• 제목/요약/키워드: Cathodic

검색결과 752건 처리시간 0.025초

희생양극재의 매입에 의한 콘크리트 중의 전기방식 효과 (Effects of the Protection for Rebars by Embeded Sacrificial Anode in Concrete)

  • 김성수;김홍삼;김종필
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2001년도 가을 학술발표회 논문집
    • /
    • pp.1207-1212
    • /
    • 2001
  • Reinforced concrete has defects in durability due to carbonation, freezing and thawing, and penetration of chloride ions with elapse of time in spite of super structure. Especially steel corrosion in concrete due to penetration of chloride ions has result in a severe decline in service life. The principal purpose of this study is to estimate effects of sacrificial anode cathodic system, one of the electrochemical methods in order to control of steel corrosion in concrete. There are chloride content in concrete in cracked and non cracked specimen with cathodic protection. To investigate the effect of sacrificial anode cathodic protection, potential-decay with current density, corrosion ratio, etc. are measured. We have the excellent effect for control steel corrosion adaption sacrificial anode cathodic system.

  • PDF

Ni 전극 계면에서 전기화학적 spike 발진 (Electrochemical spike oscillation st the Ni electrode interface)

  • 천장호;손광철;라극환
    • 전자공학회논문지A
    • /
    • 제33A권12호
    • /
    • pp.83-89
    • /
    • 1996
  • The electrochemical spike oscillations at the nickel (Ni) electrode/(0.05M KHC$_{8}$H$_{4}$O$_{4}$) buffer solution (pH 9) interface have been studied using voltammetric and chronoamperometric methods. The nature of the periodic cathodic current spikes is the activation controlled currents due to the hydrogen evolution reaction and depends onthe fractioanl surface coverage of the adsorbed hydrogen intermediate or the cathodic potential. There is two kinds of the waveforms corresponding to two kinds of the cathodic current spike oscillations. The widths, periods, and amplitudes of the cathodic current spikes are 4 ms or 5ms, 151 ms or 302 ms, and < 30 mA or < 275 mA, respectively. The fast discharge and recombination reaction steps are 1.5 times and twice and faster than the slow discharge and recombination reaction steps. The fast and slow discharge and recombination reaction steps are 1.5 times and twice faster than the slow discharge and recombination reaction steps. The fast and slow discharge and recombination reactions corresponding to the fast and slow adsorption sites at the Ni cathode.

  • PDF

해양환경중에서 A1-합금희생양극에 의한 음극방식특성 (A Study on the Characteristics of Cathodic Protection by Al-Alloy Sacrificial Anode in Marine Environment)

  • 이연호
    • 수산해양기술연구
    • /
    • 제28권1호
    • /
    • pp.53-60
    • /
    • 1992
  • In this study, cathodic protection experiment was carried out by Al-alloy sacrificial anode in marine environments which have specific resistance($\rho$) if 25~7000$\Omega$.cm and investigated protection potential, current density and loss rate of Al-alloy sacrificial anode. The main results resistance($\rho$) of 400$\Omega$.cm, the cathodic protection potential appears high about-720 mV(SCE). But below specific resistance($\rho$) of 300$\Omega$.cm, the cathodic protection potential appears low about-770 mV(SCE) and simultaneously, cathode is protected sufficiently. 2) The loss rate of Al-Alloy sacrificial anode became large with decreasing specific resistance and increasing the ratio(A sub(c)/A sub(a) of bared surface area of anode and cathode. 3) The loss rate of Al-alloy sacrificial anode(w) to the mean current density of anode(i) is as follows. w=ai+b (a, b : experimental constants)

  • PDF

백금족 전력 계면에서 전기화학적 Impulse 발진 (Electrochemical Impulse Oscillations at the Platinum Group Electrode Interfaces)

  • 전장호;손광철;라극환
    • 전자공학회논문지A
    • /
    • 제32A권3호
    • /
    • pp.143-151
    • /
    • 1995
  • The electrochemical impulse oscillations of the cathodic currents at the platinum group (Pt, Pd) electrode/(0.05M KHC$_{8}H_{4}O_{4}$) buffer solution interfaces have been studied using voltammetric, chronoamperometric, and electrochemical impedance methods. The periodic impulses of the cathodic currents are the activation controlled currents due to the hydrogen evolution reaction, and depend on the fractional surface coverage of the adsorbed hydrogen intermediate and potential. The oscillatory mechanism of the cathodic current impulses is connected with the unstable steady state of negative differential resistance. The widths and periods of the cathodic current impulses are 4ms or 5ms and 152.5ms or 305ms, respectively. The H$^{+}$ discharge reaction step is 38 or 61 times faster thatn the recombination reaction steps and the H$^{+}$ mass transport processes. The atom-atom recombination reaction step is twice faster thatn the atom-ion recombination reaction step. The two kinds of active sites corresponding to the atom-atom and atom-ion recombination reaction steps exist on the platinum group electrode surfaces.

