SiC 소결에 미치는 Al2O3-RE2O3 첨가제의 영향과 SiCf/SiC 복합체의 제조 (Effects of Al2O3-RE2O3 Additive for the Sintering of SiC and the Fabrication of SiCf/SiC Composites)

  • 유현우;카티 라주;박지연;윤당혁
    • 한국세라믹학회지
    • /
    • 제50권6호
    • /
    • pp.364-371
    • /
    • 2013
  • The sintering behavior of monolithic SiC is examined using the binary sintering additive of $Al_2O_3$-rare earth oxide ($RE_2O_3$, where RE = Sc, Nd, Dy, Ho, or Yb). Through hot pressing at 20 MPa and $1750^{\circ}C$ for 1 h in an Ar atmosphere for 52 nm fine ${\beta}$-SiC powder added with 5 wt% sintering additive, a SiC density of > 97% is achieved, which indicates the effectiveness of $Al_2O_3-RE_2O_3$ system as a sintering of additive for SiC. Based on this result, 7 wt% of $Al_2O_3-Sc_2O_3$ is tested as an additive system for the fabrication of a continuous SiC fiber-reinforced SiC-matrix composite ($SiC_f$/SiC). Electrophoretic deposition combined with the application of ultrasonic pulses is used to efficiently infiltrate the matrix phase into the voids of $Tyranno^{TM}$-SA3 fabric. After hot pressing, a composite density of > 97% is obtained, along with a maximum flexural strength of 443 MPa.

LPS-SiC 세라믹스 제조특성에 미치는 소결온도의 영향 (Effects of Sintering Temperature on Fabrication Properties of LPS-SiC Ceramics)

  • 박이현;정헌채;김동현;윤한기
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2004년도 춘계학술대회
    • /
    • pp.204-209
    • /
    • 2004
  • SiC materials have been extensively studied for high temperature components in advanced energy system and advanced gas turbine. However, the brittle characteristics of SiC such as low fracture toughness and low strain-to fracture still impose a severe limitation on practical applications of SiC materials. For these reasons, $SiC_f/SiC$ composites can be considered as a promising for various structural materials, because of their good fracture toughness compared with monolithic SiC ceramics. But, high temperature and pressure lead to the degradation of the reinforcing fiber during the hot pressing. Therefore, reduction of sintering temperature and pressure is key requirements for the fabrication of $SiC_f/SiC$ composites by hot pressing method. In the present work, Monolithic LPS-SiC was fabricated by hot pressing method in Ar atmosphere at 1760 $^{\circ}C$, 1780 $^{\circ}C$, 1800 $^{\circ}C$ and 1820 $^{\circ}C$ under 20 MPa using $Al_2O_3-Y_2O_3$ system as sintering additives in order to low sintering temperature. The starting powder was high purity ${\beta}-SiC$ nano-powder with an average particle size of 30 nm. Monolithic LPS-SiC was evaluated in terms of sintering density, micro-structure, flexural strength, elastic modulus and so on. Sintered density, flexural strength and elastic modulus of fabricated LPS-SiC increased with increasing the sintering temperature. In the micro-structure of this specimen, it was found that grain of sintered body was grown from 30 nm to 200 nm.

  • PDF

진공 증착법으로 제작한 PVDF 박막의 유전 특성과 전기전도도에 대한 연구 (A Study on the Dielectric Properties and Electrical Conduction of PVDF Thin Films by Physical Vapor Deposition)

  • 강성준;이원재;장동훈;윤영섭
    • 대한전자공학회논문지SD
    • /
    • 제37권5호
    • /
    • pp.9-15
    • /
    • 2000
  • 본 논문에서는 진공 증착법 (Physical Vapor Deposition) 과 전계인가를 통해 두께 3㎛ 의 PVDF (polyvinylidene fluoride) 박막을 제작하여 적외선 흡수분석과 유전특성 및 전기전도 현상을 조사하였다. 진공 증착법으로 제작한 PVDF 박막을 적외선 흡수 분광기 (FT-IR) 로 분석한 결과, 509.45 [cm/sup -1/] 와 1273.6 [cm/sup -1/]의 특성피크가 검출되는 것으로 보아 제작된 PVDF 박막이 β형임을 확인할 수 있었다. β형 PVDF 박막의 유전특성을 측정한 결과, 비유전률은 주파수가 증가함에 따라 지속적으로 감소하는 이상분산을 나타내었고 유전손실은 온도의 증가에 따라 200㎐ 에서 7000㎐ 로 유전 흡수점이 이동함을 관찰할수 있었는데, 이는 디바이 이론과 일치하는 것이었다. 유전손실의 온도 의존성으로부터 구한 활성화 에너지(ΔH) 는 21.64㎉/mo1e 로 조사되었다. β형 PVDF 박막의 누설전류밀도에 대한 온도의존성과 전계의존성을 조사하여 PVDF 박막의 전기전도기구가 이온전도임을 확인할 수 있었다.

