• Title/Summary/Keyword: Butt joint welding

Search Result 179, Processing Time 0.028 seconds

A Study on the Development of High Deposition Automatic Vertical Welding of Erection Stage in Shipbuilding (조선 탑재용접용 대입열 수직자동용접법의 개발에 관한 연구)

  • Park, Ju-Yong;Choe, Woo-Hyeon
    • Journal of Welding and Joining
    • /
    • v.26 no.5
    • /
    • pp.66-73
    • /
    • 2008
  • Welding work in pre-erection or erection stage of shipbuilding construction to be carried out in flat and vertical upward position mostly and Electrogas welding(EGW) is actively applied especially for vertical butt joint of thicker steel plate recently. In this study considered how to develope and improve mechanical properties of weld metal and HAZ in high heat input welding processes such as EGW and Electroslag welding(ESW) with its welding equipment in order to extend the application range to the longitudinal members and hatch coaming parts of container ship. Some components of welding system and parameters were modified to get the faster travel speed and reduce weld heat input, and also by adding additional filler rods or tubes increase the amount of deposited weld metal. With the test get some good date can apply to actual fabrication work and recommend items to manufacture welding materials make better. Above all things it's a fruition that to prepare the possibility of application of ESW to shipbuilding construction which fill up the gap of stoppage days of more than 20 years.

An Experiment Study for S/N Ratio of Bead Geometry for Guaranteeing the Welding Quality in Bellows Weld Joint (벨로우즈 용접부의 품질확보를 위한 비드형상 S/N비에 관한 실험적 연구)

  • Lee, Jong-Pyo;Kim, Ill-Soo;Park, Min-Ho;Jin, Byeong-Ju;Kim, In-Ju;Kim, Ji-Sun
    • Journal of Welding and Joining
    • /
    • v.35 no.2
    • /
    • pp.43-51
    • /
    • 2017
  • The automatic welding systems, have received much attention in recent years, because they are highly suitable not only to increase the quality and productivity, but also to decrease manufacturing time and cost for a given product. Automatic welding work in semiconductor or space industry to be carried out in pipe line and butt joint mostly and plasma arc welding(PAW) is actively applied. To get the desired quality welds in automated welding system is challenging, a mathematical model is needed that has complete control over the relevant process parameters in order to obtain the required mechanical properties. However, In various industries the welding process mathematical model is not fully formulated for the process parameter and on the welding conditions, therefore only partial variables can be predicted. Therefore, this paper investigates the interaction between the welding parameters and mechanical properties for predicting the weld bead geometry by analyzing the S/N ratio.

The effect of initial stress induced during the steel manufacturing process on the welding residual stress in multi-pass butt welding

  • Park, Jeong-ung;An, Gyubaek;Woo, Wanchuck
    • International Journal of Naval Architecture and Ocean Engineering
    • /
    • v.10 no.2
    • /
    • pp.129-140
    • /
    • 2018
  • A residual stress generated in the steel structure is broadly categorized into initial residual stress during manufacturing steel material, welding residual stress caused by welding, and heat treatment residual stress by heat treatment. Initial residual stresses induced during the manufacturing process is combined with welding residual stress or heat treatment residual stress, and remained as a final residual stress. Because such final residual stress affects the safety and strength of the structure, it is of utmost importance to measure or predict the magnitude of residual stress, and to apply this point on the design of the structure. In this study, the initial residual stress of steel structures having thicknesses of 25 mm and 70 mm during manufacturing was measured in order to investigate initial residual stress (hereinafter, referred to as initial stress). In addition, thermal elastic plastic FEM analysis was performed with this initial condition, and the effect of initial stress on the welding residual stress was investigated. Further, the reliability of the FE analysis result, considering the initial stress and welding residual stress for the steel structures having two thicknesses, was validated by comparing it with the measured results. In the vicinity of the weld joint, the initial stress is released and finally controlled by the weld residual stress. On the other hand, the farther away from the weld joint, the greater the influence of the initial stress. The range in which the initial stress affects the weld residual stress was not changed by the initial stress. However, in the region where the initial stress occurs in the compressive stress, the magnitude of the weld residual compressive stress varies with the compression or tension of the initial stress. The effect of initial stress on the maximum compression residual stress was far larger when initial stress was considered in case of a thickness of 25 mm with a value of 180 MPa, while in case of thickness at 70 mm, it was 200 MPa. The increase in compressive residual stress is almost the same as the initial stress. However, if initial stress was tensile, there was no significant change in the maximum compression residual stress.

