• Title/Summary/Keyword: Compressive Strength Experiment

Search Result 613, Processing Time 0.024 seconds

배합강도 $100N/mm^2$인 초고강도 콘크리트의 레미콘 생산성에 관한 실험적 연구 (An Experimental Study on the Ready-mixed concrete Production of Ultra-High Strength Concrete with Mixing Strength of $100N/mm^2$)

  • 정진;진용만;강훈;이상수
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2004년도 추계 학술발표회 제16권2호
    • /
    • pp.759-764
    • /
    • 2004
  • In this study, the experiment was carried out to investigate and analyze the ready-mixed concrete production of ultra-high strength concrete with mixing strength of $100N/mm^2$ according to types of mineral admixtures. The main experimental variables were water/binder ratio $25.0\%$, water content $160kg/m^3$ and mineral admixtures such as fly ash, silica fume and meta kaolin. According to the test results, the principle conclusions are summarized as follows. 1) even if it secures similar slump, the viscosity appear to difference by mixing condition relatively. 2) The autogeneous shrinkage of ultra-high strength concrete is profitable that use admixture, and heat of hydration is desirable that apply considering countermeasure enough in the advance. 3) The concrete that use SF10+MK10 on 56days could confirm that it is possible that achieve compressive strength more than $100N/mm^2$ under mixing conditions that is appearing by compressive strength $102.7N/mm^2$.

  • PDF

무시멘트 기반 하이드로볼을 활용한 투수블록의 강도 특성 (Noncement-based Hydroball Evaluation of Permeable Block Strength Properties)

  • 황우준;이창우;이상수
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2022년도 가을 학술논문 발표대회
    • /
    • pp.207-208
    • /
    • 2022
  • Since 1960, the green area has decreased due to rapid urbanization and the artificial surface has increased, and the repair and water function of the previous surface has decreased due to the decrease in rainwater absorption capacity. In addition, the risk of carbon dioxide and fine dust is emerging due to the use of fossil fuels due to urbanization. As a result, permeable blocks, an eco-friendly product, are in the spotlight. Therefore, this study was conducted to examine the strength properties of the permeable block using a hydroball. As a result of the experiment, the flexural strength and compressive strength tended to decrease as the hydroball replacement rate increased. It is judged that the hydroball absorbs a large amount of moisture during the mixing process and lacks moisture required for curing, resulting in a decrease in strength. According to KS F 4419, since the hydroball replacement rate is satisfied up to 20%, further research is needed to analyze the adsorption performance of air pollutants in the future and evaluate their utilization as a permeable block in the future.

  • PDF

공간적으로 보강된 복합재료의 강도예측 (Strength Prediction of Spatially Reinforced Composites)

  • 유재석;장영순;이상의;김천곤
    • Composites Research
    • /
    • 제17권5호
    • /
    • pp.39-46
    • /
    • 2004
  • 본 연구에서는 공간적으로 보강된 복합재(SRC)의 강도를 예측하였다. 각 방향의 라드(rod)와 라드의 체적에 비례하는 기지의 강성으로 표현되는 구조요소(structural element)를 정의하고, 이 구조요소에 파손판단식을 적용하여 SRC의 강도를 예측하였다. 라드의 파손판단식의 경우는 최대파손변형률을, 기지의 경우는 수정된 Tsai-Wu 파손판단식을 각기 적용하였다. 또한 SRC의 강도를 예측하기 위해서 라드와 SRC의 물성치를 측정하였다. 측정된 물성치는 라드의 인장 파손변형률, 3D SRC의 압축 파손변형률, $45^{\cir}$ 회전된 방향에서의 인장 및 압축 강도와 전단강도들이다. 3D/4D SRC의 강도분포는 각 SRC의 라드방향에서 크게 나타나고 라드에서 벗어날수록 작은 강도 값을 보였다. 강도의 전체분포를 보다 빠르게 계산하기 위해서 하중증분을 유동적으로 사용하였고, 하중이력을 구할 때는 균일한 하중이력을 사용하였다. 3D SRC의 라드방향 압축실험결과 해석의 비교에서 초기 기울기는 서로 잘 일치하였고, 강도값은 18% 정도의 차이를 보였다.

