• Title/Summary/Keyword: Calcium hydroxyapatite

Search Result 188, Processing Time 0.026 seconds

Clinical application and classification of bone graft material according to component (임상가를 위한 특집 2 - 구성성분별 골이식재의 분류와 임상적용)

  • Kim, Young-Kyun
    • The Journal of the Korean dental association
    • /
    • v.48 no.4
    • /
    • pp.263-274
    • /
    • 2010
  • I classified the bone graft material according to the component. Most bone graft material is composed of inorganic and organic constituent. Organic component such DBM is associated with osteoinduction. Inorganic components such as hydroxyapatite, $\beta$-TCP, calcium sulfate, bioactive glass, polymer are associated with osteoconduction. Autogenous bone graft is ideal material. We can select any biocompatible material for the restoration of small filling defect with intact bony wall. However, we should select first osteogenetic and osteoinductive material to regenerate the viable bone tissue.

IMPLANTATION OF TOOTHASH COMBINED WITH PLASTER OF PARIS;CLINICAL APPLICATIONS (치아회분말과 치과용 연석고의 혼합매식술;임상적 적용)

  • Kim, Young-Kyun;Yeo, Hwan-Ho
    • Maxillofacial Plastic and Reconstructive Surgery
    • /
    • v.16 no.2
    • /
    • pp.130-136
    • /
    • 1994
  • Toothash and plaster of Paris (Calcium sulfate) have been studied for bone substitute through experimental studies and clinical studies. Toothash is like resorbable hydroxyapatite. Plaster of Paris is resorbable and biocompatible. The toothash combined with plaster of Paris has the advantages of individual characteristics. The authors used this composite material in the jaw defect filling. In operation, we could manage this implant material easily and remove the dead space. During the followup period, this composite material was resorbed gradually and substituted as new-forming bone from the surrounding tissue. Complications were minor and treated completely without problems.

  • PDF

Beneficial effect of vitamin K on bone health (비타민 K의 골 건강 증진 효과)

  • Jang, Young-Ho
    • Journal of Korean society of Dental Hygiene
    • /
    • v.11 no.4
    • /
    • pp.419-426
    • /
    • 2011
  • Originally, vitamin K was defined as a factor for blood coagulation. Now more attention is focused on vitamin K for bone metabolism and bone health. Vitamin K is a coenzyme for glutamate carboxylase which converts glutamate residues to ${\gamma}$-carboxyglutamate(Gla) residues. Gla residues have calcium binding ability and bound to hydroxyapatite crystals in bone. Vitamin K promotes the carboxylation of osteocalcin and matrix Gla-protein, vitamin K-dependent proteins and improves bone mineral density and bone mass. Vitamin K deficiency causes reductions in bone mineral density and increases the risk of osteoporotic bone fractures, resulting from undercarboxylated osteocalcin. This paper is to provide a brief information of vitamin K and its role in bone health.

SIL VER-IMPREGNATED HAP-COATING ON ALUMINA SUBSTRATE FOR PREVENTION OF INFECTION

  • Kim, T.N.;Feng, Q.L.;Wu, J.;Kim, J.O.
    • Journal of the Korean Vacuum Society
    • /
    • v.6 no.S1
    • /
    • pp.27-33
    • /
    • 1997
  • Recently ion beam assistant deposition (IBAD) was successfully used to produce a dense ultra-adherent and pinhole-free hydroxyapatite (HAp) layer on alumina substrate. After that the HAp-coated alumina was immersed in 20ppm and 100ppm $AgNO_3$ solution at room temperature for 48 hours to carry out the ions exchange between $Ag^+\;and\;Ca^+$ in HAp. The obvious antimicrobial effect against E.Coli, P. Aeruginosa and S. Epidermidis was observed in the samples treated with 20ppm $AgNO_3$ Solution, In contrast to this the untreated samples did not show any bactericidal effect. Scanning electron microscope(SEM) study showed that Ag homogeneously distributed on the surface. X-ray diffraction (XRD) demonstrated that the surface structure in the samples without Ag was HAp whereas with Ag is HAp and AgCaP. It appears that silver ions exchange with calcium ions in HAp does not cause significant changes in the structure of HAp coatings.