  • PDF

The Performance of Cathodic Protection with ICCP

  • Oh, Jin-Seok
    • Journal of Advanced Marine Engineering and Technology
    • /
    • 제28권8호
    • /
    • pp.1286-1290
    • /
    • 2004
  • This paper describes the anti-corrosion system on underwater structures of ships. Metals and alloys have several positions in the series such as immunity, corrosion and passivity. The iron potential has to change from the corrosion position to the anodic protection or cathodic protection for preventing corrosion by providing corrosion protection system such as ICCP(Impressed Current Cathodic Protection). The purpose of ICCP system is to eliminate the rusting or corrosion, which occurs on metal immersed in water. The system includes a power supply unit, which consists of a transformer, a converter. a controller, etc. This paper presents the protection performance of ICCP under dynamic condition such as velocity. The variation of potential and current density with time and environment factors are also described Finally, the experimental results will be explained and analysed.

희생양극식 음극방식이 적용된 해안 교량 구조물의 방식거동 (Cathodic Protection Behavior of Coastal Bridge Structure with Sacrificial Anode Cathodic Protection System)

  • 하지명;진충국;정진아
    • Corrosion Science and Technology
    • /
    • 제11권6호
    • /
    • pp.242-246
    • /
    • 2012
  • This measurement represents the effectiveness of sacrificial anode cathodic protection (SACP) system in a coastal bridge structure. To verify the cathodic protection (CP) effect, the monitoring sensor (DMS-100) that could measure potential, corrosion rate, current, concrete resistivity, and temperature was embedded. The measurement conducted for three years after CP system was installed. Specifically, due to the fact that fresh water and sea water was repeated in the bridge structure, this bridge structure presented special CP behavior. Measurement factors were CP potential, CP current, concrete resistivity, and depolarization potential. In addition, visual inspection was also carried out. As a result of current and depolarization measurement, CP system was well activated in most piers.

Determination of Low-temperature Electrochemical Properties of Selected Cation-exchange Membranes for Cathodic Protection Analysis

  • Ko, Moon-Young;Kwon, Byeong-Min;Hong, Byung-Pyo;Byun, Hong-Sik
    • Korean Membrane Journal
    • /
    • 제10권1호
    • /
    • pp.8-12
    • /
    • 2008
  • The electrochemical properties of Nafion type membranes as a function of temperature to examine the key factors affecting the cathodic protection process at low temperatures was investigated in this study. Variable temperature experiments for AC impedance, DC resistance were conducted. The resistances of 3 Nafion membranes (N 324, N 450, N MAC) were measured in 30% KOH (aq) for a range of temperatures between $-30^{\circ}C$ and room temperature. Membrane resistance increases exponentially with decreasing temperature. This behaviour is most significant at operational temperatures below $0^{\circ}C$. These membranes are stable under the low temperature and caustic conditions of the heat exchange system, but they place a much higher restriction on the cathodic protection of the stainless heat exchange stack. N 450 has the lowest AC impedence and DC resistance at temperatures below $0^{\circ}C$ and consequently is most suitable membrane of the three, for low temperature applications.

RC조 구조물의 최적 음극방식 조건 설정을 위한 함수율의 영향에 대한 평가 (Effect of Moisture on the Current Density for Optimized Cathodic Protection Condition in RC Structures)

  • 박동천;조규환;안재철
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2013년도 춘계 학술논문 발표대회
    • /
    • pp.29-30
    • /
    • 2013
  • Steel corrosion is the most serious problem in RC structures. Even though patch repair method is normally applied in repair system, the effectiveness is not enough. Cathodic protection in active repair method to deteriorated RC structures. FEM model was developed to simulate the optimized cathodic protection condition. Iro oxidation, hydrogen evolution and oxygen reduction were considered to expect current distribution. Moisture content in concrete which can affect the electrolyte conductivity was used as initial condition.

  • PDF

전위변화에 의한 콘크리트내의 철근방식에 관한 연구 (Study on the Corrosionproofing in Concrete by Cathodic Protection)

  • 임서형
    • 한국구조물진단유지관리공학회 논문집
    • /
    • 제3권2호
    • /
    • pp.213-220
    • /
    • 1999
  • The purpose of this study is to apply cathodic protection to reinforced concrete structure and provide fundamental data to prevent the corrosion. The theory of cathodic protection of steel in concrete is to apply sufficient direct current so that corroding anodes on the steel are prevented from discharging ions. Two methods are used to supply the external current. In one, the protected metal is the cathode by connecting it to a more active metal. In the second, an external direct current power source supplies the current. The first is the sacrificial-anode system and the second the impressed-current system. The study results showed that the corrosion of the reinforcing steel in concrete could be enormously decreased by using protective current. The sacrificial anode and concrete nave to be adhered closely each in order to prevent the corrosion of reinforcing steel.

  • PDF