알루미늄 첨가에 따른 오스테나이트계 Fe-23Mn-0.4C 고망간강의 극저온 충격 특성 (Effect of Al Addition on the Cryogenic-Temperature Impact Properties of Austenitic Fe-23Mn-0.4C Steels)

  • 김상규;김재윤;윤태희;황병철
    • 한국재료학회지
    • /
    • 제31권9호
    • /
    • pp.519-524
    • /
    • 2021
  • The impact properties of two austenitic Fe-23Mn-0.4C steels with different Al contents for cryogenic applications are investigated in this study. The 4Al steel consists mostly of austenite single-phase microstructure, while the 5Al steel exhibits a two-phase microstructure of austenite and delta-ferrite with coarse and elongated grains. Charpy impact test results reveal that the 5Al steel with duplex phases of austenite and delta-ferrite exhibits a ductile-to-brittle transition behavior, while the 4Al steel with only single-phase austenite has higher absorbed energy over 100 J at -196 ℃. The SEM fractographs of Charpy impact specimens show that the 4Al steel has a ductile dimple fracture regardless of test temperature, whereas the 5Al steel fractured at -100 ℃ and -196 ℃ exhibits a mixed fracture mode of both ductile and brittle fractures. Additionally, quasi-cleavage fracture caused by crack propagation of delta-ferrite phase is found in some regions of the brittle fracture surface of the 5Al steel. Based on these results, the delta-ferrite phase hardly has a significant effect on absorbed energy at room-temperature, but it significantly deteriorates low-temperature toughness by acting as the main site of the propagation of brittle cracks at cryogenic-temperatures.

치과용 세라믹의 파단면분석(fractography)에 대한 문헌고찰 (Literature review on fractography of dental ceramics)

  • 송민규;차민상;고경호;허윤혁;박찬진;조리라
    • 구강회복응용과학지
    • /
    • 제38권3호
    • /
    • pp.138-149
    • /
    • 2022
  • 치과용 세라믹의 파절실험 후 파절이 발생한 원인을 분석하면 세라믹의 임상적용 가능성을 높일 수 있다. 파절원인을 파악하기 위한 파단면분석은 주사전자현미경 등 영상기술의 발달로 점차 널리 적용되고 있는데 이를 정확히 해석하기 위해서는 실험조건 설정이 중요하다. 파절시편이 오염되지 않도록 보관하고 세척하며, 관찰을 위해 금속 전처리가 필요하다. 파절은 양상에 따라 주로 금속에서 관찰되는 보조개모양 파절, 열개, 분리파손 및 세라믹에서 관찰되는 피로파절과 조가비 모양 파절이 있다. 세라믹의 주된 파절원인인 피로파절을 실험실에서 재현하기 위해 느린 균열성장을 관찰할 수 있는 동적 하중이 필수적이며 하중조건과 하중횟수 등을 적절히 설정해야 한다. 세라믹의 파단면에서 나타나는 대표적인 특징은 해클이며 다양한 해클의 형태를 잘 관찰하여 세라믹 파절의 원인과 과정을 분석할 수 있도록 하는 것이 필요하다. 파단면분석은 치과용 세라믹의 파절을 심층적으로 파악할 수 있는 유용한 방법이므로 정확한 실험과정을 따르고 결과해석에 유의해야 한다.

오스테나이트계 Fe-18Mn-18Cr-0.61N 고질소강의 인장 및 충격 특성에 미치는 냉간 가공의 영향 (Effect of Cold Working on Tensile and Charpy Impact Properties of a High-Nitrogen Fe-18Mn-18Cr-0.61N Austenitic Steel)

  • 이승용;이상인;황병철
    • 열처리공학회지
    • /
    • 제27권3호
    • /
    • pp.121-126
    • /
    • 2014
  • High-nitrogen Fe-18Mn-18Cr-N austenitic steels with higher yield strength have been recently developed and used for generator retaining rings because they have non-magnetic, high strength, high ductility, and good corrosion resistance. In the present study, a high-nitrogen Fe-18Mn-18Cr-0.61N austenitic steel was fabricated and then tensile and Charpy impact tests were conducted on them in order to investigate the effect of cold working on the mechanical properties. Although the yield and tensile strengths usually increased with cold working, the ductility and impact toughness significantly decreased after cold working. On the other hand, the high-nitrogen austenitic steel exhibited a ductile-brittle transition due to unusual brittle fracture at low temperatures despite having a face-centered cubic structure. The ductile-brittle transition temperature obtained from Charpy impact tests could be remarkably increased by $60^{\circ}C$ after 20% cold working because of the enhanced cleavage-like brittle fracture.

