In existing ceramic mold manufacturing processes, inorganic binder systems (Si-Na, two-component system) are applied to ensure the effective firing strength of the ceramic mold and core. These inorganic binder systems makes it possible to manufacture a ceramic mold and core with high dimensional stability and effective strength. However, as in general sand casting processes, when molten metal is injected at room temperature, there is a limit to the production of thin or complex castings due to reduced fluidity caused by the rapid cooling of the molten metal. In addition, because sodium silicate generated through the vitrification reaction of the inorganic binder is converted into a liquid phase at a temperature of 1,000 ℃. or higher, it is somewhat difficult to manufacture parts through high-temperature casting. Therefore, in this study, a high-strength ceramic mold and core test piece with effective strength at high temperature was produced by applying a Si-Na-Ti three-component inorganic binder. The starting particles were coated with binary and ternary inorganic binders and mixed with an organic binder to prepare a molded body, and then heat-treated at 1,000/1,350/1,500 ℃ to prepare a fired body. In the sample where the two-component inorganic binder was applied, the glass was liquefied at a temperature of 1,000 ℃ or higher, and the strength decreased. However, the firing strength of the ceramic mold sample containing the three-component inorganic binder was improved, and it was confirmed that it was possible to manufacture a ceramic mold and core via high temperature casting.
In aqueous tape casting of alumina slurry systems, the relationships between the suspension compositions and the defects of the dried tapes were discussed. The suspensions compositions were controlled with the ratios of the solids, water and organics binder contents. The effects of the thickness of dried tape and kinds of binder system were also examined. In the defect free region, the apparent viscosity showed nearly same value due to the count balancing effect of solid and organic binder content on the apparent viscosity. When water content was constant, increasing solid led to decrease of organic binder content. The defect free region was narrowed with increasing of casting thickness. When linear type acrylic emulsion binders system (D1000 and D 1035) were used, defect free zone formed the belt type in the triangle of solid, water and organic binder content according to the line of constant water contents. However the defect free region was not found in the cross-link type emulsion binder system (D 1050).
The effects of slip composition and processing conditions on the fabrication of ceramic heat exchanger cores by doctor blade process were investigated. Since the effects of those two variables were inter-dependent, the effects of binder system, binder plus plasticizer, were extensively studied for a limited range of processing conditions and a pre-determined ceramic composition. The content of binder system and the ratio of binder to plasticizer were identified as main variables to affect densities and mechanical properties of green sheets, compressive properties and bond strengths of laminates, and shrinkages and their anisotropy of sintered laminates. However, sintered densities and water absorptions of laminates were not influenced by either the content of binder system or the ratio of binder to plasticizer, when the debinded laminates had a relatively high density (relative density of >55% in this study).
The previous study reported that the quaternary copolymer of MMA, BA, MAA, and NEA was expected to be a good monomer composition for a binder polymer with good rubbing fastness for digital textile printing(DTP) pigment ink. However, the rubbing fastness of the dyed fabric with the quaternary copolymer binder containing pigment ink is not enough to be commercially used. Therefore, this study aims to optimize MMA:BA:MAA:NEA composition for improved rubbing fastness. And the binder polymer with various MMA:BA:MAA:NEA compositions were synthesized using miniemulsion polymerization. The particle size, viscosity, molecular weight, and Tg of the synthesized binder were evaluated. And the color strength and rubbing fastness of the black pigment ink dyed cotton fabrics with the prepared binders were also evaluated. Then, the stiffness of undyed and dyed cotton fabrics were evaluated to investigate the changes in touch as the binder structure changes.
A new binder system and debinding process for low carbon residue in the injection molding of Nd(Fe, Co)B powder are investigated. In the injection molding of magnetic materials, it is demanded to reduce carbon residue which deteriorates their magnetic properties. The binder system developed is composed of polyethylene glycols (PEGs) and polypropylene (PP). PEG was selected as a major binder is component to be extracted in a molecular state by solvent extraction in ethanol, which step would leave no residue. PP was selected as a minor binder component to be subsequently removed by thermolysis which step would leave carbon residue. The behaviors of solvent extraction with the variations of PEG molecular weight, temperature, and time were examined. The dependency of residual carbon content on thermolysis atmosphere was also studied. Opened pore channels introduced in a green body by the solvent extraction and microstructures of the sintered magnets were observed using SEM.
