The formation of high $T_c$ phase is very sluggish and c parameter of unit cell of high $T_c$ phase is about $37{\AA}$. High $T_c$ oxide superconductor with a $T_c$ above 100 K has been successfully prepared by solid state reaction method in BiSrCaCuO system by Pb adding. The microstructure related to the formation of the high $T_c$ phase has been investigated. As compared with YBCO compound, the formation reaction of the high $T_c$ requires long time heat treatment. It is due to the transformation from the low $T_c$ phase to high $T_c$ phase. The sintering just below the melting point of the calcined powder mixture is effective on the formation of the high $T_c$ phase in Pb-added BiSrCaCuO system. The growth of the high $T_c$ superconducting phase has a thin plate shape, which is characterized by the c parameter of $37{\AA}$. The formation of the high $T_c$ phases is delayed by the excessive addition of Pb. The lattice parameter(c) of the unit cell (both the low and high $T_c$ phases) is increased with increase of Pb.
B $i_{1.84}$P $b_{0.34}$S $r_{1.91}$C $a_{2.03}$C $u_{3.06}$$O_{10+{delta}$의 출발조성비로 99.99%의 순도를 갖는 B $i_2$$O_3$, PbO, SrC $O_3$, CaC $O_3$, CuO 분말 시약을 사용하여 고상반응법으로 합성하였다. 이렇게 합성된 Bi계 110 K 단일상의 고온초전도 물질을 다시 분말 상태로 만든 후, AgO, A $u_2$$O_3$, MgO 금속산화물 분말을 각각 50 wt%의 비율로 혼합하였다. AgO, A $u_2$$O_3$, MgO의 금속분말이 혼합된 시편들을 820~85$0^{\circ}C$로 각각 최종 소결시킨 후, 각 시편들에 대하여 XRD, $T_{c}$, SEM, EDS 등의 실험을 진행하였다. 얻어진 시편들의 $T_{c}$는 순수한 Bi-2223 상보다 낮지만, AgO 금속분말을 50 wt% 혼합한 시편의 임계전이온도가 99.58 K로 A $u_2$$O_3$나 MgO를 50 wt% 혼합한 시편들보다 더 높게 나타났다. 또한, 표면 입자(grain)의 배열 상태는 AgO 금속분말을 50 wt% 혼합한 시편이 A $u_2$$O_3$나 MgO를 50 wt% 혼합한 시편들보다 더 치밀화 되는 경향을 나타내었다.내었다.나타내었다.내었다.
Seong Han Kim;Dong Hoon Lee;Jong Sik Park;Seung Koo Cho;Sung Han Lee;Keu Hong Kim
Bulletin of the Korean Chemical Society
/
제15권2호
/
pp.115-118
/
1994
Samples of ($Bi_{2-x}Sb_x)PbSr_2Ca_2Cu_3O_y$, compositions with x=0.0, 0.1, and 0.2 were prepared by solid-state reaction. The solubility of Sb into the 2223 phase is lower than 0.05 for the ratio of Sb/Bi. The lack of stability of the Sb-substituted $Bi_2O_2$ double layers is likely to cause the solubility low. There is no great dependence of lattice parameters on the Sb-content, and bonds around the square-pyramidal Cu atom are not affected by the $Sb^{3+}$ ion substituted. The superconducting transition temperature of this system is decreased gradually with increase of Sb, which is tentatively attributable to the perturbation of the Bi 6p-O 2p band and/or to the low volume fraction of the 2223 phase.
In the ($Bi_{1-x}Pb_{x}$)$_2$$Sr_2$$Ca_2$$Cu_{3.6}$$O_{y}$ (x=0∼0.5) superconductors, DTA and XRD-pattern analyses were performed to obviousely define optimal calcining and sintering temperature. And, understanding behaviors of High-Tc phase with preparation condition of superconductors, that is, calcining and sintering temperature, sintering time, and variation of Pb contents, in order to make single phase of superconductor, microstructure and its composition were analyzed with SEM, XRD, and EDAX. continuously, the cause of phase transition was define with synthetically studying mutural relation between measured electrical resistivity and current density. Also, in order to design enhancement of critical current density, Jc required for realization, samples varied with pressing condition were made, and measured its, Jc.
During Bi(Pb)-Sr-Ca-Cu-O superconductor wire fabrication the effect of the initial packing density on the final characteristics of superconductor wire was systematically studied. To increase the powder packing density with uniform distribution of superconducting core a billet insertion method processed by CIP was applied instead of the commonly used vibration and ramming method of powder insertion into silver sheath. Compared with the vibration and ramming method the billent insertion technique processed by CIP cause the 30% incre-specimen with 130${\mu}{\textrm}{m}$(core thickness : 45 ${\mu}{\textrm}{m}$)and 5.24 mm width processed at 84$0^{\circ}C$for 200hrs. shows specimen with 130${\mu}{\textrm}{m}$ (core thickness ; 45${\mu}{\textrm}{m}$)and 5.24 mm width processed at 84$0^{\circ}C$ for 200 hrs. shows maximum 34A for Ic and 16, 700 A/cm2 for Ic measured at 77K and 0T. Also the sample rolled 3 times shows maximum 7, 2A for Ic and 11, 000 A/cm2 for 77K and 0T. Based on X-ray experimental results the formation of Bi-2223 and texture were significantly well developed at the interface between the superconducting core and silver sheath as compared with those of the interior area of superconducting core.