The Effect of Welding Condition on Tensile Properties of Friction Stir Welds of KS5J32 Al Alloy (KS5J32 Al합금 마찰교반접합부의 인장성질에 미치는 접합조건의 영향)

  • Yoon, Tae-Jin;Kim, Sang-Ju;Kim, Nam-Kyu;Song, Sang-Woo;Kang, Chung-Yun
    • Journal of Welding and Joining
    • /
    • v.29 no.5
    • /
    • pp.82-89
    • /
    • 2011
  • The effect of welding condition on tensile properties of KS5J32 Al Alloy was investigated under various welding conditions. The 1.6 mm thick KS5J32 alloy sheets were joined by friction stir welding (FSW) technique with butt joint. The tool rotation speeds were 1000, 1250 and 1500 rpm, and the welding speeds were varied within the range from 100 to 600 mm/min. Voids mainly occurred at the advancing side of the tool probe, when the tool rotation speed was low, due to insufficient materials flow. When the weld pitch exceeded 0.4 mm/rev, voids were observed under all welding conditions and the area of voids increased with increasing weld pitch. For void-free specimens, fracture always occurred at base materials. However voids affected the location of fractures, base metal or welded zone, when the voids existed within the welds.

The Optimization of Laser Welding Process for Electrical Steel Coil Joining Using the Taguchi Method (다구찌 방법을 이용하는 전기강판 코일 연결용 레이저 용접 공정의 최적화)

  • Shin, Joong-Han;Kim, Do-Hee
    • Journal of the Korean Society of Manufacturing Process Engineers
    • /
    • v.21 no.9
    • /
    • pp.63-70
    • /
    • 2022
  • Laser welding has attracted great attention as a tool used to join electrical steel coils. In this study, laser butt welding for electrical steel coil joining was conducted using the Taguchi method. It was found that structural defects such as void sand cracks were not produced in welds. This indicated that the performance of laser welding in electrical steel was excellent. According to the Taguchi analysis, the total welding quality index (TWQI) considering the bead height and roughness and tensile strength of the weld joint was almost evenly affected by laser power, welding speed, and focal position. The optimum welding conditions to maximize the TWQI were a laser power of 1220W, welding speed of 90 mm/s, and a focal position of 1mm. The regress model predicting the TWQI was also developed using the surface response method. We found that the model predicts measured values with an average error of 16.36%.

FATIGUE DESIGN OF BUTT-WELDED TUBULAR JOINTS

  • Kim, D. S.;S. Nho;F. Kopp
    • Proceedings of the KWS Conference
    • /
    • 2002.10a
    • /
    • pp.127-132
    • /
    • 2002
  • Recent deepwater offshore structures in Gulf of Mexico utilize butt welded tubular joints. Application of welded tubular joint includes tendons, production risers, and steel catenary risers. Fatigue life assessment of these joints becomes more critical because the structures to which they are attached are allowed to undergo cyclic and sometimes large displacements around an anchored position. Estimating the fatigue behavior of these tubular members in the design stage is generally conducted by using S-N curves specified in the codes and standards. Applying the stress concentration factor of the welded structure to S-N approach often results in very conservative assessment because the stress field acting on the tubular has a non-uniform distribution through the thickness. Fracture mechanics and fitness for service (FFS) technology have been applied in the design of the catenary risers. This technology enables the engineer to establish proper requirements on weld quality and inspection acceptance criteria to assure satisfactory structural integrity during its design life. It also provides guidance on proper design curves to be used and a methodology for accounting for the effects of non-uniform stress distribution through the wall thickness. An attempt was made to develop set of S-N curves based on fracture mechanics approach by considering non-uniform stress distribution and a threshold stress intensity factor. Series of S-N curves generated from this approach were compared to the existing S-N curves. For flat plate butt joint, the S-N curve generated from fracture mechanics matches with the IIW class 100 curve when initial crack depth was 0.5 mm (0.02"). Similar comparison with API X′ was made for tubular joint.. These initial crack depths are larger than the limits of inspection by current Non-destructive examination (NDE) means, such as Automatic Ultrasonic Inspection (AUT). Thus a safe approach can be taken by specifying acceptance criteria that are close to limits of sizing capability of the selected NDE method. The comparison illustrates conservatism built into the S-N design curve.