In the lamination process of multi-layer ceramic modules, the occurrence of delamination comes into repeatedly. To completely improve the lamination process of LTCC sheets, a binder film was introduced between the layers. The binder film did not originate the delamination until the thickness under $40{\mu}m$. After lamination, the thickness of the binder film was determined by the infilteraion of binder by the pressure, and after the bake-out, was dependent on the decomposition of binder resin. Any detectable defect was not observed in the multilayer structure with Ag inner electrodes.
The fabrication process of micro pattern structure with high precision and high aspect ratio using powder injection molding (PIM) is developed. In the PIM process, the metal powder is mixed with the binder systems and the mixture is injected into the metal mold. The injection molded green parts are debinded and sintered to reach final shape and properties. In this method, the optimization of physical properties such as fluidity and strength of the binder system is essential for perfect filling the high aspect ratio micro-pattern. For this purpose, the correlation between the properties of the binder system and feedstock and ${\mu}-PIM$ process was investigated, and a binder system with low viscosity at low temperature(about $110^{\circ}C$) and high strength after cooling was investigated and applied. Employing this process, high precision parts with line type micro pattern structure which has pattern size $160{\mu}m$ and aspect ratio more than 2 can be manufactured.
Song, Danoh;Lee, Seung Hyun;Kim, Kyuman;Ryou, Myung-Hyun;Park, Won Ho;Lee, Yong Min
Applied Chemistry for Engineering
/
v.26
no.6
/
pp.674-680
/
2015
A solvent-soluble polyimide (PI) polymeric binder was synthesized by a two-step reaction for silicon (Si) anodes for lithium-ion batteries. Polyamic acid was first prepared through ring opening between two monomers, bicyclo[2,2,2]oct-7-ene-2,3,5,6-tetracarboxylic dianhydride (BCDA) and 4,4-oxydianiline (ODA), followed by condensation reaction. Using the synthesized PI polymeric binder (molecular weight = ~10,945), the coating slurry was then prepared and Si anode was fabricated. For the control system, Si anode based on polyvinylidene fluoride (PVDF, molecular weight = ~350,000) having the same constituent ratio was prepared. During precycling, PI polymeric binder revealed much improved discharge capacity ($2,167mAh\;g^{-1}$) compared to that of using PVDF polymeric binder ($1,740mAh\;g^{-1}$), while the Coulombic efficiency of two systems were similar. PI polymeric binder improved the cycle retention ability during cycles compared to that of using PVDF, which is attributed to an improved adhesion property inside Si anode diminishing the dimensional stress during Si volume changes. The adhesion property of each polymeric binder in Si anode was confirmed by surface and interfacial cutting analysis system (SAICAS) (Si anode based on PI polymeric binder = $0.217kN\;m^{-1}$ and Si anode based on PVDF polymeric binder = $0.185kN\;m^{-1}$).
The binder polymers for digital textile printing(DTP) pigment inks were prepared using miniemulsion polymerization with various monomer compositions to study effects of monomer compositions on particle size distribution, average molecular weight, Tg, and color strength and rubbing fastness of the dyed fabrics with the prepared binder based pigment ink. The monomers used were MMA(Methyl methacrylate), BA(Butyl acrylate), MAA(Methacrylic acid), NMA(N-methylol acrylamide), NEA(N-ethylol acrylamide) and the ratios of the monomers were changed. The particle size was the smallest with 136nm when the MMA to BA weight ratio was 4:16 and the largest with 290nm when the MMA, BA, MAA, NEA ratio was 2.5:17:0.25:0.25. However, the glass transition temperature was lowest with $-41.90^{\circ}C$ and the color strength and rubbing fastness of the resulting sample were the best when the MMA, BA, MAA, NEA ratio was used. This suggested that the introduction of the NEA monomer to the binder polymer for the pigment ink could be an efficient way to enhance the rubbing fastness of the DTP pigment inks present.
To improve rubbing fastness of the printed fabrics, the binder polymers for Digital Textile Printing(DTP) pigment inks were synthesized with miniemulsion polymerization using various acrylic monomers, which are MMA(Methyl methacrylate), BA(Butyl acrylate), and Self-crosslinking monomers, such as NEA(N-Ethylol acrylamide) and MAA (Methacrylic acid). The acrylic monomer compositions were varied when synthesizing the binder polymers and their particle size distributions, average molecular weights, and Tgs were investigated. The prepared binder polymers were applied to prepare Cyan, Black, Yellow and Magenta pigment ink for DTP and the prepared inks were used to dye cotton fabrics. Then, color strength, and rubbing fastness were also investigated to study the effect of the comonomer compositions of the binder polymer on the color strength and rubbing fastness of the resulting pigment inks.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.