.649-657
    • /
    • 2014
  • In this paper, effects of magnetic water on different properties of cement paste including fluidity, compressive strength, time of setting and etc, has been studied in concrete laboratory of Sahand University of Technology. For production of magnetic water, three devices including an AFM called device(made in UAE), a device marked AC(made in Germany) and finally a device was designed and made in Concrete Laboratory of Sahand University of Technology) have been used. The results show that, intensity and direction of magnetic field, velocity and time of water passing through magnetic device, and amount and type of Colloidal particles have direct effects on properties of magnetic water and using such a water in making cement paste, increases its fluidity and compressive strength up to 10%.

Effect of temperature on the behavior of self-compacting concretes and their durability

  • Salhi, M.;Li, A.;Ghrici, M.;Bliard, C.
    • Advances in concrete construction
    • /
    • v.7 no.4
    • /
    • pp.277-288
    • /
    • 2019
  • The formulation of self-compacting concretes (SCC) and the study of their properties at the laboratory level were currently well mastered. The aim of this work is to characterize SCC under hot climatic conditions and their effects on the properties of fresh and hardened SCC. Particularly, the effect of the initial wet curing time on the mechanical behavior such as the compressive strength and the durability of the SCCs (acid and sulfate attack) as well as the microstructure of SCCs mixtures. In this study, we used two types of cement, Portland cement and slag cement, three water/binder (W/B) ratio (0.32, 0.38 and 0.44) and five curing modes. The obtained results shows that the compressive strength is strongly influenced by the curing methods, 7-days of curing in the water and then followed by a maturing in a hot climate was the optimal duration for the development of a better compressive strength, regardless of the type of binder and the W/B ratio.

Mechanical Properties of Recycled Aggregate Concrete (재생골재 치환률에 따른 콘크리트의 역학적 특성)

  • 이명규;윤건호
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 1999.10a
    • /
    • pp.119-122
    • /
    • 1999
  • In this paper, the properties of concrete used recycled aggregate are analyzed. The specimens are manufactured for the compressive strength of 210㎏/㎠ with recycled aggaregate ratio of 0%, 20%, 40%, 60%, 80%, 100%, respectivey. At curing 28days, compressive strength, tensile strength, flexural strength, dry-shrinkage, static modulus of elasticity and poission's ratio have been tested according to replacement ratio of recycled aggregate.

  • PDF

The Properties of Inter-Locking Block with the Variation of Particle Grading and Shape of Aggregate (골재의 입도와 입형 변화에 따른 인터로킹 블록의 특성)

  • 이상태;김기철;신병철;김진선;권상준;한천구
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 1998.04b
    • /
    • pp.661-664
    • /
    • 1998
  • In this paper, the properties of inter-lacking block by the kind of aggregate and fineness modulus are investigated. According to the experimental results, compressive strength and flexural strength increase and absorption ratio decrease with larger fineness modulus in the range of 2.15~4.20. Flexural strength with river sand is higher than that with crushed sand by about 19%, compressive strength with river sand, that with crushed sand by about 11% and absorption ratio with river sand is smaller than that with crushed sand by abort 2%.

  • PDF

Mechanical properties and durability of self consolidating cementitious materials incorporating nano silica and silica fume

  • Mahdikhani, Mahdi;Ramezanianpour, Ali Akbar
    • Computers and Concrete
    • /
    • v.14 no.2
    • /
    • pp.175-191
    • /
    • 2014
  • In recent years, the emergence of nanotechnology and nanomaterial has created hopes to improve various properties of concrete. Nano silica as one of these materials has been introduced as a cement replacement material for concrete mixture in construction applications. It can modify the properties of concrete, due to high pozzolanic reactions and also making a denser microstructure. On the other hand, it is well recognized that the use of mineral admixtures such as silica fume affects the mechanical properties and durability of cementitious materials. In addition, the superior performance of self-consolidating concrete (SCC) and self-consolidating mortars (SCM) over conventional concrete is generally related to their ingredients. This study investigates the effect of nano silica and silica fume on the compressive strength and chloride permeability of self-consolidating mortars. Tests include compressive strength, rapid chloride permeability test, water permeability, capillary water absorption, and surface electrical resistance, which carried out on twenty mortar mixtures containing zero to 6 percent of nano silica and silica fume. Results show that SCMs incorporating nano silica had higher compressive strength at various ages. In addition, results show that nano silica has enhanced the durability SCMs and reduced the chloride permeability.