셀룰로오즈 섬유 함유 콘크리트의 작업 성능 및 강도 평가 (Evaluation of Workability and Strength in Concrete with Cellulose Fibers)

  • 류화성;이상석;권성준
    • 한국건설순환자원학회논문집
    • /
    • 제8권2호
    • /
    • pp.198-203
    • /
    • 2020
  • 콘크리트는 초기에 인장강도가 확보되지 못하므로 건조수축과 같은 재료적인 균열이 발생하게 된다. 본 연구에서는 셀룰로오즈 섬유를 0.0 ~ 2.0% 혼입한 콘크리트를 대상으로 공기량, 슬럼프와 같은 작업성을 평가하였으며, 재령에 따른 압축 및 인장강도를 평가하였다. 혼입률이 증가할수록 1.0kg/㎥ 수준에서는 공기량 및 슬럼프에서 저하를 확인할 수 없었으며, 이러한 작업성은 2시간까지 유효하게 작용하였다. 강도 평가에서는 혼입률이 증가할수록 인장 및 압축강도가 개선되었으며, 압축강도의 경우 7 ~ 9%수준으로, 인장강도에서는 7 ~ 22% 수준으로 증가하였다. 인장강도에서 증가율이 상대적으로 크게 평가되었는데, 이러한 효과는 균열저항성에 크게 도움을 주리라 판단된다. 본 연구를 통하여 2분간의 혼입 시간, 셀룰로오즈 섬유 1.0kg/㎥의 혼입률 수준이면 120분간 작업성에 큰 영향이 없으리라 평가된다.

Al 분말의 산화에 의한 $Al_2O_3$ 소결에 관한 연구 (A Study on alumina Sintering through the Oxidation of AI Powder.)

  • 박정현;안주삼;김해두
    • 한국세라믹학회지
    • /
    • 제19권3호
    • /
    • pp.179-186
    • /
    • 1982
  • This research is to aim at the study of sintering mechanism through the observation of microstructure by scanning electron microscopy, after the mixture of 30wt% $Al_2O_3$ (White Alundum) powder is fired in air at the temperature range of 1350~150$0^{\circ}C$ in order to sinter $Al_2O_3$-Al through the oxidation of Al powder. The results obtained in this experiment are as follows: 1. While the compressive strength of $Al_2O_3$(WA) body fired at $1450^{\circ}C$ for 5hrs in air is 150kg/$\textrm{cm}^2$, that of Al-$Al_2O_3$ body fired at 135$0^{\circ}C$, $1400^{\circ}C$ for 5hrs in air is 1100kg/$\textrm{cm}^2$, 1600kg/$\textrm{cm}^2$ respectively, and the higher the firing temperature, the more the compressive strength increases. These results from the sintering effect between $Al_2O_3$(WA) grains and surrounding Al-oxidation layer. 2. While the compressive strength of Al2O3(WA) body fired at 150$0^{\circ}C$ for 5hrs in air is 250kg/$\textrm{cm}^2$, the compressive strength of Al-$Al_2O_3$body fired under the same condition is 2050kg/$\textrm{cm}^2$ and water absorption 9.0%, porosity 23.3%, bulk density 2.60gr/$cm^3$. It is assumed that these results come from not only the grain growth of oxidized Al grains but also the increase of bonding strength between $Al_2O_3$(WA) grains.

  • PDF

국내 해성점토의 비배수 전단강도 분석을 통한 설계 적용성 평가 (Assessment on Design Applicability of Analysis of the Undrained Shear Strength in Korea Coastal Marine Clay)

  • 김명환;송창섭
    • 한국농공학회논문집
    • /
    • 제58권1호
    • /
    • pp.61-71
    • /
    • 2016
  • This study performed the physical and mechanical experiment on the samples of costal marine clays individually collected in western and southern regions to identify the characteristics of western and southern costal marine clay. Based on the experiment result, the characteristics of costal marine clay is identified undrained shear strength. Based on the experiment result on the physical and mechanical characteristics of costal marine clays, the regression is presented that can analyze the mechanical characteristics of undrained shear strength in costal marine clay of Korea, region of Korea and western-southern region. The correlation of uniaxial compressive strength and undrained shear strength was suitable for use of western-southern region correlation equation. The test result of Jeonnam Yeosu area compares with prediction results of previous researchers formula and western-southern region formula. Prediction results appear highest reliability on the 0.827 of coefficient of determination in the prediction results of the western-southern region formula.

Ready mixed concrete behavior of granulated blast furnace slag contained cement

  • Karim, M. Razaul;Islam, A.B.M. Saiful;Chowdhury, Faisal I.;Rehman, Sarder Kashif Ur;Islam, Md. Rabiul
    • Computers and Concrete
    • /
    • 제21권2호
    • /
    • pp.139-147
    • /
    • 2018
  • Due to enhanced construction requirement, ready mixed concrete are being popular day by day. The current study aimed to develop ready mixed concrete using GBFS contained cement and determine its properties of fresh and hardened states. A real scale experiment was set up in a ready mixed plant for measuring workability and compressive strength. The workability was tested after mixing (within 5 minutes), 30, 60, 90, 120 and 150 minutes of the running of bulk carrier. The ready mixed carrier employed spinning motion i.e., rotating around its axis with 20 RPM and running on road with 1km/h speed. The mixing ratio of cement: sand:gravel, water to cement ratio, super plasticizer were, 1:1.73:2.47, 0.40 and 6% of cement, respectively. The chemical composition of raw material was determined using XRF and the properties of cements were measured according to ASTM standards. The experimental results confirm that the cement with composition of 6.89% of GBFS, 4% of Gypsum and 89.11% of clinker showed the good compressive strength and workability of concrete after 150 minutes of the spinning motion in bulk carrier.

