P-type and N-type $Bi_2Te_3/PbTe$ Functional Gradient Materials for Thermoelectric Power Generation

  • Lee, Kwang-Yong;Oh, Tae-Sung
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part2
    • /
    • pp.1223-1224
    • /
    • 2006
  • The p-type $(Bi_{0.2}Sb_{0.8})_2Te_3/(Pb_{0.7}Sn_{0.3})$Te functional gradient material (FGM) was fabricated by hot-pressing the mechanically alloyed $(Bi_{0.2}Sb_{0.8})_2Te_3$ and the 0.5 at% $Na_2Te-doped$ $(Pb_{0.7}Sn_{0.3})Te$ powders. Also, the n-type $Bi_2(Te_{0.9}Se_{0.1})_3/PbTe$ FGM was processed by hot-pressing the mechanically alloyed $Bi_2(Te_{0.9}Se_{0.1})_3$ and the 0.3 wt% Bi-doped PbTe powders. With ${\Delta}T$ larger than $300^{\circ}C$, the p-type $(Bi_{0.2}Sb_{0.8})_2Te_3/(Pb_{0.7}Sn_{0.3})Te$ FGM exhibited larger thermoelectric output power than those of the $(Bi_{0.2}Sb_{0.8})_2Te_3$ and the 0.5 at% $Na_2Te-doped$ $(Pb_{0.7}Sn_{0.3})Te$ alloys. For the n-type $Bi_2(Te_{0.9}Se_{0.1})_3/PbTe$ FGM, the thermoelectric output power superior to those of the $Bi_2(Te_{0.9}Se_{0.1})_3$ and the 0.3 wt% Bi-doped PbTe was predicted at ${\Delta}T$ larger than $300^{\circ}C$.

  • PDF

산화물 환원공정에 의해 제조된 Bi2Te2.7Se0.3 분말의 열전특성 (Thermoelectric Properties of Bi2Te2.7Se0.3 Powder Synthesized by an Oxide-Reduction Process)

  • 박배건;이길근;김우열;하국현
    • 한국분말재료학회지
    • /
    • 제18권5호
    • /
    • pp.437-442
    • /
    • 2011
  • The present study focused on the synthesis of Bi-Te-Se-based powder by an oxide-reduction process, and analysis of the thermoelectric properties of the synthesized powder. The phase structure, chemical composition, and morphology of the synthesized powder were analyzed by XRD, EPMA and SEM. The synthesized powder was sintered by spark plasma sintering. The thermoelectric properties of the sintered body were evaluated by measuring its Seebeck coefficient, electrical resistivity, and thermal conductivity. $Bi_2Te_{2.7}Se_{0.3}$ powder was synthesized from a mixture of $Bi_2O_3$, $TeO_2$, and $SeO_2$ powders by mechanical milling, calcination, and reduction. The sintered body of the synthesized powder exhibited n-type thermoelectric characteristics. The thermoelectric properties of the sintered bodies depend on the reduction temperature. The Seebeck coefficient and electrical resistivity of the sintered body were increased with increasing reduction temperature. The sintered body of the $Bi_2Te_{2.7}Se_{0.3}$ powder synthesized at $360^{\circ}C$ showed about 0.5 of the figure of merit (ZT) at room temperature.

방전플라즈마 소결된 Bi0.5Sb1.5Te3의 열/전기적 특성 (The Electric and Thermal Properties of Spark Plasma Sintered Bi0.5Sb1.5Te3)

  • 이길근;최영훈;하국현
    • 한국분말재료학회지
    • /
    • 제19권4호
    • /
    • pp.285-290
    • /
    • 2012
  • The present study was focused on the analysis of the electric and thermal properties of spark plasma sintered $Bi_{0.5}Sb_{1.5}Te_3$ thermoelectric material. The crystal structure, microstructure, electric and thermal properties of the sintered body were evaluated by measuring XRD, SEM, electric resistivity, Hall effect and thermal conductivity. The $Bi_{0.5}Sb_{1.5}Te_3$ sintered body showed anisotropic crystal structure. The c-axis of the $Bi_{0.5}Sb_{1.5}Te_3$ crystal aligned in a parallel direction with applied pressure during spark plasma sintering. The degree of the crystal alignment increased with increasing sintering temperature and sintering time. The electric resistivity and thermal conductivity of the $Bi_{0.5}Sb_{1.5}Te_3$ sintered body showed anisotropic characteristics result from crystal alignment.

