• 제목/요약/키워드: Clad materials

검색결과 130건 처리시간 0.025초

Al 4343/3N03/4343 합금 3층 clad 재의 sagging 특성에 미치는 냉간압연조건의 영향 (Effect of cold rolling condition on sagging properties of Al 4343/3N03/4343 three-layer clad materials)

  • 김목순
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 1999년도 춘계학술대회논문집
    • /
    • pp.157-160
    • /
    • 1999
  • Aluminum 4343(filler thickness ; 10${\mu}{\textrm}{m}$/Al 3N03(core 80${\mu}{\textrm}{m}$)/Al 4343(filler 10${\mu}{\textrm}{m}$) clad sheet which is recently developed as brazing sheet materials for automotive condensers was fabricated by castinglongrightarrowhot rollinglongrightarrowcold rollinglongrightarrowintermediate annealing(IA)longrightarrowfinal cold rolling(CR). and the effect of IA/CR conditions on microstructure and sagging resistance were investigated the sheet which were fabricated by optimum conditions (IA'ed at 42$0^{\circ}C$ followed by CR'ed to 20~45%) showed good sagging resistance because the core obtained a coarsely recrystallized grain structure during brazing and consequently inhibited filled alloy penetration into the core.

  • PDF

Nb/Ni Clad 전극을 이용한 고효율 CCFL 개발 (Development of CCFL with Nb/Ni Gad Electrode for high efficiency)

  • 박기덕;양승수;박두성;김서윤;임영진
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2005년도 하계학술대회 논문집 Vol.6
    • /
    • pp.441-443
    • /
    • 2005
  • According as CCFL(Cold Cathode Fluorescent lamp) of light source in Backlight unit for Note PC (Personal computer) is presently needed to low power consumption and long life time, the development focus of CCFL is going on the discharge gas, phosphor and electrode material. First of all, discharge voltage characteristic of CCFL is closely connected with electrode material For low discharge voltage, the characteristic of electrode material is needed to low work function, low sputtering ratio and superior manufacturing property. We developed new CCFL with Nb/Ni Clad electrode superior to conventional CCFL. Because Nb/Ni Clad electrode with Ni material and Nb material, the electrical characteristic is superior to other electrode materials. The electrode of Nb/Ni Clad is composed that Ni of outside material has superior manufacturing property and Nb of inside material has low work function. Nb/Ni Clad of new electrode material is made by process of Rolling mill at high pressure and heat treatment. We compared electrical characteristic of Nb/Ni clad electrode with conventional Mo electrode by measurement. Mo electrode and Nb/Ni Clad electrode of cup type with diameter 1.1 mm and length 3.0mm are used to this experiment. Material content of Mo electrode is Mo 100%. But, Nb/Ni Clad electrode is composed by content of Nb 40% and Ni 60%. The result of comparison measurement between new CCFL with Nb/Ni Clad electrode and conventional CCFL was appeared that CCFL with Nb/Ni Clad electrode had superior characteristic than conventional CCFL. As a result of experiment, we completed Note PC with low power consumption and long life time by application of new CCFL with Nb/Ni Clad electrode.

  • PDF

Cu clad Al 복합경량 busbar의 현황과 제조 (A precesses of Cu dad Al busbar for light weight)

  • 우병철;김봉서;변우봉;이희웅
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 1996년도 하계학술대회 논문집 C
    • /
    • pp.1654-1656
    • /
    • 1996
  • Generallly speaking, busbar made with Cu or Cu alloys and producted by plastic manufacturing process. In this study, we reacarch the trend and manufacturing of Cu clad Al busbar for low cost and light weight which used for a electric power suply of distributing board. The objectives of this study is the trend of busbar on electric power supply, the process and application for Cu clad Al busbar and the relation between electric properites and manufacturing operating process on contact parties

  • PDF

Er 첨가 황화물계 광섬유의 제조 및 분광학적 특성 (Spectroscopic Properties of Er-doped Sulfide Fiber)