  • PDF

Influence of Reproductive Status, Serum Type and Estradiol-17β Supplementation on the in vitro Maturation of Canine Oocytes

  • Heru, Fibrianto Yuda;Kim, Min-Kyu
    • 농업과학연구
    • /
    • 제35권2호
    • /
    • pp.167-176
    • /
    • 2008
  • Supplementation of serum and estrogen in in vitro maturation(IVM) medium was shown to improve embryo development and quality in several species. This study investigates the effect of ovarian estrus stage on canine oocyte quality and supplementation of medium with canine serum or estrogen on IVM of canine oocytes. As results, in experimental 1, IVM oocytes collected from follicular stage ovaries to MII stages($10.2{\pm}1.5%$) was higher (p<0.05) with 10% canine estrus stage serum than control($1.3{\pm}1.6%$), anoestrus stage serum($4.0{\pm}1.6%$), luteal stage serum($2.7{\pm}1.7%$) and 10% FBS($1.3{\pm}1.6$). In experimental 2, 10% canine estrus stage serum supplementation has highest maturation rate to MII stages($10.0{\pm}1.8%$) and there were significant differences(P<0.05) with another treatment in follicular stages group. In order to investigate the synergic effect of estrous serum and estrogen supplementation, different estrous stage groups of oocytes were cultured with 2 ug/ml estrogen plus various concentrations of different reproductive stage serum and FBS(experimental 3). As results, the rate of maturation to metaphase II(MII) stage was significantly higher(p<0.05) in oocytes from the follicular stage supplemented with estrogen and 10% canine estrus stage serum(11.5%) compared to the other groups(6.0 - 8.8%). The present study was demonstrated that canine serum and the estrus cycle of the bitch affect the meiotic competence of oocytes. Hormonal influences within the follicle may be one of the factors responsible for the greater proportion of maturation of oocyte to MII from bitches at the follicular phase.

  • PDF

Ti-30Ta-xZr 합금의 표면에 TiN/Ti 다층막코팅효과 (Effects of TiN/Ti Multilayer Coating on the Ti-30Ta-xZr Alloy Surface)

  • 김영운;정용훈;조주영;최한철;방몽숙
    • 한국표면공학회지
    • /
    • 제42권4호
    • /
    • pp.161-168
    • /
    • 2009
  • Effects of TiN/Ti multilayer coating on the Ti-30Ta-xZr alloy surface were studied by using various experiments. The Ti-30Ta containing Zr (5, 10 and 15 wt%) were melted 10 times to improve chemical homogeneity by using a vacuum furnace. And then samples were homogenized for 24 hrs at $1000^{\circ}C$. The specimens were prepared for TiN/Ti coating by cutting and polishing. The prepared specimens were coated with TiN/Ti multilayers by using DC magnetron sputtering method. The analyses of coated surface and coated layer were carried out by field emission scanning electron microscope(FE-SEM), EDX, and X-ray diffractometer(XRD). From the microstructure and XRD analysis of Ti-30Ta-xZr alloys, The equiaxed structure was changed to needle-like structure with increasing Zr content. And $\alpha$-peak and elastic modulus increased as Zr content increased. The $\alpha$ and $\beta$ phase predominantly were found in the specimen containing high Zr content. According to the analysis of TiN/Ti coating layer, the surface defects and structures of Ti-30Ta-xZr were covered with TiN/Ti coating layer and surface roughness decreased.