Optimization of Spark Plasma Sintering Temperature Conditions for Enhancement of Thermoelectric Performance in Gas-Atomized Bi0.5Sb1.5Te3 Compound

  • Jeong, Kwang-yong;Lee, Chul Hee;Dharmaiah, Peyala;Hong, Soon-Jik
    • 한국분말재료학회지
    • /
    • 제24권2호
    • /
    • pp.108-114
    • /
    • 2017
  • We fabricate fine (<$20{\mu}m$) powders of $Bi_{0.5}Sb_{1.5}Te_3$ alloys using a large-scale production method and subsequently consolidate them at temperatures of 573, 623, and 673 K using a spark plasma sintering process. The microstructure, mechanical properties, and thermoelectric properties are investigated for each sintering temperature. The microstructural features of both the powders and bulks are characterized by scanning electron microscopy, and the crystal structures are analyzed by X-ray diffraction analysis. The grain size increases with increasing sintering temperature from 573 to 673 K. In addition, the mechanical properties increase significantly with decreasing sintering temperature owing to an increase in grain boundaries. The results indicate that the electrical conductivity and Seebeck coefficient ($217{\mu}V/K$) of the sample sintered at 673 K increase simultaneously owing to decreased carrier concentration and increased mobility. As a result, a high ZT value of 0.92 at 300 K is achieved. According to the results, a sintering temperature of 673 K is preferable for consolidation of fine (<$20{\mu}m$) powders.

기계적 밀링공정에 의해 제조된 Bi0.4Sb1.6Te3 소결체의 열전특성 (Thermoelectric Properties of Bi0.4Sb1.6Te3 Sintered Body Fabricated by Mechanical Grinding Process)

  • 이길근;신승철;김우열;하국현
    • 한국분말재료학회지
    • /
    • 제13권5호
    • /
    • pp.313-320
    • /
    • 2006
  • The present study is to analyze the thermoelectric properties of $Bi_{0.4}Sb_{1.6}Te_3$ thermoelectric materials fabricated by the mechanical grinding process. The $Bi_{0.4}Sb_{1.6}Te_3$ powders were prepared by the combination of mechanical milling and reduction treating methods using simply crushed pre-alloyed $Bi_{0.4}Sb_{1.6}Te_3$ powder. The mechanical milling was carried out using the tumbler-ball mill and planetary ball mill. The tumbler-ball milling had an effect on the carrier mobility rather than the carrier concentration, whereas, the latter on the carrier concentration. The specific electric resistivity and Seebeck coefficient decreased with increasing the reduction-heat-treatment time. The thermal conductivity continuously increased with increasing the reduction-heat-treatment time. The figure of merit of the $Bi_{0.4}Sb_{1.6}Te_3$ sintered body prepared by the mechanical grinding process showed higher value than one of the sintered body of the simply crushed powder.

Bi-Te계 n형 열전분말의 열전특성에 미치는 Cu 도핑의 영향 (Thermoelectric Properties in the Cu Doping Effects of the n-type Bi-Te Powders)

