• 제목/요약/키워드: Bonding condition

검색결과 437건 처리시간 0.026초

Al 분말의 산화에 의한 $Al_2O_3$ 소결에 관한 연구 (A Study on alumina Sintering through the Oxidation of AI Powder.)

  • 박정현;안주삼;김해두
    • 한국세라믹학회지
    • /
    • 제19권3호
    • /
    • pp.179-186
    • /
    • 1982
  • This research is to aim at the study of sintering mechanism through the observation of microstructure by scanning electron microscopy, after the mixture of 30wt% $Al_2O_3$ (White Alundum) powder is fired in air at the temperature range of 1350~150$0^{\circ}C$ in order to sinter $Al_2O_3$-Al through the oxidation of Al powder. The results obtained in this experiment are as follows: 1. While the compressive strength of $Al_2O_3$(WA) body fired at $1450^{\circ}C$ for 5hrs in air is 150kg/$\textrm{cm}^2$, that of Al-$Al_2O_3$ body fired at 135$0^{\circ}C$, $1400^{\circ}C$ for 5hrs in air is 1100kg/$\textrm{cm}^2$, 1600kg/$\textrm{cm}^2$ respectively, and the higher the firing temperature, the more the compressive strength increases. These results from the sintering effect between $Al_2O_3$(WA) grains and surrounding Al-oxidation layer. 2. While the compressive strength of Al2O3(WA) body fired at 150$0^{\circ}C$ for 5hrs in air is 250kg/$\textrm{cm}^2$, the compressive strength of Al-$Al_2O_3$body fired under the same condition is 2050kg/$\textrm{cm}^2$ and water absorption 9.0%, porosity 23.3%, bulk density 2.60gr/$cm^3$. It is assumed that these results come from not only the grain growth of oxidized Al grains but also the increase of bonding strength between $Al_2O_3$(WA) grains.

  • PDF

외부부착 보강된 교량 바닥판 균열폭의 반경험적인 예측 (Semi-Empirical Prediction of Crack Width of the Strengthened Bridge Deck with External Bonding Plastic)

  • 심종성;오홍섭
    • 콘크리트학회논문집
    • /
    • 제14권2호
    • /
    • pp.231-238
    • /
    • 2002
  • 콘크리트 교량 바닥판은 건조수축 및 온도변화 등에 의하여 초기 1차균열이 발생하고, 사용기간 동안 반복되는 차량하중의 크기와 철근 간격 등에 의하여 초기 균열이 이방향 균열로 점차 발전하게 된다. 그러나 현재 사용되고 있는 대부분의 균열 예측식이 일방향 부착-슬립이론에 기초하고 있기 때문에 철근과 보강재의 간격에 따라 변화되는 교량 바닥판의 균열폭을 예측하고 보강된 바닥판의 사용성을 평가하기에는 많은 어려움이 있다. 따라서 본 연구에서는 시험결과에 기초하여 성능향상된 바닥판의 균열 메카니즘을 구명하였으며, 이로부터 사용성을 평가할 수 있는 새로운 균열예측식을 제안하였다. 제안된 균열예측식은 기존 균열식에 비하여 예측결과가 우수한 것으로 나타났으나, 철근 항복 이후 철근과 보강재의 변형률이 급격히 증가할 때 오차범위가 커지는 것으로 나타나 추가적인 연구가 필요한 것으로 판단된다. 따라서 보다나은 균열예측을 위해서는 피로 하중하에서의 철근 항복이후에 대한 추가적인 연구가 필요한 것으로 판단된다.

