Analysis for Densification Behavior and Grain Growth of Nanocrystalline Ceramic Powder under High Temperature (나노 세라믹 분말의 고온 치밀화와 결정립 성장의 해석)

  • Kim, Hong-Gee;Kim, Ki-Tae
    • Proceedings of the KSME Conference
    • /
    • 2000.04a
    • /
    • pp.363-368
    • /
    • 2000
  • Densification, grain growth, and phase transformation of nanocrystalline ceramic powder were investigated under pressureless sintering, sinter forging, and hot pressing. A constitutive model for densification of nanocrystalline ceramic powder was proposed and implemented into a finite element program (ABAQUS). A grain growth model was also proposed by including the effect of applied stress on grain growth when phase transformation occurs. Finite element results by using the proposed models well predicted densification behavior, deformation, and grain growth of nanocrystalline titania powder during pressureless sintering, sinter forging, and hot pressing.

  • PDF

Investigation on Interfacial Microstructures of Stainless Steel/Inconel Bonded by Directed Energy Deposition of alloy Powders (레이저 직접 용착공정으로 형성된 스테인레스/인코넬 합금 계면의 미세조직 분석)

  • Eom, Yeong Seong;Kim, Kyung Tae;Jung, Soo-Ho;Yu, Jihun;Yang, Dong Yeol;Choe, Jungho;Sim, Chul Yong;An, Seung Jun
    • Journal of Powder Materials
    • /
    • v.27 no.3
    • /
    • pp.219-225
    • /
    • 2020
  • The directed energy deposition (DED) process of metal 3D printing technologies has been treated as an effective method for welding, repairing, and even 3-dimensional building of machinery parts. In this study, stainless steel 316L (STS316L) and Inconel 625 (IN625) alloy powders are additively manufactured using the DED process, and the microstructure of the fabricated STS316L/IN625 sample is investigated. In particular, there are no secondary phases in the interface between STS316L and the IN625 alloy. The EDS and Vickers hardness results clearly show compositionally and mechanically transient layers a few tens of micrometers in thickness. Interestingly, several cracks are only observed in the STS 316L rather than in the IN625 alloy near the interface. In addition, small-sized voids 200-400 nm in diameter that look like trapped pores are present in both materials. The cracks present near the interface are formed by tensile stress in STS316L caused by the difference in the CTE (coefficient of thermal expansion) between the two materials during the DED process. These results can provide fundamental information for the fabrication of machinery parts that require joining of two materials, such as valves.

Densification behavior of ceramic powder under cold compaction (냉간압축 하에서 세락믹 분말의 치밀화 거동)

  • Choi, Seung-Wan;Kim, Gi-Tae
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.22 no.4
    • /
    • pp.924-938
    • /
    • 1998
  • Densification behavior of ceramic powder under cold compaction was investigated. Experimental data were obtained for zirconia powder and alumina powder under triaxial compression with various loading conditions. A special form of the Cap model was proposed from experimental data under triaxial compression for a yield function of ceramic powder. The proposed yield function was inplemented into a finite element program (ABAQUS) to study densification behaviors of zirconia and alumina powders under die compaction. The effect of friction between the powder and die wall was also investigated. Density distributions of powder compacts were measured and compared with finite element results.

Eco-friendly Self-cooling System of Porous Onggi Ceramic Plate by Evaporation of Absorbed Water

  • Katsuki, Hiroaki;Choi, Eun-Kyong;Lee, Won-Jun;Kim, Ung-Soo;Hwang, Kwang-Taek;Cho, Woo-Seok
    • Journal of the Korean Ceramic Society
    • /
    • v.55 no.2
    • /
    • pp.153-159
    • /
    • 2018
  • Porous ceramic plates were prepared from Onggi clay and bamboo charcoal powder at 1100 and $1200^{\circ}C$ and their porous properties and water absorption, and the cooling effect of porous plates, were investigated to produce eco-friendly porous ceramics for a self-cooling system that relies on the evaporation of absorbed water. Porous properties were dependent on the particle size of charcoal powder pore forming additive and the firing temperature; properties were also found to be dependent on the total pore volume, average pore size and porosity, which had values of $0.103-0.243cm^3/g$, 0.81 - 2.56 mm and 20.9 - 38.2%, respectively, at $1100^{\circ}C$ and $0.04-0.18cm^3/g$, 0.33 - 2.03 mm and 10.8 - 30.9%, respectively, at $1200^{\circ}C$. Cooling temperature difference of flowing air parallel to surface of porous ceramic plates fired with two kinds of charcoal powder at $1100^{\circ}C$ was $3.5-3.6^{\circ}C$ at $26^{\circ}C$ and 60% of relative humidity in a closed box. Cooling temperature difference was dependent on the number of porous plates and the distance between porous plates. A simple and eco-friendly cooling system using porous ceramic plates fired from Onggi clay and charcoal powder was proposed.