  • 최용규;임동성;김경헌;박세호;허종
    • 한국세라믹학회지
    • /
    • 제37권8호
    • /
    • pp.781-786
    • /
    • 2000
  • An Er-doped sulfide fiber was drawn, and its spectroscopic properties were analyzed. Compositions of a 1000 ppmwt Er3+-doped core and an undoped clad were Ge30-Ga1-Asg-S61 and Ge30-As8-S62, in at.%, respectively. Refractive index of the core composition was approximately 0.01 high than that of the clad. In order to enhance the mechanical stability as well as to prevent infiltration of impurity ions such as OH-, an UV-curable polymer was used for the coating. The optical loss of a fiber formed directly from a polymer coated core rod without cladding was ∼15 dB/m at 1.06$\mu\textrm{m}$. In the case of a fiber with core/clad structure, the optical loss was so high that the stimulated emission of erbium fluorescence was not evident. It is believed that presence of inhomogeneous core/clad interface and crystalline aggregates precipitated in the clad region were responsible for the high optical loss. On the other hand, fluorescence characteristics of Er3+ embedded in the core region were more or loss deteriorate compared to fiber preform, which is attributed to the redistribution of the Er ions along with the partial crystallization of the core glass during the fiberization process.

  • PDF

레이저 클래딩 공정 조건이 코발트 합금-텅스텐 카바이드 혼합 코팅층의 균열 발생에 미치는 영향 (Cracking Susceptibility of Laser Cladding Process with Co-Based Metal Matrix Composite Powders)

  • 이창민;박형권;이창희
    • Journal of Welding and Joining
    • /
    • 제32권6호
    • /
    • pp.41-46
    • /
    • 2014
  • In this study, cracking susceptibility of laser cladding was investigated according to the processing parameters such as laser power, scan speed and feeding rate with blended powders of stellite#6 and technolase40s (WC+NiCr). The solidification microstructure of clad was composed of Co-based dendrite structures with ${\gamma}+Cr7C3$ eutectic phases at the dendritic boundaries. The crack propagation showed transgranular fracture along dendritic boundaries due to brittle chrome carbide at the eutectic phases. From results of fractography experiments, the fracture surface was typical cleavage brittle fracture in the clad and substrate. The number of clad cracks, caused by a tensile stress after the solidification, increased with increase of laser power, scan speed and feeding rate. Increase of the laser power caused large pores by facilitating WC decarburizing reaction. And the pores affected increase of crack susceptibility. High scan speed caused increment of clad cracks due to thermal stress and WC particle fractures. Also, increase of the feeding rate accompanied an amount of WC particles causing crack initiation and decarburizing reaction.

유한요소법을 이용한 Al/Cu 층상복합재료의 압출공정해석 (Extrusion Process Analysis of Al/Cu Clad Composite Materials by Finite Element Method)

  • 김정인;강충길;권혁천
    • Composites Research
    • /
    • 제12권5호
    • /
    • pp.87-97
    • /
    • 1999
  • 층상복합재료란 이종재료들을 적층하여 계면에서 확산에 의하여 새로운 금속조직을 제어하는 것으로 정의한다. 기계적 성질이 다른 금속이 결합하여 서로의 단점을 보완·개선함으로써 재료의 기계적 성질을 한층 더 향상시킬 뿐만 아니라, 동시에 전기적 성질도 향상시킬 수 있는 재료로 그 종류는 다양하며 용도도 광범위하다. 본 연구에서는 Al/Cu 피복이종복합재료를 직·간적압출하는데 필요한 성형 조건을 도출하기 위하여 유한요소 상용 package인 DEFORM을 이용하여 이종복합재료의 거동해석을 수행하였다. 압출해석에 필요한 물성치를 구하기 위하여 본 연구에서 제조한 재료를 이용하여 압축실험을 수행하였으며, 압출방법, 압출온도, 피복재의 두께 등의 변화에 다른 이종복합재료의 거동을 파악하였다. 또한 해석결과를 바탕으로 이종복합재료의 열간압출실험의 결과와 비교·검토하였다.