PCB 기판을 이용한 RF용 SAW 필터 개발 (Development of the RF SAW filters based on PCB substrate)

  • 이영진;임종인
    • 대한전자공학회논문지SD
    • /
    • 제43권11호
    • /
    • pp.8-13
    • /
    • 2006
  • 최근 RF용 탄성표면파 필터는 HTCC 패키지를 이용한 칩스케일 패키지 공법으로 제작되고 있다. 본 연구에서는 HTCC 패키지를 이용하는 대신에 BT 레진 계열의 PCB 기판을 이용하여 $1.4{\times}1.1$$2.0{\times}1.4mm$ 규격을 가지는 새로운 SAW RF 필터를 개발하였다. 본 기술을 적용하여 기존대비 약 40% 이상의 재료비 절감효과를 얻을 수 있다. 다층 PCB 기판과 $LiTaO_3$ 탄성표면파 기간간의 플립 본딩 조건을 최적화하였고, 적절한 PCB 재료선정을 통하여 PCB 기판 및 에폭시 라미네이팅 필름간의 열팽창계수 차이로 인해 발생하는 응력을 최소화시켰다. 이렇게 개발된 탄성표면파 필터는 기존의 제품에 비해 신뢰성 및 전기적 특성면에서 향상된 특성을 보였다.

누설 레일리 표면파를 이용한 TiN 코팅 부재의 특성평가 (Characterization of TiN Layered Substrate using Leaky Rayleigh Surface Wave)

  • 권성덕;김학준;송성진
    • 비파괴검사학회지
    • /
    • 제26권1호
    • /
    • pp.7-11
    • /
    • 2006
  • 기계부품의 세라믹 코팅 층은 사용 중 그 표면특성이 변하므로 잔류수명 예측과 신뢰성 확보를 위해 비파괴적으로 세라믹 코팅 층의 특성을 평가하는 것은 매우 중요하다. 이를 위해 본 인구는 AISI 1045 강과 오스테나이트 스테인리스 304 강 모재위에 매우 얇은 TiN 세라믹 층을 코팅한 시편에 내하여 누설 레일리(Rayleigh) 표면파를 이용한 TiN 코팅부재의 특성평가를 시도하였다. 후방복사 측정기법으로 코팅 층 내의 표면파의 전파특성이 평가되었고 표면 거칠기, 코팅 층 두께, 마모조긴 둥이 다양한 시편들에 대해 후방복사 프로파일이 측정되었다. 후방복사 프로파일의 정점각과 크기는 시편의 조건들에 따라 민감하게 변하였고, 정점각의 증가는 코팅 층 접합 강도의 저하로 설명되었다. 결과들은 후방복사 기법을 이용한 표면파의 분산성 평가가 코팅 층의 특성 평가에 매우 유용함을 보여주었다.

형상기억복합재료에 대한 온라인 모니터링 시스템 개발 (Development of On-line Monitoring System for Shape Memory Alloy Composite)

  • 이진경;박영철;이민래;이동화;이규창
    • 비파괴검사학회지
    • /
    • 제23권1호
    • /
    • pp.7-13
    • /
    • 2003
  • 형상기억복합재료를 제조하기 위하여 핫프레스 방법을 이용하여 최적의 제조조건을 도출하였으며 냉간압연에 의해 기지재와 강화재의 계면접합을 강화하여 강도를 증가시켰다. 이러한 방법에 의해 제조된 형상기억복합재료에 대하여 외부 하중에 의한 손상정도와 균열의 발생을 감지하여 균열 발생 및 진전을 억제하는 온라인 모니터링 시스템을 개발하고자 한다. 이를 위하여 음향방출 신호의 파라미터를 이용하여 손상에 따른 최적의 AE 파라미터를 도출하였으며 가역시스템을 이용하여 형상기억합금을 가열함으로써 형상기억합금의 수축에 의한 복합재료 내부에 균열진전을 억제시키는 시스템을 개발하였다

트리클로로에틸렌의 유통·사용 실태조사 결과 (A Survey on the status of using trichloroethylene(TCE) in Korea)