A Study on the Fabrication and Mechanical Properties of $WC-Co-Al_2O_3$ Ceramic Composites Using WC Powders Synthesized by SHS Method and Commercial WC Powders (SHS 화학로법에 의해 합성된 WC 분말과 상용 WC 분말을 이용한 $WC-Co-Al_2O_3$ 세라믹 복합체의 제조 및 그 기계적 특성에 관한 연구)

  • Lee, K.R.;Cho, D.H.;Lee, H.B.;Park, S.
    • Journal of the Korean Ceramic Society
    • /
    • v.32 no.12
    • /
    • pp.1392-1400
    • /
    • 1995
  • WC-10wt%Co-Al2O3 ceramic composites, using both the SHS (Self-propagating High Temperature Synthesis) synthesized WC powder method and commercial WC powder, were prepared by varing WC-Co/Al2O3 vol% ratio and sintering temperature (1350℃∼1650℃) for 1 hr in Ar atmosphere. Mechanical characterization has been investigated by Instron meterial testing system and Vicker's hardness test. Compositional and structural chracterizations were carried out by energy-dispersive analysis of X-ray (EDAX) data and scanning electron microscope (SEM). Electrical characterization was carried out by the electrical resistivity measurement using 4-point probe method. As sintering period increased and Al2O3 contents decreased in WC-10wt%Co-Al2O3 ceramic composite, shrinkage and relative density increased, resulting in maximum values at 1600℃. Also the major matrix phase changed with increasing Al2O3 content from 0 to 100 vol%. It was also identified by SEM, EDAX, and electrical resistivity measurement. Based on the results of analysis of flexural strength, toughness and hardness, the mechanical properties of WC-10wt%Co-Al2O3 ceramic composites using the SHS synthesized WC powder were better than those WC-10wt%Co-Al2O3 ceramic composites using commercial WC powder because WC-10wt%Co-Al2O3 ceramic composites using the SHS synthesized WC powder were sintered very well due to small initial particle size. By the addition of 40 vol% Al2O3 [60(WC=10wt%Co)-40Al2O3], it was possible to obtain a proper candidate as a superalloy.

  • PDF

Effect of Dietary Ceramic Powder on Laying Performance, Pathogenic Bacterial Count in Caecal Content and Excreta, Malodorous Substances in Excreta and Fatty Acid composition or Egg Yolk in Laying Hens (Ceramic 분말의 첨가가 산란계의 생산성, 맹장 및 배설물중 병원성 미생물의 수, 배설물충의 악취물질 및 난황중 지방산 조성에 미치는 영향)

  • Son J. H.
    • Korean Journal of Poultry Science
    • /
    • v.32 no.4
    • /
    • pp.261-268
    • /
    • 2005
  • The purpose of this study was to evaluate the effect of dietary ceramic powder on laying performance, Pathogenic bacterial (E. coli, salmonella) counts in caecal contents and excreta, malodorous substances $(NH_3,\;H_2S,\;VFA)$ in excreta and fatty acid composition of e99 yolk in laying hens. Three hundred sixty layers at 34 weeks of age were divided into three groups of 120 hens each and each group was fed diets containing 0 (control), 0.4, or 0.8 ceramic powder for six weeks. It is concluded that $0.4\%$ ceramic powder supplementation of diets decreased of E. coli, salmonella counts in the intestine and emission of $NH_3$ and VFA gas from excreta, and improved the laying Performance and ratio of egg yolk fatty acids contents.

Synthesis of β-SiC Powder using a Recycled Graphite Block as a Source (그라파이트 블록을 원료로써 재활용한 β-SiC 분말 합성)

  • Nguyen, Minh Dat;Bang, Jung Won;Kim, Soo-Ryoung;Kim, Younghee;Jung, Eunjin;Hwang, Kyu Hong;Kwon, Woo-Teck
    • Resources Recycling
    • /
    • v.26 no.1
    • /
    • pp.16-21
    • /
    • 2017
  • This paper relates to the synthesis of a source powder for SiC crystal growth. ${\beta}-SiC$ powders are synthesized at high temperatures (>$1400^{\circ}C$) by a reaction between silicon powder and carbon powder. The reaction is carried out in a graphite crucible operating in a vacuum ambient (or Ar gas) over a period of time sufficient to cause the Si+C mixture to react and form poly-crystalline SiC powder. End-product characterizations are pursued with X-ray diffraction analysis, SEM/EDS, particle size analyzer and ICP-OES. The purity of the end-product was analyzed with the Korean Standard KS L 1612.

Characteristics of WO3-CuO Powder Mixture Prepared by High-Energy Ball Milling in a Bead Mill for the Synthesis of W-Cu Nanocomposite Powder (W-Cu 나노분말 합성을 위해 비드밀에서 고에너지 볼밀링 공정에 의해 제조된 WO3-CuO 혼합분말의 특성 연구)

  • Park, Hae-Ryong;Ryu, Sung-Soo
    • Journal of Powder Materials
    • /
    • v.24 no.5
    • /
    • pp.406-413
    • /
    • 2017
  • A Nanosized $WO_3$ and CuO powder mixture is prepared using novel high-energy ball milling in a bead mill to obtain a W-Cu nanocomposite powder, and the effect of milling time on the structural characteristics of $WO_3-CuO$ powder mixtures is investigated. The results show that the ball-milled $WO_3-CuO$ powder mixture reaches at steady state after 10 h milling, characterized by the uniform and narrow particle size distribution with primary crystalline sizes below 50 nm, a specific surface area of $37m^2/g$, and powder mean particle size ($D_{50}$) of $0.57{\mu}m$. The $WO_3-CuO$ powder mixtures milled for 10 h are heat-treated at different temperatures in $H_2$ atmosphere to produce W-Cu powder. The XRD results shows that both the $WO_3$ and CuO phases can be reduced to W and Cu phases at temperatures over $700^{\circ}C$. The reduced W-Cu nanocomposite powder exhibits excellent sinterability, and the ultrafine W-Cu composite can be obtained by the Cu liquid phase sintering process.