Effect of vitamin C on azoxymethane (AOM)/dextran sulfate sodium (DSS)-induced colitis-associated early colon cancer in mice

  • Jeon, Hee-Jin;Yeom, Yiseul;Kim, Yoo-Sun;Kim, Eunju;Shin, Jae-Ho;Seok, Pu Reum;Woo, Moon Jea;Kim, Yuri
    • Nutrition Research and Practice
    • /
    • 제12권2호
    • /
    • pp.101-109
    • /
    • 2018
  • BACKGROUD/OBJECTIVES: The objective of this study was to investigate the effects of vitamin C on inflammation, tumor development, and dysbiosis of intestinal microbiota in an azoxymethane (AOM)/dextran sulfate sodium (DSS)-induced inflammation-associated early colon cancer mouse model. MATERIALS/METHODS: Male BALB/c mice were injected intraperitoneally with AOM [10 mg/kg body weight (b.w)] and given two 7-d cycles of 2% DSS drinking water with a 14 d inter-cycle interval. Vitamin C (60 mg/kg b.w. and 120 mg/kg b.w.) was supplemented by gavage for 5 weeks starting 2 d after the AOM injection. RESULTS: The vitamin C treatment suppressed inflammatory morbidity, as reflected by disease activity index (DAI) in recovery phase and inhibited shortening of the colon, and reduced histological damage. In addition, vitamin C supplementation suppressed mRNA levels of pro-inflammatory mediators and cytokines, including cyclooxygenase-2, microsomal prostaglandin E synthase-2, tumor necrosis $factor-{\alpha}$, Interleukin $(IL)-1{\beta}$, and IL-6, and reduced expression of the proliferation marker, proliferating cell nuclear antigen, compared to observations of AOM/DSS animals. Although the microbial composition did not differ significantly between the groups, administration of vitamin C improved the level of inflammation-related Lactococcus and JQ084893 to control levels. CONCLUSION: Vitamin C treatment provided moderate suppression of inflammation, proliferation, and certain inflammation-related dysbiosis in a murine model of colitis associated-early colon cancer. These findings support that vitamin C supplementation can benefit colonic health. Long-term clinical studies with various doses of vitamin C are warranted.

Effects of glutathione s-transferase (GST) M1 and T1 polymorphisms on antioxidant vitamins and oxidative stress-related parameters in Korean subclinical hypertensive subjects after kale juice (Brassica oleracea acephala) supplementation

  • Lee, Hye-Jin;Han, Jeong-Hwa;Park, Yoo Kyoung;Kang, Myung-Hee
    • Nutrition Research and Practice
    • /
    • 제12권2호
    • /
    • pp.118-128
    • /
    • 2018
  • BACKGROUND/OBJECTIVES: Glutathione s-transferase (GST) is involved in the formation of a multigene family comprising phase II detoxification enzymes, involved in the detoxification of reactive oxygen species. This study evaluated whether daily supplementation with kale juice could modulate levels of plasma antioxidant vitamins and oxidative stress-related parameters. We further examined whether this modulation was affected by combined GSTM1 and T1 polymorphisms. SUBJECTS/METHODS: Totally, 84 subclinical hypertensive patients having systolic blood pressure (BP) over 130 mmHg or diastolic BP over 85 mmHg, received 300 mL of kale juice daily for 6 weeks. Blood samples were drawn before start of study and after completion of 6 weeks. RESULTS: After supplementation, we observed significant decrease in DNA damage and increase in erythrocyte catalase activity in all genotypes. Plasma level of vitamin C was significantly increased in the wild/null and double null genotypes. The plasma levels of ${\beta}-carotene$, erythrocyte glutathione peroxidase activity, and nitric oxide were increased only in the wild/null genotype after kale juice supplementation. CONCLUSIONS: The effect of kale juice was significantly greater in the GSTM1 null genotype and wild/null genotype groups, suggesting possibility of personalized nutritional prescriptions based on personal genetics.