  • 조형열;조성현;유장진;김병규;박승현;강성규
    • 한국산업보건학회지
    • /
    • 제17권3호
    • /
    • pp.254-260
    • /
    • 2007
  • Trichloroethylene(TCE) is widely used as a degreasing solvent in workplaces. TCE is primarily toxic to the nervous system, however, systemic disorder like Stevens-Johnson syndrome has been recently reported in small-scale factories, where the government has had limited information of chemical use. A survey was performed to investigate the actual condition of using TCE and to provide practical information to occupational health service agencies and professionals. This survey was carried out on 103 factories out of 430 factories which were conducted periodic work environment measurement for TCE. Degreasing was the most popular reason for using TCE in Korea, which reached to 94%. TCE was also used as a solvent for rubber in the coating or molding process, and adhesives in the bonding process. Metal fabrication was the most common as 23%, followed by assembling automobile parts (17%), and machinery (12%). Workers exposed to TCE during full-shift were 52% while 48% were exposed during short period of the shift or intermittently. Manual or semi-automatic work occupied 87% while automatic work was just 13%. Though automatic work by a closed system was generally lower exposed to TCE, compared to manual work, it can cause a high exposure when the maintenance system is improper. Semi-automatic work especially like open-top degreasing process can cause a high exposure when local exhaust system with condensing and refrigerating coils in the degreaser does not work well. In conclusion, the survey showed nationwide status of TCE exposure in various aspects. It can be used to monitor workplaces and workers exposed to TCE to prevent occupational diseases.

Sr-Ferrite와 GC를 이용한 자기연마재 개발 (Development of the Magnetic Abrasive Using Sr-Ferrite and GC)

  • 윤여권;김상백;김희남
    • 한국안전학회지
    • /
    • 제26권2호
    • /
    • pp.13-19
    • /
    • 2011
  • The magnetic polishing is the useful method to finish using magnetic power of magnet. That method is one of precision polishing techniques and has an aim of the clean technology using for the pure of gas and inside of the clean pipe. The magnetic abrasive polishing method is not so common for machine that it is not spreaded widely. There are rarely researcher in this field because of non-effectiveness of magnetic abrasive. Therefore, in this paper deals with development of the magnetic abrasive using Sr-Ferrite. In this development, abrasive grain GC used to resin bond fabricated low temperature. And Sr-Ferrite of magnetic abrasive powder fabricated that Sr-Ferrite was crused into 200 mesh. The XRD analysis result show that only GC abrasive and Sr-Ferrite crystal peaks detected which explains resin bond was not any more chemical reaction. From SEM analysis it is found that GC abrasive and Sr-Ferrite were strong bonding with each other by bond. The magnetic polishing is performed by polishing the surface of pipe by attracting magnetic abrasives with magnetic fields. This can be widely applied for finishing machinery fabrications such as various pipes and for other safety processes. In this paper, we could have investigated in to the changes of the movement of magnetic abrasive grain. In reference to this result, we could have made the experiment which is set under the condition of the magnetic flux density, polishing velocity according to the form of magnetic brush.

상악매복견치의 진단 및 처치 (DIAGNOSIS AND TREATMENT PLAN OF MAXILLARY IMPACTED CANINE)

  • 경승현;황충주
    • 대한치과교정학회지
    • /
    • 제23권2호
    • /
    • pp.165-177
    • /
    • 1993
  • Upper canine is important because it protects and maintains the stability of the dental arch and also, joins the anterior with the posterior teeth. The incidence of impaction of upper canine is the second most frequent next to the third molar because it takes a long period of time to develop, and has a complicated path of eruption, and erupts lately. After the age of 10, clinical and radioglaphic examination can be used in revealing the possibility of impaction and efforts should be put to reduce the side effects. To prevent impaction, selective extraction of primary canine at the age of 8 to 9 could be considered and prolonged retention of primary canine in oral cavity should be avoided at this time. Once the impaction is iden, the first stage of the treatment is to lcocalize the lesion by radiographic examination and According to the severity, orthodontic traction or autotransplantation should be considered and comprehensive diagnosis and treatment plan of malocclusion should be established. Generally, labial impaction is due to arch length discrepancy and palatal impaction is due to malposition or morphologic pathosis of lateral incisors rather than arch length discrepancy. In surgical procedure, peridontal problems should be considered and the minimum amount of bone and soft tissue should be reduced and direct bonding method of many attachment methods should be recommended. Especially in traction of labially impacted canine, it should be guided to erupt through the keratinized zone and proper forced magnitude should be applied. The importance of periodontal condition should always be in mind following the patient education to mintain the good oral hygiene at each stage of treatment. Properly managed impacted canine can provide function and esthetic by proper diagnosis and treatment if extraction of canine is not indicated.