  • 박민수;구혜영;하국현;박용호
    • 한국분말재료학회지
    • /
    • 제22권4호
    • /
    • pp.254-259
    • /
    • 2015
  • $Bi_2Te_3$ related compounds show the best thermoelectric properties at room temperature. However, n-type $Bi_2Te_{2.7}Se_{0.3}$ showed no improvement on ZT values. To improve the thermolectric propterties of n-type $Bi_2Te_{2.7}Se_{0.3}$, this research has Cu-doped n-type powder. This study focused on effects of Cu-doping method on the thermoelectric properties of n-type materials, and evaluated the comparison between the Cu chemical and mechanical doping. The synthesized powder was manufactured by the spark plasma sintering(SPS). The thermoelectric properties of the sintered body were evaluated by measuring their Seebeck coefficient, electrical resistivity, thermal conductivity, and hall coefficient. An introduction of a small amount of Cu reduced the thermal conductivity and improved the electrical properties with Seebeck coefficient. The authors provided the optimal concentration of $Cu_{0.1}Bi_{1.99}Se_{0.3}Te_{2.7}$. A figure of merit (ZT) value of 1.22 was obtained for $Cu_{0.1}Bi_{1.9}Se_{0.3}Te_{2.7}$ at 373K by Cu chemical doping, which was obviously higher than those of $Cu_{0.1}Bi_{1.9}Se_{0.3}Te_{2.7}$ at 373K by Cu mechanical doping (ZT=0.56) and Cu-free $Bi_2Se_{0.3}Te_{2.7}$ (ZT=0.51).

INFLUENCE OF SPARK PLASMA SINTERING TEMPERATURE ON MICROSTRUCTURE AND TTHERMOELECTRIC PROPERTIES OF Cu-DOPED Bi0.5Sb1.495Te3 COMPOUND

  • CHUL-HEE LEE;PEYALA DHARMAIAH;JUN-WOO SONG;KWANG-YONG JEONG;SOON-JIK HONG
    • Archives of Metallurgy and Materials
    • /
    • 제65권3호
    • /
    • pp.1105-1110
    • /
    • 2020
  • Due to air pollution, global warming and energy shortage demands new clean energy conversion technologies. The conversion of industrial waste heat into useful electricity using thermoelectric (TE) technology is a promising method in recent decades. Still, its applications are limited by the low efficiency of TE materials in the operating range between 400-600 K. In this work, we have fabricated Cu0.005Bi0.5Sb1.495Te3 powder using a single step gas atomization process followed by spark plasma sintering at different temperatures (623, 673, 723, and 773 K), and their thermoelectric properties were investigated. The variation of sintering temperature showed a significant impact on the grain size. The Seebeck coefficient values at room temperature increased significantly from 127 µVK to 151 µV/K with increasing sintering temperature from 623 K to 723 K due to decreased carrier concentration. The maximum Z T values for the four samples were similar in the range between 1.15 to 1.18 at 450 K, which suggest these materials could be used for power generation in the mid-temperature range (400-600 K).

Reduction of Thermal Conductivity Through Complex Microstructure by Dispersion of Carbon Nanofiber in p-Type Bi0.5Sb1.5Te3 Alloys

  • P. Sharief;B. Madavali;Y. Sohn;J.H. Han;G. Song;S.H. Song;S.J. Hong
    • Archives of Metallurgy and Materials
    • /
    • 제66권3호
    • /
    • pp.803-808
    • /
    • 2021
  • The influence of nano dispersion on the thermoelectric properties of Bi2Te3 was actively investigating to wide-spread thermoelectric applications. Herein this report, we have systematically controlled the microstructure of Bi0.5Sb1.5Te3 (BST) alloys through the incorporation of carbon nanofiber (CNF), and studied their effect on thermoelectric properties, and mechanical properties. The BST/x-CNF (x-0, 0.05, 0.1, 0.2 wt.%) composites powder was fabricated using high energy ball milling, and subsequently consolidated the powder using spark plasma sintering. The identification of CNF in bulk composites was analyzed in Raman spectroscopy and corresponding CNF peaks were recognized. The BST matrix grain size was greatly reduced with CNF dispersion and consistently decreased along CNF percentage. The electrical conductivity was reduced and Seebeck coefficient varied in small-scale by embedding CNF. The thermal conductivity was progressively diminished, obtained lattice thermal conductivity was lowest compared to bare sample due to induced phonon scattering at interfaces of secondary phases as well as highly dense fine grain boundaries. The peak ZT of 0.95 achieved for 0.1 wt.% dispersed BST/CNF composites. The Vickers hardness value of 101.8 Hv was obtained for the BST/CNF composites.