수소화물에 의한 Zr-2.5Nb 압력관의 상온 수소취화 거동 (Hydrogen Embrittlement of Zr-2.5Nb Pressure Tube at Room Temperature by Precipitated Hydride)

  • 오동준;부명환;김영석
    • 대한기계학회논문집A
    • /
    • 제27권3호
    • /
    • pp.455-463
    • /
    • 2003
  • The aim of this study is to investigate the hydrogen embrittlement of Zr-2.5Nb CANDU pressure tube at room temperature. The transverse tensile and fracture toughness tests were performed at various hydrogen concentrations using transverse tensile specimens and CCT (curved compact tension) specimens. These specimens were directly machined from the pressure tube retaining original curvatures. Based on the results of these tests. the hydrogen embrittlement phenomenon was clearly observed and fracture toughness parameters of Zr-2.5Nb pressure tube materials such as, $K_{J(0.2)}$.$J_{ML}$.dJ/da, were dramatically decreased with the increasement of the hydrogen concentration. From microscopic observation by SEM and TEM, it was also revealed that various shapes dimples, fissures and quasi-cleavage were found at the hydrogen-absorbed materials with hydrides while traditional shape dimples were generally located at the as-received materials Through the comparison of the hydride and fissure lengths with the hydrogen concentration the new evaluation method of hydrogen embrittlement was suggested.

SA516/70강의 저온피로크랙 전파 하한계특성에 관한 연구 (A Study on Fatigue Crack Propagation Threshold Characteristics in SA516/70 Steel at Low Temperature)

  • 박경동;김정호;박형동;최병국
    • 동력기계공학회지
    • /
    • 제4권4호
    • /
    • pp.41-47
    • /
    • 2000
  • Fatigue crack propagation rate and threshold characteristics of the SA516/70 steel which is used for the low temperature pressure vessels, were studied in the room temperature of $25^{\circ}C$ and low temperature ranges of $-10^{\circ}C,\;-30^{\circ}C,\;-60^{\circ}C\;and\;-80^{\circ}C$ with stress ratio of R=0.1. In the logarithmic relationship between the fatigue crack propagation rate($d{\alpha}/dN$) and stress intensity factor range ${\Delta}K$, the linear relationship was obtained up to $d{\alpha}/dN=4.425{\times}10^4mm/cycle$ in the same of room temperature, but in low temperature case, the relationship was extended to the range of low crack propagation rate. The fractured specimens were examined by SEM. Tested results showed that specimen failed at low temperature exhibit the quasi-cleavage fracture formation however considerable ductility proceed final fracture.

  • PDF

순수 타이타늄 기반 산화물분산강화 합금의 미세조직 및 기계적 특성 (Microstructure and Mechanical Properties of Oxide Dispersion Strengthened alloy Based on Commercially Pure Titanium)

  • 박태성;김정한
    • 한국분말재료학회지
    • /
    • 제25권4호
    • /
    • pp.327-330
    • /
    • 2018
  • This study is conducted as a preliminary research to verify the feasibility of Ti-based Oxide dispersion strengthened (ODS) alloy. Pure-Ti powder is mixed with $Y_2O_3$ powder and subsequently, mechanically alloyed at $-150^{\circ}C$. The Ti-based ODS powder is hot-isostatically pressed and subsequently hot-rolled for recrystallization. The microstructure consists of elongated grains and Y excess fine particles. The oxide particle size is larger than that of the typical Fe-based ODS steel. Tensile test shows that the tensile ductility is approximately 25%, while the strength is significantly higher than that of pure Ti. The high-temperature hardness of the Ti-ODS alloy is also significantly higher than that of pure Ti at all temperatures, while being lower than that of Ti-6Al-4V. The dimple structure is well developed, and no evidence of cleavage fracture surface is observed in the fracture surface of the tensile specimen.