  • PDF

EFFECT OF VARIOUS MECHANICAL TREATMENTS OF HYDROXYAPATITE-COATED IMPLANT SURFACES (Hydroxyapatite 피막 처리된 임프란트에 대한 여러가지 기계적 표면처리방법이 임프란트 표면조도 및 성상에 미치는 영향)

  • Yang, Kyung-Ran;Jung, Oh-Chul;Lee, Jae-Mok;Suh, Jo-Young
    • Journal of Periodontal and Implant Science
    • /
    • v.24 no.1
    • /
    • pp.131-143
    • /
    • 1994
  • For maintenance of exposed implant in healthy state, it is necessary to treat the surface of implant fixture and provide the surface adjustable to surrounding tissues. Variable techniques have been introduced such as citric acid and air-abrasive system to treat the failed implant. Although when the rough surface of HA coated implant was exposed to oral environment, the surface treatment method with citric acid or air-abrasive system is effective for removal of bacterial endotoxin, it is unsuccessful to prevent plaque deposition due to difficulty in removal of rough surface of HA coated implant. Thus, in this study the method that removes bacterial endotoxin and makes smooch surface without alteration of surface characteristics was studied. HA coated disc manufactured by IMZ Co. Was treated with high speed diamond bur, low speed diamond bur, stone bur, rubber point, jetpolisher. And then its surface state was examined with profilometer and SEM to evaluate the surface smoothness, and its surface component was analyzed with EDX to evaluate wheter the surface characteristics were altered or not. As a result, following results were obtained. When the surface roughness of each implant disc was measured by profilometer, the group I showed a $R_{max}\;2.11{\mu}m$ and the group II, III, IV, V showed a $R_{max2}\;4.17{\mu}m$, $7.28{\mu}m$, $8.61{\mu}m$ and $39.44{\mu}m$ respectively. That is, surface smoothness was highest in the group I and it has been gradually decreased in the group II, III, IV and V. Under the SEM examination, the group I showed relatively smooth surface and the group II showed slightly rougher surface than the group I due to partially remaining HA particles while most HA particle was removed. The group III and IV showed rough topography due to HA particles that was not grinded, and HA coated surface in group V showed very irregular surface with deep groove and prominence. In cross-sectional view, the group I showed uniform surface, and the group III, IV showed rough surface due to remaining HA particles but the thickness of HA coating was remarkably reduced. The group II has similar pattern in group I, and the group V showed about $40{\mu}m$ thickness although it was not constant. By analysis of surface component with EDX, the group II in which the grinding was effective showed a small quantity of calcium and phosphorous and the group III, IV, in which the grinding was incomplete showed calcium and phosphorus peak. In all experimental group, no other than titanium, aluminum, calcium, phosphorus was observed.

  • PDF

Characteristic Analysis and Fabrication of Bioceramic Scaffold using Mixing Ratios of TCP/HA by Fused Deposition Modeling (압출 적층 조형 기술을 이용한 TCP/HA 의 혼합비율에 따른 바이오 세라믹 인공지지체의 제작 및 특성 연구)

  • Sa, Min-Woo;Kim, Jong Young
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.38 no.11
    • /
    • pp.1273-1281
    • /
    • 2014
  • Tissue engineering is an emerging research field that has the potential to restore, regenerate and repair damaged bone tissue and organs. Tricalcium phosphate and hydroxyapatite biomaterials-based calcium phosphate are excellent materials that have both osteoconduction and biocompatibility for bone tissue regeneration. In this study, solution structures were successfully fabricated using a fused deposition modeling system based on deposition and heating devices. The morphology characteristics of the bioceramic scaffolds sintered at a temperature of $1,300^{\circ}C$ were analyzed by scanning electron microscopy. The effects of various blended TCP/HA ratio on the microstructure and shrinkage were studied. The mechanical properties of the scaffolds were measured using a compression testing machine from stress-strain curves on the crosshead velocity of 1 mm/min. The fabricated scaffolds were evaluated by cell proliferation tests of MG-63 cells. The results of this study suggest that the blended TCP(75 wt%)/HA(25 wt%) scaffold is an appropriate scaffold for bone tissue regeneration.

Review on the Correlation between Bone Mass, Skinfold Thickness and the Volume of Urine collagen Peptide in Postmenopausal Women (폐경 후 여성의 골량과 피부두겹두께 및 뇨 콜라겐펩타이드 양의 관련성에 대한 고찰)