Influence of Particle Properties of Crushed Sand on the Qualities of Concrete (부순모래의 입자특성이 콘크리트의 품질에 미치는 영향)

  • Yoo Seung-Yeup;Sohn Yu-Shin;Lee Seung-Hoon;Lee Gun-Cheol;Yoon Gi-Won;Han Cheon-Goo
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2005.05a
    • /
    • pp.89-92
    • /
    • 2005
  • This study investigates influence of particle properties of crushed sand on the duality of concrete. The test shows that an increase of fineness modulus(FM) resulted in high slump and air contents, while compressive strength decreased due to decreased adhesion with reduction of surface area. As grain shape become rounder, the slump of concrete increased, due to reduction of internal friction, and increased air contents. The reduction of adhesion by abrasion of surface declined compressive strength during the process of manufacturing crushed sand. Increase of powder contents decreased slump and it also decreased air contents due to the effect of filling air void. In addition. using powder contents increased compressive strength, but could not find any difference of bleeding and tensile strength with particle properties.

  • PDF

Engineering Geological Properties of Some Domestic Marbles (국내산(國內産) 대리석(大理石)의 지질공학적(地質工學的) 특성(特性))

  • Cheong, Young Wook;Chon, Hyo Taek
    • Economic and Environmental Geology
    • /
    • v.23 no.4
    • /
    • pp.411-424
    • /
    • 1990
  • Mechanical, physical and petrographic properties of seventeen marble specimens collected from ten marble mines in Korea were investigated. Studied marbles were mainly composed of calcite, dolomite, and various amounts of serpentine, tremolite, olivine, quartz and opaque minerals. Complete and sutured textures were dominant. Compressive strength measured normal to the bedding plane is larger almost two times than that measured parallel to the bedding plane. From the results of Shore hardness test on marbles, water content was an important factor to decrease Shore hardness values. Engineering geological properties, especially, compressive strength, Young's modulus, wear resistance and water absorption could be controlled by the presence of quartz, and the type of marble texture. Water absorption-porosity, compressive strength-Young's modulus, and impact strength index-Los Angeles abrasion couples show good correlation. According to the comparative utility as commercial stone, it could be concluded that marbles from the Banglim mine, Songbo mine, Kwangdeok mine and Bongjeong mine were superior to that of other studied marbles.

  • PDF

Strength and permeation properties of alccofine activated low calcium fly ash geopolymer concrete

  • Jindal, Bharat Bhushan;Singhal, Dhirendra;Sharma, Sanjay;Yadav, Aniket;Shekhar, Shubham;Anand, Abhishek
    • Computers and Concrete
    • /
    • v.20 no.6
    • /
    • pp.683-688
    • /
    • 2017
  • This paper presents the experimental investigations on the compressive strength and permeation properties of geopolymer concrete prepared with low calcium fly ash as the primary binder activated with different percentage of Alccofine. The durability aspect was investigated by performing permeable voids and water absorption tests since permeability directly influences the durability properties. The test results show that Alccofine significantly improves the compressive strength and reduces the water permeability thus enhances the durability of geopolymer concrete at ambient curing regime which encourages the use of geopolymer concrete at ambient curing condition thus promising its use in general construction also.

A Study on the Quality Deviation of High-Strength Concrete from Multiple Ready Mixed Concrete Companies (다수 레미콘사에서 납품된 콘크리트 품질 편차에 관한 연구)

  • Park, Dong-Cheon;Seok, Won-Kyun;Jeon, Hyun-Soo;Kim, Young-Sun
    • Journal of the Korea Institute of Building Construction
    • /
    • v.22 no.6
    • /
    • pp.577-583
    • /
    • 2022
  • On large-scale sites, concrete is often delivered from a number of ready-mixed concrete companies, but even if the same concrete mixture table is used, it is thought that there will be a difference in quality due to differences in materials and manufacturing equipment. Due to a lack of previous research in this area, this study measured the properties of fresh concrete, compressive strength, and chlorine ion diffusion coefficient using the concrete supplied by 12 ready-mixed companies in Busan. The fresh concrete properties met the criteria. The compressive strength increased by 137% for 30MPa, 131% for 45MPa, and 117% for 80MPa by specified compressive strength. For the chlorine ion diffusion coefficient, the average value for each specified compressive strength could be derived without significant variation. The higher the compressive strength, the greater the deviation , and the lower the compressive strength, the greater the deviation in the chlorine ion diffusion coefficient.

The Analysis of Internal & External Stabilities and Factors for D.C.M Design (DCM 설계에서 주요 인자의 결정과 내.외적 안정해석)

  • Lee, Choong-Ho;Jung, Seung-Yong;Han, Sang-Jae
    • Proceedings of the Korean Geotechical Society Conference
    • /
    • 2009.09a
    • /
    • pp.793-808
    • /
    • 2009
  • This paper presents procedure and prediction method of internal and external stabilities when designing D.C.M, with main factors to be considered, such as chemical reaction of additive, physical properties of stabilized body and mixing strength. Results show that through case studies, a design unconfined compressive strength of stabilized body (hereafter referred to as 'compressive strength') directly depends on the quantity of cement, which is decided by laboratory test, and the compressive strength enormously affects internal and external stabilities. So laboratory mixing test to obtain the compressive strength for design allowable stress should be given careful considerations.

  • PDF