  • PDF

Weld Quality Assessment Method for Short-Circuit Mode in GMAW

  • Kim, J.M.;Yoo, C.D.
    • International Journal of Korean Welding Society
    • /
    • v.1 no.2
    • /
    • pp.1-6
    • /
    • 2001
  • A weld quality assessment method is proposed in this work, which can be applied to the short-circuit mode in GMAW. Information about the welding signal trajectory, distribution of the signal duration at each sub-regions and short-circuit frequency is used to evaluate the weld quality. The weighted penalty, which is determined experimentally, is imposed for each abnormal signal. Performance of the proposed method is compared with the Simpson's method under the conditions of shielding gas reduction, workpiece surface contamination and joint gap in the butt and fillet welds. Although the proposed method predicts the weld quality with reasonable accuracy, further modification and extension to other metal transfer modes are needed as a further study.

  • PDF

A Study on Bead Height Control of GMAW by Short Circuit Time Ratio (단락시간비를 이용한 GMAW의 비드 높이 제어에 관한 연구)

  • 감병오;조상명;김상봉
    • Journal of Ocean Engineering and Technology
    • /
    • v.16 no.2
    • /
    • pp.53-59
    • /
    • 2002
  • This paper shows the experimental results controlling the height of surface and back bead in GMAW by analyzing the unexpected gaps between base metals produced in welding and by controlling welding velocity due to the variation of the gap between base metals in thin-plate welding. The back bead behavior and burn-through in I-type butt joint $CO_2$ welding of thin mild steel are analyzed in the views of short circuit time ratio and short circuit frequency. It is shown through experimental consideration that the short circuit time ratio method is more reasonable than the short circuit frequency method in analyzing the formulation of back bead under changing the gap between base metals. Based on the these results, welding manipulator is designed so as to satisfy the bead height control in real time by measuring the short circuit time ratio. To show the effectiveness of the developed bead formulation control system, the experiment is implemented under two welding conditions such as increasing gap from 0mm to 0.8mm and gradually increasing gap from 0mm to 1.2mm. The experimental results show that the bead formulation can be controlled uniformly in spite of the variation of the gap between base metals.

Laser Weldability of Sheet steels for Tailored Blank Manufacturing(1) (테일러드 블랭크용 박판 강재의 레이저 용접성 (1))

  • 김기철
    • Journal of Welding and Joining
    • /
    • v.16 no.1
    • /
    • pp.77-87
    • /
    • 1998
  • This paper deals with the effect of laser welding parameters on the weld formation. Thin steels for automotive application were prepared so as to be welded with high power carbon dioxide laser system. Major process parameters were position of focus and travel speed. The effect of shielding gas was also discussed by employing the high speed photometry. Test results showed that the optimal position of focus varied in accordance with the joint configuration; bead-on-plate, butt or lap welding. It was recommended that the position of focus for the lap welding be located at slightly inner part of the material to be welded. In this case, however, it was noticeable that the weld penetration ratio, d/t$_{0}$ dropped drastically at the critical region. Results also demonstrated that both the bead width and penetration reduced as the travel speed increased. The penetration ratio showed two distinct regions; stabilized zone at the lower range of the travel spped and sudden drop zone at the higher range of travel speed. Lower limit of the penetration for acceptable weld was proved to be about 90% of the parent metal thickness based on the physical properties of the weld. Mixed gas application for both the shielding of molten metal and laser induced plasma control was recommended as far as the penetration was concerned.d.

  • PDF

THE JOINT CHARACTERISTICS OF FRICTION STIR WELDED AZ91D MAGNESIUM ALLOYS

  • Kim, Jong-Woong;Lee, Won-Bae;Yeon, Yun-Mo;Jung, Seung-Boo
    • Proceedings of the KWS Conference
    • /
    • 2002.10a
    • /
    • pp.516-521
    • /
    • 2002
  • A study was carried out to grow an understanding of the microstructural development of friction stir welds on an AZ91D magnesium alloy, and to evaluate the mechanical properties of the welds. AZ91D plates with the thickness of 4mm were used, and the microstructural development of the weld zone was investigated using optical and scanning electron microscopes. Square butt welding joint with good quality was obtained at the conditions of under 187mm/min of travel speed with 1100 to 1250 rpm of tool rotation speed. The microstructure within the weld region consisted of fine equiaxed grains with no evidence of the original dendritic structure. The hardness tests showed slightly increased harness in the weld region, and the minimum hardness measured is in that of the parent material. Tensile strength of the weld zone was remarkably improved due to very fine recrystallized structure. XRD pattern of weld zone revealed the removal of $\beta$ intermetallic compounds, $Mg_{17}$Al$_{12}$, which had been distributed in the base metal.l.

  • PDF