  • PDF

동피복 강 선재 인발 공정의 유한요소해석 (Finite Element Analysis of Copper Clad Steel Wire Drawing Process)

  • 김현수;김병민;조형호;조훈
    • 소성∙가공
    • /
    • 제14권2호
    • /
    • pp.147-152
    • /
    • 2005
  • The objective of this study is to develop an optimal drawing die for the clad wire drawing process. Cu-clad wire, which has the advantages of the high strength of a steel core and the electro-conductivity, corrosion resistance of a copper layer, is widely being used in the field of the telecommunications, electric-electronic and military technology industries. It is important to obtain uniformly coated rate when producing clad wires. Drawing process of clad wire will be influenced on damage and coated rate of core and sleeve for process variables such as semi-die angle and reduction in area. Therefore, in this study, the finite-element result obtained in this study was analyzed to the effect of the various forming parameters, which included the semi-die angle and reduction in area. The coated rate will be predicted with observation of copper coated rate variation according to total reduction in area and the optimal pass schedule will be set up through proper reduction in area and semi-die angle variation.

Cu-Al 층상 복합재료 직접압출시 금속의 유동상태와 경도 변화 (Variations of Metal Flow State and Hardness on the Direct Extrusion of Copper Clad Aluminum Rods)

  • 강원영;윤여권;박성훈;김희남
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2000년도 추계학술대회논문집A
    • /
    • pp.759-765
    • /
    • 2000
  • A composite material consists of two or more different material layers. Copper clad aluminum composite materials are being used for economic and structural reasons. This study is concerned with experimental investigation in the direct extrusion of copper clad aluminum rods through conical dies. The suggestion are given for the proper extrudability of copper clad aluminum rods via hot direct extrusion. This paper presents the variation of flow state and hardness at a variable of extrusion ratio and semi-angle of die. By measuring after and before extrusion radius ratio of Cu sleeve and Al core, proportional flow state has been considered. And also by measuring hardness, through extrusion way, a variation of hardness has been considered.

  • PDF

Fe-Ni 합금 클래드 리드 프레임을 이용한 전자 재료 접합부의 품질향상과 그 신뢰성 (Quality improvement on joints of electronic materials and its reliability by Fe-Ni alloy clad lead frame)

  • 신영의;최인수;안승호
    • Journal of Welding and Joining
    • /
    • 제13권2호
    • /
    • pp.82-95
    • /
    • 1995
  • This paper discusses distribution of thermal stress, strain at near the joint and investigates the reliability of solder joints of electronic devices on a printed circuit board. As Electronic devices are composed of different materials, thermal stresses generate at near the interface, such as solder joints and interface between lC device and lead frame pad due to the differences of thermal expansion coefficients, As results of thermal stress, strain, micro crack often occurs thermal fatigue fracture at the interface of different materials, The initiation and propagation of micro crack depend on the environmental conditions, such as storage temperature and thermal cycling. Finally, this paper experimentally shows a way to suppress micro cracks by using Fe-Ni alloy clad lead frame, and investigates crack and thermal fatigue fracture of TSOP(Thin small outline package) type on printed circuit board.

  • PDF

직접압출에 의한 Cu-Al 층상 복합재료 봉의 계면접합 (Interface Bonding of Copper Clad Aluminum Rods by the Direct Extrusion)

  • 김희남;윤여권;강원영;박성훈;이승평
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 2000년도 추계학술대회 논문집
    • /
    • pp.437-440
    • /
    • 2000
  • Composite material consists of more than two materials and make various kinds of composite materials by combining different single materials. Copper clad aluminum composite material is composed of Al and Cu, and it has already been put to practical use in Europe because of its economic benefits. This paper presents the interface bonding according to the variation of extrusion ratio and semi-angle die by observing the interface between Cu and Al using metal microscope. By that result, we can predict the conditions of the interface bonding according to the extruding conditions.

  • PDF