  • Park, Mi-Jung
    • Journal of Korean Biological Nursing Science
    • /
    • v.3 no.2
    • /
    • pp.91-103
    • /
    • 2001
  • The bone is composed of the bone matrix of collagen and hydroxyapatite, the mixture of calcium and phosphours. The bone tissue is considered to the special connective tissue that possesses extracellular matrix made by collagen fiber deposited with mineral complex. In order to maintain bone mass measured by the sum of bone matrix and hydroxyapatite, bone resorption by osteoclast during lifetime and bone remodeling to form bone by osteoblast in its resorption region repeat continuously. The osteoblast has a mesodermic fetal origin like fibroblast for the formation of form tissues. Two cells express identical genes and synthesize the identical collagen type I as the major component of the formation of bone matrix and skin. Therefore, it is considered that the decrease of skinfold thickness and the decrease of bone mass related to the age, the change of two tissues composed of collagen type I is caused by the same genetic mechanism. The decrease of bone mass is caused by the change of the amount and structure of bone matrix by several factors and the amount of minerals deposited on bone matrix. Especially, in case of female, the deficiency of estrogen by menopause makes these changes rapidly increased. The decrease of bone mass and skinfold thickness is due to the decrease of the amount of collagen and its structural change the common component of bone tissue and skin tissue. Therefore, the relationship of the amount of cross-linked peptide N-telopeptide, collagen metabolite which excretes as urine. Based upon the proved results about the significant relationship of bone mass, the amount of bone collagen, the amount of skin collagen and skinfold thickness, the bone mass may be expected through a facile determination of skinfold thickness.

  • PDF

Bone-like Apatite Morphology on Si-Zn-Mn-hydroxyapatite Coating on Ti-6Al-4V Alloy by Plasma Electrolytic Oxidation

  • Park, Min-Gyu;Choe, Han-Cheol
    • Proceedings of the Korean Institute of Surface Engineering Conference
    • /
    • 2017.05a
    • /
    • pp.158-158
    • /
    • 2017
  • Titanium and its alloys have been used in the field dental and orthopedic implants because of their excellent mechanical properties and biocompatibility. Despite these attractive properties, their passive films were somewhat bioinert in nature so that sufficient adhesion of bone cells to implant surface was delayed after surgical treatment. Recently, plasma electrolyte oxidation (PEO) of titanium metal has attracted a great deal of attention is a comparatively convenient and effective technique and good adhesion to substrates and it enhances wear and corrosion resistances and produces thick, hard, and strong oxide coatings. Silicon(Si), Zinc(Zn), and Manganese(Mn) have a beneficial effect on bone. Si in particular has been found to be essential for normal bone and cartilage growth and development. And, Zn has been shown to be responsible for variations in body weight, bone length and bone biomechanical properties. Also, Mn influences regulation of bone remodeling because its low content in body is connected with the rise of the concentration of calcium, phosphates and phosphatase out of cells. The objective of this work was research on bone-like apatite morphology on Si-Zn-Mn-hydroxyapatite coating on Ti-6Al-4V alloy by plasma electrolytic oxidation. Anodized alloys were prepared at 280V voltage in the solution containing Si, Zn, and Mn ions. The surface characteristics of PEO treated Ti-6Al-4V alloy were investigated using XRD, FE-SEM, and EDS.

  • PDF

Evaluation of Bioactivity of Ti-6Al-7Nb Alloys with Various Hydrothermal Treatment Times (열수처리 시간에 따른 Ti-6Al-7Nh 합금의 생체활성 평가)

  • Kwon O. S.;Choi S. K.;Park K. B.;Lee M. H.;Bae T. S.;Lee O. Y.
    • Korean Journal of Materials Research
    • /
    • v.14 no.12
    • /
    • pp.876-884
    • /
    • 2004
  • This study was to investigate whether the bioactivity of the anodized and hydrothermally treated Ti-6Al-7Nb alloy were affected by the time of hydrothermal treatment. Anodizing was performed at current density 30 $mA/cm^2$ up to 300 V in electrolyte solutions containing $DL-{\alpha}-glycerophosphate$ disodium salt hydrate $(DL-{\alpha}-GP)$ and calcium acetate (CA). Hydrothermal treatment was done at $300^{\circ}C$ for 30 min, 1 hr, 2 hrs, and 4 hrs to produce a thin film layer of hydroxyapatite (HA). The bioactivity was evaluated from HA formation on the surfaces in a Hanks' solution with pH 7.4 at $36.5^{\circ}C$ for 10, 20, and 30 days. Anodic oxide films were porous with pore size of $1\sim4{\mu}m\;and\;3\sim4{\mu}m$ thickness. The anodic oxide films composed with strong anatase peak with presence of rutile peak, and showed the increase in intensity of anatase peak after hydrothermal treatment. It was shown that the intensity of anatase peak increased with increasing the time of hydrothermal treatment but was no difference in rutile peak. The corrosion voltage was the highest in the group of hydrothermal treatment for 2 hrs (Ecorr: -338.6 mV). The bioactivity in Hank's solution was accelerated with increasing the time of hydrothermal treatment.