Bi-2223 초전도체계에서 석출물을 flux-pinning center로 이용할 수 있는지 가능성을 타진하기 위하여 $Bi_{1.8}$P $b_{0.4}$S $r_{2}$C $a_{2.2}$C $u_3$$O_{8}$ 조성을 가진 Bi-2223/Ag 선재를 반응온도, 산소분압, 시간 등을 변화시키면서 열처리를 행하였다. 열처리 후 석출물들은 XRD, SEM, TEM, EDS로 분석하였다. Bi-2223 모상내의 (Ca, Sr)$_2$(Pb,Bi) $O_4$, B $i_{0.5}$ P $b_3$S $r_2$C $a_2$Cu $O_{12+}$$\delta$/ (3221)와 같은 2차상들의 크기와 분포는 2223 입자들의 연결성을 파괴하지 않고 열처리 조건에 의해서 조절할 수 있었다. 서냉 열처리가 된 시편은 임계전류밀도( $J_{c}$)값이 증가하였는데, 이는 2223 입자내 나노미터 크기로 형성된 석출물들이 flux-pinning sites로 작용한 것으로 추정된다.다.
The effect of La0.7Sr0.3MnO3 (LSMO) addition on the superconducting property of Bi1.6Pb0.4Sr2Ca2Cu3O10+δ ((Bi, Pb)-2223) polycrystalline samples was studied. LSMO (0.3 wt.% to 2.0 wt.%) added (Bi, Pb)-2223 samples were prepared by using a solid-state reaction method. The XRD analyses show that as the LSMO addition increases, the volume fraction of the Bi-2223 phase is gradually decreased. The critical temperature (Tc) exhibits a gradual decrease with a single transition as the LSMO amount increases up to 1.0 wt.%, but a further addition of LSMO induces an abrupt decrease of Tc with a dual transition. The analyses on the local structure of the CuO2 plane from the X-ray absorption fine structure (EXAFS) measurements showed that for the samples with low concentration of LSMO up to 1.0 wt.%, the Cu-O bond length and the CuO2 plane ordering do not degrade from the values of pure (Bi, Pb)-2223, while they get worsen with a further increase of LSMO addition. These results open up the possibility of LSMO as artificial pinning centers of the (Bi, Pb)-2223 system for power application.
We have performed the electrochemical method to fabricate high temperature superconducting (TlPbBi) -(SrBa)-Ca-Cu-O films. The precursors of the superconducting sample were codeposited at a periodic pulsed-potential cycle (1 second at -4V and 1 second at -1V) on a silver substrate. The variation of structure, microstructure and element were analysed by ICP and SEM techniques. The specimens were consisted predominantly of the Tl-1212 phase and have a transition temperature of 80~87 K in low magnetic field. It was showed that each grain has the stoichiometric ratio of $T1_{0.7}$Pb_$Bi_{0.3}$$_Sr{0.1}$$Ba_{2.4}$$Ca_{0.2}$$Cu_{1.2}$$2.5/O_{x}$ by EDX analysis.sis.
Polycrystalline Tl-1223 superconductors with a chemical composition of (Tl, Pb, Bi)TEX>$ (Sr, Ba)<_2$$Ca_2$$Cu_3$$O_{x}$ were synthesized by the solid state reaction method. The optimum chemical composition was $Tl_{0.8}$$Pb_{0.2}$$Bi_{0.2}$$Sr_{1.8}$$Ba_{0.2}$$Ca_{2.2}$$Cu_3$$O_{x}$ And the optimum sintering temperature and time were $905^{\circ}C$ and 7.5h, respectively. The sample was evaluated for their superconducting properties by magnetization measurement. The critical temperature $T_{c}$ is 120 K and the critical current density $J_{c}$ (T=5K, 0T) is estimated to be ∼ $10^{5}$ A/$\textrm{cm}^2$ for $Tl_{0.8}$$Pb_{0.2}$$Bi_{0.2}$$Sr_{1.8}$$Ba_{0.2}$$Ca_{2.2}$$Cu_3$$O_{x}$ .
We joined 19-multifilamentary (Bi, Pb)$_2$Sr$_2$Ca$_2$Cu$_3$O$_{x}$ Superconducting tapes and fabricated double-pancake coils by using resistive- and superconducting-joint methods. The joint resistance of the coils were characterized by the field decay technique and standard four-probe method. It was evaluated that joint resistance was 3.21$\times$10$^{-11}$$\Omega$ in the superconducting-joint coil, which is approximately 4 orders of magnitude smaller than that in the resistive-joint coil (107$\times$10$^{-9}$$\Omega$). The low value of joint resistance obtained by superconducting-joint is expected to be suitable for the practical applications in the persistent current mode.e.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.