자기 통전식 SiC세라믹 발열체 개발을 위한 기초 특성 연구 (Study of Basic Properties to Develope SiC Ceramic Heater by Self-Charge with Electricity)

  • 신용덕;고태헌;주진영
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2007년도 Techno-Fair 및 추계학술대회 논문집 전기물성,응용부문
    • /
    • pp.124-125
    • /
    • 2007
  • The composites were fabricated $\beta$-SiC and $TiB_2$ powders with the liquid forming additives of 8, 12, 16[wt%] $Al_2O_3+Y_2O_3$ as a sintering aid by pressureless annealing at $1,650[^{\circ}C]$ for 4 hours. Reactions between SiC and transition metal $TiB_2$ were not observed in the microstructure and the phase analysis of the pressureless annealed SiC-$TiB_2$ electroconductive ceramic composites. The relative density, the flexural strength, the Young's modulus and the Vicker's hardness showed the highest value of 82.29[%], 189.5[MPa], 54.60 [GPa] and 2.84[GPa] for SiC-$TiB_2$ composites added with 16[wt%] $Al_2O_3+Y_2O_3$ additives at room temperature. The relative density of SiC-$TiB_2$ composites was lowered due to gaseous products of the result of reaction between SiC and $Al_2O_3+Y_2O_3$. The electrical resistivity showed the lowest value of 0.012[${\Omega}{\cdot}cm$] for 16[wt%] at 25[$^{\circ}C$]. The electrical resistivity was all negative temperature coefficient resistance (NTCR) in the temperature ranges from 25[$^{\circ}C$] to 700[$^{\circ}C$].

  • PDF

$Ag_2-Li_2O-CaO-TiO_2-P_2O_5$계의 다공성 글라스 세라믹스의 항균 특성 (Antibacterial Properties of $Ag_2-Li_2O-CaO-TiO_2-P_2O_5$Porous Class Ceramics)

  • 강원호;윤영진;이용수;홍범수;염곤;김창수;석만균
    • 한국산학기술학회논문지
    • /
    • 제1권1호
    • /
    • pp.27-32
    • /
    • 2000
  • 인산염계 Ag₂OㆍLi₂OㆍCaOㆍTiO₂ㆍP₂O/sub 5/ 조성에 CuO를 0.05∼l.5 mole 첨가하여 다공성 글래스 세라믹스를 제조하였으며. 제조된 모유리는 최적 핵형성을 위해 610℃. 최고 결정성장을 위해 840℃에서 열처리하였다. 1N-HC1에서 β-Ca₃(PO₄)결정상만을 선택적으로 용출하였으며 LiTi₂(PO₄)₃상과 AgTi₂(PO₄)₃결정상이 존재하는 Glass Ceramics를 제조하였다. 다공성 글래스 세라믹스의 항균효과 및 특성을 평가하였다. Staphylococcus aureus와 Salmonella typhi 균이 본 연구에 사용되었으며, 탁월한 항균효과를 나타내는 것으로 평가되었다.

  • PDF

천이금속에 따른 SiC계 복합체의 전기적 특성 (Electrical Properties of SiC Composites by Transition Metal)

  • 신용덕;서재호;주진영;고태헌;김영백
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2007년도 제38회 하계학술대회
    • /
    • pp.1303-1304
    • /
    • 2007
  • The composites were fabricated, respectively, using 61[vol.%]SiC-39[vol.%]$TiB_2$ and using 61[vol.%]SiC-39[vol.%]$ZrB_2$ powders with the liquid forming additives of 12[wt%] $Al_{2}O_{3}+Y_{2}O_{3}$ by hot pressing annealing at $1650[^{\circ}C]$ for 4 hours. Reactions between SiC and transition metal $TiB_2$, $ZrB_2$ were not observed in this microstructure. ${\beta}{\rightarrow}{\alpha}$-SiC phase transformation was occurred on the SiC-$TiB_2$ and SiC-$ZrB_2$ composite. The relative density, the flexural strength and Young's modulus showed the highest value of 98.57[%], 226.06[Mpa] and 86.38[Gpa] in SiC-$ZrB_2$ composite at room temperature respectively. The electrical resistivity showed the lowest value of $7.96{\times}10^{-4}[{\Omega}{\cdot}cm]$ for SiC-$ZrB_2$ composite at $25[^{\circ}C]$. The electrical resistivity of the SiC-$TiB_2$ and SiC-$ZrB_2$ composite was all positive temperature coefficient resistance (PTCR) in the temperature ranges from $25[^{\circ}C]$ to $700[^{\circ}C]$. The resistance temperature coefficient of composite showed the value of $6.88{\times}10^{-3}/[^{\circ}C]$ and $3.57{\times}10^{-3}/[^{\circ}C]$ for SiC-$ZrB_2$ and SiC-$TiB_2$ composite in the temperature ranges from $25[^{\circ}C]$ to $700[^{\circ}C]$.

  • PDF