배기가스를 정화하는 흡음재의 특성에 관한 연구 (A Study on Properties of Sound Absorbing Materials with Characteristics of Exhaust-gas Purge)

  • 이승한;황보광수;장석수
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2001년도 봄 학술발표회 논문집
    • /
    • pp.935-940
    • /
    • 2001
  • This study search for absorbing sound and exhaust-gas which aims to manufacture continuous void by using clay and foam, the surface of materials is covered with $TiO_{2}$ powder as heat treatment. According to the results of the experiment, the increase of thickness of manufactured sound absorbing materials caused the increase of absorption rate in the range of low and middle sound and thus it can be an important factor of improving absorption rate. Sound absorbing materials could satisfy 70% of the average of sound absorption ratio in 7cm thickness. Also, the manufactured sound absorbing materials is covered with $TiO_{2}$ showed an excellency in the clarification of exhaust-gas under ultraviolet rays treatment when 70% of removal rate and about 10% of generation rate of $NO_{2}$ is settled by the flow of 2 $\ell$/min NO gas. Especially, manufactured sound absorbing materials could improve compressive strength of continuos porous concrete. in the case of 7% bubble addition, when the substitution rate of coagulator was 30% and 20%, compressive strength was 45kgf/$cm^{2}$ and 65kgf/$cm^{2}$ respectively. As the substitution rate of coagulator reducing, compressive strength increased after preforming burnt clay.

  • PDF

숏크리트 구성 재료에 따른 콘크리트 성능에 관한 실험적 연구 (An experimental study on performance of concrete with constituent materials of shotcrete)

  • 김상명;신진용;마상준;남관우;김기호
    • 한국터널지하공간학회 논문집
    • /
    • 제10권1호
    • /
    • pp.59-68
    • /
    • 2008
  • 골재 특성, 혼화재, 그리고 급결제 등이 콘크리트에 미치는 역학적 영향성을 평가하였다. 굵은골재 치수가 13 mm에서 8 mm로 작아질수록 유동 특성은 감소되었으나, 경화 콘크리트의 강도 및 동탄성계수는 크게 증가했다. 실리카흄 치환 적용 시 plain과 비교해 압축 강도 및 동탄성계수가 개선되었고, 고로슬래그 미분말을 적용한 경우 28일 재령에서 압축강도는 다소 증진되었다. 초기 수화 반응 및 압축 강도는 알루미네이트계 급결제를 적용한 시편이 다소 우수했고, 28일 강도 특성은 알칼리프리계 급결제 적용 시 크게 개선되었다.

  • PDF

강송의 기초적 재질에 관한 연구(제1보) (Studies on the Fundamental Properties of the Wood of Gumgangsong(Pinus densoflora for. erecta Uyeki) (Part 1))

  • 김정환;이원희;홍선천
    • 한국가구학회지
    • /
    • 제10권2호
    • /
    • pp.55-61
    • /
    • 1999
  • This research was carried out to investigate the fundamental properties such as the structure of annual ring, density distribution, compressive strength with parallel to grain, relative crystallinity, and microfibril angle of Gumgangsong(Pinus densoflora for. erecta Uyeki). The wood specimens, Gumgangsong and Sonamu(Pinus densiflora S. et Z.), for this experiment were prepared at Ulijingoon Sokwangri and Kyungpook university's forest in Kyungpook province, respectively. Average annual ring width is $2.0mm{\pm}0.3$ in heartwood of Gumgangsong. The respectively of heart wood was over 60 percent in Gumgangsong and 20~50 percent in Sonamu. Heartwood density were ranged from 0.5 to $0.8{\;}g/cm^3$ in Gumgangsong and from 0.4 to $0.5{\;}g/cm^3$ in sonamu. Compressive strength in Gumgangsong and Sonamu was about $30{\pm}5MPa$ and $25{\pm}5MPa$, resepectively. But the relative crystallinity and microfibril angle of two species were not different clearly. From these results of Gumgangsong and Sonamu, therefore, it was considered the main difference factors for both species were annual ring width and heartwood percentage.

  • PDF