  • PDF

고기능성 복합재료의 제조와 그 특성평가에 관한 연구 (A Study on the Preocessing of high Runctional Composites and the Evaluation of Its Characteristics)

  • 김윤해
    • Journal of Advanced Marine Engineering and Technology
    • /
    • 제22권2호
    • /
    • pp.139-145
    • /
    • 1998
  • Filament winding method is widely used for composite fabrications using low viscosity liquid for-mation and processing asymmetrical structures of pressure vessel pipe rocket motor case etc. The filament winding method is affected by several parameters such as pot life of process time viscosi-ty of resin filament winding temperature and schedules curing condition and post curing condi-tion of resin. To develope high functional composite materials the rotation(5, 15, 20, 30rpm) of the winding machine was controlled by D.C motor. And the wiper to give proper tension was equipped between strand and resin bath. The resin is hooked by the design wiper. The adequate cure schedule was found by DSC. NOL ring test is carried out to investigate the basic physical properties such as design technology. The void contents in filament winding is generally higher than that of the prepreg laminated plate. These high contents of void can make a crack in resin in spite of low deformation. These problem was solved by giving tension in processing. To improve the characteristics of fiber volume fraction void contents resin/fiber bonding the winding speedc is changed under constant tension. It was found that resin impregnation was not different from in fiber contents void contents at the range of 0.5~1kg tension but it was found that resin was not impregnated at the above of 1.5kg tension. In burst test a pure PE liner was failed at a nozzle part under the $14kg/\textrm{cm}^2$ pressure but a pressure vessel of CNG was failed at a cylinder part under the $200kg/\textrm{cm}^2$ pressure.

  • PDF

Effect of chlorhexidine application on the bond strength of resin core to axial dentin in endodontic cavity

  • Kim, Yun-Hee;Shin, Dong-Hoon
    • Restorative Dentistry and Endodontics
    • /
    • 제37권4호
    • /
    • pp.207-214
    • /
    • 2012
  • Objectives: This study evaluated the influence of chlorhexidine (CHX) on the microtensile bonds strength (${\mu}TBS$) of resin core with two adhesive systems to dentin in endodontic cavities. Materials and Methods: Flat dentinal surfaces in 40 molar endodontic cavities were treated with self-etch adhesive system, Contax (DMG) and total-etch adhesive system, Adper Single Bond 2 (3M ESPE) after the following surface treatments: (1) Priming only (Contax), (2) CHX for 15 sec + rinsing + priming (Contax), (3) Etching with priming (Adper Single Bond 2), (4) Etching + CHX for 15 sec + rinsing + priming (Adper Single Bond 2). Resin composite build-ups were made with LuxaCore (DMG) using a bulk method and polymerized for 40 sec. For each condition, half of specimens were submitted to ${\mu}TBS$ after 24 hr storage and half of them were submitted to thermocycling of 10,000 cycles between $5^{\circ}C$ and $55^{\circ}C$ before testing. The data were analyzed using ANOVA and independent t-test at a significance level of 95%. Results: CHX pre-treatment did not affect the bond strength of specimens tested at the immediate testing period, regardless of dentin surface treatments. However, after 10,000 thermocycling, all groups showed reduced bond strength. The amount of reduction was greater in groups without CHX treatments than groups with CHX treatment. These characteristics were the same in both self-etch adhesive system and total-etch adhesive system. Conclusions: 2% CHX application for 15 sec proved to alleviate the decrease of bond strength of dentin bonding systems. No significant difference was shown in ${\mu}TBS$ between total-etching system and self-etching system.