내부식용 API 5L X70 다전극 SAW 용접부의 내면 저온인성에 미치는 외면 입열의 영향 (Effect of Heat Input of Outside Weld on Low Temperature Toughness of Inside Weld for Multiple Electrode SA Welded API 5L X70 with Sour Gas Resistance)

  • 안현준;이희근;박용규;은성수;강정윤
    • Journal of Welding and Joining
    • /
    • 제32권1호
    • /
    • pp.93-101
    • /
    • 2014
  • This study aims to investigate the effect of heat input of outside SAW weld on low temperature toughness($-20^{\circ}C$) of inside SAW weld for API 5L X70 with sour gas resistance. As increasing heat input of the outside weld, low temperature toughness of the inside weld was decreased. Especially, in spite of the same heat input, the value of low temperature toughness was fluctuated. On the basis of fracture and microstructure analysis, the low temperature toughness is correlated with the fracture area ratio of shear lips and four kinds of fracture sections. These sections were divided with size and shape of dimple correlated with grain boundary ferrite and cleavage correlated acicular and polygonal ferrite in grain. Therefore, it was seen that these sections were two of final solidification area in the inside weld and the outside weld, no reheated zone and reheated zone in the inside weld. In conclusion, it is thought that the difference of low temperature toughness at the same heat input is due to the fact that each of impact test specimens could have the different microstructure, even though the notch was machined under the error tolerance of 1mm. It is because the final solidification area of the inside weld is very narrow.

탄소함량이 다른 경량철강판의 냉간 압연에 의한 파괴기구 (Fracture Mechanisms of Cold-Rolled Light-Weight Steel Plates Containing Different Carbon Content)

  • 한승엽;신상용;이성학;김낙준;곽재현;진광근
    • 대한금속재료학회지
    • /
    • 제48권5호
    • /
    • pp.377-386
    • /
    • 2010
  • An investigation was conducted into the effects of $\kappa$-carbides on the cracking phenomenon, which often occurred in cold-rolled light-weight steel plates. Three kinds of steels were fabricated by varying the C content, and their microstructures and tensile properties were investigated. In the two steels that contained a high carbon content, the band structures of ferrites and $\kappa$-carbides that were severely elongated along the rolling direction were well developed, whereas continuous arrays of $\kappa$-carbides were formed in the steel that contained a low carbon content. Detailed microstructural analyses of the deformed region beneath the tensile fracture surface showed that the cracks initiated at arrays of $\kappa$-carbides or $\kappa$-carbides formed interfaces between the band structures, which initiated cleavage fractures in the ferrite bands, while the bands populated with a number of $\kappa$-carbides did not play an important role in propagating the cracks. Thus, the minimization of interfacial $\kappa$-carbides or $\kappa$-carbide arrays by increasing the carbon content was essential for preventing cracking from occurring during cold rolling.

고강도 구조용 내화강의 피로특성 및 음향방출신호의 시간-주파수 해석 (Fatigue Characteristics of High Strength Fire Resistance Steel for Frame Structure and Time-Frequency Analysis its Acoustic Emission Signal)

  • 김현수;남기우;강창룡
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2000년도 춘계학술대회논문집A
    • /
    • pp.67-72
    • /
    • 2000
  • Demand for now nondestructive evaluation are growing to detect fatigue crack growth behavior to predict long term performance of materials and structure in aggressive environments especially when they are In non-visible area. Acoustic emission technique is well suited to these problems and has drawn a keen interests because of its dynamic detection ability, extreme sensitivity and location of growing defects. In this study, we analysed acoustic emission signals obtained in fatigue and tensile test of high strength fire resistance steel for frame structure with time-frequency analysis methods. The main frequency range is different in the noise and the fatigue crack propagation. It could be classified that it were also generated by composite fracture mechanics of cleavage, dimple, inclusion separation etc.

  • PDF

高張力鋼 아이크溶接 본드部의 疲勞特性에 미치는 擴散性 水素의 影響에 관한 硏究 (The effect of diffusible hydrogen on the fatigue cracking of the arc welded part in the high tensile strength steel)

  • 김영식;구자영
    • 대한기계학회논문집
    • /
    • 제10권6호
    • /
    • pp.830-836
    • /
    • 1986
  • 본 연구에서는 이러한 사실에 착안하여 프랑스의 Granjon에 의해 이미 개발된 용접부의 재용성이 탁월한 종래의 정적임플란트(implant)시험기를 정한.고안하여 아아 크용접부의 피로특성에 영향을 미칠 수 있는 제영향인자를 재현하여 간편하게 피로시 험을 할 수 있는 동적 임플란트시험기를 개발하였다. 이러한 시험기를 이용하여 저 온.고압력용강재에 대해서 다음과 같은 항목들을 구명할 목적으로 본 연구는 수행된 것이다.